ASME SA517 Grade H is a quenched-and-tempered high-strength alloy vessel plate under ASME SA-517/SA-517M. Yield 690 MPa, tensile 795–930 MPa, max thickness 50 mm. China mill Distributor SHH STEEL supplies SA517 Gr.H / A517 Gr.H with 3.1 or 3.2 certificates.
Keywords
ASME SA517 Grade H, SA517 Gr.H, SA517GRH, SA517 GR H, SA-517 Grade H, ASTM A517 Grade H, A517GRH, QT high strength vessel plate, ASME SA-517, SA517 Grade H supplier
Equivalent Grades
ASTM A517 Gr H / ASME SA517 Gr H / JIS — / GB Q550CF (near) / EN 10028-6 P500Q (near) — Material Specification: ASME SA-517 / ASTM A517 — Delivery: Quenched + Tempered (Q+T)
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Material Comparison
High-Strength QT Vessel Service
Weldability
Heat Treatment
Delivery Condition
Dimensions
Tolerances
Supplementary Requirements
Equivalent Material Grades
Applications
Why Choose SHH STEEL
FAQ
Conclusion

What is ASME SA517 Grade H Steel ?

ASME SA517 Grade H is the 50 mm grade in the SA-517 family, sitting with Grade S on the same thickness ceiling. The tensile table is the 690 MPa class used by the rest of the specification. The alloy is not. Grade H carries a modest nickel band (0.30–0.70%) plus chromium and molybdenum. If the drawing says Grade H, a Grade B or Grade F heat is not a substitute. As Direct Mill Supply by SHH STEEL, the plate is produced to ASME SA-517/SA-517M.

The same plate is written SA517 Gr.H, SA517GRH, SA517 GR H, SA-517 Grade H, SA517 Grade H, ASTM A517 Grade H, A517 Gr.H, A517GRH and A/SA517 Grade H. They all mean Grade H in ASME SA-517. The ASTM companion is A517/A517M.

ASME SA-517 lists eight grades—A, B, E, F, H, P, Q and S. They share one mechanical table where thickness overlaps. They do not share alloy content or maximum thickness. Grade H and Grade S stop at 50 mm (2 in.). Grade A and Grade B stop at 32 mm. Grade F stops at 65 mm. Grade P stops at 100 mm. Grade Q and Grade E stop at 150 mm.

The steel is killed and made to fine austenitic grain practice under ASME SA-20. Heat treatment is mandatory quench and temper: austenitize at not less than 900 °C, quench in water or oil, temper at not less than 620 °C. As-rolled or normalize-only plate is not SA517 Gr.H.

Do not mix this page with ASME SA515 or ASME SA516. Those are carbon vessel plates. ASME SA517 Grade H is a QT alloy plate. It is also not structural A514. A514 is a structural specification. SA-517 is a pressure-vessel specification with SA-20 general requirements and Code testing.

For Code work the plate is used under ASME Section VIII. Dual marking ASME SA517 Grade H / ASTM A517 Grade H is available. Certificates can be EN 10204 3.1 or EN 10204 3.2.

When a project is still choosing high-strength vessel plate, a China mill Agent path through SHH STEEL puts SA517GRH next to ASME SA537 Class 2, ASTM A537, ASME SA387 and ASTM A285, so the buyer can see whether they actually need 690 MPa QT or a lower-strength carbon / Cr-Mo route.

Material Specification

Specification Element Requirement SHH STEEL Compliance
Grade ASME SA517 Grade H / SA517 Gr.H / SA517GRH Confirmed
Product Specification ASME SA-517/SA-517M Applied
Companion Spec ASTM A517 Grade H / A517GRH Dual cert available
General Requirements ASME SA-20 / ASTM A20 Applied
Code Context ASME Section VIII As specified
Product Form Pressure vessel / boiler plate Available
Steel Practice Killed, fine austenitic grain Confirmed
Heat Treatment Quench and temper (mandatory) Confirmed
Maximum Thickness (Grade H) 50 mm (2 in.) Per SA-517
Typical Supply 8 mm – 50 mm By mill enquiry
Width / Length Up to about 4000 mm / 12000 mm Mill capability
Certification EN 10204 3.1 or 3.2 / third-party As ordered

This plate belongs to the Pressure Vessel Steel Plates family. It is not a structural HSLA Steel Plates substitute and not a Carbon Steel Plates grade.

Chemical Composition

Chemistry for ASME SA517 Grade H is reported as heat analysis and, when specified, product analysis under ASME SA-517/SA-517M. Grade H is a Ni-Cr-Mo alloy with a lower nickel band than Grade F or Grade P.

