ASTM A666 UNS S30400 Cold Worked Stainless Steel Sheet at SHH STEEL warehouse

ASTM A666 UNS S30400 Cold Worked Stainless Steel Sheet

ASTM A666 UNS S30400 Cold Worked Stainless Steel Sheet: cold-worked austenitic grade to ASTM A666, sheet in 2B and No.1 finishes from stock in China. SHH STEEL supplies mill-direct material with EN 10204 3.1/3.2 certificates, third-party inspection and cutting to size.
Keywords
A666 S30400 sheet, S30400 sheet, S30400 stainless sheet supplier, ASTM A666 S30400, S30400 sheet stock China
Equivalent Grades:
EN 1.4301 X5CrNi18-10; GB/T 06Cr19Ni10 (S30408); JIS SUS304
Share:
Overview
Specification
Chemical Composition
Mechanical Properties
Performance
Grade Selection
Heat Treatment
Surface Finishes
Tolerances
Stock
Equivalent Grades
Related Grades
Applications and Fabrication
Testing and Inspection
Specification Mistakes
Buyer Concerns
How to Order
FAQ
Conclusion

What is ASTM A666 UNS S30400 Cold Worked Stainless Steel Sheet?

Technical reviewer: Jack · Updated: 2026-10-21

Equivalent grades: UNS S30400 (Type 304) ≈ EN 1.4301 X5CrNi18-10 ≈ GB/T 06Cr19Ni10 (S30408) ≈ JIS SUS304.

UNS S30400 (Type 304) is a cold-worked austenitic grade. Type 304 work-hardens more slowly than 301, so A666 limits it to the lower tempers. Cold-worked 304 sheet is used where the corrosion resistance of 304 is needed with higher strength or springiness.

ASTM A666 covers austenitic stainless steel sheet, strip, plate and flat bar in the annealed condition or cold worked to defined tempers: 1/16, 1/8, 1/4, 1/2, 3/4 and full hard, depending on the grade. It is the specification used when high-strength stainless sheet is bought for structural, transport and spring applications.

This page sets out the ASTM A666 requirements for UNS S30400 (Type 304) sheet: specification summary, chemistry, mechanical properties, corrosion resistance, heat treatment, finishes and tolerances, current stock, equivalents, fabrication and testing. SHH STEEL supplies it mill-direct from China with EN 10204 3.1 certificates, optional third-party inspection and in-house cutting.

UNS S30400 (Type 304) sheet: specification summary

Item UNS S30400 (Type 304) data
Standard ASTM A666, annealed or cold-worked austenitic stainless steel sheet, strip, plate and flat bar
General requirements ASTM A480/A480M
Conditions annealed, or cold worked to 1/16, 1/8, 1/4, 1/2, 3/4 or full hard (grade-dependent)
Ordering temper may be ordered by tensile strength or by yield strength
Typical gauges 0.3–3.0 mm cold rolled
Widths up to 1250 mm; slit coil to order
Finishes 2B and bright cold-rolled; tempered sheet is not annealed after rolling
Certificates EN 10204 3.1; 3.2 on request
Grade family austenitic

Size range. Sheet is normally cold rolled from about 0.3–0.5 mm up to 3 mm and hot rolled from about 3 mm to just under 5 mm. Coil widths of 1000, 1219, 1250 and 1500 mm are standard; slitting and cut-to-length lines produce narrower strip and exact lengths. Sheets thinner than 0.5 mm or wider than 1500 mm should be confirmed before ordering. UNS S30400 (Type 304) is produced regularly by several mills; common sizes are held in stock, and other sizes are rolled in the mill’s scheduled campaigns for the grade.

Chemical composition of UNS S30400 (Type 304) (ASTM A666)

Element wt %
C 0.07 max
Si 0.75 max
Mn 2.00 max
P 0.045 max
S 0.030 max
Cr 17.5–19.5
Ni 8.0–10.5
N 0.10 max

Single values are maximums unless marked min. Ranges are heat (cast) analysis limits.

PREN check (Cr + 3.3 Mo + 16 N): about 17.5 at the specification minimums and about 19.3 at mid-range. Where corrosion resistance is critical, write a minimum PREN on the order and ask for the calculated value from the heat analysis on the certificate.

