GOST 19281 09G2 Steel Plate | 09G2 HSLA Rolled Steel Plate | GOST 19281 Steel - SHH STEEL

GOST 19281 09G2 Steel Plate | 09G2 HSLA Rolled Steel Plate

GOST 19281 09G2 (09Г2) steel plate is a manganese high-strength rolled steel under GOST 19281-2014, whose official English title is High strength rolled steel. General specification. The ordering property is the strength class, not the grade name alone. Annex A Table A.2 lists the 09G2 family for plate, universal wide strip and bent profiles in class 295 up to 32 mm, and lists the copper-bearing variant 09G2D at class 345 up to 50 mm. Base 09G2 is not listed in Table A.2 at classes 265, 315, 325, 355, 375, 390 or 440. Variants 09G2-1 (composition 1) and 09G2D (copper-bearing) are covered on this page; they are not separate articles. As of 12 November 2026, the 2014 edition remains in force, applied with Amendment 1 from 1 June 2020, until 1 December 2026. SHH STEEL produces and exports this plate to the ordered 2014 requirements, including Amendment 1.
Grade
09G2
Standard
GOST 19281-2014
Official English title
High strength rolled steel. General specification.
Table A.2 plate classes
295 (family); 345 (09G2D)
Table 7 silicon
0.17–0.37 %
Table 10 at class 295, ≤20 mm (2016)
ReH 305 N/mm²; Rm 440 N/mm²
CEV, GS option (Amd 1)
0.43 % at class 295; 0.46 % at class 345
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why choose Us
Our Service
FAQ
Conclusion

General Description of GOST 19281 09G2 Steel Plate

GOST 19281 09G2 Steel Plate is listed in Table 7 under unalloyed quality steels, with ladle silicon 0.17–0.37 %, manganese 1.40–1.80 % and carbon not more than 0.12 %. That heading and the lower silicon range distinguish it from 09G2S (alloyed, silicon 0.50–0.80 %) and from 10G2S1 (alloyed, silicon 0.80–1.10 %). A shared class 295 listing in part of Table A.2 is not interchangeability.

The first mention of the Cyrillic designation is 09Г2. Composition-1 is written 09G2-1 (09Г2-1); the copper-bearing variant is 09G2D (09Г2Д) and 09G2D-1. Those variants are specified on this page. Composition-1 keeps the same silicon range and sets manganese as an upper limit only (not more than 1.80 %), and is not recommended, under Table 7 note 7, for articles the customer will heat-treat. The D variant specifies copper 0.15–0.30 %. Clause 5.2.1.3 and its note state that class 295 product of 09G2D and 09G2D-1 is manufactured up to 32 mm inclusive, which matches the Table A.2 class 295 listing.

09G2 is not a grade in the GOST 5520 boiler and pressure-vessel list. Do not treat a GOST 5520 09G2S plate as this product; that is a different designation and a different product standard.

GOST 19281 09G2 Steel Plate Material Specification

As of 12 November 2026, GOST 19281-2014 remains in force. It was introduced on 1 January 2015, replaces GOST 19281-89, and has restricted validity until 1 December 2026. It is applied with Amendment 1, which has been in force from 1 June 2020. This page is written to the 2014 edition, with Amendment 1 where that amendment is known. GOST 19281-2025 has been adopted and takes effect on 1 December 2026, so buyers should confirm which edition applies to their order. The 2025 edition has a right of early application; this page does not tabulate 2025 requirements. Two one-page corrections issued after Amendment 1 were not inspected for this page; confirm any later correction against the official text of the edition stated on the order.

The official English title of GOST 19281-2014 is “High strength rolled steel. General specification.” The standard covers hot-rolled plate, universal wide strip, bars, sections and bent profiles of high strength for general-purpose structures with welded, riveted or bolted connections. This page is the plate product. For 09G2, Table A.2 recommends plate in class 295 up to 20 mm (09G2 family only) and over 20–32 mm (with the 09G2S family and 16GS). At class 345, up to 50 mm, Table A.2 lists 09G2D, not base 09G2 or 09G2-1. This is a narrower recommended class range than 09G2S or 10G2S1.

