JIS G3459 SUS347TP Stainless Steel Pipe | JIS G3459 Stainless Steel Pipe - SHH STEEL

JIS G3459 SUS347TP Stainless Steel Pipe

JIS G3459 SUS347TP stainless steel pipe (347 / UNS S34700), austenitic, Table 3 cast analysis, Rm min 520 N/mm² / proof min 205 N/mm², solution annealed. SHH STEEL can produce and supply seamless or welded routes with mill certificates.
Grade
SUS347TP (347 / UNS S34700 — body alias)
Standard
JIS G3459:2021
Product form
Seamless and welded stainless steel pipe, delivery solution annealed
Size
Typically OD 10.5–660.4 mm (6A–650A); schedule or measured wall by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Pipe Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is JIS G3459 SUS347TP Stainless Steel Pipe

Piping packages that cite Japanese product standards look to JIS G3459:2021 — Stainless steel pipes — rather than inventing a mill grade from AISI shorthand alone. SUS347TP is the Table 1 symbol for this austenitic chemistry. Pick SUS347TP under JIS G3459 when the welding procedure and corrosion file already assume niobium stabilisation.

Mill path for SUS347TP: Table 1 process/finish symbols, Table 2 heat treatment, Table 3 cast chemistry, Table 4 tensile floors. SHH STEEL can make and supply the grade to that stack with hydrostatic or NDT acceptance as ordered. Typical use: refinery and chemical welded lines, high-temperature steam piping, and duties preferring Nb over Ti stabilisation.

Body text may mention 347 / UNS S34700 for cross-reference, but the H1 and order line stay on SUS347TP. Silent alias swaps are how wrong carbon ceilings and wrong tensile tables enter the MTC. Keep this caution in view: optional stabilisation HT 850–930 °C; Nb-bearing fillers required — 308 alone is the wrong habit.

Order the standard the drawing and regulatory file actually require. Inside this G3459 series, compare SUS347HTP, SUS321TP, SUS304LTP, SUS316TiTP before stretching surface finish or schedule alone. Duty thread: Nb-stabilised 18-8 austenitic pipe for weld-zone IGC control as the niobium twin to 321. Document the medium, design temperature, and weld map beside the SUS347TP line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Corrosion framing beside SUS347TP: Nb ties carbon in the HAZ; chloride pitting still tracks Mo-free 18-8.

Inside this JIS G3459 series, compare SUS347HTP, SUS321TP, SUS304LTP, SUS316TiTP. Hub: JIS G3459. ASTM/ASME related product pages (not interchangeable by default): A312 TP347.

Chemical Composition of JIS G3459 SUS347TP

Table 3 sets the melt limits for SUS347TP. Highlight band: C ≤0.08, Si ≤1.00, Mn ≤2.00, P ≤0.045, S ≤0.030, Ni 9.00–13.00, Cr 17.00–19.00. Product analysis, when ordered, applies JIS G 0321 stainless product tolerances on top of Table 3. Alias note: 347 / UNS S34700. Every ladle analysis for SUS347TP is checked against those windows before the heat is released to piercing, welding, or finishing, and the same numbers reappear on the inspection document. Application context for SUS347TP stays refinery and chemical welded lines, high-temperature steam piping, and duties preferring Nb over Ti stabilisation.

The composition table below is the cast window SHH STEEL quotes against for SUS347TP. Edition framing is JIS G3459:2021. Use thread: refinery and chemical welded lines, high-temperature steam piping, and duties preferring Nb over Ti stabilisation. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 3, SHH STEEL will confirm melt feasibility for SUS347TP before the order is acknowledged. Size practice for SUS347TP remains seamless process pipe common; welded routes with Nb-matched procedures.

Grade C Si Mn P S Ni Cr Nb
SUS347TP ≤0.08 ≤1.00 ≤2.00 ≤0.045 ≤0.030 9.00–13.00 17.00–19.00 ≥10×C%

Mechanical Properties of JIS G3459 SUS347TP

Table 4 mechanical acceptance for SUS347TP: Rm min 520 N/mm², proof stress min 205 N/mm², elongation (No.11/12 longitudinal) min 35%. Elongation rules change for walls under 8 mm and are not mandatory below 40 mm OD (record only unless agreed). Delivery framing: solution annealed. Tensile sampling follows clause 13 for the ordered test unit of SUS347TP, and retests follow clause 14 when a result sits under the Table 4 floor. This paragraph is locked to SUS347TP duty: Nb-stabilised 18-8 austenitic pipe for weld-zone IGC control as the niobium twin to 321.

