ASTM A690 Steel Sheet Pile

ASTM A690 steel sheet pile is marine high-strength low-alloy sheet piling with a 50 ksi [345 MPa] minimum yield, a 70 ksi [485 MPa] minimum tensile strength, and specified nickel, copper and phosphorus. The page lists typical hot-rolled Z-type mill series by geometry and distinguishes A328 and A572 Grade 50.
Keywords
ASTM A690 Steel Sheet Pile, A690 sheet pile, marine sheet piling, ASTM A690, nickel copper phosphorus steel
Equivalent Grades:
ASTM A328; ASTM A572 Grade 50 — comparisons only, not automatic substitutes. A690 H-piles used as bearing piles are a different product.
Share:
General Description
Material Specification
Available Sizes of ASTM A690 Steel Sheet Pile
Chemical Composition of ASTM A690
Mechanical Properties of ASTM A690
Shape Tolerances and Identification
Delivery Conditions, Inspection and Identification
Applications and Service Limits
ASTM A690 Compared with A328 and A572
Near-Equivalents: Not Automatic Substitutes
Sourcing ASTM A690 Steel Sheet Piles from SHH STEEL
FAQ
Conclusion

What is ASTM A690 Steel Sheet Pile?

ASTM A690 steel sheet pile is high-strength low-alloy nickel, copper and phosphorus steel sheet piling to ASTM A690/A690M, intended for marine structures where atmospheric-corrosion resistance in the splash zone is specified. Grade 50 has a minimum yield of 50 ksi [345 MPa], a minimum tensile strength of 70 ksi [485 MPa], and a minimum elongation of 18% in 8 in. [200 mm]. Nickel, copper and phosphorus are specified; they are not optional extras.

Dimensions follow the ordered A6/A6M or project profile series. These piles are filed under the steel sheet piles category in the steel structural profiles catalog. A690 is not A328 or A572 sheet piling, and it is not a weathering plate grade used as a silent substitute. H-piles to A690 used as bearing piles are a different product from interlocking sheet piles and are not tabulated here.

Material, Dimensions and the A690 Grade

The purchase order and the inspection document should name, separately:

  • ASTM A690/A690M and its edition (the ordered edition governs), as marine sheet piling;
  • the section geometry and the required length, to A6/A6M or the project series;
  • any agreed coating, higher-yield modification, interlock strength or impact test. A modified higher-yield A690 is a special agreement, not a default of the grade table on this page.

A690 is not A328 and is not A572.

ASTM A690 Sizes: Typical Hot-Rolled Mill Series

Dimensions follow the ordered ASTM A6/A6M or project profile series and are stated separately from the material grade. The tables below are typical published mill series, described by geometry only. They are not an ASTM A6 size table, and trade names are not used. A North American Z-type of a given width is not a European Z-type or a JIS U-type of similar width.

Some mill programs also offer this grade on the typical European hot-rolled U-type and Z-type series tabulated on the EN 10248-1 S355GP U-type and Z-type steel sheet pile page. Nominate the geometry on the enquiry; not every section is offered in every grade.

Typical North American hot-rolled Z-type mill series

Typical North American hot-rolled Z-type mill series, described by geometry only. These are published mill-series dimensions, not an ASTM A6 size table, and trade names are not used.

Swipe horizontally to view all dimensions.

Geometry (type × width × height × thickness) Effective width (mm) Height (mm) Flange thickness (mm) Web thickness (mm) Sectional area (cm²/m) Mass, single pile (kg/m) Wall mass (kg/m²) Moment of inertia (cm⁴/m) Elastic section modulus (cm³/m)
Z-type 559 × 229 × 9.50 559 229 9.50 9.50 136.9 60.0 107.4 11,500 973
Z-type 457 × 305 × 9.50 457 305 9.50 9.50 168.1 60.3 131.8 25,200 1,620
Z-type 575 × 378 × 15.21 / 12.67 575 378 15.21 12.67 217.8 98.2 170.9 49,300 2,608
Z-type 500 × 409 × 15.21 / 12.67 500 409 15.21 12.67 249.1 97.6 195.3 67,000 3,263

ASTM A690 Chemical Composition

The figures below are the A690 limits as reprinted in an official mill specification sheet. Carbon is 0.22% maximum. Manganese is 0.60% to 0.90%, with the mill footnote that for each 0.01% carbon below the maximum, manganese may rise 0.06% up to 1.10%; the ordered edition governs that footnote. Silicon is 0.40% maximum. Phosphorus is 0.08% to 0.15%, sulphur 0.04% maximum, copper 0.50% minimum, and nickel 0.40% to 0.75%. Do not treat A690 chemistry as an A572 or A328 analysis with copper added.

Swipe horizontally to view all dimensions.

