ASTM A829 4615 Alloy Steel Plate
What is ASTM A829 Grade 4615 plate?
ASTM A829 4615 Alloy Steel Plate is nickel-molybdenum alloy structural plate under ASTM A829/A829M. The heat-analysis windows and the Table 3 tensile-range rule on this page come from A829/A829M-00 (2000), a dated numerical reference rather than figures from a later edition.
Grade 4615 is usually specified to chemical composition. ASTM A829/A829M-00 Table 1 lists carbon 0.12-0.18 %, manganese 0.40-0.65 %, silicon 0.15-0.40 %, phosphorus 0.035 % max, sulfur 0.040 % max, nickel 1.65-2.00 % and molybdenum 0.20-0.30 %. That table shows no requirement for chromium or vanadium. Tensile properties may also be specified when they are compatible with the composition, the delivery condition and the plate thickness.
The 2000 edition lists four delivery conditions: as-rolled (hot rolled), annealed, normalized, and normalized and tempered. It does not list a quenched-and-tempered condition. As-rolled plate of this grade should not be assumed to meet typical quenched-and-tempered bar strengths published for SAE 4615.
SHH STEEL produces and exports ASTM A829 Grade 4615 plate to the ordered edition, delivery condition, dimensions and extra tests written on the enquiry. The numeric chemistry and tensile-range rules on this page are from A829/A829M-00. This grade belongs to our Alloy Steel Plates range under ASTM A829/A829M.
Material specification for ASTM A829 Grade 4615
The items below follow ASTM A829/A829M-00, Standard Specification for Alloy Structural Steel Plates, approved 10 September 2000 and published October 2000. Thickness, width, length and the inspection document are stated on the enquiry rather than listed here as stock or capacity ranges. If your project specifies a later ASTM A829/A829M edition, write that edition on the enquiry; the numeric tables on this page remain those of the 2000 text.
| Parameter | Detail |
|---|---|
| Standard | ASTM A829/A829M-00, Standard Specification for Alloy Structural Steel Plates |
| Grade designation | Grade 4615, nickel-molybdenum alloy structural steel. Table 1 also lists UNS G46150 and SAE number 4615 |
| Product form | Alloy structural steel plate |
| Usual ordering basis | Chemical composition (clause 1.2 and 5.1); tensile properties may also be specified when compatible with composition, condition and thickness (clauses 1.2.1 and 6.1) |
| Alternative chemistry order | Clause 5.2 and Table 2 allow a custom heat analysis to be specified instead of a named Table 1 grade. Table 2 sets range widths, not product-analysis tolerances |
| Delivery conditions listed in 2000 | Condition AR, as rolled (hot rolled); Condition A, annealed; Condition N, normalized; Condition NT, normalized and tempered. A quenched-and-tempered condition is not listed in A829/A829M-00 |
| Heat-treated supply | When a heat-treated condition is specified, plates shall be heated to a suitable temperature at or above the upper critical temperature, but not exceeding 1700°F [925°C], held long enough to reach essentially uniform temperature, and cooled as appropriate for the ordered condition (clause 4.2.1) |
| Grain practice | Fine grain practice unless coarse austenitic grain size is specified on the order (clauses 3.1.4 and 4.1) |
| Forms | Form I rectangular; Form II circular and semi-circular; Form III sketch, including rings |
| Edge categories | Edge 1 mill edge; Edge 2 universal mill edge; Edge 3 sheared edge; Edge 4 gas-cut edge; Edge 5 special cut edge. Unless otherwise specified, Edge 3 shall be furnished; Edge 4 may be furnished in place of Edge 3 at the supplier’s option |
| Finishes | Finish 1 as-rolled (hot-rolled); Finish 2 blast cleaned; Finish 3 blast cleaned and oiled; Finish 4 pickled; Finish 5 pickled and oiled; Finish 6 painted, one prime coat; Finish 7 painted, one prime coat and one finish coat. Plates are usually specified to Finish 1 |
| General delivery | Material shall conform to the current edition of ASTM A6/A6M unless a conflict exists, in which case A829/A829M-00 prevails (clause 7.1) |
| Supplementary requirements | They do not apply unless specified on the order. Titles listed as suitable with this specification are S1 Vacuum Treatment, S2 Product Analysis, and S8 Ultrasonic Examination, by reference to A6/A6M |
| Certification | A report of the heat analysis and of all tests required by the order, together with certification that the material was manufactured to this specification (clause 8.1) |
| Units | Inch-pound and SI values are each standard and are not exact equivalents; do not combine the two systems (clause 1.9) |
| Our supply | We produce and export Grade 4615 to the ASTM form, edge, finish and delivery condition agreed on the order |
Chemical composition of ASTM A829 Grade 4615
ASTM A829/A829M-00 clause 5.1 requires the heat analysis of a named grade to conform to Table 1, unless the order instead specifies a custom heat analysis under clause 5.2. The figures below are the Table 1 heat-analysis limits for Grade 4615 in A829/A829M-00 (2000). They are a dated numerical reference from that edition. They are not taken from a later A829/A829M edition, and they must not be read as manufacturer or later-edition values without checking the ordered text.
