ASTM A841 Grade B Class 2 Steel Plate | A841/A841M TMCP Vessel Plate
What is ASTM A841 Grade B Class 2 steel plate?
ASTM A841 Grade B Class 2 covers killed, fine-austenitic-grain steel plate produced by the thermo-mechanical control process under ASTM A841/A841M. The plates are intended primarily for welded pressure vessels. Tmcp vessel shells, penstock and high-toughness tank talk when the po cites a841 gr.b cl.2, and dual mark packages with sa-841 gr.b cl.2.
Class 2 on Grade B shares tensile numbers with Class 2 on Grades A and C, but chemistry stays Grade B. Mills often dual-certify ASTM A841 Grade B Class 2 with ASME SA-841 Grade B Class 2 when both books are listed. Code stamping for ASME Section VIII still follows the SA- designation path and the applicable code year.
This page treats ASTM A841 as the base product standard. ASME SA-841/SA-841M is the related specification used for ASME Boiler and Pressure Vessel Code applications. Cross-link to the live code page: ASME SA841 Grade B Class 2. Hubs: ASTM A841 · ASME SA841 · Pipeline Steel Plates.
Same-Grade Classes: ASTM A841 Grade B Class 1 · Grade B Class 2 (this page). Other ASTM A841 pages: Grade A Class 1 · Grade C Class 1 · Grade D Class 3 · Grade E Class 4 · Grade F Class 7 · Grade G Class 10 · Grade A Class 2 · Grade B Class 1 · Grade C Class 2 · Grade E Class 5 · Grade F Class 6 · Grade G Class 8 · Grade G Class 9.
Material Specification for ASTM A841 Grade B Class 2
| Parameter | Specification |
|---|---|
| Standard | ASTM A841/A841M (primary reference A841/A841M-17; confirm ordered edition on the MTC) |
| Grade / Class | Grade B Class 2 |
| Companion ASME spec | SA-841/SA-841M Grade B Class 2 (SA841 product page) |
| General requirements | ASTM A20/A20M |
| Family | TMCP steel plates for pressure vessels |
| Product form | Plate (hot-rolled TMCP) |
| Maximum nominal thickness (Grade B) | 100 mm |
| Class tensile window | Grade max 100 mm for A/B/C; Class 2 tensile bands cover <=65 mm and >65 mm. |
| Delivery condition | TMCP (thermo-mechanical control process); stamped TMC |
| Grain practice | Killed; fine austenitic grain size per A20 |
| Surface / edge | As-rolled or shot blasted; mill edge or cut edge |
| Dimensional practice | ASTM A20/A20M |
| Certification | EN 10204 3.1 / 3.2; dual ASTM A841 + ASME SA-841 marking when ordered |
| Density | 7.85 g/cm³ |
Chemical Composition of ASTM A841 Grade B Class 2 (heat and product analysis)
Heat (ladle) analysis limits below follow ASTM A841/A841M Table 1 for Grade B. Product analysis, when performed, shall stay within Table 2 tolerances relative to those heat limits (Product analysis, when made, shall not deviate from heat-analysis limits by more than ASTM A841/A841M Table 2 tolerances (and A20 practice as applicable).). Always verify the ordered edition and the mill test certificate before fabrication or substitution.
| Element | Heat analysis (Grade B) | Product analysis note |
|---|---|---|
| Carbon (C) | <=0.15 | Table 2 tolerance vs heat limit |
| Manganese (Mn), t <= 40 mm | 0.70-1.35 | Table 2 tolerance vs heat limit |
| Manganese (Mn), t > 40 mm | 1.00-1.60 | Table 2 tolerance vs heat limit |
| Phosphorus (P) | <=0.030 | Table 2 tolerance vs heat limit |
| Sulfur (S) | <=0.025 | Table 2 tolerance vs heat limit |
| Silicon (Si) | 0.15-0.50 | Table 2 tolerance vs heat limit |
| Copper (Cu) | <=0.35 | Table 2 tolerance vs heat limit |
| Nickel (Ni) | <=0.60 | Table 2 tolerance vs heat limit |
| Chromium (Cr) | <=0.25 | Table 2 tolerance vs heat limit |
| Molybdenum (Mo) | <=0.30 | Table 2 tolerance vs heat limit |
| Niobium (Nb / Cb) | <=0.03 | Table 2 tolerance vs heat limit |
| Vanadium (V) | <=0.06 | Table 2 tolerance vs heat limit |
| Titanium (Ti) | By agreement 0.006-0.02 (then Al min waived) | Table 2 tolerance vs heat limit |
| Boron (B) | – | No Table 1 requirement |
| Aluminum (Al) | >=0.020 total or >=0.015 acid soluble (unless Ti option) | Table 2 tolerance vs heat limit |
Mn may rise per CE note. Higher Ni and Mo caps than Grade A.
