ASTM A204 Grade C Steel Plate
What is ASTM A204 Grade C steel plate?
ASTM A204 Grade C Steel Plate is molybdenum-alloy steel plate for welded boilers and other pressure vessels under ASTM A204/A204M-17 (Reapproved 2022), Standard Specification for Pressure Vessel Plates, Alloy Steel, Molybdenum. That edition was approved 1 September 2022 and reapproves A204/A204M-17. The specification is available in three grades with different strength levels. Grade C has a Table 2 tensile strength of 75–95 ksi [515–655 MPa] and a minimum yield strength of 43 ksi [295 MPa].
Clause 1.2 lists only Grades A, B and C. That is the formal inventory. Heat-analysis molybdenum for every grade is 0.45–0.60 %. The steel shall be killed.
Plates 1½ in. [40 mm] and under in thickness are normally supplied in the as-rolled condition and may be ordered normalized, normalized and tempered, or stress relieved. Plates over 1½ in. [40 mm] shall be normalized or normalized and tempered. The specification does not require every thickness to be normalized.
This page is not EN 10028-2 16Mo3 plate and not an ASME Code approval document. A related specification SA-204/SA-204M appears in Section II of the ASME Boiler and Pressure Vessel Code; that pointer does not make an ASTM-marked plate Code-approved.
SHH STEEL produces and exports ASTM A204 Grade C plate to the ordered edition, thickness, heat-treatment condition and extra tests written on the enquiry. This grade belongs to our Boiler & Pressure Vessel Steel Plates range under ASTM A204.
Material specification for ASTM A204 Grade C
The items below follow ASTM A204/A204M-17 (Reapproved 2022). Thickness, width, length and the inspection document are stated on the enquiry rather than listed here as stock or capacity ranges.
| Parameter | Detail |
|---|---|
| Standard | ASTM A204/A204M-17 (Reapproved 2022), Pressure Vessel Plates, Alloy Steel, Molybdenum. Approved 1 September 2022; last previous edition A204/A204M-17; originally approved in 1937. DOI 10.1520/A0204_A0204M-17R22 |
| Grade designation | Grade C |
| Product form | Steel plate. Coils are excluded from qualification until they are processed into finished plates (clause 3.3) |
| Intended use named in the scope | Molybdenum-alloy steel plates intended particularly for welded boilers and other pressure vessels |
| Thickness scope | Limited only by the capacity of the composition to meet the specified mechanical property requirements (clause 1.3). Carbon maxima in Table 1 change with thickness |
| General requirements | Specification A20/A20M. If this specification conflicts with A20/A20M, this specification prevails (clause 3.4) |
| Steelmaking | The steel shall be killed (clause 4.1) |
| Chemistry basis | Table 1, unless modified in accordance with A20/A20M Supplementary Requirement S17 when specified |
| Mechanical basis | Table 2 tension-test requirements |
| Heat treatment | Clauses 5.1 and 5.2: normally as-rolled at 1½ in. [40 mm] and under, with ordered normalizing, normalizing and tempering, or stress relieving permitted; normalized or normalized and tempered required over 1½ in. [40 mm] |
| Related ASME specification | SA-204/SA-204M in Section II of the ASME Boiler and Pressure Vessel Code (ASTM footnote 2). That is a pointer, not a Code approval of an ASTM-marked plate |
| Units | Inch-pound and SI values are separate standards; do not combine the two systems |
| Our supply | We produce and export Grade C to the thickness, condition and tests agreed on the order |
Chemical composition of ASTM A204 Grade C
The figures below are the ASTM A204/A204M-17 (Reapproved 2022) Table 1 chemical requirements for Grade C. Carbon maxima apply to both heat and product analyses. They are not EN 10028-2 16Mo3 values and not a manufacturer typical.
