New Products /back


15NiCuMoNb5-6-4,EN10028-2

2011年4月14日 by admin

EN10028-2,15NiCuMoNb5-6-4,15NiCuMoNb5-6-4,15NiCuMoNb5-6-4,15NiCuMoNb5-6-4

 

Adopt Standard: EN10028-2

Grade:P235GH,P265GH,P295GH,P355GH,16Mo3,18MnMo4-5,20MnMoNi4-5,15NiCuMoNb5-6-4,20MnMoNi4-5,15NiCuMoNb5-6-4,13CrMo4-5,13CrMoSi5-5,10CrMo9-10,12CrMo9-10,X12CrMo5,13CrMoV9-10,12CrMoV12-10,X10CrMoVNb9-1.

 

15NiCuMoNb5-6-4 steel grade

15NiCuMoNb5-6-4 steel grade is one of grade in En10028-2, which is non alloy and alloy steels with specified elevated temperature properties.

In accordance with en10020, 15NiCuMoNb5-6-4 steel grade is alloy special steels.

15NiCuMoNb5-6-4 Grade delivery condition is normalized and tempered or quenched and tempered.

 

Gangsteel could supply 15NiCuMoNb5-6-4 steel grade in super thick steel plate for fabricators serving the oil and gas industry, heat exchangers, weldable pressure vessels and boilers

For more information in 15NiCuMoNb5-6-4 steel grade in the following:


15NiCuMoNb5-6-4 Chemical composition cast analysis

Element

15NiCuMoNb5-6-4  Max %

Element

15NiCuMoNb5-6-4 max %

C

0.17

Cr

0.30

Si

0.25-0.50

Cu

0.50-0.80

Mn

0.80-1.20

Mo

0.25-0.50

P

0.025

Nb

0.015-0.045

S

0.010

Ni

1.00-1.30

AL

0.015 min

Ti

 

N

0.020

V

0.02

 

15NiCuMoNb5-6-4 Mechanical properties

Grade

Condition

Thickness

Yield Strength

Tensile Strength

Elongation

Impact Energy

(mm)

MPa (min)

MPa

% (min)

(KV J) (min)

 

 

 

 

-20 degree

15NiCuMoNb5-6-4

+NT OR +QT

≤ 16

460

610-780

16

27

16> to ≤40

  460

610-780

16

27

40> to ≤60

440

610-780

16

27

60> to ≤100

430

600-760

16

27

100> to ≤150

420

590-740

16

27

150> to ≤250

410

580-740

16

27

Noted: +NT mean Normalized and tempered; +QT mean Quenched and tempered

 

If you want to find our stock in 15NiCuMoNb5-6-4 or inquiry from our gangsteel, please feel free to contact us by email or calling.

 

Tags: EN10028-2  15NiCuMoNb5-6-4  15NiCuMoNb5-6-4  15NiCuMoNb5-6-4  15NiCuMoNb5-6-4 steel  