New Products /back


EN10028-2,P235GH,Grade P235GH,P235GH steel,P235GH steel plate

2011年4月14日 by admin

EN10028-2,P235GH,Grade P235GH,P235GH steel,P235GH steel plate

 

Adopt Standard: EN10028-2

Grade:P235gh,p265gh,p295gh,p355gh,16Mo3,18MnMo4-5,20MnMoNi4-5,15NiCuMoNb5-6-4, 20MnMoNi4-5,15NiCuMoNb5-6-4,13CrMo4-5,13CrMoSi5-5,10CrMo9-10,12CrMo9-10,X12CrMo5,13CrMoV9-10,12CrMoV12-10,X10CrMoVNb9-1.

 

P235GH steel grade is one of grade in En10028-2, which is non alloy and alloy steels with specified elevated temperature properties.

 

In accordance with en10020, P235gh,p265gh, p295gh and p355gh are non alloy quality steels. All of other grade are alloy special steels.

P235GH Grade delivery condition is normalizing or be replaced with normalizing rolling at the discretion of manufactures.

 

Gangsteel could supply P235GH steel grade in super thick steel plate for fabricators serving the oil and gas industry, heat exchangers, weldable pressure vessels and boilers

 

For more information in P235GH steel grade in the following:
P235GH Chemical composition cast analysis

Element

P235GH  Max %

Element

P235GH max %

C

0.16

Cr

0.30

Si

0.35

Cu

0.30

Mn

0.60-1.20

Mo

0.08

P

0.015

Nb

0.020

S

0.015

Ni

0.30

AL

0.020 min

Ti

0.30

N

0.012

V

0.02

 

P235GH Mechanical properties

Grade

Type

Thickness

Yield Strength

Tensile Strength

Elongation

Impact Energy

(mm)

MPa (min)

MPa

% (min)

(KV J) (min)

 

 

 

 

-20 degree

P235GH

Normalized

≤ 16

235

360-480

24

27

16> to ≤40

  225

360-480

24

27

40> to ≤60

215

360-480

24

27

60> to ≤100

200

360-480

24

27

100> to ≤150

185

350-480

24

27

150> to ≤250

170

340-480

24

27

 

If you want to find our stock in P235GH or inquiry from our gangsteel, please feel free to contact us by email or calling.

EN10028-2,P235GH,Grade P235GH,P235GH steel,P235GH steel plate,P235GH grade

 

 

Tags: EN10028-2  P235GH  Grade P235GH  P235GH steel  P235GH steel plate  