Adopt Standard: EN10028-2

Grade:P235GH,P265GH,P295GH,P355GH,16Mo3,18MnMo4-5,20MnMoNi4-5,15NiCuMoNb5-6-4,20MnMoNi4-5,15NiCuMoNb5-6-4,13CrMo4-5,13CrMoSi5-5,10CrMo9-10,12CrMo9-10,X12CrMo5,13CrMoV9-10,12CrMoV12-10,X10CrMoVNb9-1.

 

 

18MnMo4-5 steel grade

18MnMo4-5 steel grade is one of grade in En10028-2, which is non alloy and alloy steels with specified elevated temperature properties.

In accordance with en10020, 18MnMo4-5 steel grade is alloy special steels.

18MnMo4-5 Grade delivery condition is normalized and tempered or quenched and tempered.

 

Gangsteel could supply 18MnMo4-5 steel grade in super thick steel plate for fabricators serving the oil and gas industry, heat exchangers, weldable pressure vessels and boilers

For more information in 18MnMo4-5 steel grade in the following:


18MnMo4-5 Chemical composition cast analysis

Element

18MnMo4-5  Max %

Element

18MnMo4-5 max %

C

0.20

Cr

0.30

Si

0.40

Cu

0.30

Mn

0.90-1.50

Mo

0.45-0.60

P

0.015

Nb

 

S

0.005

Ni

0.30

AL

 

Ti

 

N

0.012

V

 

 

 

 

18MnMo4-5 Mechanical properties

Grade

Condition

Thickness

Yield Strength

Tensile Strength

Elongation

Impact Energy

(mm)

MPa (min)

MPa

% (min)

(KV J) (min)

 

 

 

 

-20 degree

18MnMo4-5

+NT

≤ 60

345

510-650

20

27

+NT

60> to ≤150

  325

510-650

20

27

+QT

150> to ≤250

310

480-620

20

27

Noted: +NT mean Normalized and tempered; +QT mean Quenched and tempered

 

If you want to find our stock in 18MnMo4-5 or inquiry from our gangsteel, please feel free to contact us by email or calling.

 