ASTM A841 Grade A Class 1 Steel Plate | ASTM A841 Pressure Vessel Steel - SHH STEEL

ASTM A841 Grade A Class 1 Steel Plate | A841/A841M TMCP Vessel Plate

ASTM A841 Grade A Class 1 is TMCP steel plate under ASTM A841/A841M for welded pressure vessels. It is the entry Class 1 strength line on Grade A under the ASTM base TMCP vessel-plate book. Minimum yield on the primary thickness band is 345 MPa (50 ksi) with tensile 485-620 MPa (70-90 ksi). Maximum nominal thickness for Grade A is 100 mm. SHH STEEL supplies Grade A Class 1 plate with EN 10204 3.1 (or 3.2) mill test certificates. Matching ASME code page: ASME SA841 Grade A Class 1 Steel Plate.
Equivalent Grades:
Companion code name: ASME SA-841/SA-841M Grade A Class 1 (see https://www.steelspecs.com/products/asme-sa841-grade-a-class-1-steel-plate/). Approximate TMCP vessel talk only: EN 10028-5 P355M/P460M family for Class 1/2 windows; do not auto-substitute A537/SA537 heat-treated plate or API 5L line-pipe plate. Confirm against project specs.
Heat Treatment
Produced by thermo-mechanical control process (TMCP). Not a normalized-only or Q&T delivery book. Plates are marked TMC. Warm forming / PWHT limits apply (650 C except Grade G at 530 C) when 6.1 is met.
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
ASTM A841 vs ASME SA841
Equivalent Material Grade
Grade A Class 1 vs siblings
Why choose Us
Our Service
FAQ
Conclusion

What is ASTM A841 Grade A Class 1 steel plate?

ASTM A841 Grade A Class 1 covers killed, fine-austenitic-grain steel plate produced by the thermo-mechanical control process under ASTM A841/A841M. The plates are intended primarily for welded pressure vessels. Welded pressure-vessel shells and heads, atmospheric and low-pressure storage courses, and plate destined for vessels where astm a841 is the purchase standard and asme sa-841 acceptance is handled separately on the mtc or dual mark.

Do not confuse Class 1 with heat-treated A537 Class 1 / SA537 Cl.1. Those are normalized or quenched-and-tempered C-Mn-Si routes, not TMCP Grade A. A841 is a pressure-vessel TMCP plate specification. It is sometimes discussed next to pipeline TMCP plate RFQs because both use controlled rolling, but line-pipe chemistry and toughness packages still belong under API 5L / ISO 3183 / project annexes, not as an automatic A841 substitute.

This page treats ASTM A841 as the base product standard. ASME SA-841/SA-841M is the related specification used for ASME Boiler and Pressure Vessel Code applications. Cross-link to the live code page: ASME SA841 Grade A Class 1. Hubs: ASTM A841 · ASME SA841 · Pipeline Steel Plates.

Same-Grade Classes: Grade A Class 1 (this page) · ASTM A841 Grade A Class 2. Other ASTM A841 pages: Grade B Class 2 · Grade C Class 1 · Grade D Class 3 · Grade E Class 4 · Grade F Class 7 · Grade G Class 10 · Grade A Class 2 · Grade B Class 1 · Grade C Class 2 · Grade E Class 5 · Grade F Class 6 · Grade G Class 8 · Grade G Class 9.

Material Specification for ASTM A841 Grade A Class 1

Parameter Specification
Standard ASTM A841/A841M (primary reference A841/A841M-17; confirm ordered edition on the MTC)
Grade / Class Grade A Class 1
Companion ASME spec SA-841/SA-841M Grade A Class 1 (SA841 product page)
General requirements ASTM A20/A20M
Family TMCP steel plates for pressure vessels
Product form Plate (hot-rolled TMCP)
Maximum nominal thickness (Grade A) 100 mm
Class tensile window Grade max 100 mm for A/B/C; Class 1 tensile bands cover <=65 mm and >65 mm.
Delivery condition TMCP (thermo-mechanical control process); stamped TMC
Grain practice Killed; fine austenitic grain size per A20
Surface / edge As-rolled or shot blasted; mill edge or cut edge
Dimensional practice ASTM A20/A20M
Certification EN 10204 3.1 / 3.2; dual ASTM A841 + ASME SA-841 marking when ordered
Density 7.85 g/cm³

Chemical Composition of ASTM A841 Grade A Class 1 (heat and product analysis)

Heat (ladle) analysis limits below follow ASTM A841/A841M Table 1 for Grade A. Product analysis, when performed, shall stay within Table 2 tolerances relative to those heat limits (Product analysis, when made, shall not deviate from heat-analysis limits by more than ASTM A841/A841M Table 2 tolerances (and A20 practice as applicable).). Always verify the ordered edition and the mill test certificate before fabrication or substitution.

