ASTM A829 1335 Alloy Steel Plate | ASTM A829 Alloy Steel - SHH STEEL

ASTM A829 1335 Alloy Steel Plate

ASTM A829 1335 is a high-manganese alloy structural steel plate, usually ordered by heat chemistry for engineering parts that start as plate rather than as an HSLA structural member. Its carbon window sits between Grades 1330 and 1340, so later machining or heat treatment should follow the ordered composition and condition. It can be supplied as-rolled, annealed, normalized, or normalized and tempered. SHH STEEL produces and exports ASTM A829 Grade 1335 plate to the chemistry, delivery condition and tests written on the order.
Equivalent Grades:
AISI/SAE 1335
Heat Treatment
As-rolled (AR); annealed (A); normalized (N); normalized and tempered (NT).
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why choose Us
Our Service
FAQ
Conclusion

What is ASTM A829 Grade 1335 plate?

ASTM A829 1335 Alloy Steel Plate is high-manganese alloy structural plate under ASTM A829/A829M. The heat-analysis windows and the Table 3 tensile-range rule on this page come from A829/A829M-00 (2000), a dated numerical reference rather than figures from a later edition.

Grade 1335 is usually specified to chemical composition. ASTM A829/A829M-00 Table 1 lists carbon 0.32-0.39 % and manganese 1.50-1.90 %, with silicon 0.15-0.40 %, phosphorus 0.035 % max and sulfur 0.040 % max. That table shows no requirement for nickel, chromium, molybdenum or vanadium. Tensile properties may also be specified when they are compatible with the composition, the delivery condition and the plate thickness.

The 2000 edition lists four delivery conditions: as-rolled (hot rolled), annealed, normalized, and normalized and tempered. It does not list a quenched-and-tempered condition. As-rolled plate of this grade should not be assumed to meet typical quenched-and-tempered bar strengths published for SAE 1335.

SHH STEEL produces and exports ASTM A829 Grade 1335 plate to the ordered edition, delivery condition, dimensions and extra tests written on the enquiry. The numeric chemistry and tensile-range rules on this page are from A829/A829M-00. This grade belongs to our Alloy Steel Plates range under ASTM A829/A829M.

Material specification for ASTM A829 Grade 1335

The items below follow ASTM A829/A829M-00, Standard Specification for Alloy Structural Steel Plates, approved 10 September 2000 and published October 2000. Thickness, width, length and the inspection document are stated on the enquiry rather than listed here as stock or capacity ranges. If your project specifies a later ASTM A829/A829M edition, write that edition on the enquiry; the numeric tables on this page remain those of the 2000 text.

Parameter Detail
Standard ASTM A829/A829M-00, Standard Specification for Alloy Structural Steel Plates
Grade designation Grade 1335, high-manganese alloy structural steel (SAE 13xx family). Table 1 also lists UNS G13350 and SAE number 1335
Product form Alloy structural steel plate
Usual ordering basis Chemical composition (clause 1.2 and 5.1); tensile properties may also be specified when compatible with composition, condition and thickness (clauses 1.2.1 and 6.1)
Alternative chemistry order Clause 5.2 and Table 2 allow a custom heat analysis to be specified instead of a named Table 1 grade. Table 2 sets range widths, not product-analysis tolerances
Delivery conditions listed in 2000 Condition AR, as rolled (hot rolled); Condition A, annealed; Condition N, normalized; Condition NT, normalized and tempered. A quenched-and-tempered condition is not listed in A829/A829M-00
Heat-treated supply When a heat-treated condition is specified, plates shall be heated to a suitable temperature at or above the upper critical temperature, but not exceeding 1700°F [925°C], held long enough to reach essentially uniform temperature, and cooled as appropriate for the ordered condition (clause 4.2.1)
Grain practice Fine grain practice unless coarse austenitic grain size is specified on the order (clauses 3.1.4 and 4.1)
Forms Form I rectangular; Form II circular and semi-circular; Form III sketch, including rings
Edge categories Edge 1 mill edge; Edge 2 universal mill edge; Edge 3 sheared edge; Edge 4 gas-cut edge; Edge 5 special cut edge. Unless otherwise specified, Edge 3 shall be furnished; Edge 4 may be furnished in place of Edge 3 at the supplier’s option
Finishes Finish 1 as-rolled (hot-rolled); Finish 2 blast cleaned; Finish 3 blast cleaned and oiled; Finish 4 pickled; Finish 5 pickled and oiled; Finish 6 painted, one prime coat; Finish 7 painted, one prime coat and one finish coat. Plates are usually specified to Finish 1
General delivery Material shall conform to the current edition of ASTM A6/A6M unless a conflict exists, in which case A829/A829M-00 prevails (clause 7.1)
Supplementary requirements They do not apply unless specified on the order. Titles listed as suitable with this specification are S1 Vacuum Treatment, S2 Product Analysis, and S8 Ultrasonic Examination, by reference to A6/A6M
Certification A report of the heat analysis and of all tests required by the order, together with certification that the material was manufactured to this specification (clause 8.1)
Units Inch-pound and SI values are each standard and are not exact equivalents; do not combine the two systems (clause 1.9)
Our supply We produce and export Grade 1335 to the ASTM form, edge, finish and delivery condition agreed on the order