Heat Analysis — ASME SA517 Grade H / SA517 Gr.H

Element Heat Analysis (%)
Carbon (C) 0.12 – 0.21
Manganese (Mn) 0.95 – 1.30
Phosphorus (P), max 0.025
Sulfur (S), max 0.025
Silicon (Si) 0.15 – 0.35
Nickel (Ni) 0.30 – 0.70
Chromium (Cr) 0.40 – 0.65
Molybdenum (Mo) 0.20 – 0.30

Product Analysis — SA517GRH / A517 Grade H

Element Product Analysis (%)
Carbon (C) 0.10 – 0.23
Manganese (Mn) 0.87 – 1.41
Silicon (Si) 0.13 – 0.37
Nickel (Ni) 0.27 – 0.73
Chromium (Cr) 0.36 – 0.69
Molybdenum (Mo) 0.18 – 0.33
P, S Per SA-20 / order

A Grade F heat cannot be recertified as Grade H. Nickel on Grade F is 0.70–1.00%. A Grade B heat cannot be recertified as Grade H either: Grade B has no specified nickel. If the drawing says ASME SA517 Grade H, the ladle must sit in the Grade H table. SHH STEEL reports heat analysis on every certificate and adds product analysis when ASME SA-20 or the vessel specification requires it.

Tighter phosphorus, sulfur or residuals are supplementary. Vacuum carbon deoxidation and other A20 chemistry items are available when written on the order.

Mechanical Properties

Where Grade H is permitted (50 mm and under), it uses the high line of the SA-517 tensile table.

Tensile Requirements — ASME SA517 Grade H per ASME SA-517/SA-517M

Property ≤ 50 mm (2 in.), within Grade H limit
Tensile strength 795 – 930 MPa (115 – 135 ksi)
Yield strength, min 690 MPa (100 ksi)
Elongation in 50 mm, min 16%
Reduction of area, rectangular, min 35%
Reduction of area, round, min 45%

There is no 100 mm or 150 mm line on Grade H. The specification itself ends at 50 mm. A 60 mm inquiry is not Grade H, even though Grade F would still be inside 65 mm.

Density is 7.85 g/cm³. Hardness after QT is typically in a high-strength vessel range; a special HBW window is a supplementary requirement.

ASME SA-517 requires transverse Charpy V-notch testing with a minimum lateral expansion of 0.38 mm (0.015 in.) on each specimen. The test temperature is agreed between purchaser and manufacturer. Write the temperature on the PO.

Specimens follow ASME SA-20. If simulated PWHT is specified, coupons from the same SA517 Gr.H heat follow the vessel cycle before tensile and impact testing. On QT 690 MPa plate that request should be on the mill order whenever the shop will PWHT the vessel.

Material Comparison

Grade Alloy emphasis Max thickness Same strength table where allowed?
SA517 Gr.A / B Cr-Mo family, 32 mm 32 mm Yes
SA517 Gr.H Lower-Ni Cr-Mo 50 mm Yes
SA517 Gr.S Mn-Mo family 50 mm Yes
SA517 Gr.F Ni-Cr-Mo-B 65 mm Yes
SA517 Gr.P Higher Ni-Cr-Mo 100 mm Yes
SA517 Gr.Q Ni-Cr-Mo-V 150 mm Yes
A514 Structural QT Structural spec Not a vessel spec

Order ASME SA517 Grade H when the drawing names Grade H and thickness is 50 mm or less. If thickness exceeds 50 mm, Grade H is not available under SA-517. Grade F is the next common step to 65 mm. SHH STEEL does not swap H for F or S on a Code vessel without a written revision.

HSLA Steel Plates and S690QL structural plate are not ASME SA-517. If the equipment is Section VIII, stay on SA517 / A517.

High-Strength QT Vessel Service

ASME SA517 Grade H exists because some vessels need 690 MPa yield on the Grade H nickel band and stay inside 50 mm. The 50 mm ceiling is the specification limit, not a mill preference.

Allowable stress for Code work comes from ASME Section II Part D for SA-517 Grade H, not from a mill flyer. Impact temperature is an order number.

Typical use is high-pressure process vessels, intermediate-thin courses and other fusion-welded parts specified to SA-517 Grade H. It is not a cryogenic 3.5Ni or 9Ni grade, and it is not a creep-focused Cr-Mo grade such as SA387.

Weldability

SA517GRH is a high-strength QT alloy. Welding is not the same job as welding SA516 Gr.70.