Element Heat analysis (Grade A) Product analysis note
Carbon (C) <=0.20 Table 2 tolerance vs heat limit
Manganese (Mn), t <= 40 mm 0.70-1.35 Table 2 tolerance vs heat limit
Manganese (Mn), t > 40 mm 1.00-1.60 Table 2 tolerance vs heat limit
Phosphorus (P) <=0.030 Table 2 tolerance vs heat limit
Sulfur (S) <=0.030 Table 2 tolerance vs heat limit
Silicon (Si) 0.15-0.50 Table 2 tolerance vs heat limit
Copper (Cu) <=0.35 Table 2 tolerance vs heat limit
Nickel (Ni) <=0.25 Table 2 tolerance vs heat limit
Chromium (Cr) <=0.25 Table 2 tolerance vs heat limit
Molybdenum (Mo) <=0.08 Table 2 tolerance vs heat limit
Niobium (Nb / Cb) <=0.03 Table 2 tolerance vs heat limit
Vanadium (V) <=0.06 Table 2 tolerance vs heat limit
Titanium (Ti) By agreement 0.006-0.02 (then Al min waived) Table 2 tolerance vs heat limit
Boron (B) – No Table 1 requirement
Aluminum (Al) >=0.020 total or >=0.015 acid soluble (unless Ti option) Table 2 tolerance vs heat limit

Mn may rise per CE note. Values are heat-analysis maximums unless a range or minimum is shown.

CE option (Grades A/B): For Grades A and B, manganese may exceed 1.35% on heat analysis up to 1.60% provided CE on heat analysis does not exceed 0.47% (or S77 value when invoked), using CE = C + Mn/6 + (Cr+Mo+V)/5 + (Ni+Cu)/15. When that option is used, product-analysis Mn shall not exceed heat-analysis Mn by more than 0.12 percentage points.

Mechanical Properties of ASTM A841 Grade A Class 1

Tensile requirements for Grade A Class 1 from ASTM A841/A841M Table 3. Two tension tests are required from each plate-as-rolled (one corner coupon from each end). If warm forming or PWHT will be applied, order simulated heat treatment of test coupons (A20 S3 / A841 6.1).

Property t <= 65 mm t > 65 mm
Yield strength, min 345 MPa (50 ksi) 310 MPa (45 ksi)
Tensile strength 485-620 MPa (70-90 ksi) 450-585 MPa (65-85 ksi)
Elongation in 50 mm (2 in), min 22% 22%
Elongation in 200 mm (8 in), min 18% 18%
Density (approx.) 7.85 g/cm³ 7.85 g/cm³

Grade max 100 mm for A/B/C; Class 1 tensile bands cover <=65 mm and >65 mm.

Notch toughness (default if not specified on the PO): Longitudinal CVN per A20. Default if not ordered: -40 C (-40 F), average >=15 ft-lbf [20 J] for three full-size specimens. Purchaser-specified CVN packages override these defaults when written on the order.

Delivery Conditions for Grade A Class 1 (TMCP)

Grade A Class 1 shall be produced by the thermo-mechanical control process. ASTM A841 is not an as-rolled carbon plate book and is not a quenched-and-tempered vessel-plate book. Each plate is legibly stamped with TMC following the stamped specification designation.

Forming / PWHT: Warm forming / PWHT not exceeding 1200 F [650 C] when 6.1 simulated-coupon requirements are met. If warm forming or PWHT will be used, the order must state temperatures and times so test coupons can be simulated (A841 6.1 / A20 S3).

Because TMCP strength and toughness come from the rolling schedule, re-normalizing or uncontrolled high-temperature forming can destroy the as-delivered property package. State fabrication heat cycles on the purchase order.

