JIS G4312 SUH310 Heat Resistant Steel Plate
What is JIS G4312 SUH310 Heat Resistant Steel Plate?
Equivalent grades: SUH310 ≈ UNS S31000 ≈ EN 1.4845 X8CrNi25-21 (nearest) ≈ GB/T 20Cr25Ni20 (S31020).
SUH310 is a heat-resistant grade. SUH310 is the JIS 25Cr-20Ni heat-resisting grade with up to 0.20 % carbon. It resists oxidation up to about 1100 °C and is used for highly loaded furnace parts.
JIS G 4312 is the Japanese Industrial Standard for heat-resisting steel plate, sheet and strip. It includes the SUH heat-resisting grades and several SUS grades that are also used at temperature. Plate is hot rolled and supplied solution treated or annealed and pickled.
This page sets out the JIS G 4312 requirements for SUH310 plate: specification summary, chemistry, mechanical properties, high-temperature behaviour, heat treatment, finishes and tolerances, current stock, equivalents, fabrication and testing. SHH STEEL supplies it mill-direct from China with EN 10204 3.1 certificates, optional third-party inspection and in-house cutting.
SUH310 plate: specification summary
| Item | SUH310 data |
|---|---|
| Standard | JIS G 4312, heat-resisting steel plate, sheet and strip |
| Product forms | hot-rolled plate (No.1) and cold-rolled sheet and strip (2D, 2B) |
| Typical thickness | 3–50 mm hot rolled; 0.5–6 mm cold rolled |
| Widths | 1219, 1500, 2000 mm |
| Lengths | 2438, 3048, 6000 mm or cut to size |
| Heat treatment | solution treated (austenitic) or annealed (ferritic) |
| Tests | chemical analysis, tensile, hardness |
| Certificates | mill certificate; EN 10204 3.1 / 3.2 on request |
| Grade family | heat-resistant |
Size range. Plate is produced on Steckel or reversing mills from about 5 mm up to 80–100 mm depending on grade, with widths of 1500–2500 mm and lengths up to 12 m; thinner plate of 3–12 mm is often cut from hot-rolled coil. Very heavy or wide plates, and plates with tight flatness, should be confirmed before ordering. SUH310 is a specialty grade made by a limited number of mills in campaign rolling. Stock covers the common sizes listed below; for project quantities or unusual sizes, plan for a mill campaign and reserve the heat early.
Chemical composition of SUH310 (JIS G 4312)
| Element | wt % |
|---|---|
| C | 0.20 max |
| Si | 1.50 max |
| Mn | 2.00 max |
| P | 0.040 max |
| S | 0.030 max |
| Cr | 24.00–26.00 |
| Ni | 19.00–22.00 |
Single values are maximums unless marked min. Ranges are heat (cast) analysis limits.
For heat-resistant grades the key elements are chromium (oxide scale), nickel (austenite stability, carburisation resistance) and silicon, aluminium or rare earths where present (scale adhesion). Sulfur and phosphorus are kept low to protect hot ductility and weldability.
Mechanical properties of SUH310 plate
| 0.2 % proof stress min, N/mm² | Tensile strength min, N/mm² | Elongation min, % | Hardness max, HBW |
|---|---|---|---|
| 205 | 590 | 35 | 201 |
The minimum proof strength is 205 MPa. For high-temperature design, room-temperature values are only an acceptance check; use creep and stress-rupture data from the standard’s informative annexes or the ASME allowable stresses where Code rules apply. Tension tests are taken in the direction stated in the standard; where a hardness limit is given, it is a maximum that confirms correct annealing.
High-temperature behaviour of SUH310
This is a heat-resistant grade: it is selected for oxidation resistance, strength and structural stability at high temperature rather than for wet corrosion. Chromium forms the protective oxide, nickel stabilises the austenite against thermal cycling and carburisation, and silicon, rare earths or nitrogen, where present, improve scale adhesion or creep strength. The maximum useful temperature in air depends on atmosphere, thermal cycling and load, so published scaling temperatures are a guide, not a design value.
Sulfur-bearing gases attack high-nickel alloys, while carburising or nitriding atmospheres favour higher nickel; vanadium-bearing ash and molten salts need special evaluation. Long exposure in the 600–900 °C range can form sigma phase in high-chromium grades and reduce room-temperature toughness, which matters for parts that are cleaned or repaired cold. Creep-rupture values are given in the standard’s informative annexes or by the mill and should be used for design instead of room-temperature strength.