| Element | ASTM A204/A204M-17 (2022) Table 1 (mass %) |
|---|---|
| Carbon, max, Up to 1 in. [25 mm] incl. | 0.23 |
| Carbon, max, Over 1 in. to 2 in. [50 mm] incl. | 0.26 |
| Carbon, max, Over 2 in. to 4 in. [100 mm] incl. | 0.28 |
| Carbon, max, Over 4 in. [100 mm] | 0.28 |
| Manganese, max, heat analysis | 0.90 |
| Manganese, max, product analysis | 0.98 |
| Phosphorus, max (heat and product) | 0.025 |
| Sulfur, max (heat and product) | 0.025 |
| Silicon, heat analysis | 0.15–0.40 |
| Silicon, product analysis | 0.13–0.45 |
| Molybdenum, heat analysis | 0.45–0.60 |
| Molybdenum, product analysis | 0.41–0.64 |
Clause 6.1 allows Table 1 to be modified in accordance with Supplementary Requirement S17, Vacuum Carbon-Deoxidized Steel, in Specification A20/A20M, when that supplementary requirement is specified. Product analysis, when required, is an order item (S2), not an automatic extra.
Mechanical properties and thickness limits
ASTM A204/A204M-17 (Reapproved 2022) clause 1.3 states that the maximum thickness of plates is limited only by the capacity of the composition to meet the specified mechanical property requirements. That sentence is not a mill rolling-capacity list. The tensile values below are Table 2 for Grade C. Tension tests represent the plates as required by clause 7.1 and by the general requirements of Specification A20/A20M.
| Property | ASTM A204/A204M-17 (2022) Table 2 |
|---|---|
| Tensile strength | 75–95 ksi [515–655 MPa] |
| Yield strength, min | 43 ksi [295 MPa] |
| Elongation in 8 in. [200 mm], min | 16 % |
| Elongation in 2 in. [50 mm], min | 20 % |
Yield strength is determined by either the 0.2 % offset method or the 0.5 % extension-under-load method. See Specification A20/A20M for elongation adjustment; that adjustment table is not reprinted here.
This specification does not specify a mandatory Charpy or drop-weight test. Supplementary Requirement S5 (Charpy V-notch impact test) and S6 (drop-weight test, for material 0.625 in. [16 mm] and over in thickness) apply only when they are written on the purchase order. This page does not invent impact energies and does not treat any construction-code toughness rule as an automatic A204 guarantee.
Delivery conditions for ASTM A204 Grade C
ASTM A204/A204M-17 (Reapproved 2022) states:
- The steel shall be killed.
- Plates 1½ in. [40 mm] and under in thickness are normally supplied in the as-rolled condition. Those plates may be ordered normalized, normalized and tempered, or stress relieved.
- Plates over 1½ in. [40 mm] in thickness shall be normalized or normalized and tempered.
Do not treat normalizing as a universal delivery condition for every thickness. Write the required condition on the order, especially when plate 1½ in. [40 mm] and under must be normalized, normalized and tempered, or stress relieved rather than as-rolled.
Supplementary requirements in A20/A20M that this specification lists as suitable, and that apply only when specified in the purchase order, include S1 vacuum treatment, S2 product analysis, S3 simulated post-weld heat treatment of mechanical test coupons, S4.1 additional tension test, S5 Charpy V-notch impact test, S6 drop-weight test (for material 0.625 in. [16 mm] and over), S7 high-temperature tension test, S8 ultrasonic examination in accordance with A435/A435M, S9 magnetic-particle examination, S11 ultrasonic examination in accordance with A577/A577M, S12 ultrasonic examination in accordance with A578/A578M, and S17 vacuum carbon-deoxidized steel.
Note 1: for plates produced from coil and furnished without heat treatment or with stress relieving only, three test results are reported for each qualifying coil. Additional coil-to-plate rules are in A20/A20M. That note is not a rolling-width or coil-capacity claim.
We produce and export Grade C to the agreed condition.
Welding and vessel fabrication
ASTM A204 plates are intended particularly for welded boilers and other pressure vessels. A welding procedure suitable for the grade, thickness, delivery condition and intended service should be qualified before production welding. This page does not invent preheat temperatures, heat-input limits or hardness caps.
Grade C is a killed C-Mo plate with heat-analysis molybdenum of 0.45–0.60 % and a thickness-dependent carbon maximum. Any post-weld heat treatment of the finished vessel is a matter for the construction code or procedure named on the project, not an automatic requirement of this plate specification. Supplementary Requirement S3 covers simulated post-weld heat treatment of mechanical test coupons only when the purchaser specifies it.
