JIS G4401 SK75 Tool Steel Plate
What is JIS G 4401 SK75 plate?
We produce and export JIS G 4401 SK75 as carbon tool steel plate. SK75 is a water-hardening carbon tool steel with a heat-analysis carbon range of 0.70–0.80 %. Typical tools include stamps, punches, circular saws, springs and press dies. Wear resistance after hardening rises, and toughness falls, as carbon increases through the JIS G 4401 series.
Composition and hardness values on this page follow JIS G 4401:2009. Specify the edition required on the purchase order.
SHH STEEL produces and exports JIS G 4401 SK75 plate to the ordered edition, delivery condition, dimensions and extra tests written on the enquiry.
Material specification for JIS G 4401 SK75
The items below follow JIS G 4401:2009. Thickness, width, length and the inspection document are stated on the enquiry rather than listed here as stock or capacity ranges.
| Parameter | Detail |
|---|---|
| Standard | JIS G 4401:2009, Carbon tool steels |
| Official symbol | SK75 (1983 reference symbol SK6) |
| Product form on this page | Steel plate (鋼板). JIS G 4401:2009 also covers other product forms, including steel strip |
| How designations are listed | Official symbols (種類の記号) in JIS G 4401:2009 Table 1 |
| Steelmaking | Killed steel. Unless otherwise specified, hot rolled or hot forged at a forging reduction ratio of 4S or more |
| Usual plate delivery | As-hot-rolled unless otherwise specified (JIS G 4401:2009 clause 4) |
| Annealed plate | Usual after cold rolling when that form is agreed (JIS G 4401:2009 clause 4) |
| Chemical analysis | Heat analysis (溶鋼分析) to JIS G 4401:2009 Table 1. That edition does not set a separate product-analysis table |
| Plate hardness | JIS G 4401:2009 Table 3, including columns for cold-rolled plate and strip when that form is agreed |
| Other-form hardness | JIS G 4401:2009 Table 2 applies to annealed products other than plates and strips (Brinell) |
| Appearance of plate and strip | Hot-rolled plate and strip: JIS G 3193 clause 7. Cold-rolled plate and strip: JIS G 3141 clause 12 |
| Dimensions of plate and strip | Hot-rolled plate and strip: JIS G 3193 (thickness tolerances in clause 5 apply below 160 mm; 160 mm and above by agreement). Plate flatness: JIS G 4401:2009 Table 6 for thickness below 160 mm; 160 mm and above by agreement. Cold-rolled plate and strip sizes: JIS G 3141; thickness tolerance A of JIS G 3141 Table 16 |
| Decarburization of plate | By agreement. JIS G 4401:2009 Table 7 depths apply to hot-rolled round bar only |
| Marking | JIS G 4401:2009 clause 11: mark the symbol, heat or inspection number, manufacturer name or abbreviation, quantity or mass, and dimensions. Cold-rolled plate or strip adds a −C suffix after the symbol unless that suffix is omitted by agreement |
| Enquiry information | Name the JIS G 4401 symbol, the edition required, plate as the product form, delivery condition, dimensions and any extra tests or document type |
| Inspection document | When a report is requested and no document type is named, JIS G 4401:2009 refers to JIS G 0415 inspection document 2.3 or inspection certificate 3.1.B |
| Units | Composition in percent by mass; hardness on the scales named in the tables |
| Our supply | We produce and export SK75 plate to the ordered edition, delivery condition, dimensions and extra tests |
Chemical composition of JIS G 4401 SK75
JIS G 4401:2009 Table 1 is heat analysis. Elements not listed in that table shall not be added intentionally except as needed to finish the heat, unless agreed. Note a) of that table states that copper shall not exceed 0.25 %, chromium shall not exceed 0.30 % and nickel shall not exceed 0.25 %, as impurities.
| Element | SK75 heat analysis, JIS G 4401:2009 Table 1 (wt. %) |
|---|---|
| Carbon (C) | 0.70–0.80 |
| Silicon (Si) | 0.10–0.35 |
| Manganese (Mn) | 0.10–0.50 |
| Phosphorus (P) | 0.030 max |
| Sulfur (S) | 0.030 max |
| Copper (Cu), impurity max (note a) | 0.25 |
| Chromium (Cr), impurity max (note a) | 0.30 |
| Nickel (Ni), impurity max (note a) | 0.25 |
Carbon ranges of neighbouring symbols overlap. Order by the official symbol, not by a carbon midpoint taken from the name.