Weldability of Grade A Class 1

Grade A Class 1 is intended for welded construction. Qualify WPS/PQR to the project code (ASME IX when the vessel is code-stamped, or the applicable fabrication standard). Prefer low-hydrogen consumables matched to the strength and toughness package. Preheat and interpass follow thickness, carbon equivalent, joint restraint and the approved procedure.

Grades A and B allow a controlled Mn/CE option on heat analysis. Review CE on the MTC before fixing preheat. For Grades A and B, manganese may exceed 1.35% on heat analysis up to 1.60% provided CE on heat analysis does not exceed 0.47% (or S77 value when invoked), using CE = C + Mn/6 + (Cr+Mo+V)/5 + (Ni+Cu)/15. When that option is used, product-analysis Mn shall not exceed heat-analysis Mn by more than 0.12 percentage points.

Related pages: ASME SA841 Grade A Class 1 · Grade A Class 1 (this page) · ASTM A841 Grade A Class 2.

Dimensional Tolerances for Grade A Class 1

Dimensional tolerances for Grade A Class 1 follow ASTM A20/A20M unless the purchase order cites another agreement. Flatness, width, length and edge condition should be stated for nested vessel courses and head blanks.

Respect the Grade A maximum nominal thickness of 100 mm and the Class 1 tensile thickness bands. Ultrasonic examination, when required, is ordered via A20 supplementary requirements or A435 / A577 / A578 as applicable.

Applications and service limits for Grade A Class 1

Typical purchasing contexts for Grade A Class 1:

  • Welded pressure vessels ordered to ASTM A841 (base standard) with or without dual ASME SA-841 marking
  • Storage tanks and process vessels that specify TMCP vessel plate rather than normalized A516 / SA516
  • Export dual-cert packages listing both ASTM A841 and ASME SA-841 Grade A Class 1
  • Fabricated equipment where TMCP is preferred over heat-treated A537 for the same yield window
  • RFQs that mention pipeline or penstock TMCP plate but still cite A841 as the vessel-plate document (confirm governing spec)

A841 is a pressure-vessel TMCP plate specification. It is sometimes discussed next to pipeline TMCP plate RFQs because both use controlled rolling, but line-pipe chemistry and toughness packages still belong under API 5L / ISO 3183 / project annexes, not as an automatic A841 substitute.

Related: ASME SA841 Grade A Class 1 · ASTM A841 hub · ASME SA841 hub · Pipeline Steel Plates · Grade B Class 2 · Grade C Class 1 · Grade D Class 3 · Grade E Class 4 · Grade F Class 7 · Grade G Class 10 · Grade A Class 2 · Grade B Class 1 · Grade C Class 2 · Grade E Class 5 · Grade F Class 6 · Grade G Class 8 · Grade G Class 9.

ASTM A841 vs ASME SA-841 for Grade A Class 1 (code acceptance and MTC)

ASTM A841/A841M is the ASTM International product specification for TMCP pressure-vessel plates. ASME SA-841/SA-841M is the related specification adopted for ASME BPVC Section II use. Chemistries and tensile Class tables are aligned; the procurement difference is usually code acceptance, stamping language and how the MTC references the books.

Topic ASTM A841 (this page) ASME SA-841
Role Base ASTM product standard Code-adopted companion for ASME BPVC work
Typical PO text ASTM A841 Grade A Class 1 ASME SA-841 Grade A Class 1 / SA841 Gr.A Cl.1
MTC practice Report A841 edition, Grade, Class, TMCP/TMC, chemistry, tensile, CVN Report SA-841 (and often dual A841) when ASME code stamping is required
General reqs ASTM A20/A20M ASME SA-20 / ASTM A20 pathway
Product page This page ASME SA841 Grade A Class 1

Dual certification is available when the mill produces one plate that meets both books and marks both designations. A purchase order that only says Grade letter without Class is incomplete for every A841/SA-841 combination.

Equivalent and related grades for ASTM A841 Grade A Class 1

These designations are commonly compared with ASTM A841 Grade A Class 1. They are approximate, not automatic substitutes.