If repair welding of the plate is not acceptable, or if the purchaser must approve the procedure, the order shall say so.
Form, finish and dimensions
Testing and retesting methods, permitted variations in dimensions and mass, quality and repair of defects, marking, loading and ordering information follow Specification A20/A20M except where this specification prevails. This page does not reprint the A20 tolerance tables and does not list stock sizes or mill-capacity ranges.
Coils are not qualified to this specification until they have been processed into finished plates. Operations that then become the processor’s responsibility include decoiling, leveling, cutting to length, testing, inspection, conditioning, heat treatment if applicable, packaging, marking, loading and certification.
We produce and export Grade C to the dimensions and surface requirements agreed on the enquiry.
Applications and specification limits
Grade C is specified for welded boilers and other pressure vessels that name ASTM A204/A204M and this grade. Allowable design stresses, temperature limits and toughness rules come from the construction code or purchaser specification on the project, not from this plate standard alone. This page does not publish piping-code or boiler-code allowable-stress tables.
This page is not EN 10028-2 16Mo3 plate, not EN 10028-2 P265GH carbon vessel plate, not ASTM A302 manganese-molybdenum plate, not a chromium-molybdenum grade such as A387, and not a quenched-and-tempered structural plate. It is not by itself an ASME Code design approval.
Compare ASTM A204 Grade C with other steel products
ASTM A204 Grade C Steel Plate is molybdenum-alloy pressure-vessel plate under ASTM A204/A204M, not carbon vessel plate and not a chromium-molybdenum grade. The comparison uses three products we already publish. They are related by engineering use or similar names, not equivalents. Unpublished ASTM A204 sibling grades are not linked here.
| Material | Alloy / type | Delivery condition | Mechanical requirements | Typical service | Substitution limit |
|---|---|---|---|---|---|
| ASTM A204 Grade C Steel Plate (this product) | ASTM A204/A204M-17 (2022) Table 1 for Grade C: carbon maxima by thickness from 0.23 % (up to 1 in.) to 0.28 % (over 4 in.); Mn 0.90 % max heat / 0.98 % max product; P and S 0.025 % max; Si 0.15–0.40 % heat; Mo 0.45–0.60 % heat (0.41–0.64 % product). | Killed steel. Plates 1½ in. [40 mm] and under are normally as-rolled and may be ordered normalized, normalized and tempered, or stress relieved. Plates over 1½ in. [40 mm] shall be normalized or normalized and tempered | Table 2: tensile 75–95 ksi [515–655 MPa]; yield min 43 ksi [295 MPa]; elongation 16 % in 8 in. / 20 % in 2 in. | Welded boilers and other pressure vessels that specify ASTM A204 Grade C | Not interchangeable with an ASME SA-204 stamp, with EN 10028-2 16Mo3 or with carbon vessel plate unless the project specification allows it |
| ASME SA204 Grade C Steel Plate | ASME SA-204/SA-204M Grade C molybdenum vessel plate (from our live SA204 Grade C page) | Our live SA204 pages describe killed steel, as-rolled supply commonly used at 40 mm and under, and normalizing commonly used over 40 mm. The ASTM 17 (2022) text used on this page also allows normalized-and-tempered or stress-relieved options as written in clauses 5.1 and 5.2 | From our SA204 Grade C page: tensile 515–655 MPa, yield 295 MPa. | Code work that names SA-204/SA-204M rather than ASTM A204/A204M | Related Code specification, not an automatic substitute stamp. ASTM footnote 2 points readers to SA-204/SA-204M in Section II of the ASME Boiler and Pressure Vessel Code; that pointer is not itself a Code approval of an ASTM-marked plate. Order the mark and the Code edition the project names. |
| EN 10028-2 16Mo3 Steel Plate | European 0.3 % molybdenum high-temperature vessel plate, steel number 1.5415 (from our 16Mo3 page). That page also states a molybdenum window of 0.25–0.35 % | From our 16Mo3 page: a normalized European high-temperature vessel plate | From our 16Mo3 page: yield 275 MPa at ≤ 16 mm; tensile 440–590 MPa | European high-temperature 0.3Mo boilers and vessels specified to EN 10028-2 | Not an equivalent. Heat-analysis molybdenum on A204 is 0.45–0.60 %, which is not the 0.25–0.35 % window described on our 16Mo3 page. Tensile bands and delivery rules also differ. |
| EN 10028-2 P265GH Steel Plate | European non-alloy high-temperature vessel plate, steel number 1.0425 (from our P265GH page) | Usually normalized (+N); our P265GH page also notes as-rolled for some thicknesses | From our P265GH page: yield 265 MPa at ≤ 16 mm; tensile 410–530 MPa | Boilers, drums and other EN 10028-2 high-temperature carbon vessels | Different alloy family. Do not take P265GH figures, including any 27 J at 0 °C order option named on that page, as ASTM A204 requirements. |
Related published ranges: Boiler & Pressure Vessel Steel Plates and ASTM A204. Also ASME SA204 and EN 10028-2.