Procedures for Code work are qualified to ASME Section IX. Consumables should match the required joint strength, toughness and nickel. Hydrogen control, preheat and interpass are mandatory. QT plate in this strength class will crack if it is started cold and wet on a restrained joint.

Preheat depends on thickness, restraint, hydrogen and the qualified WPS. After welding, many shops want to PWHT. On QT plate that decision has to be engineered. A shop cycle that is too hot or too long can drop yield below the SA-517 table. Simulated PWHT of mill coupons should be on the purchase order whenever the vessel specification includes PWHT.

Do not copy an SA516, Grade B or Grade F procedure onto ASME SA517 Grade H without review. Procedure review can go through steel welding services. The fabricator owns the qualified WPS.

Heat Treatment

Heat treatment of ASME SA517 Grade H follows ASME SA-517/SA-517M:

  • Heat to not less than 900 °C (1650 °F)
  • Quench in water or oil
  • Temper at not less than 620 °C (1150 °F)

That sequence is the product. As-rolled plate is not SA517 Grade H. Normalized-only plate is not SA517 Grade H.

Holding time follows mill practice and ASME SA-20 thickness rules. If the purchaser fixes a tempering band or a maximum tempering temperature because later PWHT is planned, those limits go on the mill instruction and onto the certificate.

SHH STEEL reports the actual heat-treatment condition on the MTC for every SA517 Gr.H plate.

Delivery Condition

Delivery condition for this grade is quenched and tempered. That is the only standard condition.

The certificate lists ASME SA517 Grade H and, when dual certified, ASTM A517 Grade H; heat number; heat analysis; product analysis when ordered; tensile results; reduction of area; Charpy lateral expansion and test temperature; heat-treatment temperatures; and supplementary tests.

Surface is vessel-plate quality. Shot blasting and shop primer are available. Decorative 2B or BA finishes are not used on QT vessel plate.

Certificates may be EN 10204 3.1 or EN 10204 3.2. BV, LR, DNV, TUV, SGS or the buyer’s agency can witness quench, temper, mechanical tests and documents when the order says so.

Dimensions

Usual supply range from SHH STEEL for SA517 Gr.H QT high strength vessel plate:

  • Thickness: 8 mm – 50 mm (Grade H maximum in ASME SA-517 is 50 mm)
  • Width: up to about 4000 mm
  • Length: up to about 12000 mm

If the inquiry is 55 mm, say so immediately. That thickness is outside Grade H. Cut-to-length shells and nest sizes are available inside the 50 mm limit.

Tolerances

Dimensional limits follow ASME SA-20. Thickness, width, length, flatness and camber are vessel-plate tolerances. QT plate can move during quench; extra-flatness is a negotiated item.

Ultrasonic testing to A435 or A578 is commonly added. Finished sizes go through steel cutting services. Thermal cutting of 690 MPa QT plate needs preheat and edge control.

Supplementary Requirements

Most ASME SA517 Grade H orders add tests beyond the base table.

Simulated PWHT. Same-heat coupons follow the vessel cycle. Tensile and Charpy are run after that cycle.

Charpy details. Base spec is lateral expansion 0.38 mm, temperature agreed. Purchasers often add energy minima and a stated test temperature.

NDE. UT to A435 / A577 / A578; edge MT/PT after cutting.

Hardness survey. Surface HBW/HV after QT or after simulated PWHT.

Restricted chemistry. Tighter P, S, residuals or vacuum treatment per A20.

HIC / NACE. Only when the datasheet cites TM0284 or MR0175 / ISO 15156. Grade H is not automatically sour-service plate.

Z-direction. A770 or Z15/Z25/Z35 when the joint is strained.

Third-party. Witness of quench, temper, testing and documents. Output can be EN 10204 3.2.

These tests run through steel testing service. If it is not on the purchase order, it is not assumed.

Equivalent Material Grades

Designation Standard Notes
ASME SA517 Grade H / SA517 Gr.H / SA517GRH ASME SA-517/SA-517M Code name on this page
ASTM A517 Grade H / A517GRH ASTM A517/A517M Companion spec
A517 / SA517 QT 690 vessel plate Commercial Strength search name
EN 10028-6 P690Q / P690QL related EN Project-specific comparison only
GB high-strength QT vessel related GB Project-specific dual cert

For stamping, write ASME SA517 Grade H or dual SA517 / A517 Grade H. Nearby vessel pages: ASME SA537, ASTM A537, ASME SA516, ASTM A516.

Applications

ASME SA517 Grade H / SA517 Gr.H is selected when a Section VIII or equivalent vessel needs QT alloy strength on the Grade H chemistry and thickness stays at or below 50 mm.