| Element | A829/A829M-00 Table 1 heat analysis (wt. %) |
|---|---|
| Carbon | 0.12-0.18 |
| Manganese | 0.40-0.65 |
| Phosphorus | 0.035 max |
| Sulfur | 0.040 max |
| Silicon | 0.15-0.40 |
| Nickel | 1.65-2.00 |
| Molybdenum | 0.20-0.30 |
Table 1 of A829/A829M-00 shows no requirement for chromium or vanadium for this grade (the table marks those columns with an ellipsis). This named grade is a nickel-molybdenum plate, not a chromium-molybdenum plate.
Clause 5.2 allows the purchaser to specify a custom heat analysis instead of a named Table 1 grade. In that case the permitted width of each specified element range is set by Table 2, which defines the arithmetical difference between the two limits of the specified range. Table 2 is not a product-analysis tolerance table, and it is not used to rewrite the Table 1 windows on this named-grade page.
Supplementary Requirement S2, Product Analysis, does not apply unless it is specified on the purchase order. A829/A829M-00 lists S2 by title and refers to ASTM A6/A6M for the standardized supplementary requirements. This page does not reprint A6 product-analysis deviations.
Mechanical properties and optional tests
ASTM A829/A829M-00 plates are usually specified to chemical composition (clause 1.2). Tensile properties may also be specified when they are compatible with the chemical composition, the delivery condition and the plate thickness (clauses 1.2.1 and 6.1).
When tensile requirements are specified, clause 6.2 requires that the specified tensile strength range shall be not less than the applicable width in Table 3. Table 3 does not publish a minimum yield strength or a minimum tensile strength for Grade 4615. It only sets how wide the purchaser’s specified tensile-strength range must be, based on the specified maximum tensile strength:
| Specified maximum tensile strength | Minimum tensile-strength range width (Table 3) |
|---|---|
| Up to 70 ksi [480 MPa] | 15 ksi [100 MPa] |
| Over 70 to 110 ksi [480 to 760 MPa] | 20 ksi [135 MPa] |
| Over 110 to 140 ksi [760 to 965 MPa] | 25 ksi [170 MPa] |
There is no automatic as-delivered strength package for Grade 4615. If tensile, hardness or toughness results are required, state the values as a compatible range and name the delivery condition and thickness. Typical quenched-and-tempered bar figures for the same SAE number must not be read as A829 plate minima. A829/A829M-00 does not list a quenched-and-tempered delivery condition.
Delivery conditions for ASTM A829 Grade 4615
ASTM A829/A829M-00 lists four delivery conditions:
- Condition AR — as rolled (hot rolled)
- Condition A — annealed
- Condition N — normalized
- Condition NT — normalized and tempered
We produce and export Grade 4615 to the agreed condition. An enquiry that only says “4615 plate” is incomplete, because as-rolled, annealed, normalized and normalized-and-tempered plate are not interchangeable supply states. A quenched-and-tempered condition is not listed in the 2000 text. If the project needs a processing route other than the four listed conditions, that route must be written explicitly on the order and agreed.
As-rolled plate is often used for parts that will be heat treated later. That later cycle is not an automatic as-delivered A829 guarantee.
