ASTM A666 UNS S20100 Cold Worked Stainless Steel Sheet at SHH STEEL warehouse

ASTM A666 UNS S20100 Cold Worked Stainless Steel Sheet

ASTM A666 UNS S20100 Cold Worked Stainless Steel Sheet: cold-worked Cr-Mn-Ni-N austenitic (200 series) grade to ASTM A666, sheet in 2B and No.1 finishes from stock in China. SHH STEEL supplies mill-direct material with EN 10204 3.1/3.2 certificates, third-party inspection and cutting to size.
Keywords
A666 S20100 sheet, S20100 sheet, S20100 stainless sheet supplier, ASTM A666 S20100, S20100 sheet stock China
Equivalent Grades:
EN 1.4372 X12CrMnNiN17-7-5; GB/T 12Cr17Mn6Ni5N (S35350)
Share:
Overview
Specification
Chemical Composition
Mechanical Properties
Performance
Grade Selection
Heat Treatment
Surface Finishes
Tolerances
Stock
Equivalent Grades
Related Grades
Applications and Fabrication
Testing and Inspection
Specification Mistakes
Buyer Concerns
How to Order
FAQ
Conclusion

What is ASTM A666 UNS S20100 Cold Worked Stainless Steel Sheet?

Technical reviewer: Jack · Updated: 2026-10-21

Equivalent grades: UNS S20100 (Type 201) ≈ EN 1.4372 X12CrMnNiN17-7-5 ≈ GB/T 12Cr17Mn6Ni5N (S35350).

UNS S20100 (Type 201) is a cold-worked Cr-Mn-Ni-N austenitic (200 series) grade. Type 201 replaces part of the nickel of 301 with manganese and nitrogen. Cold worked, it reaches 301-type strength at lower alloy cost, but its corrosion resistance is lower than 301 and 304.

ASTM A666 covers austenitic stainless steel sheet, strip, plate and flat bar in the annealed condition or cold worked to defined tempers: 1/16, 1/8, 1/4, 1/2, 3/4 and full hard, depending on the grade. It is the specification used when high-strength stainless sheet is bought for structural, transport and spring applications.

This page sets out the ASTM A666 requirements for UNS S20100 (Type 201) sheet: specification summary, chemistry, mechanical properties, corrosion resistance, heat treatment, finishes and tolerances, current stock, equivalents, fabrication and testing. SHH STEEL supplies it mill-direct from China with EN 10204 3.1 certificates, optional third-party inspection and in-house cutting.

UNS S20100 (Type 201) sheet: specification summary

Item UNS S20100 (Type 201) data
Standard ASTM A666, annealed or cold-worked austenitic stainless steel sheet, strip, plate and flat bar
General requirements ASTM A480/A480M
Conditions annealed, or cold worked to 1/16, 1/8, 1/4, 1/2, 3/4 or full hard (grade-dependent)
Ordering temper may be ordered by tensile strength or by yield strength
Typical gauges 0.3–3.0 mm cold rolled
Widths up to 1250 mm; slit coil to order
Finishes 2B and bright cold-rolled; tempered sheet is not annealed after rolling
Certificates EN 10204 3.1; 3.2 on request
Grade family Cr-Mn-Ni-N austenitic (200 series)

Size range. Sheet is normally cold rolled from about 0.3–0.5 mm up to 3 mm and hot rolled from about 3 mm to just under 5 mm. Coil widths of 1000, 1219, 1250 and 1500 mm are standard; slitting and cut-to-length lines produce narrower strip and exact lengths. Sheets thinner than 0.5 mm or wider than 1500 mm should be confirmed before ordering. UNS S20100 (Type 201) is one of the high-volume grades produced by most Chinese stainless mills, so common sizes are held in stock and non-stock sizes are usually rolled within a normal mill cycle.

Chemical composition of UNS S20100 (Type 201) (ASTM A666)

Element wt %
C 0.15 max
Si 1.00 max
Mn 5.5–7.5
P 0.060 max
S 0.030 max
Cr 16.0–18.0
Ni 3.5–5.5
N 0.25 max

Single values are maximums unless marked min. Ranges are heat (cast) analysis limits.

PREN check (Cr + 3.3 Mo + 16 N): about 16.0 at the specification minimums and about 19.0 at mid-range. Where corrosion resistance is critical, write a minimum PREN on the order and ask for the calculated value from the heat analysis on the certificate.