Standard / family Grade Relation Product page
ASTM A841/A841M Grade A Class 1 This page –
ASME SA-841/SA-841M Grade A Class 1 Code companion SA841 matching page
ASTM A841/A841M Grade A Class 2 Same Grade, different Class Grade A Class 2
EN 10028-5 P355M / P460M / P460ML talk TMCP vessel comparison only –
ASTM A537 / ASME SA537 Cl.1 / Cl.2 Heat-treated C-Mn-Si; not TMCP A841 –
API 5L / ISO 3183 PSL2 TMCP pipe grades Line-pipe track; different product form rules Pipeline Steel Plates
Category A841 / SA841 hubs Family navigation ASTM A841 · ASME SA841

ASTM A841 Grade A Class 1 vs sibling Classes / related Grades (selection aid)

Selection aid for ASTM A841 Grade A Class 1. Same-Grade Classes share chemistry; Class sets the tensile package. Cross-Grade rows are not substitutes.

Designation Yield (primary band) Tensile (primary band) Grade thickness cap Page
Grade A Class 1 345 MPa 485-620 MPa 100 mm grade max This page
Grade A Class 2 415 MPa 550-690 MPa 100 mm grade max Grade A Class 2
Grade B Class 1 same Class tensile same Class tensile 100 mm Grade B Class 1 (different chemistry)

Why choose SHH STEEL for ASTM A841 Grade A Class 1

  • China mill-direct supply of ASTM A841/A841M Grade A Class 1 TMCP vessel plate
  • EN 10204 3.1 mill test certificates; 3.2 and third-party inspection (SGS, TUV, BV, ABS) on request
  • Dual ASTM A841 + ASME SA-841 marking when ordered (see matching SA841 page)
  • Grade A thickness window respected (max 100 mm); Class 1 tensile and CVN packages as ordered
  • Cutting, beveling and shot blasting available to shorten fabrication lead time
  • Family coverage: ASTM A841 hub · ASME SA841 hub · Pipeline Steel Plates · Grade A Class 1 (this page) · ASTM A841 Grade A Class 2

Supply, cutting and inspection for Grade A Class 1

Item SHH STEEL supply note
Thickness Within Grade A max 100 mm and Class 1 tensile bands; confirm mill capability on enquiry
Size Width and length per mill rolling; cut-to-size / nest sizes on request
Delivery condition TMCP (TMC stamped); not normalized-only or Q&T unless a different standard is ordered
Processing Cutting, beveling, shot blasting available
Mill certificate EN 10204 3.1 standard; 3.2 on request; dual A841/SA-841 when ordered
Third-party inspection SGS, TUV, BV or ABS can be arranged
Quotation needs ASTM A841 Grade A Class 1, thickness x width x length, quantity, CVN package, warm-forming/PWHT simulation if any, dual SA-841 mark yes/no, inspection level

FAQ

Is ASTM A841 the same as ASME SA841?
They are companion specifications. ASTM A841/A841M is the ASTM base product standard. ASME SA-841/SA-841M is used for ASME BPVC applications. See ASME SA841 Grade A Class 1 and the ASTM vs ASME section on this page.
What Class combinations exist for Grade A?
Grade A Class 1 (this page) · ASTM A841 Grade A Class 2. Class sets the tensile package; Grade sets chemistry and thickness cap.
What is the maximum thickness for Grade A?
100 mm nominal maximum under ASTM A841/A841M. Class 1 tensile bands: Grade max 100 mm for A/B/C; Class 1 tensile bands cover <=65 mm and >65 mm.
What CVN defaults apply if the PO is silent?
Longitudinal CVN per A20. Default if not ordered: -40 C (-40 F), average >=15 ft-lbf [20 J] for three full-size specimens. Always prefer an explicit CVN package on the order.
Can A841 plate replace API 5L pipeline plate?
Not automatically. A841 is a pressure-vessel TMCP plate specification. Pipeline plate / line-pipe rules sit under API 5L, ISO 3183 or project annexes. See Pipeline Steel Plates.

Request a quotation

Send ASTM A841 Grade A Class 1, thickness x width x length, quantity, CVN package, any warm-forming/PWHT simulation temperatures, dual ASME SA-841 marking requirement, and inspection level. SHH STEEL will return mill availability, certification scope and a quotation.

Contact: admin@steelspecs.com · +86-18939509537 · +86-021-62716097

More options: ASTM A841 · ASME SA841 Grade A Class 1 · ASME SA841 hub · Pipeline Steel Plates · Grade A Class 1 (this page) · ASTM A841 Grade A Class 2

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X