ASTM A841 Grade G Class 9 Steel Plate | A841/A841M TMCP Vessel Plate
What is ASTM A841 Grade G Class 9 steel plate?
ASTM A841 Grade G Class 9 covers killed, fine-austenitic-grain steel plate produced by the thermo-mechanical control process under ASTM A841/A841M. The plates are intended primarily for welded pressure vessels. Low-temperature high-nickel tmcp vessels and related equipment ordered to astm a841 grade g class 9.
Sits between Class 8 (550 MPa, to 40 mm) and Class 10 (620 MPa, to 50 mm). Forming temperature for Grade G is limited to 530 C when 6.1 is met. Magnet handling after heat treatment needs care because Grade G is susceptible to magnetization.
This page treats ASTM A841 as the base product standard. ASME SA-841/SA-841M is the related specification used for ASME Boiler and Pressure Vessel Code applications. Cross-link to the live code page: ASME SA841 Grade G Class 9. Hubs: ASTM A841 · ASME SA841 · Pipeline Steel Plates.
Same-Grade Classes: ASTM A841 Grade G Class 8 · Grade G Class 9 (this page) · ASTM A841 Grade G Class 10. Other ASTM A841 pages: Grade A Class 1 · Grade B Class 2 · Grade C Class 1 · Grade D Class 3 · Grade E Class 4 · Grade F Class 7 · Grade G Class 10 · Grade A Class 2 · Grade B Class 1 · Grade C Class 2 · Grade E Class 5 · Grade F Class 6 · Grade G Class 8.
Material Specification for ASTM A841 Grade G Class 9
| Parameter | Specification |
|---|---|
| Standard | ASTM A841/A841M (primary reference A841/A841M-17; confirm ordered edition on the MTC) |
| Grade / Class | Grade G Class 9 |
| Companion ASME spec | SA-841/SA-841M Grade G Class 9 (SA841 product page) |
| General requirements | ASTM A20/A20M |
| Family | TMCP steel plates for pressure vessels |
| Product form | Plate (hot-rolled TMCP) |
| Maximum nominal thickness (Grade G) | 50 mm |
| Class tensile window | Class 9 covers both <=40 mm and 40-50 mm bands. Grade G max 50 mm. |
| Delivery condition | TMCP (thermo-mechanical control process); stamped TMC |
| Grain practice | Killed; fine austenitic grain size per A20 |
| Surface / edge | As-rolled or shot blasted; mill edge or cut edge |
| Dimensional practice | ASTM A20/A20M |
| Certification | EN 10204 3.1 / 3.2; dual ASTM A841 + ASME SA-841 marking when ordered |
| Density | 7.85 g/cm³ |
Chemical Composition of ASTM A841 Grade G Class 9 (heat and product analysis)
Heat (ladle) analysis limits below follow ASTM A841/A841M Table 1 for Grade G. Product analysis, when performed, shall stay within Table 2 tolerances relative to those heat limits (Product analysis, when made, shall not deviate from heat-analysis limits by more than ASTM A841/A841M Table 2 tolerances (and A20 practice as applicable).). Always verify the ordered edition and the mill test certificate before fabrication or substitution.