Order the plate by strength class and by grade. The classes used in the standard are 265, 295, 315, 325, 345, 355, 375, 390 and 440. Each class is a specified minimum yield strength in N/mm², subject to any higher Table 10 cell for a named grade and thickness. Inspection categories, delivery condition, guaranteed weldability (GS) and any copper-bearing or composition-1 variant must be stated on the order; they are not implied by the grade name.

GOST 19281 09G2 Steel Plate Chemical Composition

Table 7 ladle analysis for 09G2 and the variants covered on this page, visually inspected in the 2016 reprint. Amendment 1 does not change these numeric cells (it rewrites notes 4 and 5). P and S are maxima. Values are mass fraction, %.

Grade C Si Mn P max S max Cr Ni Cu V
09G2 ≤0.12 0.17–0.37 1.40–1.80 0.030 0.035 ≤0.30 ≤0.30 ≤0.30 ≤0.12
09G2-1 ≤0.12 0.17–0.37 ≤1.80 0.030 0.035 ≤0.30 ≤0.30 ≤0.30 ≤0.12
09G2D ≤0.12 0.17–0.37 1.40–1.80 0.030 0.035 ≤0.30 ≤0.30 0.15–0.30 ≤0.12
09G2D-1 ≤0.12 0.17–0.37 ≤1.80 0.030 0.035 ≤0.30 ≤0.30 0.15–0.30 ≤0.12

Table 7 is ladle analysis. Table 8 gives product-analysis deviations, visually inspected in the 2016 reprint (Amendment 1 does not change these element rows for the grades on this page). For elements whose Table 7 cell is an upper limit only, Table 8 note 2 applies only the plus deviations. Carbon is specified as an upper limit on every grade on this page, so only the plus carbon deviation applies in the product analysis.

Element Product-analysis deviation, %
C ±0.02
Mn ±0.10
Si ±0.05
Cr ±0.05
Ni ±0.05
Cu ±0.05
S ±0.005
P +0.005 (plus only)
N ±0.005
V +0.02 / −0.01
Ti +0.010 / −0.005
Nb +0.010 / −0.005
Al +0.010 / −0.005

Arsenic shall not exceed 0.08 % in steel of all grades (Table 7 note 1). Nitrogen in steel that is not alloyed with nitrogen shall not exceed 0.008 % without secondary metallurgy, or 0.010 % with secondary metallurgy. Amendment 1 allows nitrogen up to 0.012 % inclusive provided the product meets the official Tables 11 and 12 for impact after mechanical ageing, regardless of the ordered category, including an order without a category. A further nitrogen-equivalent provision is stated in note 3; confirm that provision against the official text.

Amendment 1, Table 7 note 4: steel of grades 09G2, 09G2-1, 09G2S, 09G2S-1 and 10KhSND shall be deoxidized with aluminium in the range 0.02–0.06 %. The actual aluminium mass fraction, controlled in the ladle sample, is stated in the quality document. Amendment 1 note 5 permits microalloying with aluminium, titanium and niobium, calculated to give aluminium not more than 0.05 %, titanium not more than 0.04 % and niobium not more than 0.05 %, unless other mass fractions are stated in Table 7 and its notes; those elements are controlled and stated in the quality document.

Table 7 note 7: composition-1 grades (the digit 1 after a hyphen in the designation) are not recommended for articles the customer will heat-treat. If the purchaser will heat-treat the plate, do not select a composition-1 variant on that recommendation alone; agree the grade and the treatment with the manufacturer.

GOST 19281 09G2 Steel Plate Mechanical Properties

Table 10 gives minimum yield strength (ReH, σт), tensile strength (Rm, σв) and percentage elongation after fracture (δ5) for plate, universal wide strip and bent profiles. The yield minimum equals the strength class, except where Table 10 states a higher figure for a named grade group (see the class 295 row for 09G2). Amendment 1 rewrote the thickness column of Table 10 for strength classes 295, 345, 355 and 440. The yield, tensile-strength and elongation minima below were read from the 2016 reprint of Table 10, whose mechanical columns Amendment 1 did not describe as replaced. Use the official Amendment 1 (2021 consolidated) table for the current thickness bands of those four classes, including any footnote that applies to thicker product. A 2016 footnote that treated some thicker bands as non-rejectable until 1 January 2016 has elapsed.

