ISO 630-2 SG345 Steel Plate | SG345 General Structural Plate (Annex B)
What is ISO 630-2 SG345 plate?
ISO 630-2 SG345 is grade SG345 of ISO 630-2:2021 (Edition 3), the international standard for technical delivery conditions for structural steels for general purposes. This grade is covered in Annex B. ISO 630-1 supplies the general technical delivery conditions.
ISO 630-2 specifies eight grades and up to four qualities. Annex A covers S235, S275, S355 and S460. Annex B covers SG205, SG250, SG285 and SG345. Clause 4.3 states that the two annexes are to be regarded separately; each is independent of the other. An Annex A S-grade is not a substitute for this Annex B grade.
Each SG grade is available in up to four qualities: A (no impact testing), B (impact at 20 °C), C (impact at 0 °C) and D (impact at −20 °C). Not every grade is available in every quality. This page is written at grade level; the purchaser must state the quality on the order. Impact energy values sit in Table B.4 and are not transcribed here.
SHH STEEL reviews enquiries against the ordered ISO 630-2:2021 edition, the Annex B grade and quality, and the inspection document. Reconfirm the edition when placing a later order.
Material specification for ISO 630-2 SG345
As of 12 November 2026, ISO 630-2:2021 (Edition 3, April 2021) remains the published edition. It cancels and replaces ISO 630-2:2011 and was technically revised. This page is written to the 2021 edition.
| Ordering item | Basis |
|---|---|
| Standard | ISO 630-2:2021, Edition 3 |
| General requirements | ISO 630-1 |
| Grade | SG345 (Annex B) |
| Quality | State A, B, C or D; not all qualities may be available |
| Product form | Reversing-mill plate enquiry; the standard also covers wide flats, sections and bars |
| Thickness | The official scope sets no restriction on nominal thickness for SG205, SG250, SG285 and SG345 for flat products, sections and long products. That is not a stock list. |
| Delivery condition | State a required condition if one is needed; otherwise clause 6.2 leaves it to the manufacturer |
| Inspection document | Specify the document type; see ISO 630-1 |
Mandatory purchaser information is specified in ISO 630-1. Options include a particular delivery condition, transverse impact testing and special steelmaking. State any option at enquiry.
ASTM A572 Grade 50 heat-analysis comparison (not ISO Table B.1)
Clause 6.3.1 requires the heat analysis of Annex B grades to comply with Table B.1. Clause 6.3.2 refers the permitted deviations for SG205, SG250, SG285 and SG345, relative to the heat analysis, to Table B.2. Those official tables are not in the 2021 preview consulted for this work, and they are not transcribed here as ISO normative rows.
The following figures are ASTM A572 Grade 50 comparison/reference data for a 345 MPa yield class, taken as ASTM A572 Grade 50 plate maxima. They are not ISO Table B.1 limits.
| Element | Cast / heat analysis, mass % |
|---|---|
| C | ≤0.23 |
| Mn | ≤1.35 |
| P | ≤0.030 |
| S | ≤0.030 |
| Si | ≤0.40 |
These are typical ASTM A572 Grade 50 plate maxima used as a 345 MPa-class comparison. Confirm the thickness-dependent ASTM row on the related product page. They are not ISO Table B.1 limits.
Clause 6.3.3 gives maximum CEV requirements for Annex A grades in Table A.3. That table does not apply to Annex B. Any CEV agreement for an SG grade must be taken from the official Annex B text, not from Table A.3.
ASTM A572 Grade 50 mechanical comparison (not ISO Table B.3)
The designation SG345 identifies a 345 MPa yield-strength class in Annex B. Tensile properties at room temperature shall comply with Table B.3, and Charpy V-notch properties with Table B.4. Those official tables are not in the 2021 preview and are not transcribed here as ISO normative limits.
Quality B is impact-tested at 20 °C, quality C at 0 °C and quality D at −20 °C (clause 4.2). Quality A has no impact test. Those are specified test temperatures, not design temperatures and not impact-energy values. Confirm Table B.4 against the official text. Specimen orientation is longitudinal unless a transverse test is agreed.
The following values are related-specification comparison/reference data. They must not be treated as ISO Table B.3 or Table B.4 limits and must not be used as allowable design stresses.
| Property | Comparison value |
|---|---|
| Yield strength, min (ASTM A572 Grade 50) | 345 MPa (50 ksi) |
| Tensile strength, min | 450 MPa (65 ksi) |
The 345 MPa yield coincides with the SG345 yield class. GB/T 1591 Q355B and EN 10025-2 S355JR are nearby 355 MPa-class plates, and ISO 630-2 S355B is the Annex A 355 MPa grade in this same standard. None of those is an automatic equivalent.
Delivery condition and ordering options for SG345
At the manufacturer’s discretion, clause 6.2 requires products to be delivered in the as-rolled condition, the normalized-rolled condition, the normalized condition, or the thermomechanical processed condition, unless a particular condition is agreed at the time of order. The actual condition shall be recorded on the inspection document.
Clause 8.2.2 sets the Annex B test unit: products of the same form, grade, quality, delivery condition and thickness range as specified in Table B.3, by heat and 50 tonnes or part thereof. By agreement at the time of ordering, two tests by heat may be used. Do not apply the Annex A 60-tonne or 80-tonne rules to this grade.
Weldability and fabrication review for SG345
SG345 is intended, as the standard’s scope describes, for welded or bolted structures in the as-delivered condition. That statement is not a qualified welding procedure. The fabricator must establish consumables, preheat, heat input and any post-weld treatment through the applicable procedure qualification and design requirements.