Grade Rm min (N/mm²) Proof stress min (N/mm²) A No.11/12 long. min (%) A No.5 trans. min (%) A No.4 long. min (%) A No.4 trans. min (%)
SUS347TP 520 205 35 25 30 22

Ambient values from JIS G3459:2021 Table 4 for SUS347TP. Heat treatment (Table 2): 980 °C min, rapid cool (stabilisation 850–930 °C may be ordered). Elongation reductions apply for walls under 8 mm; elongation is not mandatory below 40 mm OD (record unless agreed). Note: hot-finished SUS321TP / SUS321HTP may use 460 / 180 N/mm² by agreement.

Manufacture of JIS G3459 SUS347TP Pipe (Seamless and Welded)

SHH STEEL can produce SUS347TP as seamless S or as A/L/E welded pipe, then heat-treat and pickle (or bright-anneal) per Table 2. Bevel ends are available by agreement; plain ends are the default when the PO is silent. Seamless and welded options remain available for SUS347TP; the acknowledgement repeats the Table 1 symbols so production cannot silently change route after the PO is firm. Size practice for SUS347TP remains seamless process pipe common; welded routes with Nb-matched procedures.

After forming, SUS347TP receives Table 2 treatment — 980 °C min, rapid cool (stabilisation 850–930 °C may be ordered). Austenitic heats take solution annealing with rapid cooling; hot-finished seamless may omit separate solution treatment when hot-worked and rapidly cooled in-line under the Table 2 note, unless the purchaser forbids it. Use thread: refinery and chemical welded lines, high-temperature steam piping, and duties preferring Nb over Ti stabilisation.

Marking carries the grade symbol SUS347TP, process/finish marks, manufacturer ID, and other clause-15 items. Size hint: seamless process pipe common; welded routes with Nb-matched procedures. Weld thread: 347 fillers; control heat input; consider stabilisation after severe cold work. Hydrostatic pressure or NDT class for SUS347TP is frozen with the size list so quality planners can book the correct benches before the pipe is cut to length. This paragraph is locked to SUS347TP duty: Nb-stabilised 18-8 austenitic pipe for weld-zone IGC control as the niobium twin to 321.

Dimensions and Tolerances for JIS G3459 SUS347TP

Dimensional order lines for SUS347TP should state OD × wall (or schedule 5S/10S/20S/40/80/…), length type, and end finish. Tolerances follow clause 10 by process route. Use: refinery and chemical welded lines, high-temperature steam piping, and duties preferring Nb over Ti stabilisation. Tolerance class follows the process route ordered for SUS347TP, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Application context for SUS347TP stays refinery and chemical welded lines, high-temperature steam piping, and duties preferring Nb over Ti stabilisation.

OD and wall tolerances differ for hot-finished seamless versus cold-finished / welded routes — quote the process symbol with the size. Caution: optional stabilisation HT 850–930 °C; Nb-bearing fillers required — 308 alone is the wrong habit. Fixed lengths and multiple cut lengths for SUS347TP are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Keep the SUS347TP caution visible here: optional stabilisation HT 850–930 °C; Nb-bearing fillers required — 308 alone is the wrong habit.

Equivalent Grades for JIS G3459 SUS347TP

SUS347TP is the JIS G3459 designation. Alias 347 / UNS S34700 appears only as a cross-walk. Compare sisters SUS347HTP, SUS321TP, SUS304LTP, SUS316TiTP when the medium or temperature outgrows this mark. Hook: lock SUS347TP on the PO. When a dual-cert path is required, list both JIS G3459 SUS347TP and the ASTM mark with separate test scopes instead of assuming one chemistry line clears both files. This paragraph is locked to SUS347TP duty: Nb-stabilised 18-8 austenitic pipe for weld-zone IGC control as the niobium twin to 321.

