Adopt Standard: EN10028-2

Grade:P235GH,P265GH,p295gh,p355gh,16Mo3,18MnMo4-5,20MnMoNi4-5,15NiCuMoNb5-6-4, 20MnMoNi4-5,15NiCuMoNb5-6-4,13CrMo4-5,13CrMoSi5-5,10CrMo9-10,12CrMo9-10,X12CrMo5,13CrMoV9-10,12CrMoV12-10,X10CrMoVNb9-1.

P295GH steel grade

P295GH steel grade is one of grade in En10028-2, which is non alloy and alloy steels with specified elevated temperature properties.

 

In accordance with en10020, P235GH,P265GH, p295gh and p355gh are non alloy quality steels. All of other grade are alloy special steels.

P295GH Grade delivery condition is normalizing or be replaced with normalizing rolling at the discretion of manufactures.

 

Gangsteel could supply P295GH steel grade in super thick steel plate for fabricators serving the oil and gas industry, heat exchangers, weldable pressure vessels and boilers

 

For more information in P295GH steel grade in the following:
P295GH Chemical composition cast analysis

Element

P295GH  Max %

Element

P295GH max %

C

0.08-0.20

Cr

0.30

Si

0.40

Cu

0.30

Mn

0.90-1.50

Mo

0.08

P

0.025

Nb

0.020

S

0.015

Ni

0.30

AL

0.020 min

Ti

0.30

N

0.012

V

0.02

 

P295GH Mechanical properties

Grade

Condition

Thickness

Yield Strength

Tensile Strength

Elongation

Impact Energy

(mm)

MPa (min)

MPa

% (min)

(KV J) (min)

 

 

 

 

-20 degree

P295GH

Normalized

≤ 16

295

460-580

21

27

16> to ≤40

   290

460-580

21

27

40> to ≤60

285

460-580

21

27

60> to ≤100

260

460-580

21

27

100> to ≤150

235

440-570

21

27

150> to ≤250

220

430-570

21

27

 

If you want to find our stock in P295GH or inquiry from our gangsteel, please feel free to contact us by email or calling.