Chemical composition of ASTM A829 Grade 1335

ASTM A829/A829M-00 clause 5.1 requires the heat analysis of a named grade to conform to Table 1, unless the order instead specifies a custom heat analysis under clause 5.2. The figures below are the Table 1 heat-analysis limits for Grade 1335 in A829/A829M-00 (2000). They are a dated numerical reference from that edition. They are not taken from a later A829/A829M edition, and they must not be read as manufacturer or later-edition values without checking the ordered text.

Element A829/A829M-00 Table 1 heat analysis (wt. %)
Carbon 0.32-0.39
Manganese 1.50-1.90
Phosphorus 0.035 max
Sulfur 0.040 max
Silicon 0.15-0.40

Table 1 of A829/A829M-00 shows no requirement for nickel, chromium, molybdenum or vanadium for this grade (the table marks those columns with an ellipsis). Those elements are therefore not listed as heat-analysis limits here.

Clause 5.2 allows the purchaser to specify a custom heat analysis instead of a named Table 1 grade. In that case the permitted width of each specified element range is set by Table 2, which defines the arithmetical difference between the two limits of the specified range. Table 2 is not a product-analysis tolerance table, and it is not used to rewrite the Table 1 windows on this named-grade page.

Supplementary Requirement S2, Product Analysis, does not apply unless it is specified on the purchase order. A829/A829M-00 lists S2 by title and refers to ASTM A6/A6M for the standardized supplementary requirements. This page does not reprint A6 product-analysis deviations.

Mechanical properties and optional tests

ASTM A829/A829M-00 plates are usually specified to chemical composition (clause 1.2). Tensile properties may also be specified when they are compatible with the chemical composition, the delivery condition and the plate thickness (clauses 1.2.1 and 6.1).

When tensile requirements are specified, clause 6.2 requires that the specified tensile strength range shall be not less than the applicable width in Table 3. Table 3 does not publish a minimum yield strength or a minimum tensile strength for Grade 1335. It only sets how wide the purchaser’s specified tensile-strength range must be, based on the specified maximum tensile strength:

Specified maximum tensile strength Minimum tensile-strength range width (Table 3)
Up to 70 ksi [480 MPa] 15 ksi [100 MPa]
Over 70 to 110 ksi [480 to 760 MPa] 20 ksi [135 MPa]
Over 110 to 140 ksi [760 to 965 MPa] 25 ksi [170 MPa]

There is no automatic as-delivered strength package for Grade 1335. If tensile, hardness or toughness results are required, state the values as a compatible range and name the delivery condition and thickness. Typical quenched-and-tempered bar figures for the same SAE number must not be read as A829 plate minima. A829/A829M-00 does not list a quenched-and-tempered delivery condition.