Heat Treatment and Delivery Condition for JIS G3459 SUS347TP

Mill heat treatment for SUS347TP: 980 °C min, rapid cool (stabilisation 850–930 °C may be ordered). Bright annealing may omit pickling when the surface is scale-free. Delivery label: solution annealed. Recorded furnace charts for SUS347TP should support the Table 2 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Corrosion framing beside SUS347TP: Nb ties carbon in the HAZ; chloride pitting still tracks Mo-free 18-8.

Certificate wording for SUS347TP should show the heat-treatment condition actually performed, not a generic “annealed” stamp that hides temperature. Use: refinery and chemical welded lines, high-temperature steam piping, and duties preferring Nb over Ti stabilisation. Field heat treatment of SUS347TP after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Size practice for SUS347TP remains seamless process pipe common; welded routes with Nb-matched procedures.

Corrosion Resistance of JIS G3459 SUS347TP

Nb ties carbon in the HAZ; chloride pitting still tracks Mo-free 18-8 Special quality annex tests are available by agreement; they are not a blanket warranty for every process medium. Family filing: austenitic. Coupon orientation, weld condition, and surface finish for SUS347TP belong in the corrosion test order so annex results can be compared to the installed spool honestly. This paragraph is locked to SUS347TP duty: Nb-stabilised 18-8 austenitic pipe for weld-zone IGC control as the niobium twin to 321.

Do not market invented PREN digits. Bring medium chemistry and SHH STEEL will map SUS347TP honestly against SUS347HTP, SUS321TP, SUS304LTP, SUS316TiTP. Role: Nb-stabilised 18-8 austenitic pipe for weld-zone IGC control as the niobium twin to 321. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for SUS347TP rather than relying on schedule thickness alone. Size practice for SUS347TP remains seamless process pipe common; welded routes with Nb-matched procedures.

Applications of JIS G3459 SUS347TP Pipe

Typical BOM language pairs JIS G3459 SUS347TP with OD × wall (or schedule), process/finish symbols, and heat-treatment condition. Primary sketch: refinery and chemical welded lines, high-temperature steam piping, and duties preferring Nb over Ti stabilisation. Spool fabricators should copy SUS347TP onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Weld-shop note tied to SUS347TP: 347 fillers; control heat input; consider stabilisation after severe cold work.

Spell SUS347TP on isometrics, spool sheets and valve specs alike. Sister options when the medium hardens: SUS347HTP, SUS321TP, SUS304LTP, SUS316TiTP. Commissioning teams benefit when the as-built dossier repeats SUS347TP beside heat numbers, linking isometric revisions to the same mill certificates. Weld-shop note tied to SUS347TP: 347 fillers; control heat input; consider stabilisation after severe cold work.

Weldability of JIS G3459 SUS347TP

Weldability of SUS347TP follows austenitic practice. Filler/shop note: 347 fillers; control heat input; consider stabilisation after severe cold work. Caution: optional stabilisation HT 850–930 °C; Nb-bearing fillers required — 308 alone is the wrong habit. Procedure qualification for SUS347TP should use the same product form and wall class as production, including any bead-worked or as-welded finish that will ship. Size practice for SUS347TP remains seamless process pipe common; welded routes with Nb-matched procedures.

For welded G3459 pipe, confirm whether bead working (B) or as-welded ERW (G) finish is acceptable to the corrosion owner. Shop note: 347 fillers; control heat input; consider stabilisation after severe cold work. Consumable lot control and shielding-gas notes for SUS347TP stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Application context for SUS347TP stays refinery and chemical welded lines, high-temperature steam piping, and duties preferring Nb over Ti stabilisation.

Surface Finishes for JIS G3459 SUS347TP

Pickled mill finish covers most piping RFQs for SUS347TP. Bright anneal, grind, or polish only when the enquiry writes a measurable target. Use: refinery and chemical welded lines, high-temperature steam piping, and duties preferring Nb over Ti stabilisation. Roughness or polish callouts for SUS347TP must name OD, ID, or both; ambiguous “bright pipe” language is clarified before finishing slots are booked. Corrosion framing beside SUS347TP: Nb ties carbon in the HAZ; chloride pitting still tracks Mo-free 18-8.

Sanitary-lean duties may add ID polish; chemical lines may prefer a clean pickle only. State the need on the SUS347TP order. Final visual standards for SUS347TP reject grinding burns, embedded free iron, and unrepaired weld undercut before bundles are closed. This paragraph is locked to SUS347TP duty: Nb-stabilised 18-8 austenitic pipe for weld-zone IGC control as the niobium twin to 321.