Mechanical properties of UNS S30400 (Type 304) sheet

Condition Yield strength 0.2 %, min Tensile strength, min
annealed 205 MPa 515 MPa (El. 40 % min)
1/16 hard 310 MPa 550 MPa
1/8 hard 380 MPa 690 MPa
1/4 hard 515 MPa 860 MPa
1/2 hard 760 MPa 1035 MPa

A666 tempers can be ordered by tensile strength or by yield strength, and the purchaser should state which. The minimum annealed yield strength is 205 MPa; at 1/2 hard the minimum yield strength is about four times higher. Elongation, bend radius and the gauges for which each temper is available fall as the temper rises; check the A666 table for your thickness before you design a bend. Cold-worked sheet loses its temper if it is heated above about 425 °C, so welding reduces strength locally.

Corrosion resistance of UNS S30400 (Type 304): PREN and limits

Austenitic stainless steels are non-hardenable by heat treatment, tough down to cryogenic temperatures and easy to form and weld. Corrosion resistance rises with chromium, molybdenum and nitrogen; the PREN of this grade at the specification minimum is about 17.5. Low-carbon (L) and stabilised versions protect welds against intergranular corrosion.

Austenitic grades are prone to chloride stress-corrosion cracking above about 60 °C in chloride environments. Where that risk exists, duplex or super-austenitic grades are the usual upgrade. Cold work raises strength but also makes some grades slightly magnetic.

How UNS S30400 (Type 304) compares with related grades

Grade Cr Ni Mo N PREN (min) YS / Rp0.2 min, MPa
UNS S30400 (Type 304) 17.5–19.5 8.0–10.5 — 0.10 max 17.5 205
UNS S30100 (Type 301) 16.0–18.0 6.0–8.0 — 0.10 max 16.0 205
UNS S30103 (Type 301L) 16.0–18.0 6.0–8.0 — 0.20 max 16.0 220
UNS S30153 (Type 301LN) 16.0–18.0 6.0–8.0 — 0.07–0.20 17.1 240

Choose UNS S30400 (Type 304) for general corrosion resistance with easy forming and welding. In warm chloride environments consider a molybdenum-bearing or duplex grade instead.

The table uses specification limits, not typical mill values, so it shows the guaranteed position of each grade. Final selection should also consider product availability in the thickness you need, welding consumables, and the inspection requirements of your project.

Heat treatment and delivery condition of UNS S30400 (Type 304)

Heat treatment: annealed condition: solution annealed, rapid cooling; tempers produced by cold rolling.

Austenitic grades are solution annealed and cooled rapidly to keep carbides in solution. They cannot be hardened by heat treatment, only by cold work.

Surface finishes for UNS S30400 (Type 304) sheet

Cold-worked sheet is supplied with a bright cold-rolled or 2B-type surface; it is not annealed after the final rolling pass, so it keeps its temper. Annealed A666 sheet comes as 2B or 2D. Protective film is recommended for visible transport and architectural panels.

Dimensions, tolerances and flatness

Dimensional tolerances follow ASTM A480/A480M. Tempered sheet is harder to level, so flatness should be agreed, especially for 1/2 hard and harder tempers. Bend-test and elongation requirements in A666 depend on thickness and temper; check the table for your gauge.

Ordering tempers. An A666 order should state the grade, the condition (annealed or the temper), whether the temper is defined by tensile or yield strength, thickness and width, finish, edge and flatness. Because tempers are rolled to order, small quantities of unusual tempers have longer lead times; 1/4 and 1/2 hard are the most common for structural sheet. For railway and bus structures, the purchaser often adds weldability or crash-test requirements from the vehicle specification.

UNS S30400 (Type 304) sheet stock in China

Thickness (mm) Width (mm) Length (mm) Finish Approx. quantity Location
0.5 1000 / 1219 2000 / 2438 2B 200+ t China
0.8 1219 2438 2B 200+ t China
1.0 1219 / 1250 2438 / 2500 2B 100+ t China
1.5 1219 / 1500 2438 / 3000 2B 100+ t China
2.0 1219 / 1500 2438 / 3000 2B 100+ t China
3.0 1500 3000 2B / No.1 100+ t China
4.0 1500 3000 / 6000 No.1 100+ t China

Quantities are approximate and stock changes daily. Send your size list for current availability; other thicknesses, widths and cut sizes can be supplied from mill production.

Packing and logistics. Sheet is packed on wooden or steel pallets with interleaving paper or PVC film, edge protectors and waterproof wrapping, typically 2–3 t per pallet. Coil is packed eye-to-wall or eye-to-sky with steel bands. We consolidate mixed grades and sizes into one container and send loading photos with the shipping documents.