Welding and thermal cutting
When the steel is to be welded, A829/A829M-00 presupposes a welding procedure suitable for the grade and the intended use or service, and refers to Appendix X3 of ASTM A6/A6M for weldability information (clause 1.8). Repairs by welding, if permitted, shall be made by competent welders using low-hydrogen electrodes selected so that the deposited weld metal is similar to the nominal composition of the base plate (clause 4.5.1). If repair by welding is not acceptable, or if the purchaser must approve the welding procedure, the order shall say so (clause 4.5.2).
Grade 4615 has a relatively low carbon window together with nickel and molybdenum. It is generally more weldable than higher-carbon nickel-chromium-molybdenum plates such as 4340, but nickel and molybdenum still raise hardenability. The procedure should still be qualified to thickness and restraint. Preheat, interpass temperature and any post-weld heat treatment depend on thickness, joint restraint and the qualified procedure. Qualify cutting and welding procedures to the project specification, the ordered delivery condition and the actual plate thickness.
Thermal cutting can harden the adjacent material. That heat-affected zone should be considered, and removed where later forming or welding requires it.
Form, edge, finish and dimensions
A829/A829M-00 defines form, edge and finish options and requires material to conform to ASTM A6/A6M except where this specification prevails (clause 7.1). Numeric thickness, width, length and flatness tolerances should be stated on the purchase order and confirmed on the mill documents. This page does not reprint A6 tolerance tables.
Unless otherwise specified, Edge 3 (sheared) shall be furnished; Edge 4 (gas cut) may be furnished in place of Edge 3 at the supplier’s option (clause 4.3). Finish 1 is the usual finish.
Applications and specification limits
Grade 4615 is specified when a low-carbon nickel-molybdenum plate is wanted. It is often chosen for parts that will later be carburized or otherwise case-hardened. Those later treatments are not automatic as-delivered A829 guarantees. Among Grades 4615, 4617 and 4620 it has the lowest Table 1 carbon window.
This is not a chromium-molybdenum plate, not a quenched-and-tempered strength-graded plate such as ASTM A514, and not a boiler or pressure-vessel plate. Do not treat it as interchangeable with Grade 8620.
Corrosion resistance is that of alloy structural steel, not stainless steel. Outdoor or chemical service needs a coating or another alloy family when the environment requires it.
Compare ASTM A829 4615 with other steel plates
ASTM A829 Grade 4615 is chemistry-ordered alloy structural plate under ASTM A829/A829M. The comparison below uses other plates we already publish. These grades are related by engineering use or chemistry family, not equivalents.
| Material | Alloy / type | Delivery condition | Mechanical requirements | Typical service | Substitution limit |
|---|---|---|---|---|---|
| ASTM A829 Grade 4615 (this plate) | Nickel-molybdenum alloy structural plate, usually ordered by heat chemistry. A829/A829M-00 Table 1: C 0.12-0.18, Mn 0.40-0.65, Si 0.15-0.40, Ni 1.65-2.00, Mo 0.20-0.30; no listed Cr or V requirement | AR, annealed, normalized, or normalized and tempered, as listed in A829/A829M-00 | No automatic as-delivered strength package. If tensile properties are specified, the tensile-strength range must be at least as wide as Table 3 of A829/A829M-00 | Low-carbon nickel-molybdenum engineering plate; later carburizing is a project process, not an automatic as-delivered guarantee | Not a chromium-molybdenum plate and not interchangeable with Grade 8620, Grade 4130 or Grade 4140 |
