EN 10025-3 S275NL Steel Plate | S275NL Fine Grain Structural Steel - SHH STEEL

EN 10025-3 S275NL Steel Plate | S275NL Fine Grain Structural Steel

EN 10025-3 S275NL is a normalized fine-grain structural steel plate with a minimum yield strength of 275 MPa and impact tested at –50°C. It offers excellent low-temperature toughness, weldability and formability. SHH STEEL is a China Mill-Direct Exporter supplying S275NL steel plate worldwide.
Equivalent material:
ASTM A633 Gr C (-50℃ impact) / JIS SM490A (L variant) / GB Q275E / ISO E275NL
Material Specification:
EN 10025-3 — Delivery: Normalized (N) or Normalized Rolled
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Tolerances
Weldability
Equivalent Material Grades
Applications
Why Choose SHH STEEL
FAQ
Conclusion

What is EN 10025-3 S275NL Steel Plate?

As a professional steel plate supplier and China Mill-Direct Exporter, SHH STEEL is pleased to present EN 10025-3 S275NL Steel Plate (Material Number: 1.0491).

S275NL is a normalized (or normalized rolled) weldable fine-grain structural steel under the European standard EN 10025-3. It provides a minimum yield strength of 275 MPa (for thickness ≤ 16 mm) and is impact tested at –50°C with a minimum energy of 27 J. Compared with S275N, S275NL offers superior low-temperature toughness, making it suitable for colder service environments. SHH STEEL sources this material directly from leading Chinese steel mills, ensuring competitive mill-direct pricing, stable quality and reliable delivery.

We supply S275NL steel plate in thicknesses from 6 mm to 150 mm (thicker plates available on request), widths up to 3000–4000 mm, and lengths up to 12000–18000 mm. Custom cutting, shot blasting and priming services are available. All plates are delivered with full Mill Test Certificates (EN 10204 3.1).

Material Specification

EN 10025-3 S275NL steel plate is produced in accordance with EN 10025-3.

Specification Element Requirement SHH STEEL Compliance
Primary Standard EN 10025-3 Full compliance
Steel Grade S275NL (1.0491) Confirmed
Delivery Condition Normalized (+N) Confirmed
Product Form Steel Plate Available
Thickness Range 6 mm – 150 mm Custom sizes available
Width / Length Up to 3000–4000 mm / 12000–18000 mm Custom cutting supported
Certification EN 10204 3.1 / 3.2 Available

Chemical Composition

According to EN 10025-3, the chemical composition is specified for both ladle analysis (cast analysis) and product analysis.

Ladle Analysis (Cast Analysis)

Element Max. / Range (%)
Carbon (C) ≤ 0.16
Silicon (Si) ≤ 0.40
Manganese (Mn) 0.50 – 1.50
Phosphorus (P) ≤ 0.025
Sulfur (S) ≤ 0.020
Niobium (Nb) ≤ 0.05
Vanadium (V) ≤ 0.05
Aluminium (Al total) ≥ 0.020
Titanium (Ti) ≤ 0.05
Chromium (Cr) ≤ 0.30
Nickel (Ni) ≤ 0.30
Molybdenum (Mo) ≤ 0.10
Copper (Cu) ≤ 0.55
Nitrogen (N) ≤ 0.015

Product Analysis

Element Max. / Range (%)
Carbon (C) ≤ 0.18
Silicon (Si) ≤ 0.45
Manganese (Mn) 0.45 – 1.60
Phosphorus (P) ≤ 0.030
Sulfur (S) ≤ 0.025
Niobium (Nb) ≤ 0.06
Vanadium (V) ≤ 0.07
Aluminium (Al total) ≥ 0.015
Titanium (Ti) ≤ 0.06
Chromium (Cr) ≤ 0.35
Nickel (Ni) ≤ 0.35
Molybdenum (Mo) ≤ 0.13
Copper (Cu) ≤ 0.60
Nitrogen (N) ≤ 0.017

Note:

  • V + Nb + Ti ≤ 0.22%
  • Mo + Cr ≤ 0.30%
  • The minimum Al content does not apply if sufficient other nitrogen-binding elements are present.