How SUH310 compares with related grades
| Grade | Cr | Ni | Mo | N | PREN (min) | YS / Rp0.2 min, MPa |
|---|---|---|---|---|---|---|
| SUH310 | 24.00–26.00 | 19.00–22.00 | — | — | — | 205 |
| UNS S30815 | 20.0–22.0 | 10.0–12.0 | — | 0.14–0.20 | — | 310 |
| UNS S30900 | 22.0–24.0 | 12.0–15.0 | — | — | — | 205 |
| UNS S31000 | 24.0–26.0 | 19.0–22.0 | — | — | — | 205 |
| UNS N08330 | 17.0–20.0 | 34.0–37.0 | — | — | — | 205 |
Choose SUH310 when oxidation resistance and strength at temperature drive the selection. For wet corrosion at room temperature, a low-carbon corrosion-resistant grade is usually a better choice, and in sulfur-rich gases a lower-nickel grade may outperform a high-nickel one.
The table uses specification limits, not typical mill values, so it shows the guaranteed position of each grade. Final selection should also consider product availability in the thickness you need, welding consumables, and the inspection requirements of your project.
Heat treatment and delivery condition of SUH310
Heat treatment: 1030–1180 °C, rapid cooling.
Heat-resistant plate is supplied solution annealed. For high-temperature service, a coarser grain size improves creep strength, while a finer grain improves fatigue and room-temperature ductility; where it matters, state the grain-size requirement on the order. Stress relief is not normally needed.
Surface finishes for SUH310 plate
Hot-rolled plate to JIS G4312 is supplied with a No.1 finish; cold-rolled sheet as 2D or 2B. Heat-resistant parts are rarely polished, but bright annealed thin sheet is possible for some ferritic grades.
Dimensions, tolerances and flatness
Dimensional tolerances follow JIS G 4312, which refers to the same tolerance tables used for JIS G4304/G4305 stainless plate and sheet. State the tolerance class and flatness requirement on the order.
JIS ordering practice. A JIS G4312 order gives the grade symbol, the product type (hot-rolled or cold-rolled), the dimensions, the finish and the tolerance requirements. Mill inspection certificates to JIS G 0415 are normal; EN 10204 3.1 or 3.2 certificates can be issued for export. Since many furnace projects in Asia are designed to JIS, while plate is bought from Chinese mills, buyers often ask for dual certification to JIS G4312 and GB/T 4238 or ASTM A240 where the limits overlap.
SUH310 plate stock in China
| Thickness (mm) | Width (mm) | Length (mm) | Finish | Approx. quantity | Location |
|---|---|---|---|---|---|
| 6 | 1500 / 2000 | 6000 | No.1 | 100+ t | China |
| 8 | 1500 / 2000 | 6000 | No.1 | 100+ t | China |
| 10 | 2000 | 6000 | No.1 | 100+ t | China |
| 12 | 2000 | 6000 | No.1 | 100+ t | China |
| 16 | 2000 / 2500 | 6000 | No.1 | 100+ t | China |
| 20 | 2000 / 2500 | 6000 / 8000 | No.1 | 100+ t | China |
| 30 | 2000 / 2500 | 6000 | No.1 | 100+ t | China |
Quantities are approximate and stock changes daily. Send your size list for current availability; other thicknesses, widths and cut sizes can be supplied from mill production.
Packing and logistics. Plate is bundled on steel or wooden skids with steel bands and edge protection, typically 3–8 t per bundle, and marked with heat and plate numbers. Cut pieces are crated. Heavy and wide plate ships in open-top or flat-rack containers or by break-bulk; we send loading photos with the shipping documents.
SUH310 equivalents in other standards
| Standard | Designation | Comment |
|---|---|---|
| ASTM / UNS | UNS S31000 | same alloy family and limits closely matched; compare each limit on the certificate |
| EN | 1.4845 X8CrNi25-21 | nearest grade only; limits differ, check before substituting |
| GB/T | 20Cr25Ni20 (S31020) | same alloy family and limits closely matched; compare each limit on the certificate |
Equivalents are close, not identical. When a project names one standard, order to that standard or ask for multiple certification and check every limit on the certificate.
