GB/T 20933 Q355P U-Type Steel Sheet Pile
What is GB/T 20933 Q355P U-Type Steel Sheet Pile?
GB/T 20933 Q355P U-type steel sheet pile is a hot-rolled interlocking pile specified to the Chinese national sheet-pile standard GB/T 20933. The current edition is GB/T 20933-2021, implemented in 2022, replacing the 2014 edition. The letter P in the grade name denotes sheet pile. Q355P is a 355 MPa yield grade in that family; Q295P is the lower-yield sister tabulated on this page. Industry citations of the 2021 edition also name Q390P, Q420P and Q460P as members of the same family; those higher grades are not given numeric tables here because a verified opened table for them was not used on this page.
The official section types in GB/T 20933 are U-type (designated PU in the standard), Z-type (PZ) and straight (PI). Example designations include 400 × 125 and 400 × 170. Mill profile names used in trade are not GB/T 20933 model numbers. These piles are not JIS A 5528 SY295 U-type steel sheet pile, not EN 10248-1 S355GP U-type and Z-type steel sheet pile, and not an H-beam or a bearing pile. Interlocks of similar width are not interchangeable by depth or mass alone. The figures below are commonly published values. They are not presented as a row-by-row extract of the official 2021 tables. The ordered edition governs.
GB/T 20933 Q355P Chemistry (Commonly Published Values)
The phosphorus and sulphur maxima below are commonly published for Q295P and Q355P. Carbon, silicon and manganese are not restated as verified figures on this page, because opened sources do not agree on those limits and this page does not invent a complete official composition table. Read C, Si, Mn, carbon equivalent and any other residual limits from the ordered edition of GB/T 20933-2021 and from the mill certificate.
Weathering Q…WP variants appear in some published tables and are not the default Q355P grade. If a weathering grade is required, it should be named on the order.
GB/T 20933 Q295P and Q355P Mechanical Properties
The yield, tensile and elongation figures below are commonly published for Q295P and Q355P. They are not presented as a complete official Table 6 extract, and no extra thickness band is invented beyond what the opened sources actually state.
If the project names Q390P, Q420P or Q460P, those grades should be specified and certified to the ordered edition; this page does not invent their tensile tables.
GB/T 20933 Q355P U-Type Sizes (Commonly Supplied Designations)
GB/T 20933 publishes U-type, Z-type and straight section types. The U-type range commonly associated with Q355P programmes certified to the 2021 edition runs from 400 × 100 to 750 × 225. Example designations often discussed for this official type are 400 × 125 and 400 × 170. Mass, moment of inertia and section modulus are not tabulated here, because a verified official or mill property table for those exact official-type rows was not adopted on this page. Confirm section properties from the ordered edition and from the mill’s section table for the designation actually rolled.
Swipe horizontally to view all dimensions.
Commonly supplied U-type designations
Swipe horizontally to view all dimensions.
European U-type or Z-type geometries of similar width, and Japanese U-type designations of similar depth, are not these official GB/T 20933 types by width or mass alone. See JIS A 5528 SY295 U-type steel sheet pile and EN 10248-1 S355GP U-type and Z-type steel sheet pile when those systems are the ones named.
GB/T 20933 Q355P U-Type Steel Sheet Pile Applications
Q355P and Q295P U-type piles are used in cofferdams, retaining walls, quay walls and foundation-pit support where a Chinese hot-rolled sheet-pile grade is named. They are not a silent substitute for ASTM A328 carbon steel sheet pile, for JIS A 5528 SY295 U-type steel sheet pile, or for a European GP pile. A sheet pile is not an H-beam or a bearing pile.
Near-Equivalents for GB/T 20933 Q355P U-Type Steel Sheet Pile
Sourcing GB/T 20933 Q355P U-Type Steel Sheet Piles from SHH STEEL
SHH STEEL supplies GB/T 20933 Q355P and Q295P U-type steel sheet piles against a named designation list, the 2021 edition unless another edition is agreed, and the inspection document type. Enquiries should state the official type (U-type, Z-type or straight), the designation, lock orientation, length, and any coating or corner-pile requirement.
GB/T 20933 Q355P U-Type Steel Sheet Pile FAQs
-
What does the P in Q355P mean?
- In GB/T 20933 the letter P denotes sheet pile. Q355P is not Q355B plate or an H-beam grade of similar yield, and it is not automatically a weathering Q…WP grade.
-
Are PU, PZ and PI mill brand names?
- No. In this standard they are the official type designations for U-type, Z-type and straight sections. Trade profile names used by individual mills are not those official model numbers.
-
Why are mass and section modulus not tabulated?
- A verified official or mill property table for the official-type U-type rows was not adopted on this page, and European U-type geometries of similar width were not used as a substitute. Confirm properties from the ordered edition and the mill’s section table.
-
Is this page the official GB/T 20933-2021 Table 5 or Table 6?
- No. The mechanical and phosphorus/sulphur figures are commonly published values. Carbon, silicon, manganese and carbon equivalent are not restated as verified figures here. The ordered edition governs.
-
Can a JIS U-type pile replace a GB/T 20933 U-type of similar width?
- No. The standards, grade names and interlocks are different. Name GB/T 20933 and the official-type designation on the enquiry.
Request a Quotation for GB/T 20933 Q355P U-Type Steel Sheet Pile