Strength class Thickness label in the 2016 Table 10 (see the Amendment 1 note) ReH min, N/mm² Rm min, N/mm² Elongation δ5 min, % Grade group in that cell
295 Up to 20.0 mm inclusive (thickness column amended — confirm the official band) 305 440 21 09G2, 09G2-1, 09G2D, 09G2D-1. This is a higher yield and tensile cell than the parallel 295 / 430 cell for 09G2SD, 16GS and 10G2S1 at the same 2016 band.
295 Over 20.0 mm up to 100.0 mm inclusive (thickness column amended — confirm the official band) 295 430 21 09G2 family with 09G2SD, 16GS and 10G2S1
345 2016 labels: up to 32.0 mm inclusive, and over 32.0 up to 50.0 mm inclusive (thickness column amended — confirm the official bands) 345 490 21 09G2D is in this group with 09G2S and 10G2S1. Base 09G2 is not in the visually read grade list.

The distinctive Table 10 cell for this family is at class 295, in the 2016 up-to-20 mm band: yield 305 N/mm² and tensile strength 440 N/mm², which are higher than the class number and higher than the parallel 295 / 430 N/mm² cell for 09G2SD, 16GS and 10G2S1. Do not apply the 305 N/mm² yield figure to 09G2S or 10G2S1, and do not apply the 295 N/mm² cell to 09G2 in that thin band. Confirm the current 295 and 345 thickness bands against Amendment 1.

Annex A is a recommended annex. Table A.2 lists grades that provide the stated strength class at the stated thickness for plate, universal wide strip and bent profiles. A listing in Table A.2 is not a certificate that every thickness in the band is interchangeable with every other grade in the same cell, and it is not a substitute for the Table 10 tensile minima of the ordered class. Footnote * permits controlled rolling (KP) or controlled rolling followed by accelerated cooling. Footnote ** permits controlled rolling, thermomechanical treatment (TMO) or thermal strengthening (TY). Amendment 1 replaced only the class 375 row of Table A.2; the other rows below were visually read from the 2016 reprint, which Amendment 1 does not rewrite.

Strength class Thickness in Table A.2 (2016 visual; not rewritten by Amendment 1 for these classes) 09G2 family listed Table A.2 footnote
295 Up to 20.0 mm inclusive 09G2, 09G2-1, 09G2D, 09G2D-1 only —
295 Over 20.0 mm up to 32.0 mm inclusive 09G2 family, with the 09G2S family and 16GS —
345 Up to 50.0 mm inclusive 09G2D is listed. Base 09G2 and 09G2-1 are not listed in this Table A.2 cell —

Table A.2 does not recommend base 09G2 at class 265 — that thin-and-thick 265 listing is the 09G2S family — or at 315, 325, 355, 375, 390 or 440. If a class outside the Table A.2 listing is proposed, agree it with the manufacturer and confirm the current figures against the official table of GOST 19281-2014 with Amendment 1 before treating it as a recommended combination.

Impact toughness for plate is specified in Table 12, which Amendment 1 replaced in full, and is selected by the inspection category ordered from Table 4, which Amendment 1 also replaced. Values are minima in J/cm² for KCU or KCV at the temperatures listed for that category, class, grade and thickness. A plus sign in Table 12 means the test is made to collect statistical data; the result is recorded in the quality document and is not a specified minimum. A minus sign means the property is not specified and is not tested. This page does not tabulate Table 12 cells, because an official-format 2021 (Amendment 1) Table 12 was not visually inspected and a third-party extract is not a substitute for that inspection. If impact is required, state the category, the temperature and the test type on the order, and confirm the current figures against the official table of GOST 19281-2014 with Amendment 1.

Amendment 1 marked some Table 12 cells as optional for two years from 1 June 2020. That two-year period has elapsed. Confirm the current application of those footnote cells, and of any later one-page correction, against the official text. Do not take impact figures from the 2016 reprint, from another standard, or from a handbook and apply them as the current official minima.