Mechanical Properties

Mechanical properties of EN 10025-3 S275NL (longitudinal direction):

Thickness (mm) Yield Strength ReH (min) Tensile Strength Rm Elongation A (min) Impact Energy KV (min)
≤ 16 275 MPa 370 – 510 MPa 24% 27 J at –50°C
> 16 ≤ 40 265 MPa 370 – 510 MPa 24% 27 J at –50°C
> 40 ≤ 63 255 MPa 370 – 510 MPa 24% 27 J at –50°C
> 63 ≤ 80 245 MPa 370 – 510 MPa 23% 27 J at –50°C
> 80 ≤ 100 235 MPa 370 – 510 MPa 23% 27 J at –50°C
> 100 ≤ 150 225 MPa 350 – 480 MPa 23% 27 J at –50°C

Density: 7.85 g/cm³

Delivery Conditions

SHH STEEL, as a China Mill-Direct Supplier, supplies EN 10025-3 S275NL steel plate in the normalized (+N) condition.

Additional options:

  • Shot blasting and shop primer
  • Ultrasonic testing (EN 10160)
  • Z-direction testing (Z15 / Z25 / Z35)
  • Third-party inspection (SGS, BV, TUV, etc.)

Tolerances

Dimensional tolerances for S275NL steel plate follow EN 10029 (for plates).

  • Thickness, width and length tolerances according to the ordered class.
  • Flatness according to EN 10029.
  • Edge conditions: Mill edge or cut edge (flame / plasma).

Tighter tolerances can be provided upon request.

Weldability

S275NL has excellent weldability due to its fine-grain structure, controlled carbon equivalent and low impurity levels. It can be welded by all conventional methods (SMAW, GMAW, FCAW, SAW) without special difficulties.

Recommended welding consumables:

Welding Process Recommended Consumables
SMAW (Stick) E7018, E7016
GMAW (MIG/MAG) ER70S-6
FCAW E71T-1
SAW EM12K + suitable flux

Preheating is generally not required for thin and medium thicknesses. Low-hydrogen consumables are recommended for thicker plates or critical low-temperature applications.

Equivalent Material Grades

Grade Standard Notes
S275NL EN 10025-3 —
1.0491 EN Material number
Q275NL / Q275E GB/T 1591 Closest Chinese equivalents
A633 Grade A (approx.) ASTM Similar fine-grain low-temperature concept
TStE 285 DIN (old) Former designation

Applications

EN 10025-3 S275NL is widely used in structural applications requiring good low-temperature toughness. Typical uses include:

Application Area Typical Components / Uses (Keywords)
Building Structures Beams, columns, frames in cold regions – S275NL Structural Steel
Bridges Bridge components – S275NL Bridge
Machinery Base plates, frames – S275NL Machinery
Low-Temperature Construction Structures requiring –50°C toughness – S275NL Construction
Storage & Tanks Low-temperature storage structures – S275NL Storage
General Fabrication Welded fine-grain structures – S275NL Fabrication

Why Choose SHH STEEL

SHH STEEL is a China Mill-Direct Exporter. We maintain long-term strategic cooperation with major Chinese steel mills and act as a first-level (primary) agent. This direct mill supply model allows us to offer competitive mill-direct pricing, faster delivery times, stable and traceable quality, and full Mill Test Certificates (EN 10204 3.1 / 3.2) for EN 10025-3 S275NL Steel Plate.

Customers benefit from reliable supply, short lead times and cost-effective solutions for fine-grain low-temperature structural steel projects worldwide. Our professional export team provides technical support and customized processing services to meet project requirements.

FAQ

What does the “NL” in S275NL mean?
“NL” indicates that the steel is supplied in the normalized condition and meets impact requirements of minimum 27 J at –50°C.
What is the difference between S275N and S275NL?
Both have the same strength level. S275N is impact tested at –20°C (40 J), while S275NL is impact tested at –50°C (27 J), offering better low-temperature toughness.
What is the material number of S275NL?
1.0491
Is S275NL suitable for low-temperature service?
Yes. With guaranteed impact toughness at –50°C, S275NL is suitable for structural applications in cold environments.

Conclusion

EN 10025-3 S275NL (1.0491) Steel Plate from SHH STEEL is a normalized fine-grain structural steel offering good strength and excellent toughness at –50°C. As a China Mill-Direct Exporter, we provide competitive pricing, fast delivery and consistent quality backed by full mill certifications. Trust SHH STEEL for your S275NL fine grain structural steel plate requirements.

Contact SHH STEEL today for stock availability, pricing and technical support. EN 10025-3 S275NL Steel Plate, S275NL steel plate, S275NL fine grain structural steel, EN 10025 S275NL, S275NL equivalent, S275NL supplier, 1.0491

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X