New Products /back


EN10028-2,P265GH,Grade P265GH,P265GH steel,P265GH steel plate

2011年4月14日 by admin

EN10028-2,P265GH,Grade P265GH,P265GH steel,P265GH steel plate

 

Adopt Standard: EN10028-2

Grade:P235GH,p265gh,p295gh,p355gh,16Mo3,18MnMo4-5,20MnMoNi4-5,15NiCuMoNb5-6-4, 20MnMoNi4-5,15NiCuMoNb5-6-4,13CrMo4-5,13CrMoSi5-5,10CrMo9-10,12CrMo9-10,X12CrMo5,13CrMoV9-10,12CrMoV12-10,X10CrMoVNb9-1.

 

P265GH steel grade is one of grade in En10028-2, which is non alloy and alloy steels with specified elevated temperature properties.

 

In accordance with en10020, P235GH,p265gh, p295gh and p355gh are non alloy quality steels. All of other grade are alloy special steels.

P265GH Grade delivery condition is normalizing or be replaced with normalizing rolling at the discretion of manufactures.

 

Gangsteel could supply P265GH steel grade in super thick steel plate for fabricators serving the oil and gas industry, heat exchangers, weldable pressure vessels and boilers

For more information in P265GH steel grade in the following:
P265GH Chemical composition cast analysis

Element

P265GH  Max %

Element

P265GH max %

C

0.20

Cr

0.30

Si

0.40

Cu

0.30

Mn

0.80-1.40

Mo

0.08

P

0.025

Nb

0.020

S

0.015

Ni

0.30

AL

0.020 min

Ti

0.30

N

0.012

V

0.02

 

P265GH Mechanical properties

Grade

Condition

Thickness

Yield Strength

Tensile Strength

Elongation

Impact Energy

(mm)

MPa (min)

MPa

% (min)

(KV J) (min)

 

 

 

 

-20 degree

P265GH

Normalized

≤ 16

265

410-530

22

27

16> to ≤40

   255

410-530

22

27

40> to ≤60

245

410-530

22

27

60> to ≤100

215

410-530

22

27

100> to ≤150

200

400-530

22

27

150> to ≤250

185

390-530

22

27

 

If you want to find our stock in P265GH or inquiry from our gangsteel, please feel free to contact us by email or calling.