SA-992 Wide Flange H Beams (ASTM A992/A992M Basis) | SA-992 Wide Flange H Beams - SHH STEEL

SA-992 Wide Flange H Beams (ASTM A992/A992M Basis)

Enquiries named SA-992 for wide-flange H beams are described here on the technical basis of ASTM A992/A992M. The yield window is 50–65 ksi [345–450 MPa] and tensile strength is 65 ksi [450 MPa] minimum. This page does not treat SA-992 as a listed ASME BPVC specification. Size tables remain on the ASTM A992 steel beam page.
Keywords
SA-992 wide flange beam, SA-992 W-shape, ASTM A992/A992M basis, SA-992 H-beam enquiry, A992 W-beam
Equivalent Grades:
Near-equivalents only, not automatic substitutes.
Share:
General Description
Material Specification
Available Sizes of SA-992 Wide Flange H Beams
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Sourcing SA-992 Wide Flange H Beams from SHH STEEL
FAQ
Conclusion

What Does an SA-992 Wide Flange H Beam Enquiry Mean?

Purchase enquiries sometimes name SA-992, or SA-992M, for rolled wide-flange H beams used in building and bridge framing. The mechanical, chemical and carbon-equivalent values on this page are those of ASTM A992/A992M. The tables and wording used here follow ASTM A992/A992M-20, which is the edition on file for this site. The edition named on the purchase order governs delivery. Public listings also describe a later A992/A992M-22 text; this page does not recast that later edition as if it had been compared line by line.

This treatment answers enquiries that use the SA-992 name without inventing an ASME specification record. It is not a claim that SA-992 or SA-992M appears in the ASME Boiler and Pressure Vessel Code, and it is not a substitute for a Code stamp or an ASME-accepted material certificate. Complete W-shape geometry remains on the existing ASTM A992 Steel Beam product page, which this companion does not repeat.

Technical Basis for SA-992 Enquiries: ASTM A992/A992M, Not a Cited BPVC Listing

ASTM A992/A992M covers rolled structural steel shapes, principally W-shapes, produced to a killed fine-grain practice. The heat analysis must stay inside the chemistry of Table 1. The tensile result must fall inside the 50–65 ksi [345–450 MPa] yield window, reach 65 ksi [450 MPa] minimum tensile strength, and keep the yield-to-tensile ratio at or below 0.85, except where the specification permits a web-location test. A carbon-equivalent value is calculated from the heat analysis and must be reported: 0.45 % maximum for shapes other than those with flange thickness over 2 in. [50 mm], and 0.47 % maximum when that flange thickness is exceeded.

The ASME BPVC Section II, Part A specification lists for the 2023 and 2025 editions, as reviewed for this site, move from SA-989/SA-989M to SA-995/SA-995M. Those lists do not contain an SA-992 or SA-992M entry. This page therefore does not assign an identical-with year, does not treat SA-992 as a listed Code specification, and does not apply an ASME mark to the product. A later Code addendum can change that record; the lists actually reviewed remain the ones named above.

Ordinary ASTM A36 and SA-36 documentation is a different case. SA-36 is listed in Section II, Part A, and the 2023 text of SA-36 is identical with ASTM A36/A36M-19. That listing evidence does not extend to SA-992.

SA-992 Enquiry Sizes: Use the ASTM A992/A992M W-Shape Tables

W-shape designations, depths, flange and web thicknesses, and nominal masses for material ordered on an ASTM A992/A992M basis are the AISC Manual, 15th Edition, Type W series already published against ASTM A6/A6M. This companion does not reprint those 283 designations. Use the complete tables on ASTM A992 Steel Beam (https://www.steelspecs.com/products/astm-a992-steel-beam/). The matching material term is ASTM A992.

An enquiry written as SA-992 should still name the W designation, the unit system, and any supplementary requirements. The tables on the A992 page are nominal reference dimensions, not a rolling programme and not a claim that every designation is available from stock.

