JIS G3118 SGV410 Steel Plate | SGV410 Carbon Vessel Plate
What is JIS G3118 SGV410 steel plate?
JIS G3118 SGV410 is a hot-rolled carbon steel plate for pressure vessels for intermediate and moderate temperature service, to JIS G 3118:2024. The standard is written for plates used in pressure vessels operating mainly from moderate to ordinary temperatures. SGV410 has a tensile strength of 410–490 N/mm² and a minimum yield point or proof stress of 225 N/mm².
JIS G 3118:2024 was revised and gazetted on 20 November 2024 and replaced JIS G 3118:2020. It is based on ISO 9328-1:2018 and ISO 9328-2:2018 with technical modifications (MOD). The current edition has three grades only: SGV410, SGV450 and SGV480, applicable from 6 mm to 200 mm thickness. The 2024 revision clarified the heat-treatment designation rules, defined yield point or proof stress, removed the elongation relaxation for plates over 90 mm and added an ordering-information clause.
SHH STEEL produces and exports JIS G3118 SGV410 plate as a producer, exporter and mill agent, to the thickness, heat-treatment symbol and inspection document written on the enquiry. The grade sits in our JIS G3118 range under Nuclear-Grade Steel Plates. The sibling grades are JIS G3118 SGV450, JIS G3118 SGV480.
Material specification for JIS G3118 SGV410
The table summarises the standard items for this grade. Sizes are agreed per order; no stock range is implied.
| Parameter | Detail |
|---|---|
| Standard | JIS G 3118:2024, Carbon steel plates for pressure vessels for intermediate and moderate temperature services |
| Grade | SGV410 |
| Applicable thickness | 6 mm to 200 mm (standard scope) |
| Steelmaking | Fine-grain killed steel |
| Heat treatment | As-rolled up to 38 mm (normalizing optional or on request); normalized over 38 mm; see Delivery Conditions |
| Austenitic grain size | No. 5 or finer |
| General delivery | JIS G 0404; inspection document JIS G 0415 3.1 unless otherwise specified |
| Dimensions | JIS G 3193 with the thickness tolerance of this standard |
| Our supply | We produce and export JIS G3118 SGV410 plate to the order |
Chemical composition of JIS G3118 SGV410
Heat analysis shall meet Table 3 of JIS G 3118:2024; product analysis (Table 4) applies when the purchaser requests it. Carbon limits depend on thickness.
| Thickness, mm | C max, heat % | Si, heat % | Mn, heat % | P max, % | S max, % |
|---|---|---|---|---|---|
| 6 to 12.5 | 0.21 | 0.15–0.40 | 0.85–1.20 | 0.020 | 0.020 |
| over 12.5 to 50 | 0.23 | 0.15–0.40 | 0.85–1.20 | 0.020 | 0.020 |
| over 50 to 100 | 0.25 | 0.15–0.40 | 0.85–1.20 | 0.020 | 0.020 |
| over 100 to 200 | 0.27 | 0.15–0.40 | 0.85–1.20 | 0.020 | 0.020 |
Product analysis: C as above, Si 0.13–0.45 %, Mn 0.80–1.25 %, P and S 0.020 % max. Plates 12.5 mm and under may have Mn 0.60–0.90 %. For each 0.01 % reduction below the carbon maximum, the manganese maximum may be raised by 0.06 %, up to 1.60 %. Alloying elements not listed may be added where necessary and must then be reported.
The carbon-equivalent clause of the standard applies to thermo-mechanically controlled SGV450 and SGV480; it does not set a Ceq limit for SGV410.