| Element | Heat analysis (Grade G) | Product analysis note |
|---|---|---|
| Carbon (C) | <=0.13 | Table 2 tolerance vs heat limit |
| Manganese (Mn), t <= 40 mm | 0.60-1.20 | Table 2 tolerance vs heat limit |
| Manganese (Mn), t > 40 mm | 0.60-1.20 (Grade G to 50 mm) | Table 2 tolerance vs heat limit |
| Phosphorus (P) | <=0.015 | Table 2 tolerance vs heat limit |
| Sulfur (S) | <=0.015 | Table 2 tolerance vs heat limit |
| Silicon (Si) | 0.04-0.15 (Si may be <0.04 if total Al >=0.030 or acid-soluble Al >=0.025) | Table 2 tolerance vs heat limit |
| Copper (Cu) | No requirement | No Table 1 limit; product analysis N/A unless ordered |
| Nickel (Ni) | 6.0-7.5 | Table 2 tolerance vs heat limit |
| Chromium (Cr) | 0.30-1.00 | Table 2 tolerance vs heat limit |
| Molybdenum (Mo) | <=0.30 | Table 2 tolerance vs heat limit |
| Niobium (Nb / Cb) | No requirement | No Table 1 limit; product analysis N/A unless ordered |
| Vanadium (V) | No requirement | No Table 1 limit; product analysis N/A unless ordered |
| Titanium (Ti) | No requirement | No Table 1 limit; product analysis N/A unless ordered |
| Boron (B) | No requirement | No Table 1 limit; product analysis N/A unless ordered |
| Aluminum (Al) | >=0.008 acid soluble | Table 2 tolerance vs heat limit |
High-nickel TMCP grade. Susceptible to magnetization. Default CVN is transverse at -195 C unless ordered otherwise.
Mechanical Properties of ASTM A841 Grade G Class 9
Tensile requirements for Grade G Class 9 from ASTM A841/A841M Table 3. Two tension tests are required from each plate-as-rolled (one corner coupon from each end). If warm forming or PWHT will be applied, order simulated heat treatment of test coupons (A20 S3 / A841 6.1).
| Property | t <= 40 mm | 40 mm < t <= 50 mm |
|---|---|---|
| Yield strength, min | 585 MPa (85 ksi) | 585 MPa (85 ksi) |
| Tensile strength | 690-825 MPa (100-120 ksi) | 690-825 MPa (100-120 ksi) |
| Elongation in 50 mm (2 in), min | 20% | 20% |
| Density (approx.) | 7.85 g/cm³ | 7.85 g/cm³ |
Class 9 covers both <=40 mm and 40-50 mm bands. Grade G max 50 mm.
Notch toughness (default if not specified on the PO): Transverse CVN per A20. Default if not ordered: -320 F [-195 C]. Lateral expansion opposite the notch >=0.015 in [0.38 mm] up to 1.25 in [31.75 mm] inclusive; >=0.019 in [0.48 mm] at 2.0 in [50 mm]; interpolate between. Purchaser-specified CVN packages override these defaults when written on the order.
Delivery Conditions for Grade G Class 9 (TMCP)
Grade G Class 9 shall be produced by the thermo-mechanical control process. ASTM A841 is not an as-rolled carbon plate book and is not a quenched-and-tempered vessel-plate book. Each plate is legibly stamped with TMC following the stamped specification designation.
Forming / PWHT: Grade G forming not exceeding 985 F [530 C] when 6.1 is met. Grade G is susceptible to magnetization; avoid magnet handling after heat treatment if residual magnetism would harm fabrication or service. If warm forming or PWHT will be used, the order must state temperatures and times so test coupons can be simulated (A841 6.1 / A20 S3).
Because TMCP strength and toughness come from the rolling schedule, re-normalizing or uncontrolled high-temperature forming can destroy the as-delivered property package. State fabrication heat cycles on the purchase order.
Weldability of Grade G Class 9
Grade G Class 9 is intended for welded construction. Qualify WPS/PQR to the project code (ASME IX when the vessel is code-stamped, or the applicable fabrication standard). Prefer low-hydrogen consumables matched to the strength and toughness package. Preheat and interpass follow thickness, carbon equivalent, joint restraint and the approved procedure.
Grade G is a 6.0-7.5% Ni TMCP alloy. Use nickel-compatible welding practice, respect the 530 C forming limit, and control residual magnetism if it would interfere with fabrication or NDE.
Related pages: ASME SA841 Grade G Class 9 · ASTM A841 Grade G Class 8 · Grade G Class 9 (this page) · ASTM A841 Grade G Class 10.
Dimensional Tolerances for Grade G Class 9
Dimensional tolerances for Grade G Class 9 follow ASTM A20/A20M unless the purchase order cites another agreement. Flatness, width, length and edge condition should be stated for nested vessel courses and head blanks.