Delivery conditions for ASTM A829 Grade 1335

ASTM A829/A829M-00 lists four delivery conditions:

  • Condition AR — as rolled (hot rolled)
  • Condition A — annealed
  • Condition N — normalized
  • Condition NT — normalized and tempered

We produce and export Grade 1335 to the agreed condition. An enquiry that only says “1335 plate” is incomplete, because as-rolled, annealed, normalized and normalized-and-tempered plate are not interchangeable supply states. A quenched-and-tempered condition is not listed in the 2000 text. If the project needs a processing route other than the four listed conditions, that route must be written explicitly on the order and agreed.

As-rolled plate is often used for parts that will be heat treated later. That later cycle is not an automatic as-delivered A829 guarantee.

Welding and thermal cutting

When the steel is to be welded, A829/A829M-00 presupposes a welding procedure suitable for the grade and the intended use or service, and refers to Appendix X3 of ASTM A6/A6M for weldability information (clause 1.8). Repairs by welding, if permitted, shall be made by competent welders using low-hydrogen electrodes selected so that the deposited weld metal is similar to the nominal composition of the base plate (clause 4.5.1). If repair by welding is not acceptable, or if the purchaser must approve the welding procedure, the order shall say so (clause 4.5.2).

Grade 1335 combines a medium carbon window with high manganese (1.50-1.90 % in Table 1). That combination can raise hardenability in the heat-affected zone compared with a leaner structural plate, so welding and thermal cutting need more care than on a low-carbon, low-manganese grade. Preheat, interpass temperature and any post-weld heat treatment depend on thickness, joint restraint and the qualified procedure. Qualify cutting and welding procedures to the project specification, the ordered delivery condition and the actual plate thickness.

Thermal cutting can harden the adjacent material. That heat-affected zone should be considered, and removed where later forming or welding requires it.

Form, edge, finish and dimensions

A829/A829M-00 defines form, edge and finish options and requires material to conform to ASTM A6/A6M except where this specification prevails (clause 7.1). Numeric thickness, width, length and flatness tolerances should be stated on the purchase order and confirmed on the mill documents. This page does not reprint A6 tolerance tables.

Unless otherwise specified, Edge 3 (sheared) shall be furnished; Edge 4 (gas cut) may be furnished in place of Edge 3 at the supplier’s option (clause 4.3). Finish 1 is the usual finish.

Applications and specification limits

Grade 1335 is specified when a high-manganese alloy structural plate is wanted and later heat treatment or machining will be planned around the ordered chemistry. Typical uses are engineering parts, shafts, levers and other components that start as plate rather than as a structural HSLA member. Its Table 1 carbon window sits between Grades 1330 and 1340.

This is not a strength-graded structural plate such as ASTM A572, and it is not a boiler or pressure-vessel plate. High manganese does not by itself make the plate a wear-resistant overlay or a tool steel. If the project needs a guaranteed as-delivered tensile package, write a compatible tensile-strength range and the delivery condition; do not assume as-rolled 1335 plate will match published quenched-and-tempered bar figures.

Corrosion resistance is that of alloy structural steel, not stainless steel. Outdoor or chemical service needs a coating or another alloy family when the environment requires it.

Compare ASTM A829 1335 with other steel plates

ASTM A829 Grade 1335 is chemistry-ordered alloy structural plate under ASTM A829/A829M. The comparison below uses other plates we already publish. These grades are related by engineering use or chemistry family, not equivalents.

