CNS 13812 SN400YB H-Beam | CNS 13812 H-Beams - SHH STEEL

CNS 13812 SN400YB H-Beam

CNS 13812 SN400YB H-beam is a Taiwanese and Japanese building-structure H-section with a 250 N/mm² yield in the thinner bands, a 400–510 N/mm² tensile range, and a 27 J impact test at 0 °C. The page also covers SN400B, SN490B and SN490YB, and lists the JIS G 3192 H-section series.
Keywords
CNS 13812 SN400YB H-Beam, SN400YB, SN490YB, SN400B, JIS G 3136
Equivalent Grades:
SN400B, SN490B, SN490YB (same family); SM490; Q355B; S355JR — comparisons only, not automatic substitutes.
Share:
General Description
Material Specification
Available Sizes of SN400YB H-Beam
Chemical Composition of SN400YB H-Beam
Mechanical Properties of SN400YB H-Beam
Delivery Conditions, Inspection and Identification
Weldability of SN400YB H-Beams
Shape Tolerances and Theoretical Mass
Applications and Service Limits
SN400YB Compared with SN490, SM490 and Q355B
Near-Equivalents: Not Automatic Substitutes
Sourcing SN400YB H-Beams from SHH STEEL
FAQ
Conclusion

What is CNS 13812 SN400YB H-Beam?

CNS 13812 SN400YB H-beam is a hot-rolled building-structure H-section whose material grade is SN400YB under CNS 13812, the Taiwan standard for rolled steel for building structures. The same SN family is specified in JIS G 3136:2022. SN marks a building-structure steel, 400 is the tensile-strength class (400–510 N/mm²), and YB is the quality with a yield window, a yield-ratio maximum and a 27 J impact requirement at 0 °C when testing applies. Related qualities on this page are SN400B, SN490B and SN490YB.

These beams are filed under steel beam profiles in the steel structural profiles category. The designation is the Japanese or Taiwanese H × B × t1 × t2 string, for example H 300×300×10×15. They are not GB/T 11263 HW, HM or HN sections, and they are not European HEA, HEB or IPE sections of a similar depth. They are also not JIS G 3106 SM490 sections, even when the same JIS G 3192 size table is used.

Material, Dimensions and the SN Quality Family

The purchase order and the inspection document should name, separately:

  • CNS 13812 and its edition (JIS G 3136:2022 may also be named when that is the contract standard); the full quality symbol SN400YB, SN400B, SN490B or SN490YB;
  • the dimensional standard actually used, CNS 1490 or JIS G 3192, and the H × B × t1 × t2 designation;
  • the carbon equivalent or Pcm, and the inspection document type.

SN400A has no standard impact test. SN400C, SN400YC, SN490C and SN490YC have additional through-thickness requirements and dashes in the thinner tensile bands; they should be named only when those qualities are actually ordered.

SN400YB H-Beam Sizes: JIS G 3192 Standard H-Sections

The table is the JIS G 3192:2024 Table 15 standard H-section series already used on the SM490 H-beam page: 53 sizes, from H 100×50×5×7 to H 918×303×19×37. Rows marked * are the 20 sizes that Table 15 identifies as other than general-purpose. The order should name CNS 1490 or JIS G 3192 as the dimensional standard actually required. Constant outside-dimension H-sections and I-beams can be reviewed when they are named. Not every mill rolls every designation in every SN quality; SN400YB is the quality most often produced as a regular programme.

Swipe horizontally to view all dimensions.