Respect the Grade G maximum nominal thickness of 50 mm and the Class 9 tensile thickness bands. Ultrasonic examination, when required, is ordered via A20 supplementary requirements or A435 / A577 / A578 as applicable.
Applications and service limits for Grade G Class 9
Typical purchasing contexts for Grade G Class 9:
- Welded pressure vessels ordered to ASTM A841 (base standard) with or without dual ASME SA-841 marking
- Storage tanks and process vessels that specify TMCP vessel plate rather than normalized A516 / SA516
- Export dual-cert packages listing both ASTM A841 and ASME SA-841 Grade G Class 9
- Low-temperature high-nickel TMCP vessels (not automatic 9% Ni substitution)
Forming temperature for Grade G is limited to 530 C when 6.1 is met. Magnet handling after heat treatment needs care because Grade G is susceptible to magnetization.
Related: ASME SA841 Grade G Class 9 · ASTM A841 hub · ASME SA841 hub · Pipeline Steel Plates · Grade A Class 1 · Grade B Class 2 · Grade C Class 1 · Grade D Class 3 · Grade E Class 4 · Grade F Class 7 · Grade G Class 10 · Grade A Class 2 · Grade B Class 1 · Grade C Class 2 · Grade E Class 5 · Grade F Class 6 · Grade G Class 8.
ASTM A841 vs ASME SA-841 for Grade G Class 9 (code acceptance and MTC)
ASTM A841/A841M is the ASTM International product specification for TMCP pressure-vessel plates. ASME SA-841/SA-841M is the related specification adopted for ASME BPVC Section II use. Chemistries and tensile Class tables are aligned; the procurement difference is usually code acceptance, stamping language and how the MTC references the books.
| Topic | ASTM A841 (this page) | ASME SA-841 |
|---|---|---|
| Role | Base ASTM product standard | Code-adopted companion for ASME BPVC work |
| Typical PO text | ASTM A841 Grade G Class 9 | ASME SA-841 Grade G Class 9 / SA841 Gr.G Cl.9 |
| MTC practice | Report A841 edition, Grade, Class, TMCP/TMC, chemistry, tensile, CVN | Report SA-841 (and often dual A841) when ASME code stamping is required |
| General reqs | ASTM A20/A20M | ASME SA-20 / ASTM A20 pathway |
| Product page | This page | ASME SA841 Grade G Class 9 |
Dual certification is available when the mill produces one plate that meets both books and marks both designations. A purchase order that only says Grade letter without Class is incomplete for every A841/SA-841 combination.
Equivalent and related grades for ASTM A841 Grade G Class 9
These designations are commonly compared with ASTM A841 Grade G Class 9. They are approximate, not automatic substitutes.
| Standard / family | Grade | Relation | Product page |
|---|---|---|---|
| ASTM A841/A841M | Grade G Class 9 | This page | – |
| ASME SA-841/SA-841M | Grade G Class 9 | Code companion | SA841 matching page |
| ASTM A841/A841M | Grade G Class 8 | Same Grade, different Class | Grade G Class 8 |
| ASTM A841/A841M | Grade G Class 10 | Same Grade, different Class | Grade G Class 10 |
| EN 10028-5 | P355M / P460M / P460ML talk | TMCP vessel comparison only | – |
| ASTM A537 / ASME SA537 | Cl.1 / Cl.2 | Heat-treated C-Mn-Si; not TMCP A841 | – |
| API 5L / ISO 3183 | PSL2 TMCP pipe grades | Line-pipe track; different product form rules | Pipeline Steel Plates |
| Category | A841 / SA841 hubs | Family navigation | ASTM A841 · ASME SA841 |
ASTM A841 Grade G Class 9 vs sibling Classes / related Grades (selection aid)
Selection aid for ASTM A841 Grade G Class 9. Same-Grade Classes share chemistry; Class sets the tensile package. Cross-Grade rows are not substitutes.