Chemical Composition for SA-992 Enquiries on an ASTM A992/A992M Basis

The heat-analysis limits below are Table 1 of ASTM A992/A992M-20. They apply when an SA-992 enquiry is described on that technical basis. Product analysis, where specified, follows the permitted variations in ASTM A992/A992M and ASTM A6/A6M. Tin is reported for information when the specification requires it.

Swipe horizontally to view all dimensions.

Element (heat analysis) Composition, %
Carbon, max 0.23
Manganese 0.50 to 1.60 A
Silicon, max 0.40
Vanadium, max 0.15 B
Columbium (niobium), max C 0.05 B
Phosphorus, max 0.035
Sulfur, max 0.045
Copper, max 0.60
Nickel, max 0.45
Chromium, max 0.35
Molybdenum, max 0.15

A Provided that the manganese-to-sulfur ratio is not less than 20 to 1, the minimum manganese for shapes with flange or leg thickness not exceeding 1 in. [25 mm] shall be 0.30 %.

B The sum of columbium and vanadium shall not exceed 0.15 %.

C Columbium and niobium are interchangeable names for the same element.

Mechanical Properties for SA-992 Enquiries on an ASTM A992/A992M Basis

The tensile requirements below are Table 2 of ASTM A992/A992M-20. They are the mechanical values used on this page for SA-992-named enquiries. They are not presented as ASME Code values.

Swipe horizontally to view all dimensions.

Property Requirement
Tensile strength, min 65 ksi [450 MPa]
Yield point 50 to 65 ksi [345 to 450 MPa] A
Yield to tensile ratio, max 0.85 B
Elongation in 8 in. [200 mm], min C 18 %
Elongation in 2 in. [50 mm], min C 21 %

A A maximum yield strength of 70 ksi [480 MPa] is permitted for structural shapes that are required to be tested from the web location.

B A maximum ratio of 0.87 is permitted for structural shapes that are tested from the web location.

C See the elongation requirement adjustments under the Tension Tests section of ASTM A6/A6M.

Certificates, Identification and What an SA-992 Enquiry Does Not Document

A mill test report for an ASTM A992/A992M W-shape should name the A992/A992M edition, the A6/A6M edition, the W designation, the heat analysis including the calculated carbon equivalent, confirmation of killed steel, the tensile results including the yield-to-tensile ratio, and any supplementary requirements that were ordered. That document is an ASTM A992/A992M certificate. It is not, by itself, an ASME SA-992 document, a Code quality system record, or proof that the heat was produced under a nuclear or boiler Code programme.

If a purchaser actually needs an ASME-accepted material, the order has to name a specification that is listed for the relevant Code section and year, together with any quality-system conditions that Code requires. This page does not supply that listing for SA-992.

Weldability and Carbon Equivalent for SA-992 Enquiries (ASTM A992/A992M Basis)

A992/A992M is written for welded construction as well as bolted framing. The reported carbon-equivalent cap (0.45 % or 0.47 %, as above) is part of that control. Welding procedure, consumable choice and preheat still follow the project welding specification and the heat analysis, not a grade name alone. Surface condition and residual mill scale are accepted within the limits of ASTM A6/A6M unless the order states a different finish.

Dimensional Tolerances for SA-992 Enquiry Beams: ASTM A6/A6M

When the technical basis is ASTM A992/A992M, shape tolerances, camber, sweep, mass tolerance and length tolerance are those of the ordered edition of ASTM A6/A6M. Detailed W-shape dimensions are not repeated here; see ASTM A992 Steel Beam. Masses on that page are nominal reference masses, not a weighing guarantee.

Applications and Service Limits for SA-992-Named Wide Flange H Beams

A992/A992M W-shapes are widely specified for building frames, bridges and similar structural work in which a controlled yield window and a carbon-equivalent cap matter. Naming an enquiry SA-992 does not move that product into a pressure-vessel, nuclear, or boiler Code application. Impact testing is not included by default; Charpy work is added only when the order specifies the relevant A6/A6M supplementary requirement and states the test temperature and acceptance value.