Material Alloy / type Delivery condition Mechanical requirements Typical service Substitution limit
ASTM A829 Grade 1335 (this plate) High-manganese alloy structural plate (SAE 13xx family), usually ordered by heat chemistry. A829/A829M-00 Table 1: C 0.32-0.39, Mn 1.50-1.90, Si 0.15-0.40; no listed Ni, Cr, Mo or V requirement AR, annealed, normalized, or normalized and tempered, as listed in A829/A829M-00 No automatic as-delivered strength package. If tensile properties are specified, the tensile-strength range must be at least as wide as Table 3 of A829/A829M-00 Engineering parts and later heat-treated components that start as high-manganese plate Not a structural HSLA plate and not a chromium-molybdenum 41xx grade
ASTM A829 4140 Alloy Steel Plate Chromium-molybdenum alloy structural plate, usually ordered by heat chemistry. Manufacturer heat-analysis windows on that page: C 0.36–0.44, Mn 0.75–1.00, Si 0.15–0.35, Cr 0.80–1.10 and Mo 0.15–0.25 As presented on that page: as-rolled, annealed, normalized, normalized and tempered, or quenched and tempered as ordered No automatic as-delivered strength package; tensile or hardness only if specified and compatible Machinery and general engineering parts, often heat treated after cutting Different chemistry family. Grade 1335 is a high-manganese plate with no listed chromium or molybdenum requirement; Grade 4140 is a chromium-molybdenum plate with manganese 0.75-1.00 % on its manufacturer page.
ASTM A829 4130 Alloy Steel Plate Chromium-molybdenum alloy structural plate, usually ordered by heat chemistry. Manufacturer heat-analysis windows on that page: C 0.28–0.33, Mn 0.40–0.60, Si 0.15–0.35, Cr 0.80–1.10 and Mo 0.15–0.25 Usually ordered by chemistry; tensile only if specified and compatible No automatic as-delivered strength package Engineering plate with a lower carbon window than Grade 4140 in the same family Different chemistry family. Grade 4130 is chromium-molybdenum plate with manufacturer manganese 0.40-0.60 %; Grade 1335 has manganese 1.50-1.90 % and no listed chromium or molybdenum requirement.
ASTM A572 Grade 50 High-strength low-alloy structural plate, microalloyed with niobium and vanadium Hot-rolled or controlled-rolled Strength-graded: minimum yield 345 MPa and tensile 450 MPa minimum (from our A572 Grade 50 page) Bridges, buildings, construction equipment, transmission towers and heavy machinery frames A572 Grade 50 is a strength-graded HSLA structural plate. Grade 1335 is chemistry-ordered high-manganese alloy plate and has no automatic yield or tensile package in A829/A829M-00.

Related published ranges: Alloy Steel Plates, Structural Steel Plates and ASTM A572/A572M.

Equivalent and related grades by country

The designations below are near equivalents or related chemistry-family grades, not certified or automatic equivalents. Chemistry windows, product form, delivery condition and any mechanical tests must match the project specification before a substitution is considered. Grades without a live page on this site are shown as plain text.

Country / region Standard Grade Similarity and key differences Substitution caveat
United States ASTM A829/A829M-00 Grade 1335 This plate. A829/A829M-00 Table 1 heat analysis: C 0.32-0.39, Mn 1.50-1.90, Si 0.15-0.40, P 0.035 max, S 0.040 max. No listed Ni, Cr, Mo or V requirement. Specify this named grade, the ordered edition, delivery condition and any tests rather than substituting another number.
United States AISI/SAE chemistry-family designation (not a plate specification) 1335 The same conventional number is used for bars and other product forms. Product form, delivery condition and mechanical tests are not automatically the same as A829 plate. Do not read typical quenched-and-tempered bar figures as A829 plate minima.

No verified EN plate grade or JIS plate grade is cited here as a near equivalent of ASTM A829 Grade 1335. An AISI/SAE 1335 bar designation is a chemistry-family name, not a substitute plate specification.