Mechanical properties of JIS G3118 SGV410
Tensile and bend properties shall meet Table 7 of JIS G 3118:2024. Test pieces are transverse to the final rolling direction. Unless otherwise specified, the yield point is the upper yield point ReH; where no yield point appears, the 0.2 % proof stress is measured.
| Property | Requirement |
|---|---|
| Yield point or proof stress, min | 225 N/mm² |
| Tensile strength | 410–490 N/mm² |
| Elongation, 6 to 40 mm, No. 1A test piece | 21 % min |
| Elongation, over 40 to 50 mm | 21 % min (No. 1A) or 25 % min (No. 10) |
| Elongation, over 50 to 200 mm, No. 10 test piece | 25 % min |
For No. 1A pieces, elongation is reduced by 1 for each 1 mm under 8 mm thickness, and by 0.5 for each 3 mm over 20 mm, to a maximum reduction of 3.
| Bend test thickness, mm | Inside radius (180°) |
|---|---|
| 6 to 25 | 0.5 × t |
| over 25 to 50 | 0.75 × t |
| over 50 to 100 | 1.0 × t |
| over 100 to 200 | 1.25 × t |
The bend test may be omitted at the manufacturer’s discretion, but the plate must still meet it, and it is performed when the purchaser specifies it. Charpy impact, ultrasonic and sulphur-print tests are not base requirements; they are agreed separately when needed.
Heat treatment and delivery condition of JIS G3118 SGV410
Heat treatment follows Table 2 of JIS G 3118:2024.
| Thickness, mm | Plate heat treatment |
|---|---|
| 6 to 38 | As-rolled; the manufacturer may normalize, and the purchaser may specify normalizing; thermo-mechanical control processing by agreement |
| over 38 to 100 | Normalized |
| over 100 to 200 | Normalized |
By agreement, accelerated cooling after normalizing followed by tempering may be applied. Where the purchaser will carry out a heat treatment in place of normalizing, the plate may be supplied as-rolled or with the treatment the purchaser specifies, and the purchaser states the test-piece heat treatment. Symbols are added after the grade: N (normalized plate), TN (normalized test piece), TMC (thermo-mechanically controlled), SR (test piece given a PWHT-equivalent treatment), for example SGV410N or SGV410NSR.
Welding JIS G3118 SGV410 plate
JIS G3118 SGV410 is a fine-grain killed carbon-manganese steel and is readily weldable with a qualified procedure. Carbon rises with thickness, so preheat should be set for the actual thickness, restraint and consumables.
Where the vessel will be stress relieved, order SR test pieces so the certificate reflects the fabricated condition.
Weld repair of surface defects requires the purchaser’s prior approval.
Dimensions and thickness tolerance
Shape, dimensions and mass follow JIS G 3193, with the thickness tolerance of JIS G 3118:2024 Table 8. The minus tolerance is 0.25 mm; where 0 mm minus is agreed, 0.25 mm is added to the plus tolerance. Widths of 5000 mm and over are by agreement.
| Thickness, mm | Plus tolerance, width under 1600 mm | Plus tolerance, width 2500 to under 3150 mm |
|---|---|---|
| 6.00 to under 6.30 | +0.75 | +1.25 |
| 16.0 to under 25.0 | +1.05 | +1.65 |
| 40.0 to under 63.0 | +1.35 | +1.95 |
| 100 to under 160 | +2.35 | +3.15 |
| 160 to 200 | +2.95 | +3.55 |
Width tolerance is cut-edge tolerance A and length tolerance A of JIS G 3193 unless otherwise specified.
Applications and standard limits
JIS G3118 SGV410 plate is used for boiler drums, pressure vessels, heat-exchanger shells and similar welded pressure equipment working at moderate and intermediate temperatures.
Listing this specification in our JIS G3118 range under the Nuclear-Grade Steel Plates family is a catalogue grouping only. It is not a nuclear qualification, an RCC-M qualification or an ASME Section III certification of SHH STEEL, of the mill or of any heat. Where plate is intended for nuclear construction, the Code edition, material organisation and quality-system rules, fracture-toughness testing and project chemistry limits must be written on the purchase order and confirmed before acceptance.