Equivalent and related grades by country
The designations below are near names or related national vessel-plate grades, not certified or automatic equivalents. Chemistry, thickness, heat treatment, supplementary tests and the required stamp must match the project specification before a substitution is considered. Grades without a live page on this site are shown as plain text.
| Country / region | Standard | Grade | Similarity and key differences | Substitution caveat |
|---|---|---|---|---|
| United States | ASTM A204/A204M-17 (Reapproved 2022) | Grade C | This molybdenum-alloy plate. Table 2 tensile 75–95 ksi [515–655 MPa] and yield min 43 ksi [295 MPa]. The formal list is three grades: A, B and C. The other current names are Grade A and Grade B. | Specify ASTM A204/A204M, this named grade, thickness (because the carbon maximum depends on thickness), heat-treatment condition and any A20 supplementary requirements. |
| United States (ASME) | ASME SA-204/SA-204M | Grade C | The related Code specification pointed to by ASTM footnote 2. From our SA204 Grade C page: tensile 515–655 MPa, yield 295 MPa. A public ASME BPVC.II.A-2023 reprint of SA-204/SA-204M prints the same Grade A/B/C list and the same Table 1, Table 2 and clauses 5.1–5.2 values used on this page. | Not an automatic substitute stamp. See our live ASME SA204 Grade C Steel Plate. Order the mark and the Code edition named on the project. This page does not claim ASME Code approval of an ASTM-marked plate and does not publish piping-code allowable stresses. |
| Europe | EN 10028-2 | 16Mo3 (1.5415) | From our 16Mo3 page: European 0.3 % molybdenum high-temperature vessel plate, steel number 1.5415, yield 275 MPa at ≤ 16 mm, tensile 440–590 MPa, with a molybdenum window of 0.25–0.35 % described on that page. | Not an equivalent. A204 heat-analysis molybdenum is 0.45–0.60 %. See EN 10028-2 16Mo3 Steel Plate. |
| United States | ASTM A302/A302M | Grade A (Mn-Mo) | Our live A302 Grade A page describes a manganese-molybdenum pressure-vessel plate with yield 310 MPa and tensile 515–655 MPa. That is a different specification and a different alloy balance from A204. | Do not treat an A302 name as an A204 substitute. The A302 Grade A page is live on this site but is a different product. |
| Japan | JIS G 3103 | SBV names used in catalogues | Some catalogues pair A204 grades with JIS G 3103 molybdenum boiler-plate names. Those JIS tables were not used as numeric sources on this page. | Compare the ordered JIS text before any substitution. No JIS numbers are reprinted here. |
| China | GB/T molybdenum vessel-plate specifications | Project-named GB grade | Chinese molybdenum or chromium-molybdenum vessel plates are written to their own GB/T documents, not to ASTM A204. | Do not assume a GB name is an automatic equivalent. |
Why choose SHH STEEL for ASTM A204 Grade C
- We produce and export ASTM A204 Grade C molybdenum vessel plate
- We review the enquiry for edition, grade, thickness, heat-treatment condition and A20 supplementary tests
- We keep Table 1 carbon maxima and the 0.45–0.60 % molybdenum window distinct from EN 10028-2 16Mo3
- We treat as-rolled supply at 1½ in. [40 mm] and under as the normal condition unless the order names another treatment
- We match documentation to what the purchase order requires
How to enquire for ASTM A204 Grade C
| Item | What to specify |
|---|---|
| Standard and grade | ASTM A204/A204M, Grade C. Name the edition required by the project; the figures on this page follow the 17 (Reapproved 2022) text |
| Product form | Finished plate. Coil is not qualified until it has been processed into plate |
| Thickness and dimensions | Thickness, width and length. Carbon maxima in Table 1 depend on thickness |