Why choose SHH STEEL for ASTM A829 Grade 1335

  • We produce and export ASTM A829 Grade 1335 alloy structural steel plate
  • We review the enquiry for edition, grade, delivery condition, dimensions and extra tests
  • We keep chemistry-ordered plate distinct from optional tensile testing, and we treat Table 3 as a range-width rule rather than as a strength minimum
  • We match documentation to what the purchase order requires

How to enquire for ASTM A829 1335 plate

Item What to specify
Standard and grade ASTM A829/A829M, Grade 1335. Numeric chemistry and tensile-range rules on this page are from the 2000 edition; write the edition your project requires
Delivery condition AR, annealed (A), normalized (N), or normalized and tempered (NT). Any other route only if written and agreed
Dimensions Required thickness, width and length; we confirm production and export feasibility against the enquiry
Form, edge and finish Use the ASTM options above if needed. Finish 1 is the usual finish
Chemistry Heat analysis to Table 1 for Grade 1335, unless a custom clause 5.2 / Table 2 analysis is written on the order; request Supplementary Requirement S2 product analysis only if the project needs it
Mechanical tests If tensile properties are required, specify them as a tensile-strength range whose width is not less than Table 3, and confirm compatibility with composition, condition and thickness
Other tests S1 vacuum treatment or S8 ultrasonic examination only when written on the order
Repair welding State any limitation or required procedure approval (clause 4.5.2)
Documentation State the inspection document type required by the project
Processing Cutting or other processing only when requested; thermal-cutting practice depends on condition and thickness

FAQ

Is ASTM A829 1335 ordered by chemistry or by mechanical properties?
Usually by chemical composition, to Table 1 of A829/A829M-00 for this named grade. Tensile properties may also be specified when they are compatible with the composition, delivery condition and plate thickness. If tensile properties are specified, the specified tensile-strength range must be at least as wide as Table 3 of the 2000 edition. Table 3 is a range-width rule, not a minimum yield or tensile strength.
How does Grade 1335 differ from the other 13xx plate grades, or from chromium-molybdenum grades such as 4130?
In A829/A829M-00 Table 1 the 13xx grades share manganese 1.50-1.90 % and have no listed nickel, chromium, molybdenum or vanadium requirement. They differ by carbon window: 1330 is 0.27-0.34 %, 1335 is 0.32-0.39 %, 1340 is 0.36-0.44 % and 1345 is 0.41-0.49 %. Grade 1335 is listed at carbon 0.32-0.39 %. Grade 4130 is a chromium-molybdenum plate with a much lower manganese window on its manufacturer page. The grades are related by engineering use, not interchangeable supply.
Does ASTM A829/A829M-00 list quenched-and-tempered 1335 plate?
No. The 2000 edition lists Condition AR, A, N and NT only. If the project needs another processing route, that route must be written explicitly on the order and agreed. Do not read typical quenched-and-tempered bar figures for SAE 1335 as automatic plate minima.
Are the numbers on this page from the current 2025 edition?
No. The heat-analysis windows and the Table 3 tensile-range widths on this page are taken from ASTM A829/A829M-00 (2000). If your project specifies a later edition, write that edition on the enquiry so we can review it against the ordered text.
What should a quotation enquiry include?
The ordered ASTM A829/A829M edition, Grade 1335, delivery condition, thickness by width by length, quantity, any tensile range (if required) or other extra tests, any NDE, any limit on repair welding, and the inspection document required by the project.

Request a quotation

Contact SHH STEEL for a quotation for ASTM A829 Grade 1335 alloy steel plate. Please include your required quantity, plate thickness, width and length, delivery destination and preferred delivery schedule so we can review your production and export requirements.

Specify the ASTM edition your project requires and the delivery condition: as-rolled, annealed, normalized, or normalized and tempered. If your project requires tensile, hardness, toughness or ultrasonic testing, include the acceptance criteria and the inspection document required. Any specified tensile strength should be written as a range whose width is not less than Table 3 of A829/A829M-00, and it must be compatible with the chemistry, delivery condition and plate thickness.

If your enquiry compares Grade 1335 with Grade 4140, Grade 4130 or a strength-graded structural plate such as A572 Grade 50, identify each grade clearly. We will review the differences in product form, chemistry and supply condition rather than assume that related grades are interchangeable.

For a detailed quotation, email your material specification, quantity and delivery requirements to our team.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X