Inspection and Testing for JIS G3459 SUS347TP

SHH STEEL reports the tests actually performed for SUS347TP — no surrogate NDT lines. Hydrostatic vs eddy-current/ultrasonic choice belongs on the PO. Caution: optional stabilisation HT 850–930 °C; Nb-bearing fillers required — 308 alone is the wrong habit. Sampling plans for SUS347TP keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Corrosion framing beside SUS347TP: Nb ties carbon in the HAZ; chloride pitting still tracks Mo-free 18-8.

NDT sensitivity levels and hydrostatic pressures follow the standard tables unless the purchaser specifies higher. Size context: seamless process pipe common; welded routes with Nb-matched procedures. Non-conforming SUS347TP lengths are segregated and retested or rejected under clause 14 rather than reworked into unmarked stock. This paragraph is locked to SUS347TP duty: Nb-stabilised 18-8 austenitic pipe for weld-zone IGC control as the niobium twin to 321.

Packaging and Shipping for JIS G3459 SUS347TP

Export packing for JIS G3459 SUS347TP is built around rust prevention and transit abrasion control. Bundle tickets repeat the grade symbol and heat number. Duty: Nb-stabilised 18-8 austenitic pipe for weld-zone IGC control as the niobium twin to 321. Bundle tickets for SUS347TP repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Keep the SUS347TP caution visible here: optional stabilisation HT 850–930 °C; Nb-bearing fillers required — 308 alone is the wrong habit.

Marking paint and ink stickers stay chloride-lean. Heat numbers on tags match the MTC for SUS347TP. Desiccant and wrap choices for SUS347TP follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Application context for SUS347TP stays refinery and chemical welded lines, high-temperature steam piping, and duties preferring Nb over Ti stabilisation.

Photographic packing records are available on request for project QA files on SUS347TP. Claims handling for SUS347TP starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Keep the SUS347TP caution visible here: optional stabilisation HT 850–930 °C; Nb-bearing fillers required — 308 alone is the wrong habit.

Why Choose SHH STEEL

Buyers choose SHH STEEL for SUS347TP because the paperwork matches the stencil: Table 3 chemistry, Table 4 tensile, Table 2 heat treatment, and honest S/A/L/E marking. Application fit: refinery and chemical welded lines, high-temperature steam piping, and duties preferring Nb over Ti stabilisation. SHH STEEL can produce and supply SUS347TP against the OD × wall, process symbol, and test scope on your RFQ without swapping in an unstated sister grade.

SHH STEEL will not invent PREN posters or warehouse tonnages. Bring OD × wall, medium notes, and test scope — we will quote SUS347TP cleanly. Ask for a written acknowledgement that names SUS347TP, the Table 1 process/finish marks, and the Table 2 heat-treatment condition before melt. SHH STEEL can make SUS347TP to that written scope.

Supply Capability

Supply capability for SUS347TP covers process/finish symbols in Table 1, heat treatment in Table 2, and mechanical acceptance in Table 4. SHH STEEL can make the sizes on your list when the mill slot fits. Role: Nb-stabilised 18-8 austenitic pipe for weld-zone IGC control as the niobium twin to 321. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for SUS347TP when the mill schedule allows. This paragraph is locked to SUS347TP duty: Nb-stabilised 18-8 austenitic pipe for weld-zone IGC control as the niobium twin to 321.

Item Capability
Standard JIS G3459:2021 stainless steel pipes
Grade symbol SUS347TP
Product form Seamless (S) and welded (A / L / E) pipe; finishes H / C / B / G
Delivery condition solution annealed
Documents Mill test certificate (JIS G 0415 / EN 10204 3.1 style as ordered)
Typical OD practice 10.5–660.4 mm (6A–650A) per standard Note 1; other by agreement
Wall / schedule Schedule 5S–160 class and measured wall within family practice

Stock / Available sizes

Stock / Available sizes for SUS347TP: common A-number bores with schedule or measured wall as the project uses. Seamless and welded availability varies by diameter — confirm route with the RFQ. Hint: seamless process pipe common; welded routes with Nb-matched procedures. SHH STEEL can supply alternate schedules and measured walls for SUS347TP once the design pressure and corrosion allowance are clear.

