JIS A 5528 SY390 U-Type Steel Sheet Pile
What is JIS A 5528 SY390 U-Type Steel Sheet Pile?
JIS A 5528 SY390 is the higher-yield hot-rolled U-type steel sheet pile grade in JIS A 5528:2021. SY marks a steel sheet pile, and 390 is the minimum yield in N/mm2. Minimum tensile strength is 490 N/mm2. Elongation is 16 % minimum on test piece No. 1A and 20 % minimum on test piece No. 14B. This page is SY390 only. It is not a geometry-only Z-type companion to the live SY295 U-type page.
Japanese A 5528 practice tabulated for this site is the U-type series (Type II to Type IVw). Hat-type sections belong to JIS A 5523, not this page. European Z-type sections belong to EN 10248 and must not be pasted onto a JIS A 5528 certificate.
Material, Dimensions and the JIS A 5528 SY390 Grade
JIS A 5528 is the material standard for these hot-rolled U-type piles. The 2021 edition is the one corroborated for chemistry and mechanicals on this site. The ordered edition governs acceptance. Shape tolerances follow the U-type limits already recorded on the SY295 page (width, height, thickness, length, camber, sweep and end out-of-square as tabulated there). A Charpy value is not specified for SY390 in JIS A 5528:2021 and is not invented here.
JIS A 5528 SY390 U-Type Sizes: Type II to Type IVw
The table lists the same typographical U-type series already verified on the SY295 page, from Type II through Type IVw. Public designations are Type II, III, IV, VL, VIL, IIw, IIIw and IVw only; mill or trade names are not used. The table is a typographical series, not a mill stock list, and not every type is assumed to be rolled in SY390 without confirmation.
Swipe horizontally to view all dimensions.
JIS A 5528 SY390 Chemical Composition
For both SY295 and SY390, JIS A 5528:2021 specifies only phosphorus and sulphur, each 0.040 % maximum. Carbon, silicon, manganese, nitrogen and carbon equivalent are not specified. Do not invent a carbon cap, and do not copy EN 10248-1 S430GP or S390GP product-analysis limits onto this Japanese grade.
Swipe horizontally to view all dimensions.
JIS A 5528 SY390 Mechanical Properties
Minimum yield is 390 N/mm2 and minimum tensile strength is 490 N/mm2. Minimum elongation is 16 % on test piece No. 1A and 20 % on test piece No. 14B. SY295, on the sister page, uses 295 / 450 N/mm2 and 18 % / 24 % elongation. Those figures must not be pasted onto an SY390 certificate. Absorbed energy at 0 C is not specified in the 2021 standard.
Swipe horizontally to view all dimensions.
Applications and Service Limits for JIS A 5528 SY390 U-Type Sheet Piles
SY390 U-type piles are used in cofferdams, retaining walls and heavier Japanese-series earth-retaining work where this yield class is named. The grade is not a hat-type JIS A 5523 product and not an EN 10248 Z-type. If SY295 will do, or if a European S430GP U or Z section is required, that product has to be ordered as such.
Near-Equivalents for JIS A 5528 SY390: Not Automatic Substitutes
SY295 is the lower-yield grade in the same standard and on the same U-type series. CNS 7851 uses the same SY names in the Taiwan standard and is not automatically this certificate. EN 10248-1 S390GP and S430GP are European GP grades with product-analysis chemistry and a Charpy requirement. They are not restamps of SY390.
Sourcing JIS A 5528 SY390 U-Type Steel Sheet Piles from SHH STEEL
Send the U-type designation (Type II to Type IVw), the length, and the JIS A 5528 edition, and name SY390 explicitly. Do not use the SY295 term for this page, and do not ask for a Z-type JIS A 5528 duplicate; Z-type enrichment is not applicable to this Japanese U-type standard. SHH STEEL reviews the grade, the section and the certificate before quoting. The size table is a typographical reference, not a warehouse list.
JIS A 5528 SY390 FAQs
-
Why is there no Z-type table on this page?
- JIS A 5528, as corroborated from official mill reprints used on this site, is a U-type series. Hat-type sections are JIS A 5523. European Z-type sections belong on EN 10248 pages, not as a geometry-only JIS duplicate.
-
Are carbon, silicon and manganese limited?
- Not in JIS A 5528:2021. Only phosphorus and sulphur are specified, each 0.040 % maximum, for both SY295 and SY390.
-
What are the elongation values?
- 16 % minimum on test piece No. 1A and 20 % minimum on test piece No. 14B. Do not use the SY295 18 % / 24 % figures.
-
Is a Charpy value required?
- No. Absorbed energy is not specified for SY390 in JIS A 5528:2021. A toughness requirement has to be added on the order if it is needed.
Conclusion
JIS A 5528:2021 SY390 is the 390 N/mm2 U-type sheet-pile grade, with 490 N/mm2 tensile strength and 16 % / 20 % elongation, on the typographical Type II to Type IVw series. It is not a Z-type duplicate of the SY295 page. Confirm the grade, the type and the certificate on the order.