Amendment 1 deletes clause 5.2.1.6, which in the 2016 reprint required a 180° bend on a mandrel of diameter equal to two specimen thicknesses and allowed the manufacturer to omit the test if it guaranteed satisfactory results at the purchaser. That deleted clause is not restated on this page as a current requirement. The amended acceptance rules still provide for recording a 180° bend result, or a manufacturer’s guarantee of that bend, on the quality document. Confirm the current bend requirement against the official 2014 text with Amendment 1.

GOST 19281 09G2 Steel Plate Delivery Conditions

The strength class is the ordering property. State GOST 19281-2014, the grade (including any composition-1 or copper-bearing variant), the strength class, the inspection category, the dimensions, the quantity and the delivery condition on the order. For 09G2, Table A.2 recommends plate in class 295 up to 20 mm (09G2 family only) and over 20–32 mm (with the 09G2S family and 16GS). At class 345, up to 50 mm, Table A.2 lists 09G2D, not base 09G2 or 09G2-1. This is a narrower recommended class range than 09G2S or 10G2S1. A Table A.2 listing is a recommended combination of grade, class and thickness; it is not a substitute for stating the class on the order, and it is not interchangeability with other grades listed in the same cell.

Delivery may be agreed as hot-rolled, heat-treated, or with controlled rolling (KP), controlled rolling followed by accelerated cooling, thermomechanical treatment (TMO) or thermal strengthening (TY), where Table A.2 or the order permits those routes (footnotes * and ** in Table A.2). Do not assume a heat-treated or thermomechanically treated delivery from the grade name alone. Record the actual condition on the quality document. If the purchaser will heat-treat the article after delivery, see Table 7 note 7 before selecting a composition-1 variant.

Copper-bearing (D) variants are supplied, when ordered, with increased resistance to atmospheric corrosion, guaranteed by the chemical composition (copper 0.15–0.30 %) and the manufacturing technology, under clause 5.2.1.3. The letter D in the designation is not implied by the base grade; state the D variant on the order if it is required.

GOST 19281 09G2 Steel Plate Weldability

When guaranteed weldability (designated GS) is ordered, Amendment 1 to clause 5.2.1.2 limits the carbon equivalent CEV to not more than 0.43 % for strength classes 265, 295, 315 and 325; 0.46 % for classes 345, 355 and 375; 0.48 % for class 390; and 0.51 % for class 440. The same clause also requires the manufacturing technology and the chemical composition, including the Table 8 product-analysis deviations, to support weldability. GS is not implied by the grade name; state it on the order if it is required.

This page does not give preheat, interpass, heat-input or post-weld heat-treatment figures. The fabricator is responsible for welding-procedure qualification, consumable selection, preheat and any post-weld heat treatment required by the project specification. Do not take those figures from another standard or from a handbook and apply them as GOST 19281 rules. A shared strength class, a Table A.2 listing alongside another grade, or a commonly compared foreign designation does not make those grades automatic welding substitutes.

GOST 19281 09G2 Steel Plate Tolerances

Dimensions, shape and permissible deviations for plate follow the plate-dimension standard cited by GOST 19281-2014 as updated by Amendment 1. State the required thickness, width, length, thickness-accuracy class, edge condition and, for plate supplied as sheets, the flatness class on the order. This page does not tabulate numerical deviation limits from that dimension standard.

Surface quality and dressing limits are those of GOST 19281-2014 with Amendment 1. Confirm the permitted defect types, dressing depth and area, and the prohibition on delamination against the official text. Ultrasonic testing is not a default requirement. If continuity testing is required, state the method, the class and the test volume on the order; they are not implied by the grade or the strength class.

GOST 19281 09G2 Steel Plate Applications and service limits

09G2 under GOST 19281-2014 is general-purpose high-strength rolled steel for welded, riveted or bolted structures. Typical uses are structural members, frames and fabricated platework where the ordered strength class, thickness and inspection category match the design. This page does not assign a design stress, a temperature limit or a code approval. Those come from the project specification and the design standard, not from the grade name.