Mill certificates, packing photos, and third-party witness can be bundled into the SUS347TP supply scope when the PO says so. Use: refinery and chemical welded lines, high-temperature steam piping, and duties preferring Nb over Ti stabilisation. SHH STEEL can produce trial lengths of SUS347TP for procedure qualification before the bulk release when the project calendar needs it.

FAQ

What is JIS G3459 SUS347TP stainless steel pipe used for?
JIS G3459 SUS347TP is stainless pipe for corrosion-resistant, low-temperature, high-temperature and fire-protection piping — refinery and chemical welded lines, high-temperature steam piping, and duties preferring Nb over Ti stabilisation. Role summary: Nb-stabilised 18-8 austenitic pipe for weld-zone IGC control as the niobium twin to 321. It is a Japanese product standard mark, not an automatic ASTM A312 certificate.
Does JIS G3459 SUS347TP cover seamless and welded pipe?
Yes. Table 1 allows seamless (S) and welded automatic-arc (A), laser (L), or electric-resistance (E) routes with finish symbols H/C/B/G. SHH STEEL can produce and supply either route for SUS347TP when the mill can meet the ordered size and tests. The title omits Seamless/Welded because the standard itself covers both — the PO must still name the process symbol.
What heat treatment applies to SUS347TP?
SUS347TP is delivered solution annealed under JIS G3459. Table 2 reference: 980 °C min, rapid cool (stabilisation 850–930 °C may be ordered). Stabilisation or other purchaser options, where allowed, must be written on the order. Certificate wording should match the treatment actually performed.
How does SUS347TP compare with sister grades SUS347HTP, SUS321TP, SUS304LTP?
SUS347TP is filed as austenitic. Typical sisters on the same RFQ are SUS347HTP, SUS321TP, SUS304LTP. Design caution: optional stabilisation HT 850–930 °C; Nb-bearing fillers required — 308 alone is the wrong habit Pick the sister when the medium or strength floor outgrows this symbol rather than stretching schedule alone.
What tests appear on the mill certificate for SUS347TP?
Expect cast analysis (Table 3), room-temperature tensile results (Table 4), dimensions, hydrostatic or NDT as ordered, and every special annex test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow JIS G 0415 or EN 10204 3.1 style when specified.
Is 347 / UNS S34700 the same as ordering SUS347TP?
No. 347 / UNS S34700 is a commercial / UNS cross-walk for body text. The purchase order should lock JIS G3459 and SUS347TP so cast limits, heat treatment, and process symbols are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for JIS G3459 SUS347TP?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for SUS347TP within the typical 10.5–660.4 mm OD practice, with schedules or measured walls by agreement. Size context: seamless process pipe common; welded routes with Nb-matched procedures. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
How should SUS347TP be welded?
Shop guidance: 347 fillers; control heat input; consider stabilisation after severe cold work. Mill heat treatment of seamless or welded pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or anneal practice as applicable. Caution: optional stabilisation HT 850–930 °C; Nb-bearing fillers required — 308 alone is the wrong habit
When should I choose a duplex or higher-Mo grade instead of SUS347TP?
Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: optional stabilisation HT 850–930 °C; Nb-bearing fillers required — 308 alone is the wrong habit Sister pointers: SUS347HTP, SUS321TP, SUS304LTP. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify JIS G3459 SUS347TP with ASTM A312 or A789?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites JIS G3459 SUS347TP does not clear ASTM acceptance by default. State both standards, sizes, and test scopes before melt.
What surface finishes are available for SUS347TP?
Pickled after heat treatment is the usual piping supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for SUS347TP when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.

Conclusion

JIS G3459 SUS347TP is stainless steel pipe for corrosion-resistant, low-temperature, high-temperature and fire-protection piping — Nb-stabilised 18-8 austenitic pipe for weld-zone IGC control as the niobium twin to 321. SHH STEEL can produce and supply it in seamless or welded routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include SUS347HTP, SUS321TP, SUS304LTP. Related ASTM pages share chemistry families but not Japanese acceptance text. Email admin@steelspecs.com with OD × wall, process symbol, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X