- Thickness: 6 mm to 200 mm per the standard
- Low-temperature service needs impact testing agreed separately; this standard has no base impact requirement
- Allowable stresses come from the code named on the order
Compare JIS G3118 SGV410 with related plates
Within JIS G3118 the grade is set by tensile strength level. SGV410 must not be replaced by a lower grade, and a higher grade changes carbon limits and welding behaviour. Related JIS plates are written to other standards.
| Grade | Tensile strength, N/mm² | Yield, min, N/mm² | Relation |
|---|---|---|---|
| JIS G3118 SGV410 | 410–490 | 225 | This page |
| JIS G3118 SGV450 | 450–540 | 245 | Same standard, different strength |
| JIS G3118 SGV480 | 480–590 | 265 | Same standard, different strength |
| JIS G3115 SPV410 | Per JIS G3115 | Per JIS G3115 | Higher-yield vessel plate, different standard |
| JIS G3103 SB450 | Per JIS G3103 | Per JIS G3103 | Boiler plate, different standard |
Equivalent and related grades for JIS G3118 SGV410
Equivalents below are engineering judgement only and are not automatic substitutes. Chemistry, heat treatment and test rules differ; any equivalence must be approved by the designer or code authority.
| Region | Grade | Note |
|---|---|---|
| USA | ASTM A516 Grade 60 | Similar tensile class carbon vessel plate; engineering judgement only |
| Europe | EN 10028-2 P265GH | Elevated-temperature carbon vessel plate; different test basis; engineering judgement only |
| Japan | JIS G3103 SB450 | Boiler and pressure vessel plate; different standard; engineering judgement only |
Why choose SHH STEEL for JIS G3118 SGV410
- SHH STEEL produces and exports JIS G3118 SGV410 plate as a producer, exporter and mill agent
- We check carbon by thickness, heat-treatment symbol and Table 7 properties against JIS G 3118:2024
- We state the heat-treatment symbol on the certificate and marking
- We do not present the Nuclear-Grade Steel Plates listing as a nuclear qualification
- We match the inspection document to the order
How to enquire for JIS G3118 SGV410
| Item | What to state |
|---|---|
| Standard | JIS G 3118:2024, SGV410 |
| Heat treatment | Symbol required, for example N, TN, TMC, SR |
| Size | Thickness, width, length and quantity |
| Extra tests | Impact, ultrasonic or other tests by agreement |
| Documentation | JIS G 0415 3.1 by default, or as specified |
Cutting and processing can be added when written on the order.
FAQ
-
What is JIS G3118 SGV410?
- A carbon steel plate for pressure vessels for intermediate and moderate temperature service to JIS G 3118:2024, with 410–490 N/mm² tensile strength and 225 N/mm² minimum yield.
-
What is the current edition?
- JIS G 3118:2024, gazetted on 20 November 2024, replacing JIS G 3118:2020. It has three grades: SGV410, SGV450 and SGV480.
-
How is it heat treated?
- Up to 38 mm as-rolled, with normalizing optional or on request; over 38 mm normalized. TMC by agreement. The symbol, such as N or SR, follows the grade.
-
What thickness does the standard cover?
- 6 mm to 200 mm. Actual sizes are agreed per order.
-
Is impact testing required?
- No base impact requirement exists in JIS G 3118. Charpy or other tests are agreed between purchaser and manufacturer when needed.
Request a quotation
Contact SHH STEEL for a quotation for JIS G3118 SGV410 carbon steel pressure vessel plate. Please send the specification and edition, grade, thickness, width, length, quantity, delivery destination and preferred delivery schedule so we can review your production and export requirements.
State the heat-treatment symbol, for example SGV410N or SGV410NSR, and any agreed impact or ultrasonic tests.
State any supplementary requirements, simulated post-weld heat treatment, impact testing, ultrasonic examination and the inspection document required, so they are agreed before the order is placed.
For a detailed quotation, email your material specification, drawing, quantity and delivery requirements to our team.
Contact: admin@steelspecs.com