| Designation | Yield (primary band) | Tensile (primary band) | Grade thickness cap | Page |
|---|---|---|---|---|
| Grade G Class 8 | 550 MPa | 620-760 MPa | 50 mm grade max | Grade G Class 8 |
| Grade G Class 9 | 585 MPa | 690-825 MPa | 50 mm grade max | This page |
| Grade G Class 10 | 620 MPa | 750-885 MPa | 50 mm grade max | Grade G Class 10 |
| Grade D Class 3 | 690 MPa | 1000-1170 MPa | 40 mm | Grade D Class 3 (Ni 1.0-5.0%, not 6.0-7.5%) |
Why choose SHH STEEL for ASTM A841 Grade G Class 9
- China mill-direct supply of ASTM A841/A841M Grade G Class 9 TMCP vessel plate
- EN 10204 3.1 mill test certificates; 3.2 and third-party inspection (SGS, TUV, BV, ABS) on request
- Dual ASTM A841 + ASME SA-841 marking when ordered (see matching SA841 page)
- Grade G thickness window respected (max 50 mm); Class 9 tensile and CVN packages as ordered
- Cutting, beveling and shot blasting available to shorten fabrication lead time
- Family coverage: ASTM A841 hub · ASME SA841 hub · Pipeline Steel Plates · ASTM A841 Grade G Class 8 · Grade G Class 9 (this page) · ASTM A841 Grade G Class 10
Supply, cutting and inspection for Grade G Class 9
| Item | SHH STEEL supply note |
|---|---|
| Thickness | Within Grade G max 50 mm and Class 9 tensile bands; confirm mill capability on enquiry |
| Size | Width and length per mill rolling; cut-to-size / nest sizes on request |
| Delivery condition | TMCP (TMC stamped); not normalized-only or Q&T unless a different standard is ordered |
| Processing | Cutting, beveling, shot blasting available |
| Mill certificate | EN 10204 3.1 standard; 3.2 on request; dual A841/SA-841 when ordered |
| Third-party inspection | SGS, TUV, BV or ABS can be arranged |
| Quotation needs | ASTM A841 Grade G Class 9, thickness x width x length, quantity, CVN package, warm-forming/PWHT simulation if any, dual SA-841 mark yes/no, inspection level |
FAQ
-
Is ASTM A841 the same as ASME SA841?
- They are companion specifications. ASTM A841/A841M is the ASTM base product standard. ASME SA-841/SA-841M is used for ASME BPVC applications. See ASME SA841 Grade G Class 9 and the ASTM vs ASME section on this page.
-
What Class combinations exist for Grade G?
- ASTM A841 Grade G Class 8 · Grade G Class 9 (this page) · ASTM A841 Grade G Class 10. Class sets the tensile package; Grade sets chemistry and thickness cap.
-
What is the maximum thickness for Grade G?
- 50 mm nominal maximum under ASTM A841/A841M. Class 9 tensile bands: Class 9 covers both <=40 mm and 40-50 mm bands. Grade G max 50 mm.
-
What CVN defaults apply if the PO is silent?
- Transverse CVN per A20. Default if not ordered: -320 F [-195 C]. Lateral expansion opposite the notch >=0.015 in [0.38 mm] up to 1.25 in [31.75 mm] inclusive; >=0.019 in [0.48 mm] at 2.0 in [50 mm]; interpolate between. Always prefer an explicit CVN package on the order.
-
Can A841 plate replace API 5L pipeline plate?
- Not automatically. A841 is a pressure-vessel TMCP plate specification. Pipeline plate / line-pipe rules sit under API 5L, ISO 3183 or project annexes. See Pipeline Steel Plates.
Request a quotation
Send ASTM A841 Grade G Class 9, thickness x width x length, quantity, CVN package, any warm-forming/PWHT simulation temperatures, dual ASME SA-841 marking requirement, and inspection level. SHH STEEL will return mill availability, certification scope and a quotation.
Contact: admin@steelspecs.com · +86-18939509537 · +86-021-62716097
More options: ASTM A841 · ASME SA841 Grade G Class 9 · ASME SA841 hub · Pipeline Steel Plates · ASTM A841 Grade G Class 8 · Grade G Class 9 (this page) · ASTM A841 Grade G Class 10