Related grades by alloy family
Same standard
Other grades in this standard: SUS309S (G4304), SUS310S (G4304), SUS430 (G4304), SUS409L (G4305), SUH309, SUH330, SUH409L.
Heat-resistant
Heat-resistant grades ranked by chromium, nickel and silicon: A240 S30908, A240 S31008, A240 S30909, A240 S31009, 1.4948 (EN 10028-7).
Applications, forming and welding of SUH310
Typical uses: furnace muffles, radiant tubes, burner nozzles, and heat-treatment equipment.
Heat-resistant plate is usually cut by plasma or waterjet, formed hot or cold, and welded with matching heat-resistant consumables. Cut by plasma, laser or waterjet and remove heat tint by pickling or grinding. For welding use a matching heat-resistant filler such as ER309, ER310 or ERNiCr-3 according to the service temperature. Keep the weld area clean and free of carbon-steel contamination, and pickle and passivate after welding where corrosion resistance matters.
Fabrication at temperature. Design furnace parts to allow for thermal expansion, which is about 1.5 times that of carbon steel, and avoid sharp corners where scale can spall. Welds should be full penetration where they carry load at temperature. For high-silicon grades, use low heat input to limit hot cracking. After long service, high-chromium plate may be embrittled by sigma phase, so repair welding of old parts needs care and sometimes a solution anneal first.
Certificates, testing and receiving inspection
Every delivery carries a mill certificate to JIS G4312 with heat analysis, tensile results and hardness, and the grade and standard as ordered. Supplementary tests we can arrange: PMI, grain-size measurement (ASTM E112) where the grade requires it, elevated-temperature tensile tests by agreement, and ultrasonic testing of heavy plate. Third-party witness by SGS, BV, TÜV, DNV, ABS or LR is available with EN 10204 3.2 certificates.
On receipt, check marking and heat number against the certificate, measure thickness at several points and confirm the finish and edge condition before cutting.
Common mistakes when specifying SUH310
- Selecting by room-temperature strength instead of creep data.
- Substituting a low-carbon corrosion grade (for example 310S for 310) without checking creep strength.
- Ignoring the atmosphere: sulfur, carburising gas and vanadium ash change the ranking of grades.
Each of these can be avoided by writing the requirement into the purchase order and checking it on the certificate before the material is cut.
Sourcing SUH310: buyer concerns and SHH STEEL solutions
| Concern | How SHH STEEL handles it |
|---|---|
| Wrong grade substitution (for example 304 for 309/310) | PMI of every plate before dispatch |
| Distortion of large furnace panels | levelled plate and cut-to-size blanks with low-stress cutting |
| Small quantities across many sizes | mixed thicknesses and grades combined in one shipment |
| Cutting and edge preparation | in-house shearing, plasma, laser and waterjet cutting, bevelling |
| Delivery delays | weekly production and shipping updates with photos |
How to order SUH310 plate
State the standard and edition (JIS G 4312), the grade (SUH310), thickness, width and length or coil, finish, quantity, tolerance class, any added chemistry limits, the supplementary tests and acceptance values from your specification, the certificate type and inspection agency, and packing. Send the list to SHH STEEL and we will reply with price, available stock and lead time.
FAQ
-
Is SUH310 the same as SUS309S/SUS310S?
- No. The SUH grades in JIS G4312 are heat-resisting grades, typically with higher carbon for strength at temperature; the SUS grades are corrosion-resistant grades with lower carbon. Choose by service temperature and welding needs.
-
Is SUH310 equivalent to UNS S31000?
- They are the same alloy designation in different standards. Limits are closely matched, but always order to the standard named in your specification or ask for multiple certification.
-
What is the maximum service temperature of SUH310?
- It depends on the atmosphere, thermal cycling and load. Published scaling temperatures are a guide for oxidation in air only; for load-bearing parts use creep-rupture data.
-
Can I order small quantities or cut sizes?
- Yes. We combine mixed thicknesses and grades into one shipment and cut plate and sheet to size in our workshop.
-
Which certificates and tests can you provide?
- Every order ships with a mill certificate (EN 10204 3.1 type) showing heat analysis and mechanical tests. Supplementary tests and 3.2 certificates with SGS, BV, TÜV or another agency are available by agreement.
Conclusion
SUH310 plate should be ordered with the points the standard leaves open written into the contract: finish, tolerance class, any extra chemistry limits and the supplementary tests your application needs. With those fixed, stock material from China is a fast and reliable route.