CE option (Grades A/B): For Grades A and B, manganese may exceed 1.35% on heat analysis up to 1.60% provided CE on heat analysis does not exceed 0.47% (or S77 value when invoked), using CE = C + Mn/6 + (Cr+Mo+V)/5 + (Ni+Cu)/15. When that option is used, product-analysis Mn shall not exceed heat-analysis Mn by more than 0.12 percentage points.
Mechanical Properties of ASTM A841 Grade B Class 2
Tensile requirements for Grade B Class 2 from ASTM A841/A841M Table 3. Two tension tests are required from each plate-as-rolled (one corner coupon from each end). If warm forming or PWHT will be applied, order simulated heat treatment of test coupons (A20 S3 / A841 6.1).
| Property | t <= 65 mm | t > 65 mm |
|---|---|---|
| Yield strength, min | 415 MPa (60 ksi) | 380 MPa (55 ksi) |
| Tensile strength | 550-690 MPa (80-100 ksi) | 515-655 MPa (75-95 ksi) |
| Elongation in 50 mm (2 in), min | 22% | 22% |
| Elongation in 200 mm (8 in), min | 18% | 18% |
| Density (approx.) | 7.85 g/cm³ | 7.85 g/cm³ |
Grade max 100 mm for A/B/C; Class 2 tensile bands cover <=65 mm and >65 mm.
Notch toughness (default if not specified on the PO): Longitudinal CVN per A20. Default if not ordered: -40 C (-40 F), average >=15 ft-lbf [20 J] for three full-size specimens. Purchaser-specified CVN packages override these defaults when written on the order.
Delivery Conditions for Grade B Class 2 (TMCP)
Grade B Class 2 shall be produced by the thermo-mechanical control process. ASTM A841 is not an as-rolled carbon plate book and is not a quenched-and-tempered vessel-plate book. Each plate is legibly stamped with TMC following the stamped specification designation.
Forming / PWHT: Warm forming / PWHT not exceeding 1200 F [650 C] when 6.1 simulated-coupon requirements are met. If warm forming or PWHT will be used, the order must state temperatures and times so test coupons can be simulated (A841 6.1 / A20 S3).
Because TMCP strength and toughness come from the rolling schedule, re-normalizing or uncontrolled high-temperature forming can destroy the as-delivered property package. State fabrication heat cycles on the purchase order.
Weldability of Grade B Class 2
Grade B Class 2 is intended for welded construction. Qualify WPS/PQR to the project code (ASME IX when the vessel is code-stamped, or the applicable fabrication standard). Prefer low-hydrogen consumables matched to the strength and toughness package. Preheat and interpass follow thickness, carbon equivalent, joint restraint and the approved procedure.
Grades A and B allow a controlled Mn/CE option on heat analysis. Review CE on the MTC before fixing preheat. For Grades A and B, manganese may exceed 1.35% on heat analysis up to 1.60% provided CE on heat analysis does not exceed 0.47% (or S77 value when invoked), using CE = C + Mn/6 + (Cr+Mo+V)/5 + (Ni+Cu)/15. When that option is used, product-analysis Mn shall not exceed heat-analysis Mn by more than 0.12 percentage points.
Related pages: ASME SA841 Grade B Class 2 · ASTM A841 Grade B Class 1 · Grade B Class 2 (this page).