| Heat treatment | As-rolled, normalized, normalized and tempered, or stress relieved, consistent with clauses 5.1 and 5.2 |
| Chemistry | Table 1 for this named grade, unless the order specifies S17 or another agreed analysis |
| Mechanical tests | Table 2 tension tests. Write S5 Charpy, S6 drop-weight, S7 high-temperature tension or extra ultrasonic / magnetic-particle examinations only when required. None of those is automatic |
| Other A20 items | S1 vacuum treatment, S2 product analysis, S3 simulated PWHT of test coupons, or S4.1 additional tension test only when required |
| Documentation | State the inspection document type required by the project |
| Processing | Cutting or other processing only when requested |
Frequently Asked Questions
-
Is ASTM A204 Grade C the same as ASME SA204 Grade C or EN 10028-2 16Mo3?
- No. SA-204/SA-204M is the related ASME Section II specification pointed to by ASTM footnote 2. From our SA204 Grade C page: tensile 515–655 MPa, yield 295 MPa. That live page is a separate product and a separate stamp; the pointer is not a Code approval of an ASTM-marked plate. EN 10028-2 16Mo3 is a European 0.3 % molybdenum vessel plate (our page: steel number 1.5415, yield 275 MPa at ≤ 16 mm, tensile 440–590 MPa, molybdenum 0.25–0.35 %). A204 heat-analysis molybdenum is 0.45–0.60 %.
-
How many formal ASTM A204/A204M grades are there?
- Clause 1.2 lists three grades: A, B and C. This page is Grade C. The other current names are Grade A and Grade B. They differ by carbon maxima and by Table 2 tensile and yield requirements; molybdenum is 0.45–0.60 % on heat analysis for all three.
-
Is every ASTM A204 Grade C plate normalized?
- No. Plates 1½ in. [40 mm] and under are normally supplied as-rolled and may be ordered normalized, normalized and tempered, or stress relieved. Plates over 1½ in. [40 mm] shall be normalized or normalized and tempered. Write the required condition on the order.
-
Does ASTM A204 Grade C automatically include a Charpy test?
- No. Table 2 is a tension-test table. Charpy testing is Supplementary Requirement S5 and applies only when the purchase order specifies it. Drop-weight testing (S6) is likewise optional and applies only to material 0.625 in. [16 mm] and thicker when specified.
-
What should a quotation enquiry include?
- ASTM A204/A204M and Grade C, the required edition, thickness by width by length, quantity, heat-treatment condition, any A20 supplementary requirements (including S5 if impact testing is required), and the inspection document required by the project.
Request a quotation
Contact SHH STEEL for a quotation for ASTM A204 Grade C molybdenum vessel plate. Please include your required quantity, thickness, width and length, delivery destination and preferred delivery schedule so we can review your production and export requirements.
Specify ASTM A204/A204M, Grade C, and the edition required by the project. Write the heat-treatment condition (as-rolled, normalized, normalized and tempered, or stress relieved) consistent with the 1½ in. [40 mm] rule. If your project requires Charpy testing, drop-weight testing, product analysis, simulated PWHT of test coupons, extra tension tests or ultrasonic examination, include those supplementary requirements and the inspection document required.
If your enquiry compares Grade C with ASME SA-204 Grade C, with EN 10028-2 16Mo3, with EN 10028-2 P265GH, or with an ASTM A302 manganese-molybdenum plate, identify each product clearly. We will review the differences in standard, alloy content and supply condition rather than assume that similar names are interchangeable.
For a detailed quotation, email your material specification, quantity and delivery requirements to our team.
Contact: admin@steelspecs.com