If a copper range or a silicon control for zinc coating is agreed, say so at enquiry; those options can affect weldability and are Annex-specific where the official text provides them. Confirm any such option against Annex B, not by copying an Annex A note.
Dimensions, surface quality and inspection
Surface condition, internal soundness, dimensions, tolerances and marking refer to ISO 630-1. This preview does not supply the full tolerance schedule; no numeric thickness deviation, flatness allowance or ultrasonic acceptance class is claimed.
State the required nominal dimensions, edge condition, surface restrictions, internal-soundness examination and document type with the enquiry. Identification must remain traceable through cutting, packing and shipment. Dimensional availability remains subject to mill confirmation. The official ‘no thickness restriction’ statement for SG grades is a scope statement, not a promise that every thickness is in stock.
Applications and service limits of SG345
SG345 may be considered for general-purpose welded or bolted structures — frames, members, plates in buildings, bridges and similar construction — where the design specification selects this exact ISO 630-2 Annex B grade and quality. These are intended-use examples, not authorization for a particular load, temperature or construction code.
Impact quality, if required by the project, must be stated. Quality A does not include an impact test. The comparison yield class is not a design allowable.
Compare SG345 with related ISO 630-2 grades
Compare the following published ISO 630-2 Annex A grades by their complete annex rows, quality and project acceptance. Annex A and Annex B are independent. These are related selections within the standard, not interchangeable materials. Other SG grades are not linked here until those product pages are live.
| ISO product | Classification | Review before a grade change |
|---|---|---|
| ISO 630-2 S355B | Annex A, quality B, 20 °C impact | Different annex and a 355 MPa class. Nearby only; not a substitute for SG345. |
| ISO 630-2 S275B | Annex A, quality B | Lower Annex A yield class. |
| ISO 630-2 S235B | Annex A, quality B | Lower Annex A yield class. The two annexes are independent. |
Related grades and substitution limits for SG345
The heading identifies a comparison topic, not a declaration of interchangeable material. No automatic foreign equivalent or dual certification is offered for SG345.
| Product / range | Verified relationship or limitation | Substitution control |
|---|---|---|
| GB/T 1591 Q355B | Related 355 MPa-class Chinese structural plate. Nearby yield class only. | Engineer approval required; not an automatic equivalent. |
| EN 10025-2 S355JR | Related 355 MPa-class European structural plate, 20 °C impact quality. | Engineer approval required; not an automatic equivalent. |
| ISO 630-2 S355B | Annex A grade in the same standard. Annex A and Annex B are independent. | Engineer approval required; not an automatic equivalent. |
Complete specification review and engineer approval are required before substitution. Chemistry, tensile and impact requirements, thickness, delivery condition and the project specification must all be checked.
Why choose SHH STEEL for SG345
SHH STEEL supports specification-led structural-plate purchasing rather than substitution by catalogue name.
- We quote the requested ISO 630-2:2021 edition, Annex B grade and quality separately from Annex A S-grades and from national-standard plates.
- Comparison figures on this page are labelled as such; they are not used as unofficial ISO Table B.1 or Table B.3 limits.
- Delivery condition, impact quality and inspection-document type are reviewed before confirmation.
- Supply capability, lead time and any additional testing remain subject to quotation confirmation.
Enquiry and supply review for SG345
Send the project material schedule for SG345. SHH STEEL will review the enquiry and identify any clarification needed before confirming the supply route.
| Enquiry item | Information required |
|---|---|
| Material identity | ISO 630-2:2021 SG345; state the quality (A, B, C or D); identify any proposed dual certification |
| Dimensions and quantity | Product form, nominal thickness, width, length, quantity and cutting drawings |
| Delivery condition | Required condition if one is particular; otherwise clause 6.2 leaves it to the manufacturer |
| Acceptance values | Complete official Annex B chemistry, tensile and impact rows for the ordered edition; say if comparison values are for enquiry only |
| Inspection document | Document type; see ISO 630-1 |
| Destination | Delivery place and any packing or marking restrictions |
Missing official Table B.1–B.4 figures on this comparison page are not waivers of the standard.
FAQ
-
Which edition applies to SG345 here?
- This page uses ISO 630-2:2021, Edition 3. As of 12 November 2026 (Asia/Shanghai) that edition remains the published text. Reconfirm the edition on the order.
-
Is SG345 the same as an Annex A S-grade?
- No. SG205, SG250, SG285 and SG345 are Annex B grades. S235, S275, S355 and S460 are Annex A. Clause 4.3 requires the two annexes to be regarded separately.
-
Are chemistry and mechanical numbers ISO normative limits?
- No. Official Tables B.1 to B.4 are not in the 2021 preview and are not transcribed as ISO limits. Numeric figures on this page are related-specification comparison/reference data, clearly labelled. Confirm the official ISO rows before supply or design use.
-
Do I need to specify a quality?
- Yes. Qualities A (no impact test), B (20 °C), C (0 °C) and D (−20 °C) are order information. Not every quality is available for every grade. This page does not add a quality suffix to the title.
-
What should I send for a quotation?
- Send ISO 630-2:2021, the grade SG345, the quality, product form and dimensions, the quantity, the delivery condition if a particular condition is required, the inspection-document type and any agreed options. The official Annex B tables must be available for a technical supply commitment.
Request a quotation for ISO 630-2 SG345 plate
Request a SHH STEEL quotation for ISO 630-2:2021 SG345 plate. Send the quality, nominal dimensions, quantity, destination and the project material specification.
Identify any required delivery condition, the inspection-document type and any impact or supplementary tests. If comparison values are being used for enquiry only, say so.
Availability, dimensions, processing, testing and lead time will be confirmed against the enquiry. Related grades are not treated as approved substitutes without engineer review.
Contact: admin@steelspecs.com