Dimensional Tolerances for Grade B Class 2
Dimensional tolerances for Grade B Class 2 follow ASTM A20/A20M unless the purchase order cites another agreement. Flatness, width, length and edge condition should be stated for nested vessel courses and head blanks.
Respect the Grade B maximum nominal thickness of 100 mm and the Class 2 tensile thickness bands. Ultrasonic examination, when required, is ordered via A20 supplementary requirements or A435 / A577 / A578 as applicable.
Applications and service limits for Grade B Class 2
Typical purchasing contexts for Grade B Class 2:
- Welded pressure vessels ordered to ASTM A841 (base standard) with or without dual ASME SA-841 marking
- Storage tanks and process vessels that specify TMCP vessel plate rather than normalized A516 / SA516
- Export dual-cert packages listing both ASTM A841 and ASME SA-841 Grade B Class 2
- Fabricated equipment where TMCP is preferred over heat-treated A537 for the same yield window
- RFQs that mention pipeline or penstock TMCP plate but still cite A841 as the vessel-plate document (confirm governing spec)
Mills often dual-certify ASTM A841 Grade B Class 2 with ASME SA-841 Grade B Class 2 when both books are listed. Code stamping for ASME Section VIII still follows the SA- designation path and the applicable code year.
Related: ASME SA841 Grade B Class 2 · ASTM A841 hub · ASME SA841 hub · Pipeline Steel Plates · Grade A Class 1 · Grade C Class 1 · Grade D Class 3 · Grade E Class 4 · Grade F Class 7 · Grade G Class 10 · Grade A Class 2 · Grade B Class 1 · Grade C Class 2 · Grade E Class 5 · Grade F Class 6 · Grade G Class 8 · Grade G Class 9.
ASTM A841 vs ASME SA-841 for Grade B Class 2 (code acceptance and MTC)
ASTM A841/A841M is the ASTM International product specification for TMCP pressure-vessel plates. ASME SA-841/SA-841M is the related specification adopted for ASME BPVC Section II use. Chemistries and tensile Class tables are aligned; the procurement difference is usually code acceptance, stamping language and how the MTC references the books.
| Topic | ASTM A841 (this page) | ASME SA-841 |
|---|---|---|
| Role | Base ASTM product standard | Code-adopted companion for ASME BPVC work |
| Typical PO text | ASTM A841 Grade B Class 2 | ASME SA-841 Grade B Class 2 / SA841 Gr.B Cl.2 |
| MTC practice | Report A841 edition, Grade, Class, TMCP/TMC, chemistry, tensile, CVN | Report SA-841 (and often dual A841) when ASME code stamping is required |
| General reqs | ASTM A20/A20M | ASME SA-20 / ASTM A20 pathway |
| Product page | This page | ASME SA841 Grade B Class 2 |
Dual certification is available when the mill produces one plate that meets both books and marks both designations. A purchase order that only says Grade letter without Class is incomplete for every A841/SA-841 combination.
Equivalent and related grades for ASTM A841 Grade B Class 2
These designations are commonly compared with ASTM A841 Grade B Class 2. They are approximate, not automatic substitutes.
| Standard / family | Grade | Relation | Product page |
|---|---|---|---|
| ASTM A841/A841M | Grade B Class 2 | This page | – |
| ASME SA-841/SA-841M | Grade B Class 2 | Code companion | SA841 matching page |
| ASTM A841/A841M | Grade B Class 1 | Same Grade, different Class | Grade B Class 1 |
| EN 10028-5 | P355M / P460M / P460ML talk | TMCP vessel comparison only | – |
| ASTM A537 / ASME SA537 | Cl.1 / Cl.2 | Heat-treated C-Mn-Si; not TMCP A841 | – |
| API 5L / ISO 3183 | PSL2 TMCP pipe grades | Line-pipe track; different product form rules | Pipeline Steel Plates |
| Category | A841 / SA841 hubs | Family navigation | ASTM A841 · ASME SA841 |
ASTM A841 Grade B Class 2 vs sibling Classes / related Grades (selection aid)
Selection aid for ASTM A841 Grade B Class 2. Same-Grade Classes share chemistry; Class sets the tensile package. Cross-Grade rows are not substitutes.