Designation (H×B×t1×t2) h (mm) b (mm) t1 (mm) t2 (mm) r (mm) A (cm²) Mass (kg/m)
H 100×50×5×7 100 50 5 7 8 11.85 9.30
H 100×100×6×8 100 100 6 8 8 21.59 16.9
H 125×60×6×8 125 60 6 8 8 16.69 13.1
H 125×125×6.5×9 125 125 6.5 9 8 30.00 23.6
H 150×75×5×7 150 75 5 7 8 17.85 14.0
H 148×100×6×9 148 100 6 9 8 26.35 20.7
H 150×150×7×10 150 150 7 10 8 39.65 31.1
H 175×90×5×8 175 90 5 8 8 22.90 18.0
H 175×175×7.5×11 175 175 7.5 11 13 51.43 40.4
* H 198×99×4.5×7 198 99 4.5 7 8 22.69 17.8
H 200×100×5.5×8 200 100 5.5 8 8 26.67 20.9
H 194×150×6×9 194 150 6 9 8 38.11 29.9
H 200×200×8×12 200 200 8 12 13 63.53 49.9
* H 248×124×5×8 248 124 5 8 8 31.99 25.1
H 250×125×6×9 250 125 6 9 8 36.97 29.0
H 244×175×7×11 244 175 7 11 13 55.49 43.6
H 250×250×9×14 250 250 9 14 13 91.43 71.8
* H 298×149×5.5×8 298 149 5.5 8 13 40.80 32.0
H 300×150×6.5×9 300 150 6.5 9 13 46.78 36.7
H 294×200×8×12 294 200 8 12 13 71.05 55.8
H 300×300×10×15 300 300 10 15 13 118.5 93.0
* H 346×174×6×9 346 174 6 9 13 52.45 41.2
H 350×175×7×11 350 175 7 11 13 62.91 49.4
H 340×250×9×14 340 250 9 14 13 99.53 78.1
H 350×350×12×19 350 350 12 19 13 171.9 135
* H 396×199×7×11 396 199 7 11 13 71.41 56.1
H 400×200×8×13 400 200 8 13 13 83.37 65.4
H 390×300×10×16 390 300 10 16 13 133.3 105
H 400×400×13×21 400 400 13 21 22 218.7 172
* H 414×405×18×28 414 405 18 28 22 295.4 232
* H 428×407×20×35 428 407 20 35 22 360.7 283
* H 458×417×30×50 458 417 30 50 22 528.6 415
* H 498×432×45×70 498 432 45 70 22 770.1 605
* H 446×199×8×12 446 199 8 12 13 82.97 65.1
H 450×200×9×14 450 200 9 14 13 95.43 74.9
H 440×300×11×18 440 300 11 18 13 153.9 121
* H 496×199×9×14 496 199 9 14 13 99.29 77.9
H 500×200×10×16 500 200 10 16 13 112.3 88.2
* H 482×300×11×15 482 300 11 15 13 141.2 111
H 488×300×11×18 488 300 11 18 13 159.2 125
* H 596×199×10×15 596 199 10 15 13 117.8 92.5
H 600×200×11×17 600 200 11 17 13 131.7 103
* H 582×300×12×17 582 300 12 17 13 169.2 133
H 588×300×12×20 588 300 12 20 13 187.2 147
* H 594×302×14×23 594 302 14 23 13 217.1 170
* H 692×300×13×20 692 300 13 20 18 207.5 163
H 700×300×13×24 700 300 13 24 18 231.5 182
* H 792×300×14×22 792 300 14 22 18 239.5 188
H 800×300×14×26 800 300 14 26 18 263.5 207
* H 890×299×15×23 890 299 15 23 18 266.9 210
H 900×300×16×28 900 300 16 28 18 305.8 240
* H 912×302×18×34 912 302 18 34 18 360.1 283
* H 918×303×19×37 918 303 19 37 18 387.4 304

SN400YB and Related SN Chemical Composition

The figures below are heat-analysis maxima as reprinted from CNS 13812 (JIS G 3136:2022). Boron is shown as less than 0.0008%. Carbon equivalent and Pcm are the tabulated maxima; the calculation in the ordered edition of the standard governs, and no formula is invented here. For SN490B the catalog reprints two Ceq maxima, 0.44 and 0.46, in two thickness bands; the 40 mm split is clear for SN490YB (0.44 then 0.46) and is not forced onto SN490B on this page. The edition named on the order governs the applicable band.

Swipe horizontally to view all dimensions.

Grade Thickness (mm) C max Si max Mn P max S max B max Ceq max Pcm max
SN400B 6 ≤ t ≤ 50 0.20 0.35 0.60–1.50 0.030 0.015 0.0008 0.36 0.26
SN400B 50 < t ≤ 100 0.22 0.35 0.60–1.50 0.030 0.015 0.0008 0.36 0.26
SN400YB 6 ≤ t ≤ 100 0.20 0.35 0.60–1.50 0.030 0.015 0.0008 0.36 0.26
SN490B 6 ≤ t ≤ 50 0.18 0.55 1.05 max 0.030 0.015 0.0008 0.44 / 0.46 (two bands; ordered edition governs the cut) 0.29
SN490B 50 < t ≤ 100 0.20 0.55 1.05 max 0.030 0.015 0.0008 0.44 / 0.46 (two bands; ordered edition governs the cut) 0.29
SN490YB 6 ≤ t ≤ 40 0.18 0.55 1.05 max 0.030 0.015 0.0008 0.44 0.29
SN490YB 40 < t ≤ 100 0.18 0.55 1.05 max 0.030 0.015 0.0008 0.46 0.29

SN400YB Mechanical Properties: Yield Window, Tensile and 0 °C Impact

The mechanical values below are those reprinted for section steels with a flange thickness of 6 mm to 40 mm. They are not extended above 40 mm on this page. For H-sections with a web thinner than 9 mm, the upper yield limit in the range columns does not apply, and the yield-ratio maximum is 85% rather than 80%. Thickness for these tables is the flange thickness of the finished section unless the order names another location.

Swipe horizontally to view all dimensions.

Grade Min. or range of yield, thinner bands (N/mm²) Yield at t = 16 mm and 16 < t ≤ 40 mm (N/mm²) Tensile strength (N/mm²) Max. yield ratio (%) Min. elongation, t ≥ 6 mm and t ≤ 16 mm (%) Min. elongation, 16 < t ≤ 40 mm (%) Impact, 0 °C (J)
SN400B ≥ 235 235–355 400–510 80 18 22 27
SN400YB ≥ 250 250–355 400–510 80 20 22 27
SN490B ≥ 325 325–445 490–610 80 17 21 27
SN490YB 325–445 325–445 490–610 80 17 21 27

Impact results are the mean of three tests at 0 °C, 27 J, for the B and YB qualities in this table. An SN400A certificate does not demonstrate that test.