Grade C max Mn Si max P S max Cu min Ni
A690 0.22 0.60–0.90 0.40 0.08–0.15 0.04 0.50 0.40–0.75

ASTM A690 Mechanical Properties

The tensile values below are the A690 Grade 50 minima. Elongation is 18% minimum in 8 in. [200 mm]. There is no default Charpy requirement unless one is agreed on the order. A modified higher-yield A690 is supplied only when it is named as a special agreement.

Grade Min. yield Min. tensile Min. elongation in 8 in. [200 mm]
A690 Grade 50 50 ksi [345 MPa] 70 ksi [485 MPa] 18%

Shape Tolerances and Identification

Shape, mass and length tolerances for these sections follow ASTM A6/A6M unless the order states otherwise. A typical mill mass tolerance under A6 is ± 2.5%, and length is commonly plus a stated allowance and minus zero; the ordered A6 edition governs.

A typical inspection mark identifies the specification, the geometry, the heat number, the producer and the length. An A690 certificate is not an A328 or A572 certificate, and an A690 sheet-pile mark is not an A690 H-pile mark.

Delivery Conditions, Inspection and Identification

These piles are commonly supplied as-rolled. The inspection document should identify ASTM A690/A690M and its edition, the section geometry, the length, the heat analysis including nickel, copper and phosphorus, and the tensile results. A plate or weathering-steel certificate does not, by itself, identify A690 sheet piling.

Applications and Service Limits

ASTM A690 steel sheet piles are used in marine structures, splash-zone walls and similar interlocking-wall works where the A690 atmospheric-corrosion chemistry is named. They are not a silent substitute for ASTM A328 carbon steel sheet pile or for ASTM A572 Grade 50 steel sheet pile, and they are not an A690 bearing pile. Interlocks of similar width are not interchangeable by depth or mass alone.

ASTM A690 Compared with A328 and A572

The comparisons below are an orientation only; they are not automatic substitutes.

Grade / designation Standard Relationship to ASTM A690 Caution
ASTM A328 ASTM A328/A328M Carbon steel sheet piling, without the nickel, copper and phosphorus ranges of A690. A328 is not A690. See ASTM A328 carbon steel sheet pile.
ASTM A572 Grade 50 ASTM A572/A572M A high-strength low-alloy grade with the same 50 ksi yield but a lower tensile minimum and different chemistry. A572 is not A690. See ASTM A572 Grade 50 steel sheet pile.
A690 H-piles ASTM A690/A690M The same specification also covers H-piles for marine use. An A690 H-pile used as a bearing pile is a different product from interlocking sheet piles and is not filed on this page.

Near-Equivalents: Not Automatic Substitutes

A near-equivalent is a starting point for a discussion, not a licence to swap certificates. If a project names ASTM A690 sheet piling, keep that specification, chemistry and geometry on the order. Related pages include ASTM A328 carbon steel sheet pile and ASTM A572 Grade 50 steel sheet pile.

Sourcing ASTM A690 Steel Sheet Piles from SHH STEEL

SHH STEEL supplies ASTM A690 steel sheet piles against a named geometry, the material edition and the inspection document type. Enquiries should state the type and geometry, the length, and any coating, corner piles or interlock-strength requirements.

The size tables are typical published mill series, not a claim that every section is rolled in this grade. Once the list is clear, a quotation can be prepared against the stated edition and certificate.

ASTM A690 Steel Sheet Pile FAQs

Is ASTM A690 the same as A572 Grade 50?
No. Both have a 50 ksi [345 MPa] minimum yield, but A690 has a 70 ksi [485 MPa] tensile minimum and specified ranges for nickel, copper and phosphorus. An A572 certificate is not an A690 certificate.
Does this page cover A690 H-piles?
No. H-piles to A690 used as bearing piles are a different product from interlocking sheet piles and are not filed under this sheet-pile leaf.
Which chemical ranges make A690 a marine grade?
The mill reprint used for this page specifies nickel 0.40–0.75%, copper 0.50% minimum, and phosphorus 0.08–0.15%, together with carbon, manganese, silicon and sulphur limits. The ordered edition of A690/A690M governs.
Are the size tables an official ASTM A6 list?
No. They are typical published mill series described by geometry. Dimensions follow the ordered A6/A6M or project profile series. Trade names are not used.

Request a Quotation for ASTM A690 Steel Sheet Pile

ASTM A690 steel sheet pile is marine high-strength low-alloy sheet piling with a 50 ksi [345 MPa] minimum yield and a 70 ksi [485 MPa] minimum tensile strength, and with specified nickel, copper and phosphorus. Nominate the geometry, ASTM A690/A690M or the edition on the order, the length, and the inspection document type. Send the size list, edition, certificate type and any processing notes; SHH STEEL will review the package and quote accordingly.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X