Silicon, manganese, phosphorus and sulfur limits are the same for all eleven symbols in JIS G 4401:2009 Table 1. Carbon is the value that changes from symbol to symbol. The note a) impurity limits for copper, chromium and nickel also apply to every symbol.
Hardness and mechanical requirements for JIS G 4401 SK75
JIS G 4401:2009 specifies hardness, not a tensile-strength package. Table 3 is the hardness table for steel plates and strips. Table 2 (informative annealing temperature and Brinell hardness) applies to annealed products other than plates and strips.
| Plate and strip hardness (JIS G 4401:2009 Table 3) | SK75 |
|---|---|
| As-hot-rolled hardness, HRC | 39 max |
| Annealed hardness, HRB | 98 max |
| Annealed hardness, HRC | — |
| Cold-rolled annealed hardness, HV | 190 max |
| As-cold-rolled hardness, HV (informative) | 190–280 (informative) |
JIS G 4401:2009 Table 3 specifies as-hot-rolled HRC (39 max) and annealed HRB (98 max) for SK75. It does not specify an annealed HRC value.
For products other than plates and strips, if Brinell measurement is difficult, JIS G 4401:2009 allows Rockwell B or Vickers instead; those hardness values are then by agreement.
| Other-form annealed hardness (JIS G 4401:2009 Table 2) | SK75 |
|---|---|
| Informative annealing temperature, °C | 730–760, slow cool |
| Hardness after annealing, HBW | 192 max |
If cold-rolled plate or strip is agreed, JIS G 4401:2009 Table 3 specifies annealed hardness 190 max HV for SK75, and lists as-cold-rolled hardness 190–280 (informative) HV as an informative value. Quenched-and-tempered hardness is not a specified requirement in JIS G 4401:2009; a quench-and-temper hardness test may be agreed as an additional test.
Delivery conditions for JIS G 4401 SK75
JIS G 4401:2009 clause 4 sets the usual supply states:
- Steel is made as killed steel and, unless otherwise specified, by hot rolling or hot forging at a forging reduction ratio of 4S or more.
- Plates and strips are as-hot-rolled unless otherwise specified.
- When plates and strips are cold-rolled by agreement, they are usually annealed.
- Products other than plates and strips are usually annealed after hot rolling or hot forging.
An enquiry that only says “SK75 plate” should still name the delivery condition, because as-hot-rolled and annealed plate are not interchangeable supply states. The informative annealing temperature in JIS G 4401:2009 Table 2 for SK75 is 730–760 °C, slow cool.
For later tool hardening, JIS G 4401:2009 Annex JA (informative) lists a standard quench of 760–820 °C, water cool, and a temper of 150–200 °C, air cool, for SK75. Those temperatures are reference values, not as-delivered hardness.
This page does not offer heat-treatment or fabrication services.
Welding and thermal cutting
JIS G 4401:2009 does not specify a welding procedure. SK75 is a carbon tool steel (heat-analysis carbon 0.70–0.80 %). It is not selected as a welded construction plate in the way a structural or pressure-vessel grade would be.
Thermal cutting can harden the adjacent material. That heat-affected zone should be considered, and removed where later forming or finishing requires it. Any cutting or joining procedure should be qualified for the carbon content, thickness and delivery condition named on the order.
Form, appearance, dimensions and decarburization
JIS G 4401:2009 clause 7.2 sends hot-rolled plate and strip dimensions to JIS G 3193. Thickness tolerances in that reference apply below 160 mm; 160 mm and above are by agreement. Plate flatness is given in JIS G 4401:2009 Table 6 for thickness below 160 mm; 160 mm and above is by agreement.
Appearance of hot-rolled plate and strip follows JIS G 3193 clause 7. Appearance of cold-rolled plate and strip follows JIS G 3141 clause 12. Decarburization depth for plate is by agreement; JIS G 4401:2009 Table 7 depths apply to hot-rolled round bar only.
