ASTM A328 Carbon Steel Sheet Pile
What is ASTM A328 Carbon Steel Sheet Pile?
ASTM A328 carbon steel sheet pile is carbon steel sheet piling to ASTM A328/A328M, used for dock walls, seawalls, cofferdams and excavations. The grade has a minimum yield of 39 ksi [270 MPa], a minimum tensile strength of 65 ksi [450 MPa], a minimum elongation of 17% in 8 in. [200 mm], and a minimum elongation of 20% in 2 in. [50 mm].
Dimensions follow the ordered A6/A6M or project profile series and are stated separately from the material grade. These piles are filed under the steel sheet piles category in the steel structural profiles catalog. A328 is not A572 sheet piling and is not A690 marine sheet piling. It is not an H-beam or a bearing pile, and it is not an EN, JIS or Chinese interlocking pile by width or mass alone.
Material, Dimensions and the A328 Grade
The purchase order and the inspection document should name, separately:
- ASTM A328/A328M and its edition (the ordered edition governs), as carbon steel sheet piling;
- the section geometry and the required length, to A6/A6M or the project series;
- whether copper steel is specified (a 0.20% minimum copper may then apply), and any agreed interlock strength, coating or impact test.
A328 is not A572 and is not A690.
ASTM A328 Sizes: Typical Hot-Rolled Mill Series
Dimensions follow the ordered ASTM A6/A6M or project profile series and are stated separately from the material grade. The tables below are typical published mill series, described by geometry only. They are not an ASTM A6 size table, and trade names are not used. A North American Z-type of a given width is not a European Z-type or a JIS U-type of similar width.
Some mill programs also offer this grade on the typical European hot-rolled U-type and Z-type series tabulated on the EN 10248-1 S355GP U-type and Z-type steel sheet pile page. Nominate the geometry on the enquiry; not every section is offered in every grade.
Typical North American hot-rolled Z-type mill series
Typical North American hot-rolled Z-type mill series, described by geometry only. These are published mill-series dimensions, not an ASTM A6 size table, and trade names are not used.
Swipe horizontally to view all dimensions.
Typical hot-rolled straight-web mill series
Typical North American hot-rolled straight-web mill series, described by effective width and web thickness. These are published mill-series dimensions, not an ASTM A6 size table, and trade names are not used.
ASTM A328 Chemical Composition
The figures below are the A328 limits as reprinted in an official mill specification sheet. Carbon, manganese and silicon are not specified in that table. Phosphorus is 0.035% maximum and sulphur is 0.04% maximum. Where copper steel is specified, copper is 0.20% minimum. The ordered edition of A328/A328M governs if it differs. Do not invent a carbon or manganese limit.
Swipe horizontally to view all dimensions.
ASTM A328 Mechanical Properties
The tensile values below are the A328 minima. Elongation is reported on both the 8 in. [200 mm] and the 2 in. [50 mm] gauge lengths. There is no default Charpy requirement unless one is agreed on the order.
Shape Tolerances and Identification
Shape, mass and length tolerances for these sections follow ASTM A6/A6M unless the order states otherwise. A typical mill mass tolerance under A6 is ± 2.5%, and length is commonly plus a stated allowance and minus zero; the ordered A6 edition governs.
A typical inspection mark identifies the specification, the geometry, the heat number, the producer and the length. An A328 certificate is not an A572 or A690 certificate.
Delivery Conditions, Inspection and Identification
These piles are commonly supplied as-rolled. The inspection document should identify ASTM A328/A328M and its edition, the section geometry, the length, the heat analysis for the elements reported, and the tensile results including the elongation gauge length. Coils are not qualified as A328 until they have been processed into finished sheet piling. A plate certificate or an H-beam certificate does not, by itself, identify A328 sheet piling.
Applications and Service Limits
ASTM A328 carbon steel sheet piles are used in dock walls, seawalls, cofferdams and excavations where a carbon sheet-piling specification is named. They are not a silent substitute for ASTM A572 Grade 50 steel sheet pile, for ASTM A690 steel sheet pile, or for EN 10248-1 S355GP U-type and Z-type steel sheet pile. Interlocks of similar width are not interchangeable by depth or mass alone.
ASTM A328 Compared with A572, A690 and EN 10248-1
The comparisons below are an orientation only; they are not automatic substitutes.
Near-Equivalents: Not Automatic Substitutes
A near-equivalent is a starting point for a discussion, not a licence to swap certificates. If a project names ASTM A328, keep that specification and geometry on the order. Related pages include ASTM A572 Grade 50 steel sheet pile and ASTM A690 steel sheet pile.
Sourcing ASTM A328 Carbon Steel Sheet Piles from SHH STEEL
SHH STEEL supplies ASTM A328 carbon steel sheet piles against a named geometry, the material edition and the inspection document type. Enquiries should state the type and geometry, the length, whether copper steel is specified, and any coating, corner piles or interlock-strength requirements.
The size tables are typical published mill series, not a claim that every section is rolled in every quality. Once the list is clear, a quotation can be prepared against the stated edition and certificate.
ASTM A328 Carbon Steel Sheet Pile FAQs
-
Is ASTM A328 the same as A572 Grade 50 sheet piling?
- No. A328 is carbon steel sheet piling with a 39 ksi [270 MPa] minimum yield and a 65 ksi [450 MPa] minimum tensile strength. A572 Grade 50 has a 50 ksi [345 MPa] minimum yield. Certify to the specification named on the order.
-
Are the size tables an official ASTM A6 list?
- No. They are typical published mill series described by geometry. Dimensions follow the ordered A6/A6M or project profile series. Trade names are not used.
-
Does A328 specify carbon and manganese?
- The mill reprint used for this page does not specify carbon, manganese or silicon. Phosphorus is 0.035% maximum and sulphur is 0.04% maximum. A 0.20% minimum copper applies when copper steel is specified. The ordered edition governs.
-
Which elongation gauges apply to A328?
- A minimum of 17% in 8 in. [200 mm] and a minimum of 20% in 2 in. [50 mm]. Report the gauge length used on the certificate.
Request a Quotation for ASTM A328 Carbon Steel Sheet Pile
ASTM A328 carbon steel sheet pile is carbon steel sheet piling with a 39 ksi [270 MPa] minimum yield and a 65 ksi [450 MPa] minimum tensile strength. Nominate the geometry, ASTM A328/A328M or the edition on the order, the length, and the inspection document type. Send the size list, edition, certificate type and any processing notes; SHH STEEL will review the package and quote accordingly.