Industry Typical components
High-pressure vessels ASME SA517 Grade H shells and SA517GRH heads
Petrochemical SA-517 Grade H process drums
Energy and process ASME SA517 Grade H QT high strength vessel plate
Intermediate-thin courses SA517 Gr.H plate to 50 mm
Dual-certified export SA517 / A517 Gr.H plate
Fabrication SA517GRH cut to nest sizes

Related pages: petrochemical industry, energy industry, steel cutting services, steel welding services, steel testing service, worldwide shipping service.

Why Choose SHH STEEL

SHH STEEL works as a China Mill Direct Exporter for plates to ASME SA-517/SA-517M. On ASME SA517 Grade H that means mill pricing, dual SA517/A517 marking, heat and product analysis including the 0.30–0.70% Ni band, mandatory QT with recorded temperatures, Charpy lateral expansion at the agreed temperature, 3.1 as standard and 3.2 when specified, and the extra tests a 690 MPa vessel shop actually writes on the PO.

We also keep the order on the right grade. Grade H is not Grade F. Grade H is not Grade S. Grade H is not A514. If the thickness is 55 mm, we will say so before anyone tries to buy Grade H. Export packing goes through worldwide shipping service. Company scope: China steel Mill Agent-SHH STEEL.

FAQ

What names are used for ASME SA517 Grade H?
Buyers write SA517 Gr.H, SA517GRH, SA517 GR H, SA-517 Grade H, ASTM A517 Grade H and A517GRH. They all mean Grade H in ASME SA-517/SA-517M. SHH STEEL prints the wording on the purchase order. Q: Is ASME SA517 G
Is ASME SA517 Grade H the same as ASTM A517 Grade H?
Chemistry and tensile limits match. ASME SA-517 is the Code version used with ASME Section VIII. ASTM A517 is the product spec. As China mill-Direct Supply, SHH STEEL dual-certifies SA517 Gr.H / A517 Gr.H when the vessel must be stamped.
What is the yield strength of SA517 Gr.H?
690 MPa minimum through 50 mm. Tensile is 795–930 MPa. Grade H is not furnished above 50 mm under ASME SA-517.
Why specify Grade H instead of Grade F or Grade S?
Strength is the same where thickness overlaps. Grade H and Grade S stop at 50 mm. Grade F stops at 65 mm. Nickel and manganese bands differ. Follow the grade on the drawing.
Is SA517GRH the same as A514 or S690QL?
No. Those are structural specifications. ASME SA517 Grade H is a pressure-vessel plate under SA-517 and SA-20. Do not substitute structural QT plate on a Section VIII vessel.
What heat treatment does ASME SA517 Grade H require?
Quench and temper. Austenitize at not less than 900 °C, quench in water or oil, temper at not less than 620 °C. As-rolled or normalize-only delivery is not this grade.
Can welding of SA517 Gr.H be qualified to ASME Section IX?
Yes. It is a fusion-welded vessel plate. Use a high-strength low-hydrogen WPS written for this alloy and thickness. The fabricator owns the procedure.
Can SHH STEEL issue EN 10204 3.2 on ASME SA517 Grade H?
Yes. EN 10204 3.1 is standard. EN 10204 3.2 or another third-party witness is arranged when it is written on the order.
What is the density of SA517 Gr.H plate?
7.85 g/cm³. SHH STEEL uses this value for shipping-weight estimates on ASME SA-517 plate.

Conclusion

ASME SA517 Grade H Steel Plate is the lower-nickel Cr-Mo, quenched-and-tempered high-strength vessel grade in ASME SA-517/SA-517M, limited to 50 mm. Whether the inquiry says SA517 Gr.H, SA517GRH, SA-517 Grade H or A517 Grade H, SHH STEEL supplies plate with heat and product analysis, recorded QT, the 690 MPa tensile line, agreed Charpy testing, optional simulated PWHT, and EN 10204 3.1 or 3.2 certification.

As a China mill Distributor, SHH STEEL provides ASME SA517 Grade H / SA517 Gr.H QT High Strength Vessel Plate for ASME Section VIII fabrication.

Contact SHH STEEL for mill rolling, QT, dual SA517/A517 marking, 3.2 inspection or a quotation.

ASME SA517 Grade H Steel Plate, SA517 Gr.H, SA517GRH, SA-517 Grade H, ASTM A517 Grade H, QT high strength vessel plate, SA517 Grade H supplier, Direct Mill Supply by SHH STEEL

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X