Numeric thickness, width, length and flatness limits should be stated on the purchase order and confirmed on the mill documents for the ordered edition.
Applications and specification limits
We produce and export SK75 plate for tools and dies that specify this JIS G 4401 symbol. Informative examples in JIS G 4401:2009 Table 1 include stamps, punches, circular saws, springs and press dies.
SK75 is a water-hardening carbon tool steel. Wear resistance, through-hardness after a later hardening cycle and toughness depend on the ordered condition, thickness and any agreed extra tests.
JIS G 4401 is a carbon tool-steel standard. It is not an alloy tool-steel specification such as JIS G 4404 or ASTM A681, not a high-speed specification such as JIS G 4403, and not an alloy structural plate specification such as ASTM A829. SK75 is not an automatic substitute for those products.
Compare JIS G 4401 SK75 with other steel plates
SK75 is a carbon tool steel plate. The comparison below is for selection only; these materials are not equivalents.
| Material | Alloy / type | Delivery condition | Mechanical requirements | Typical service | Substitution limit |
|---|---|---|---|---|---|
| JIS G 4401 SK75 (this plate) | Water-hardening carbon tool steel plate, heat-analysis carbon 0.70–0.80 % | As-hot-rolled unless otherwise specified; annealing or cold rolling by agreement | JIS G 4401:2009 Table 3: as-hot-rolled HRC 39 max; annealed HRB 98 max; annealed HRC —. No tensile package is specified. | Typical tools include stamps, punches, circular saws, springs and press dies | A different official symbol or a structural alloy plate is not an automatic substitute |
| JIS G 4401 SK85 tool steel plate | Water-hardening carbon tool steel plate, heat-analysis carbon 0.80–0.90 % | As-hot-rolled unless otherwise specified; annealing or cold rolling by agreement | JIS G 4401:2009 Table 3: as-hot-rolled HRC 43 max; annealed HRB 100 max; annealed HRC — | Typical tools include stamps, press dies, springs, band saws, jigs, cutting tools, circular saws, gauges and needles | A different official symbol from SK75, not an automatic substitute |
| JIS G 4401 SK80 tool steel plate | Water-hardening carbon tool steel plate, heat-analysis carbon 0.75–0.85 % | As-hot-rolled unless otherwise specified; annealing or cold rolling by agreement | JIS G 4401:2009 Table 3: as-hot-rolled HRC 43 max; annealed HRB 100 max; annealed HRC — | Typical tools include stamps, press dies and springs | A different official symbol from SK75, not an automatic substitute |
| ASTM A829 Grade 4140 | Chromium-molybdenum alloy structural plate, usually ordered by heat chemistry | ASTM A829/A829M-25 permits AR, A, N, NT or QT; specify the required condition. | No automatic as-delivered strength package; tensile or hardness only if specified and compatible | Machinery and general engineering parts, often heat treated after cutting | Not a carbon tool steel. Different chemistry, heat treatment and purpose from JIS G 4401 plate |
| JIS G 4401 SK105 | Water-hardening carbon tool steel; higher carbon than SK75. | As-hot-rolled plate unless otherwise specified; annealed or cold-rolled supply by agreement. | Use its own ordered specification, thickness and delivery condition; no strength or toughness value is transferred to this grade. | Hacksaws, chisels, gauges and press dies. | A distinct JIS symbol, not a substitute instruction. Higher-carbon selection changes the wear-resistance/toughness balance; verify plate hardness in the ordered condition. |
| JIS G 4401 SK120 | Water-hardening carbon tool steel; higher carbon than SK75. | As-hot-rolled plate unless otherwise specified; annealed or cold-rolled supply by agreement. | Use its own ordered specification, thickness and delivery condition; no strength or toughness value is transferred to this grade. | Drills, small punches, files and cutting tools. | A distinct JIS symbol, not a substitute instruction. Higher-carbon selection changes the wear-resistance/toughness balance; verify plate hardness in the ordered condition. |
Equivalent and related grades by country
The designations below are near names, not automatic substitutes. Confirm chemistry, product form, delivery condition and hardness before any substitution.