Mechanical properties of UNS S20100 (Type 201) sheet

Condition Yield strength 0.2 %, min Tensile strength, min
annealed 260 (201-1) / 310 (201-2) MPa 515 (201-1) / 655 (201-2) MPa (El. 40 % min)
1/16 hard 310 MPa 655 MPa
1/8 hard 380 MPa 690 MPa
1/4 hard 515 MPa 860 MPa
1/2 hard 760 MPa 1035 MPa
3/4 hard 930 MPa 1205 MPa
full hard 965 MPa 1275 MPa

A666 tempers can be ordered by tensile strength or by yield strength, and the purchaser should state which. The minimum annealed yield strength is 260 (201-1) / 310 (201-2) MPa; at 1/2 hard the minimum yield strength is about four times higher. Elongation, bend radius and the gauges for which each temper is available fall as the temper rises; check the A666 table for your thickness before you design a bend. Cold-worked sheet loses its temper if it is heated above about 425 °C, so welding reduces strength locally.

Corrosion resistance of UNS S20100 (Type 201): PREN and limits

The 200-series grades replace part of the nickel with manganese and nitrogen. Nitrogen raises the annealed strength, and the lower nickel makes the price more stable than 304. The PREN at the specification minimum is about 16.0, lower than 304, so the grades are used for indoor, dry or lightly corrosive service.

Buyers should be aware that low-cost 200-series material sometimes comes with copper or lower chromium than the standard allows. Always check the certificate chemistry, and do not use 200-series in coastal, chloride or acidic environments where 304 or 316 is needed.

How UNS S20100 (Type 201) compares with related grades

Grade Cr Ni Mo N PREN (min) YS / Rp0.2 min, MPa
UNS S20100 (Type 201) 16.0–18.0 3.5–5.5 — 0.25 max 16.0 260
12Cr17Mn6Ni5N (S35350) 16.00–18.00 3.50–5.50 — 0.05–0.25 16.8 per standard
12Cr18Mn9Ni5N (S35450) 17.00–19.00 4.00–6.00 — 0.05–0.25 17.8 per standard
UNS S20153 (Type 201LN) 16.0–17.5 4.0–5.0 — 0.10–0.25 17.6 310

Choose UNS S20100 (Type 201) for cost-sensitive indoor products where 304-level corrosion resistance is not required. For outdoor, coastal or food-contact service with salt or acids, use 304 or 316.

The table uses specification limits, not typical mill values, so it shows the guaranteed position of each grade. Final selection should also consider product availability in the thickness you need, welding consumables, and the inspection requirements of your project.

Heat treatment and delivery condition of UNS S20100 (Type 201)

Heat treatment: annealed condition: solution annealed, rapid cooling; tempers produced by cold rolling.

200-series grades are solution annealed and cooled rapidly. They work-harden faster than 304, so intermediate anneals may be needed in multi-stage forming.

Surface finishes for UNS S20100 (Type 201) sheet

Cold-worked sheet is supplied with a bright cold-rolled or 2B-type surface; it is not annealed after the final rolling pass, so it keeps its temper. Annealed A666 sheet comes as 2B or 2D. Protective film is recommended for visible transport and architectural panels.

Dimensions, tolerances and flatness

Dimensional tolerances follow ASTM A480/A480M. Tempered sheet is harder to level, so flatness should be agreed, especially for 1/2 hard and harder tempers. Bend-test and elongation requirements in A666 depend on thickness and temper; check the table for your gauge.

Ordering tempers. An A666 order should state the grade, the condition (annealed or the temper), whether the temper is defined by tensile or yield strength, thickness and width, finish, edge and flatness. Because tempers are rolled to order, small quantities of unusual tempers have longer lead times; 1/4 and 1/2 hard are the most common for structural sheet. For railway and bus structures, the purchaser often adds weldability or crash-test requirements from the vehicle specification.

UNS S20100 (Type 201) sheet stock in China

Thickness (mm) Width (mm) Length (mm) Finish Approx. quantity Location
0.5 1000 / 1219 2000 / 2438 2B 300+ t China
0.8 1219 2438 2B 300+ t China
1.0 1219 / 1250 2438 / 2500 2B 300+ t China
1.5 1219 / 1500 2438 / 3000 2B 200+ t China
2.0 1219 / 1500 2438 / 3000 2B 200+ t China
3.0 1500 3000 2B / No.1 100+ t China
4.0 1500 3000 / 6000 No.1 100+ t China

Quantities are approximate and stock changes daily. Send your size list for current availability; other thicknesses, widths and cut sizes can be supplied from mill production.

Packing and logistics. Sheet is packed on wooden or steel pallets with interleaving paper or PVC film, edge protectors and waterproof wrapping, typically 2–3 t per pallet. Coil is packed eye-to-wall or eye-to-sky with steel bands. We consolidate mixed grades and sizes into one container and send loading photos with the shipping documents.