UNS S30400 (Type 304) equivalents in other standards

Standard Designation Comment
EN 1.4301 X5CrNi18-10 same alloy family and limits closely matched; compare each limit on the certificate
GB/T 06Cr19Ni10 (S30408) same alloy family and limits closely matched; compare each limit on the certificate
JIS SUS304 same alloy family and limits closely matched; compare each limit on the certificate

Equivalents are close, not identical. When a project names one standard, order to that standard or ask for multiple certification and check every limit on the certificate.

Related grades by alloy family

Same standard

Other grades in this standard: 1.4310 plate, 1.4318 plate, SUS301 (G4304), A666 S30100, A666 S30103, A666 S30153.

Austenitic

General-purpose austenitic grades for comparison: A240 S30403, A240 S31600, A240 S31603, A240 S30500, A240 S32100.

Same grade, other specification

A240 S30400.

Applications, forming and welding of UNS S30400 (Type 304)

Typical uses: railway car bodies, bus and truck frames, structural members, conveyor parts, springs, clips, fasteners, and architectural trim.

Austenitic sheet and plate form and weld easily. Cut by plasma, laser or waterjet and remove heat tint by pickling or grinding. For welding use an ER308L, ER316L or ER347 filler matching the grade (AWS A5.9). Keep the weld area clean and free of carbon-steel contamination, and pickle and passivate after welding where corrosion resistance matters.

Welding practice. Austenitic sheet is welded with GTAW, GMAW, SMAW or laser without preheat. Keep the interpass temperature below about 150 °C, use back-purging on corrosion-critical joints and pickle afterwards. Low-carbon or stabilised grades avoid sensitisation; standard-carbon grades used at temperature may need a solution anneal after heavy welding.

Certificates, testing and receiving inspection

Every delivery carries a mill certificate to ASTM A480/A480M with heat analysis, tensile results and hardness, and the grade and standard as ordered. Supplementary tests we can arrange: intergranular corrosion testing (ASTM A262 Practice E or EN ISO 3651-2 / GB/T 4334), PMI and surface inspection. Third-party witness by SGS, BV, TÜV, DNV, ABS or LR is available with EN 10204 3.2 certificates.

On receipt, check marking and heat number against the certificate, measure thickness at several points and confirm the finish and edge condition before cutting.

Common mistakes when specifying UNS S30400 (Type 304)

  • Mixing L and standard-carbon grades in welded equipment.
  • Leaving out the finish and film side for visible parts.
  • Using the grade in warm chlorides where stress-corrosion cracking is likely.

Each of these can be avoided by writing the requirement into the purchase order and checking it on the certificate before the material is cut.

Sourcing UNS S30400 (Type 304): buyer concerns and SHH STEEL solutions

Concern How SHH STEEL handles it
Mixed-up 304/316 or L/non-L grades PMI and heat-number tracking for every sheet
Surface scratches on finished sheet PVC film, interleaving paper and wooden-case packing
Small quantities across many sizes mixed thicknesses and grades combined in one shipment
Cutting and edge preparation in-house shearing, plasma, laser and waterjet cutting, bevelling
Delivery delays weekly production and shipping updates with photos

How to order UNS S30400 (Type 304) sheet

State the standard and edition (ASTM A666), the grade (UNS S30400 (Type 304)), thickness, width and length or coil, finish, quantity, tolerance class, any added chemistry limits, the supplementary tests and acceptance values from your specification, the certificate type and inspection agency, and packing. Send the list to SHH STEEL and we will reply with price, available stock and lead time.

FAQ

Can I order A666 S30400 by yield strength instead of temper name?
Yes. A666 allows tempers to be ordered by minimum tensile or minimum yield strength. State the value and the gauge, and we will confirm which temper the mill will roll to.
Is UNS S30400 (Type 304) equivalent to EN 1.4301 X5CrNi18-10?
They are the same alloy designation in different standards. Limits are closely matched, but always order to the standard named in your specification or ask for multiple certification.
Is UNS S30400 (Type 304) magnetic?
It is essentially non-magnetic when annealed; cold work can make it slightly magnetic.
Can I order small quantities or cut sizes?
Yes. We combine mixed thicknesses and grades into one shipment and cut plate and sheet to size in our workshop.
Which certificates and tests can you provide?
Every order ships with a mill certificate (EN 10204 3.1 type) showing heat analysis and mechanical tests. Supplementary tests and 3.2 certificates with SGS, BV, TÜV or another agency are available by agreement.

Conclusion

UNS S30400 (Type 304) sheet should be ordered with the points the standard leaves open written into the contract: finish, tolerance class, any extra chemistry limits and the supplementary tests your application needs. With those fixed, stock material from China is a fast and reliable route.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X