| Designation | Yield (primary band) | Tensile (primary band) | Grade thickness cap | Page |
|---|---|---|---|---|
| Grade B Class 1 | 345 MPa | 485-620 MPa | 100 mm grade max | Grade B Class 1 |
| Grade B Class 2 | 415 MPa | 550-690 MPa | 100 mm grade max | This page |
| Grade A Class 2 | same Class tensile | same Class tensile | 100 mm | Grade A Class 2 (different chemistry) |
Why choose SHH STEEL for ASTM A841 Grade B Class 2
- China mill-direct supply of ASTM A841/A841M Grade B Class 2 TMCP vessel plate
- EN 10204 3.1 mill test certificates; 3.2 and third-party inspection (SGS, TUV, BV, ABS) on request
- Dual ASTM A841 + ASME SA-841 marking when ordered (see matching SA841 page)
- Grade B thickness window respected (max 100 mm); Class 2 tensile and CVN packages as ordered
- Cutting, beveling and shot blasting available to shorten fabrication lead time
- Family coverage: ASTM A841 hub · ASME SA841 hub · Pipeline Steel Plates · ASTM A841 Grade B Class 1 · Grade B Class 2 (this page)
Supply, cutting and inspection for Grade B Class 2
| Item | SHH STEEL supply note |
|---|---|
| Thickness | Within Grade B max 100 mm and Class 2 tensile bands; confirm mill capability on enquiry |
| Size | Width and length per mill rolling; cut-to-size / nest sizes on request |
| Delivery condition | TMCP (TMC stamped); not normalized-only or Q&T unless a different standard is ordered |
| Processing | Cutting, beveling, shot blasting available |
| Mill certificate | EN 10204 3.1 standard; 3.2 on request; dual A841/SA-841 when ordered |
| Third-party inspection | SGS, TUV, BV or ABS can be arranged |
| Quotation needs | ASTM A841 Grade B Class 2, thickness x width x length, quantity, CVN package, warm-forming/PWHT simulation if any, dual SA-841 mark yes/no, inspection level |
FAQ
-
Is ASTM A841 the same as ASME SA841?
- They are companion specifications. ASTM A841/A841M is the ASTM base product standard. ASME SA-841/SA-841M is used for ASME BPVC applications. See ASME SA841 Grade B Class 2 and the ASTM vs ASME section on this page.
-
What Class combinations exist for Grade B?
- ASTM A841 Grade B Class 1 · Grade B Class 2 (this page). Class sets the tensile package; Grade sets chemistry and thickness cap.
-
What is the maximum thickness for Grade B?
- 100 mm nominal maximum under ASTM A841/A841M. Class 2 tensile bands: Grade max 100 mm for A/B/C; Class 2 tensile bands cover <=65 mm and >65 mm.
-
What CVN defaults apply if the PO is silent?
- Longitudinal CVN per A20. Default if not ordered: -40 C (-40 F), average >=15 ft-lbf [20 J] for three full-size specimens. Always prefer an explicit CVN package on the order.
-
Can A841 plate replace API 5L pipeline plate?
- Not automatically. A841 is a pressure-vessel TMCP plate specification. Pipeline plate / line-pipe rules sit under API 5L, ISO 3183 or project annexes. See Pipeline Steel Plates.
Request a quotation
Send ASTM A841 Grade B Class 2, thickness x width x length, quantity, CVN package, any warm-forming/PWHT simulation temperatures, dual ASME SA-841 marking requirement, and inspection level. SHH STEEL will return mill availability, certification scope and a quotation.
Contact: admin@steelspecs.com · +86-18939509537 · +86-021-62716097
More options: ASTM A841 · ASME SA841 Grade B Class 2 · ASME SA841 hub · Pipeline Steel Plates · ASTM A841 Grade B Class 1 · Grade B Class 2 (this page)