Table A.2 recommends a narrower class range for this grade than for 09G2S or 10G2S1. Do not assume a class 265, 325 or 355 listing from those neighbouring grades. Do not use this plate as a boiler or pressure-vessel product solely because the same designation appears under GOST 5520; that is a different product standard with its own thickness, category and test regime. Do not treat a commonly compared foreign structural grade as approved for the same duty without engineer review of both complete specifications.

Compare 09G2 with related GOST 19281 grades

09G2 is the lower-silicon, unalloyed-quality member of this first GOST 19281 batch. It is related to 09G2S and 10G2S1, not equivalent. Sister GOST 19281 product pages are not linked here because those URLs are not live; the designations are named for comparison only.

Grade Table 7 silicon, % Table 7 heading Table A.2 plate classes (summary) Distinctive Table 10 cell
09G2 (this plate) 0.17–0.37 (composition-1: same Si, Mn ≤1.80) Unalloyed quality steels 295 (up to 32 mm); 09G2D also at 345 up to 50 mm Class 295, up to 20 mm: ReH 305 N/mm² and Rm 440 N/mm²
09G2S 0.50–0.80 (composition-1: ≤0.80) Alloyed steels 265, 295 (20–32 mm), 315*, 325 (10–20 mm), 345, 355, 375 (Amendment 1, 10–32 mm) Class 325, 10–20 mm: Rm 470 N/mm² for 09G2S and 09G2S-1
10G2S1 0.80–1.10 Alloyed steels 295 (32–100 mm), 315, 325, 345, 355, 390** Class 390: ReH 390, Rm 510 N/mm², elongation 19 %

A class 295 order for 09G2 in the up-to-20 mm band uses the 305 N/mm² yield cell; the same class for 09G2S is recommended by Table A.2 only over 20–32 mm, and Table 10 places 09G2S at class 295 in a different thickness group. Do not copy cells across grades.

GOST 19281 09G2 Steel Plate Equivalent Material Grade

No formal equivalence has been verified for the designations below. They are related designations only and are not equivalent to this GOST 19281-2014 plate. Engineer approval is required before any substitution. This page does not link any external catalogue. None of those relationships is interchangeability.

Standard Country-Region Equivalent Grade Note
GOST 19281-2014 Interstate (GOST) 09G2 This product under GOST 19281-2014, ordered by strength class. Variants 09G2-1 and 09G2D are specified on this page. Table A.2 lists class 295 up to 32 mm; 09G2D is also listed at class 345.
GB/T 1591 China GB/T 1591 Q355B Commonly compared at a 345 N/mm² yield class; not equivalent. Verify chemistry, strength class, thickness, delivery, impact category and the project specification. A similar yield class does not authorise substitution. Engineer approval is required. Not a verified formal equivalent.
EN 10025-2 Europe EN 10025-2 S355J2 Commonly compared structural plate; not equivalent. Verify chemistry, impact temperature, delivery condition, thickness limits and the project specification. Engineer approval is required. Not a verified formal equivalent.

Related high-strength structural plate systems, including GB/T 1591, EN 10025-2 and ASTM A572, are sometimes listed on comparison charts. No grade in those systems is listed as a verified equivalent on this page beyond the commonly compared products in the table. A chart cannot replace a review of chemistry, strength class, product form, delivery condition, mechanical tests and the project specification.

Why choose Us

SHH STEEL produces and exports GOST 19281 plate, including GOST 19281 09G2 Steel Plate. We review the Table 7 unalloyed-quality listing and silicon range 0.17–0.37 %, the mandatory aluminium deoxidation of 0.02–0.06 % under Amendment 1 note 4, the Table A.2 class 295 listing up to 32 mm, and the Table 10 cell of 305 N/mm² yield and 440 N/mm² tensile strength for the 09G2 family at class 295 in the 2016 up-to-20 mm band before production, and we state the actual results on the quality document. We do not treat a shared strength class, a Table A.2 cell shared with another grade, or a commonly compared foreign designation as a substitute for the ordered grade and class.