UNS S20100 (Type 201) equivalents in other standards

Standard Designation Comment
EN 1.4372 X12CrMnNiN17-7-5 same alloy family and limits closely matched; compare each limit on the certificate
GB/T 12Cr17Mn6Ni5N (S35350) same alloy family and limits closely matched; compare each limit on the certificate

Equivalents are close, not identical. When a project names one standard, order to that standard or ask for multiple certification and check every limit on the certificate.

Related grades by alloy family

Same standard

Other grades in this standard: 1.4310 plate, 1.4318 plate, SUS301 (G4304), A666 S30100, A666 S30103, A666 S30153.

200 series (Cr-Mn-Ni-N)

Lower-nickel 200-series grades: A240 S20200, A240 S30100, A240 S30400.

Austenitic

General-purpose austenitic grades for comparison: A240 S30403, A240 S31600, A240 S31603.

Same grade, other specification

A240 S20100.

Applications, forming and welding of UNS S20100 (Type 201)

Typical uses: railway car bodies, bus and truck frames, structural members, conveyor parts, springs, clips, fasteners, and architectural trim.

200-series sheet work-hardens quickly; allow for higher forming loads than 304. Cut by plasma, laser or waterjet and remove heat tint by pickling or grinding. For welding use an ER308L or ER309L filler; nitrogen-bearing 200-series welds should be kept short and the heat input moderate. Keep the weld area clean and free of carbon-steel contamination, and pickle and passivate after welding where corrosion resistance matters.

Welding practice. 200-series sheet welds like 304 but has a higher work-hardening rate and slightly higher thermal expansion. Use moderate heat input, keep the weld area clean and pickle afterwards. Avoid using 200-series filler in corrosive service; a 308L or 309L filler gives a more corrosion-resistant weld.

Certificates, testing and receiving inspection

Every delivery carries a mill certificate to ASTM A480/A480M with heat analysis, tensile results and hardness, and the grade and standard as ordered. Supplementary tests we can arrange: chemistry check of Cr, Ni, Mn, Cu and N on every heat, intergranular corrosion test where specified, and PMI. Third-party witness by SGS, BV, TÜV, DNV, ABS or LR is available with EN 10204 3.2 certificates.

On receipt, check marking and heat number against the certificate, measure thickness at several points and confirm the finish and edge condition before cutting.

Common mistakes when specifying UNS S20100 (Type 201)

  • Accepting 200-series material with copper or low chromium outside the standard.
  • Using it in coastal or chloride service.
  • Not checking the certificate for nitrogen and manganese ranges.

Each of these can be avoided by writing the requirement into the purchase order and checking it on the certificate before the material is cut.

Sourcing UNS S20100 (Type 201): buyer concerns and SHH STEEL solutions

Concern How SHH STEEL handles it
Off-spec low-cost 200-series full heat chemistry including Cu and N checked against the standard
Corrosion complaints in service application reviewed; 304 or 316 recommended where chlorides are present
Small quantities across many sizes mixed thicknesses and grades combined in one shipment
Cutting and edge preparation in-house shearing, plasma, laser and waterjet cutting, bevelling
Delivery delays weekly production and shipping updates with photos

How to order UNS S20100 (Type 201) sheet

State the standard and edition (ASTM A666), the grade (UNS S20100 (Type 201)), thickness, width and length or coil, finish, quantity, tolerance class, any added chemistry limits, the supplementary tests and acceptance values from your specification, the certificate type and inspection agency, and packing. Send the list to SHH STEEL and we will reply with price, available stock and lead time.

FAQ

Can I order A666 S20100 by yield strength instead of temper name?
Yes. A666 allows tempers to be ordered by minimum tensile or minimum yield strength. State the value and the gauge, and we will confirm which temper the mill will roll to.
Is UNS S20100 (Type 201) equivalent to EN 1.4372 X12CrMnNiN17-7-5?
They are the same alloy designation in different standards. Limits are closely matched, but always order to the standard named in your specification or ask for multiple certification.
Can UNS S20100 (Type 201) replace 304?
Only in dry indoor applications. Its corrosion resistance is lower than 304, especially in chloride or acidic environments.
Can I order small quantities or cut sizes?
Yes. We combine mixed thicknesses and grades into one shipment and cut plate and sheet to size in our workshop.
Which certificates and tests can you provide?
Every order ships with a mill certificate (EN 10204 3.1 type) showing heat analysis and mechanical tests. Supplementary tests and 3.2 certificates with SGS, BV, TÜV or another agency are available by agreement.

Conclusion

UNS S20100 (Type 201) sheet should be ordered with the points the standard leaves open written into the contract: finish, tolerance class, any extra chemistry limits and the supplementary tests your application needs. With those fixed, stock material from China is a fast and reliable route.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X