Delivery Conditions, Inspection and Identification

SN H-beams are commonly supplied as-rolled. The inspection document should identify CNS 13812 (or JIS G 3136) and its edition, the full quality symbol, the dimensional standard and designation, heat analysis, Ceq or Pcm, and tensile and impact results against the flange thickness. A plate certificate or an SM490 certificate does not, by itself, identify an SN400YB H-beam.

Weldability of SN400YB H-Beams

SN steels are specified as building-structure steels with a published Ceq and Pcm. Preheat and consumable choice should use the certified heat analysis, the certified Ceq or Pcm, the actual flange thickness and the joint design. The calculation in the ordered edition of the standard should be the one used on the certificate.

CNS 1490 or JIS G 3192 Shape Tolerances and Theoretical Mass

Shape, mass and tolerances belong to the dimensional standard named on the order, ordinarily CNS 1490 or JIS G 3192. Mass in the size table is the published theoretical figure for the JIS G 3192:2024 Table 15 series. Millimetre tolerance tables are not reproduced here.

Applications and Service Limits

SN400YB H-beams are used in building frames where a Taiwanese or Japanese SN building-structure grade, a yield window and a 0 °C impact test are specified. They are not a silent substitute for JIS G 3106 SM490 H-beam, for GB/T 11263 Q355B H-beam, or for a European S355 section.

SN400YB Compared with SN490, SM490 and Q355B

The comparisons below are an orientation only; they are not automatic substitutes.

Grade / designation Standard Relationship to SN400YB H-beam Caution
SN400B / SN490B / SN490YB CNS 13812; JIS G 3136:2022 Related SN qualities on this page, with their own yield window, carbon table or 490 N/mm² tensile class. A, B, YB and C are not interchangeable. SN400A has no standard impact test.
SM490 H-beam JIS G 3106; dimensions JIS G 3192 A Japanese welded-structure comparison, not an SN building-structure grade. SM490 is not SN490YB. See JIS G 3106 SM490 H-beam.
Q355B / S355JR GB/T 1591 or EN 10025-2, with their own dimensional standards 355 MPa-class comparisons used in export enquiries. An HW or IPE is not a JIS or CNS H-section. See GB/T 11263 Q355B H-beam and EN 10025-2 S355JR H-beam.

Near-Equivalents: Not Automatic Substitutes

A near-equivalent is a starting point for a discussion, not a licence to swap certificates. If a project names SN400YB or SN490YB, keep that quality letter, CNS 13812 or JIS G 3136, and the dimensional standard on the order.

Sourcing SN400YB H-Beams from SHH STEEL

SHH STEEL supplies CNS 13812 SN400YB H-beams, and the related SN400B, SN490B and SN490YB qualities, against a named designation list, the material edition and the inspection document type. Enquiries should state the H × B × t1 × t2 designations, the quality letter, whether CNS 1490 or JIS G 3192 is required, cut lengths or mill lengths, and any processing.

The size table is the standard series, not a claim that every designation is rolled in every quality. Once the list is clear, a quotation can be prepared against the stated edition and certificate.

SN400YB H-Beam FAQs

Is SN400YB the same as SN400B or SM490?
No. SN400YB has a 250 N/mm² lower yield in the thinner bands, a 250–355 N/mm² yield window in the thicker tabulated bands, a yield-ratio maximum and a 0 °C / 27 J impact test. SN400B uses a 235 N/mm² lower yield and a different elongation table. SM490 is a JIS G 3106 welded-structure grade, not an SN building-structure grade.
Do the mechanical tables apply above 40 mm?
The tabulated mechanical values on this page are those reprinted for finished sections with a flange thickness of 6 mm to 40 mm. Values above 40 mm are not invented here; they should be taken from the ordered edition of CNS 13812 or JIS G 3136, or agreed on the order.
Which dimensional standard should be named?
Name CNS 1490 or JIS G 3192, as the contract requires. The size table is the JIS G 3192 Table 15 series, used as reference dimensions. The edition named on the order governs mass and tolerances.
Which material edition is used on this page?
The numeric tables follow the CNS 13812 / JIS G 3136:2022 reprint in the mill catalog used for this page. The edition named on the order governs.

Request a Quotation for CNS 13812 SN400YB H-Beam

CNS 13812 SN400YB H-beam is a building-structure H-section with a 250 N/mm² yield in the thinner bands and a 27 J impact requirement at 0 °C. Nominate the H × B × t1 × t2 designation, the quality letter, CNS 13812 or JIS G 3136 and the dimensional standard on the order, and the inspection document type. Send the size list, quality, edition, certificate type and any processing notes; SHH STEEL will review the package and quote accordingly.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X