Orders are accepted against GOST 19281-2014, including Amendment 1. Enquiry details should include grade (and any -1 or D variant), strength class, inspection category, thickness, width, length, quantity, delivery condition and any agreed options (guaranteed weldability GS, ultrasonic class, microalloying agreement). See the GOST 19281 hub for the product family.

Our Service

Supply covers production to the ordered 2014 requirements, including Amendment 1, mill documentation, and export packing and shipment. Quality documents record the actual ladle analysis, tensile results for the ordered class, and, where the category requires them, impact results, including any characteristic that Table 12 marks as determined for statistical data. Guaranteed weldability and ultrasonic testing are supplied when they are agreed on the order, not by default.

To enquire, state GOST 19281-2014, grade 09G2, the strength class, the inspection category, dimensions, quantity and the required options. SHH STEEL will confirm manufacturability and the inspection plan against that order. This page is a product description; the official standard and the quality document govern acceptance.

FAQ

What is 09G2 steel plate?

09G2 (09Г2) is a manganese high-strength rolled steel under GOST 19281-2014. In Table 7 it is listed under unalloyed quality steels, with silicon 0.17–0.37 %, manganese 1.40–1.80 % and carbon not more than 0.12 %. The ordering property is the strength class. Table A.2 lists the 09G2 family for plate mainly at class 295 up to 32 mm, and lists 09G2D at class 345 up to 50 mm. Variants 09G2-1 and 09G2D are covered on this page.

Is GOST 19281-2014 still current for 09G2?

Yes, as of 12 November 2026. GOST 19281-2014 remains in force, applied with Amendment 1 from 1 June 2020, and has restricted validity until 1 December 2026. This page is written to the 2014 edition, with Amendment 1 where that amendment is known. GOST 19281-2025 has been adopted and takes effect on 1 December 2026, so buyers should confirm which edition applies to their order. The 2025 edition has a right of early application. State the edition, and Amendment 1 if the 2014 edition is ordered, together with the grade and the strength class, on the order. This page does not tabulate 2025 tables. Two one-page corrections issued after Amendment 1 were not inspected for this page.

Which strength classes can 09G2 plate be ordered in?

Table A.2 recommends the 09G2 family at class 295: up to 20 mm (this family only) and over 20–32 mm (with 09G2S and 16GS). At class 345, up to 50 mm, Table A.2 lists 09G2D, not base 09G2. The grade is not listed in Table A.2 at 265, 315, 325, 355, 375, 390 or 440. State the class on the order. A Table A.2 listing is recommended, not interchangeability with 09G2S in the 20–32 mm band.

Why is the class 295 yield 305 N/mm² for thin 09G2 plate?

In the 2016 Table 10, for class 295 up to 20 mm inclusive, the 09G2 family has a yield minimum of 305 N/mm² and a tensile minimum of 440 N/mm². That is a higher cell than the parallel 295 / 430 N/mm² group for 09G2SD, 16GS and 10G2S1. Amendment 1 rewrote the class 295 thickness column; confirm the current band against the official Amendment 1 table, and do not apply the 305 N/mm² figure to 09G2S or 10G2S1.

Are 09G2-1 and 09G2D separate products?

They are specified on this page, not as separate articles. 09G2-1 is composition 1: manganese has an upper limit only (not more than 1.80 %), and Table 7 note 7 does not recommend composition-1 steel for articles the customer will heat-treat. 09G2D is the copper-bearing variant (copper 0.15–0.30 %) with increased atmospheric-corrosion resistance under clause 5.2.1.3; class 295 09G2D plate is manufactured up to 32 mm inclusive. State the variant on the order.

Enquire about GOST 19281 09G2 Steel Plate

Enquire for GOST 19281 09G2 Steel Plate to GOST 19281-2014, including Amendment 1. State the grade 09G2, the strength class, the inspection category, dimensions, quantity, the delivery condition and any agreed options (GS weldability, a composition-1 or copper-bearing variant, ultrasonic class). SHH STEEL will confirm the inspection plan against the official tables of the edition on the order. The official standard and the quality document govern acceptance.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X