SA-992 Enquiries Compared with ASTM A992/A992M, A572 Grade 50 and SA-36

ASTM A992/A992M is the technical basis used here. The existing A992 product page already tabulates the W-shape series and should be used for size selection. A572 Grade 50 is a related high-strength low-alloy grade; it is not an automatic substitute, because A992 also caps the yield, the yield-to-tensile ratio and the carbon equivalent. SA-36 is a listed Section II, Part A specification identical with ASTM A36/A36M-19 in the 2023 book reviewed for this site, and it is a lower-yield carbon steel. That Code treatment does not transfer to SA-992. European S355JR or Chinese Q355B W- or H-series shapes follow different specifications and different geometry standards.

Near-Equivalents for SA-992 Enquiries: Not Automatic Substitutes

Designers sometimes compare A992/A992M with ASTM A572 Grade 50, EN 10025-2 S355JR or GB/T 1591 Q355B. Those comparisons are starting points only. Chemistry, yield window, tensile ratio, carbon-equivalent reporting, killed-steel practice, impact options and the governing shape standard all have to be checked against the order. None of those grades is an automatic substitute for an A992/A992M W-shape, and none of them creates an SA-992 Code listing.

Sourcing SA-992-Named Wide Flange H Beams from SHH STEEL

Send the W designation list, the ASTM A992/A992M edition required on the certificate, length and any supplementary tests. If the enquiry uses the SA-992 name, say so clearly, and state whether an ASTM A992/A992M mill test report is acceptable. SHH STEEL will review the named grade, the certificate wording and the size list before quoting. This page does not claim warehouse stock, and it does not offer an ASME SA-992 Code certificate on the basis of the review described above.

SA-992 Wide Flange H Beam FAQs

Is SA-992 listed in ASME BPVC Section II, Part A?
This site has not found an SA-992 or SA-992M entry in the Section II, Part A specification lists for the 2023 or 2025 editions reviewed. Those lists move from SA-989/SA-989M to SA-995/SA-995M. This page does not treat SA-992 as a listed Code specification and does not assign an identical-with year.
Can an ASTM A992 mill test report be used as an SA-992 certificate?
No. An ASTM A992/A992M certificate records conformance to that ASTM specification. It is not, by itself, an ASME SA-992 document or a Code quality-system record. If a Code-listed specification is required, the order has to name a specification that actually appears in the relevant Code book.
Why are the W-shape size tables on the ASTM A992 page?
The geometry is the same A6/A6M W-shape series already published for ASTM A992. Reprinting all 283 designations here would duplicate the existing product page at https://www.steelspecs.com/products/astm-a992-steel-beam/. Use that page for depths, flange and web thicknesses, and nominal masses.
Which edition of A992/A992M is used on this page?
The chemical and tensile tables follow ASTM A992/A992M-20, the edition on file here. The edition named on the purchase order governs. This page does not claim to have recast the later A992/A992M-22 text line by line.
Does naming a beam SA-992 change the yield or carbon-equivalent limits?
Not on this page. The yield window, tensile minimum, yield-to-tensile cap and carbon-equivalent limits used here are those of ASTM A992/A992M. The SA-992 enquiry name does not add a Code listing or alter those numbers.

Conclusion

SA-992-named wide flange H beam enquiries are described here on the technical basis of ASTM A992/A992M, with a 50–65 ksi [345–450 MPa] yield window, 65 ksi [450 MPa] minimum tensile strength, a 0.85 yield-to-tensile cap, and a reported carbon-equivalent limit. W-shape sizes stay on the ASTM A992 Steel Beam page. This companion does not present SA-992 as a listed ASME BPVC specification and does not treat an A992 certificate as an SA-992 Code document. Nominate the W designation, the A992/A992M edition required on the certificate, and any supplements; SHH STEEL will review the package before quoting.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response