| Country / region | Standard | Grade or designation | Similarity and key differences | Substitution caveat |
|---|---|---|---|---|
| Japan | JIS G 4401:2009 | SK75 | This plate. Water-hardening carbon tool steel with heat-analysis carbon 0.70–0.80 %. Hardness, not a tensile package, is specified. | This product |
| Japan | JIS G 4401:2009 Table 1 (1983 reference) | SK6 | Listed as the 1983 reference symbol opposite this designation in Table 1. | Use the current symbol on new orders. |
| International | ISO 4957:1999 | No direct counterpart specified | JIS G 4401:2009 Annex JB does not list an ISO 4957:1999 symbol opposite this designation. | Confirm chemistry and hardness before any substitution. |
| United States | — | No direct counterpart specified | ASTM carbon tool steels use a different designation system. | Confirm chemistry, product form and hardness before any substitution. |
| China | — | No direct counterpart specified | Chinese carbon tool steels use a different designation system. | Confirm chemistry, product form and hardness before any substitution. |
Why choose SHH STEEL for JIS G 4401 SK75
- We produce and export JIS G 4401 SK75 carbon tool steel plate
- We review the enquiry for edition, symbol, product form, delivery condition, dimensions and any extra tests
- We keep plate hardness (JIS G 4401:2009 Table 3) distinct from the other-form hardness in JIS G 4401:2009 Table 2
- We match documentation to what the purchase order requires
How to enquire for JIS G 4401 SK75 plate
| Item | What to specify |
|---|---|
| Standard and symbol | JIS G 4401 SK75 and the edition required |
| Product form | Plate |
| Delivery condition | As-hot-rolled (the usual JIS G 4401:2009 supply state for plate and strip) or annealed; say if cold-rolled plate or strip is required |
| Dimensions | Required thickness, width and length; we confirm production and export feasibility against the enquiry |
| Chemistry | Heat analysis to JIS G 4401:2009 Table 1, or to another edition if specified |
| Hardness | Plate hardness to JIS G 4401:2009 Table 3. Table 2 Brinell limits apply to products other than plate and strip |
| Decarburization | Agree a depth for plate if the project needs one; JIS G 4401:2009 Table 7 applies to hot-rolled round bar |
| Other tests | Ultrasonic examination, quench-and-temper hardness or other extra tests only when written on the order |
| Documentation | State the inspection document type required by the project |
| Processing | Cutting or other processing only when requested; thermal-cutting practice depends on carbon content, condition and thickness |
Thickness, width and length are taken from the enquiry. This page does not list stock sizes, mill capacity or fabrication services.
FAQ
-
Does JIS G 4401 cover plate, or only bars?
- Yes. JIS G 4401:2009 has separate hardness rules for steel plates and strips (clause 6.2 and Table 3) and separate appearance and dimension rules (clause 7.2, including Table 6 for plate flatness). It cites JIS G 3193 for hot-rolled plate and strip.
-
Which edition do the tables on this page follow?
- They follow JIS G 4401:2009. Specify the edition required on the purchase order.
-
Is SK75 the same as SK6?
- JIS G 4401:2009 Table 1 lists SK6 as the 1983 reference symbol. The current designation is SK75.
-
Is there an ISO 4957 equivalent for SK75?
- No direct counterpart is specified in JIS G 4401:2009 Annex JB.
-
What should a quotation enquiry include?
- JIS G 4401 SK75, the edition required, plate as the product form, delivery condition, thickness by width by length, quantity, any agreed plate-decarburization or extra tests, and the inspection document required by the project.
Request a quotation
Contact SHH STEEL for a quotation for JIS G 4401 SK75 carbon tool steel plate. Please include your required quantity, plate thickness, width and length, delivery destination and preferred delivery schedule so we can review your production and export requirements.
Specify the delivery condition: as-hot-rolled or annealed, and say if cold-rolled plate or strip is required. If your project requires a stated plate hardness, a decarburization depth, ultrasonic examination or another extra test, include the acceptance criteria and the inspection document required.
If you are considering a related designation, send the applicable standard and project specification with your enquiry so we can review chemistry and supply condition.
For a detailed quotation, email your material specification, quantity and delivery requirements to our team.
Contact: admin@steelspecs.com