| ASTM A829 8620 Alloy Steel Plate | Nickel-chromium-molybdenum alloy structural plate, usually ordered by heat chemistry. Manufacturer heat-analysis windows on that page: C 0.18–0.23, Mn 0.70–0.90, Si 0.15–0.35, Ni 0.40–0.70, Cr 0.40–0.60 and Mo 0.15–0.25 | ASTM A829/A829M-25 permits AR, A, N, NT or QT; specify the required condition. | No automatic as-delivered strength package; tensile or hardness only if specified and compatible | Engineering plate often used for parts that will later be carburized or otherwise heat treated | Grade 8620 on its manufacturer page is a nickel-chromium-molybdenum plate (C 0.18-0.23 %, Ni 0.40-0.70 %, Cr 0.40-0.60 %). Grade 4615 has nickel 1.65-2.00 % and no listed chromium requirement. |
| ASTM A829 4130 Alloy Steel Plate | Chromium-molybdenum alloy structural plate, usually ordered by heat chemistry. Manufacturer heat-analysis windows on that page: C 0.28–0.33, Mn 0.40–0.60, Si 0.15–0.35, Cr 0.80–1.10 and Mo 0.15–0.25 | Usually ordered by chemistry; tensile only if specified and compatible | No automatic as-delivered strength package | Engineering plate with a lower carbon window than Grade 4140 in the same family | Grade 4130 on its manufacturer page is a chromium-molybdenum plate (C 0.28-0.33 %, Cr 0.80-1.10 %, Mo 0.15-0.25 %) with no listed nickel window. Grade 4615 is nickel-molybdenum plate with carbon 0.12-0.18 % and no listed chromium requirement. |
| ASTM A829 4140 Alloy Steel Plate | Chromium-molybdenum alloy structural plate, usually ordered by heat chemistry. Manufacturer heat-analysis windows on that page: C 0.36–0.44, Mn 0.75–1.00, Si 0.15–0.35, Cr 0.80–1.10 and Mo 0.15–0.25 | ASTM A829/A829M-25 permits AR, A, N, NT or QT; specify the required condition. | No automatic as-delivered strength package; tensile or hardness only if specified and compatible | Machinery and general engineering parts, often heat treated after cutting | Grade 4140 on its manufacturer page is a chromium-molybdenum plate (C 0.36-0.44 %, Cr 0.80-1.10 %, Mo 0.15-0.25 %). Grade 4615 is a lower-carbon nickel-molybdenum plate without a listed chromium requirement. |
Related published ranges: Alloy Steel Plates and Structural Steel Plates.
Equivalent and related grades by country
The designations below are near equivalents or related chemistry-family grades, not certified or automatic equivalents. Chemistry windows, product form, delivery condition and any mechanical tests must match the project specification before a substitution is considered. Grades without a live page on this site are shown as plain text.
| Country / region | Standard | Grade | Similarity and key differences | Substitution caveat |
|---|---|---|---|---|
| United States | ASTM A829/A829M-00 | Grade 4615 | This plate. A829/A829M-00 Table 1 heat analysis: C 0.12-0.18, Mn 0.40-0.65, Si 0.15-0.40, P 0.035 max, S 0.040 max, Ni 1.65-2.00, Mo 0.20-0.30. No listed Cr or V requirement. Among the three 46xx plate grades it has the lowest carbon window. | Specify this named grade, the ordered edition, delivery condition and any tests rather than substituting another number. |
| United States | AISI/SAE chemistry-family designation (not a plate specification) | 4615 | The same conventional number is used for bars and other product forms. Product form, delivery condition and mechanical tests are not automatically the same as A829 plate. | Do not read typical quenched-and-tempered bar figures as A829 plate minima. |
| Japan | JIS G 4053 (bar and machine-structural steels, not a plate book) | SNCM415 / SNCM420 | SNCM415 is C 0.12-0.18, Mn 0.40-0.70, Ni 1.60-2.00, Cr 0.40-0.60, Mo 0.15-0.30. SNCM420 is C 0.17-0.23, Mn 0.40-0.70, Ni 1.60-2.00, Cr 0.40-0.60, Mo 0.15-0.30. Grade 4615 Table 1 is C 0.12-0.18, Mn 0.40-0.65, Ni 1.65-2.00, Mo 0.20-0.30, with no chromium requirement. | Not treated as near equivalents, because those JIS grades specify chromium 0.40-0.60 % while this A829 grade has no listed chromium requirement. |
SNCM415 and SNCM420 are shown only to record that they are not close chemistry matches for Grade 4615 plate. Do not order them as substitutes.
