Adopt Standard: EN10028-2

Grade:P235GH,P265GH,P295GH,P355GH,16Mo3,18MnMo4-5,20MnMoNi4-5,15NiCuMoNb5-6-4,20MnMoNi4-5,15NiCuMoNb5-6-4,13CrMo4-5,13CrMoSi5-5,10CrMo9-10,12CrMo9-10,X12CrMo5,13CrMoV9-10,12CrMoV12-10,X10CrMoVNb9-1.

 

16Mo3 steel grade

16Mo3 steel grade is one of grade in En10028-2, which is non alloy and alloy steels with specified elevated temperature properties.

In accordance with en10020, 16Mo3 steel grade is alloy special steels.

16Mo3 Grade delivery condition is Normalized or normalized and tempered or quenched and tempered.

 

Gangsteel could supply 16Mo3 steel grade in super thick steel plate for fabricators serving the oil and gas industry, heat exchangers, weldable pressure vessels and boilers

For more information in 16Mo3 steel grade in the following:


16Mo3 Chemical composition cast analysis

Element

16Mo3  Max %

Element

16Mo3 max %

C

0.12-0.20

Cr

0.30

Si

0.35

Cu

0.30

Mn

0.40-0.90

Mo

0.25-0.35

P

0.025

Nb

 

S

0.010

Ni

 

AL

 

Ti

0.30

N

0.012

V

0.02

 

16Mo3 Mechanical properties

Grade

Condition

Thickness

Yield Strength

Tensile Strength

Elongation

Impact Energy

(mm)

MPa (min)

MPa

% (min)

(KV J) (min)

 

 

 

 

+20 degree

16Mo3

Normalized

≤ 16

275

440-590

22

31

16> to ≤40

   270

440-590

22

31

40> to ≤60

260

440-590

22

31

60> to ≤100

240

430-560

22

31

100> to ≤150

220

420-570

22

31

150> to ≤250

210

410-570

22

31

 

If you want to find our stock in 16Mo3 or inquiry from our gangsteel, please feel free to contact us by email or calling.

EN10028-2,16Mo3,Grade 16Mo3,16Mo3 steel,16Mo3 steel plate,16Mo3 grade

 

Tags: EN10028-2  16Mo3  Grade 16Mo3  16Mo3 steel  16Mo3 steel plate  

0 Comments, 0 Trackbacks