Why choose SHH STEEL for ASTM A829 Grade 4615
- We produce and export ASTM A829 Grade 4615 alloy structural steel plate
- We review the enquiry for edition, grade, delivery condition, dimensions and extra tests
- We keep chemistry-ordered plate distinct from optional tensile testing, and we treat Table 3 as a range-width rule rather than as a strength minimum
- We match documentation to what the purchase order requires
How to enquire for ASTM A829 4615 plate
| Item | What to specify |
|---|---|
| Standard and grade | ASTM A829/A829M, Grade 4615. Numeric chemistry and tensile-range rules on this page are from the 2000 edition; write the edition your project requires |
| Delivery condition | AR, annealed (A), normalized (N), or normalized and tempered (NT). Any other route only if written and agreed |
| Dimensions | Required thickness, width and length; we confirm production and export feasibility against the enquiry |
| Form, edge and finish | Use the ASTM options above if needed. Finish 1 is the usual finish |
| Chemistry | Heat analysis to Table 1 for Grade 4615, unless a custom clause 5.2 / Table 2 analysis is written on the order; request Supplementary Requirement S2 product analysis only if the project needs it |
| Mechanical tests | If tensile properties are required, specify them as a tensile-strength range whose width is not less than Table 3, and confirm compatibility with composition, condition and thickness |
| Other tests | S1 vacuum treatment or S8 ultrasonic examination only when written on the order |
| Repair welding | State any limitation or required procedure approval (clause 4.5.2) |
| Documentation | State the inspection document type required by the project |
| Processing | Cutting or other processing only when requested; thermal-cutting practice depends on condition and thickness |
FAQ
-
Is ASTM A829 4615 ordered by chemistry or by mechanical properties?
- Usually by chemical composition, to Table 1 of A829/A829M-00 for this named grade. Tensile properties may also be specified when they are compatible with the composition, delivery condition and plate thickness. If tensile properties are specified, the specified tensile-strength range must be at least as wide as Table 3 of the 2000 edition. Table 3 is a range-width rule, not a minimum yield or tensile strength.
-
Is Grade 4615 a chromium-molybdenum plate, or the same as Grade 8620?
- No. A829/A829M-00 Table 1 lists Grade 4615 carbon 0.12-0.18 %, nickel 1.65-2.00 % and molybdenum 0.20-0.30 %, with no chromium requirement. Grade 8620 on our manufacturer page is listed with carbon 0.18-0.23 %, nickel 0.40-0.70 % and chromium 0.40-0.60 %. Both may be discussed for later carburizing, but they are not the same grade.
-
Does ASTM A829/A829M-00 list quenched-and-tempered 4615 plate?
- No. The 2000 edition lists Condition AR, A, N and NT only. If the project needs another processing route, that route must be written explicitly on the order and agreed. Do not read typical quenched-and-tempered bar figures for SAE 4615 as automatic plate minima.
-
Are the numbers on this page from the current 2025 edition?
- No. The heat-analysis windows and the Table 3 tensile-range widths on this page are taken from ASTM A829/A829M-00 (2000). If your project specifies a later edition, write that edition on the enquiry so we can review it against the ordered text.
-
What should a quotation enquiry include?
- The ordered ASTM A829/A829M edition, Grade 4615, delivery condition, thickness by width by length, quantity, any tensile range (if required) or other extra tests, any NDE, any limit on repair welding, and the inspection document required by the project.
Request a quotation
Contact SHH STEEL for a quotation for ASTM A829 Grade 4615 alloy steel plate. Please include your required quantity, plate thickness, width and length, delivery destination and preferred delivery schedule so we can review your production and export requirements.
Specify the ASTM edition your project requires and the delivery condition: as-rolled, annealed, normalized, or normalized and tempered. If your project requires tensile, hardness, toughness or ultrasonic testing, include the acceptance criteria and the inspection document required. Any specified tensile strength should be written as a range whose width is not less than Table 3 of A829/A829M-00, and it must be compatible with the chemistry, delivery condition and plate thickness.
If your enquiry compares Grade 4615 with Grade 8620, Grade 4130 or Grade 4140, identify each grade clearly. We will review the differences in product form, chemistry and supply condition rather than assume that related grades are interchangeable.
For a detailed quotation, email your material specification, quantity and delivery requirements to our team.