JIS G3459 SUS304TP Stainless Steel Pipe | JIS G3459 Stainless Steel Pipe - SHH STEEL

JIS G3459 SUS304TP Stainless Steel Pipe

JIS G3459 SUS304TP stainless steel pipe (304 / UNS S30400), austenitic, Table 3 cast analysis, Rm min 520 N/mm² / proof min 205 N/mm², solution annealed. SHH STEEL can produce and supply seamless or welded routes with mill certificates.
Grade
SUS304TP (304 / UNS S30400 — body alias)
Standard
JIS G3459:2021
Product form
Seamless and welded stainless steel pipe, delivery solution annealed
Size
Typically OD 10.5–660.4 mm (6A–650A); schedule or measured wall by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Pipe Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is JIS G3459 SUS304TP Stainless Steel Pipe

Piping packages that cite Japanese product standards look to JIS G3459:2021 — Stainless steel pipes — rather than inventing a mill grade from AISI shorthand alone. SUS304TP is the Table 1 symbol for this austenitic chemistry. When a Japanese project specification names JIS G3459 and “SUS304TP” rather than a vague “304 pipe”, the purchase order finally locks cast chemistry, heat treatment, and hydraulic/NDT acceptance under one product standard.

Mill path for SUS304TP: Table 1 process/finish symbols, Table 2 heat treatment, Table 3 cast chemistry, Table 4 tensile floors. SHH STEEL can make and supply the grade to that stack with hydrostatic or NDT acceptance as ordered. Typical use: plant utility water, food and beverage transfer, HVAC condensate, fire-protection headers, and general process lines that still say “304 pipe”.

Body text may mention 304 / UNS S30400 for cross-reference, but the H1 and order line stay on SUS304TP. Silent alias swaps are how wrong carbon ceilings and wrong tensile tables enter the MTC. Keep this caution in view: as-welded intergranular attack risk rises when cast carbon sits near the 0.08% ceiling — prefer SUS304LTP or a stabilised sister for corrosive welded joints.

Order the standard the drawing and regulatory file actually require. Inside this G3459 series, compare SUS304LTP, SUS316TP, SUS321TP, SUS304HTP before stretching surface finish or schedule alone. Duty thread: everyday 18-8 austenitic piping grade for corrosion-resistant, low-temperature and utility services where molybdenum is not justified. Document the medium, design temperature, and weld map beside the SUS304TP line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Application context for SUS304TP stays plant utility water, food and beverage transfer, HVAC condensate, fire-protection headers, and general process lines that still say “304 pipe”.

Inside this JIS G3459 series, compare SUS304LTP, SUS316TP, SUS321TP, SUS304HTP. Hub: JIS G3459. ASTM/ASME related product pages (not interchangeable by default): A312 TP304, A269 TP304.

Chemical Composition of JIS G3459 SUS304TP

Table 3 sets the melt limits for SUS304TP. Highlight band: C ≤0.08, Si ≤1.00, Mn ≤2.00, P ≤0.045, S ≤0.030, Ni 8.00–11.00, Cr 18.00–20.00. Product analysis, when ordered, applies JIS G 0321 stainless product tolerances on top of Table 3. Alias note: 304 / UNS S30400. Every ladle analysis for SUS304TP is checked against those windows before the heat is released to piercing, welding, or finishing, and the same numbers reappear on the inspection document. Keep the SUS304TP caution visible here: as-welded intergranular attack risk rises when cast carbon sits near the 0.08% ceiling — prefer SUS304LTP or a stabilised sister for corrosive welded joints.

The composition table below is the cast window SHH STEEL quotes against for SUS304TP. Edition framing is JIS G3459:2021. Use thread: plant utility water, food and beverage transfer, HVAC condensate, fire-protection headers, and general process lines that still say “304 pipe”. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 3, SHH STEEL will confirm melt feasibility for SUS304TP before the order is acknowledged. Keep the SUS304TP caution visible here: as-welded intergranular attack risk rises when cast carbon sits near the 0.08% ceiling — prefer SUS304LTP or a stabilised sister for corrosive welded joints.

Grade C Si Mn P S Ni Cr
SUS304TP ≤0.08 ≤1.00 ≤2.00 ≤0.045 ≤0.030 8.00–11.00 18.00–20.00

Mechanical Properties of JIS G3459 SUS304TP

Table 4 mechanical acceptance for SUS304TP: Rm min 520 N/mm², proof stress min 205 N/mm², elongation (No.11/12 longitudinal) min 35%. Elongation rules change for walls under 8 mm and are not mandatory below 40 mm OD (record only unless agreed). Delivery framing: solution annealed. Tensile sampling follows clause 13 for the ordered test unit of SUS304TP, and retests follow clause 14 when a result sits under the Table 4 floor. Application context for SUS304TP stays plant utility water, food and beverage transfer, HVAC condensate, fire-protection headers, and general process lines that still say “304 pipe”.

Grade Rm min (N/mm²) Proof stress min (N/mm²) A No.11/12 long. min (%) A No.5 trans. min (%) A No.4 long. min (%) A No.4 trans. min (%)
SUS304TP 520 205 35 25 30 22

Ambient values from JIS G3459:2021 Table 4 for SUS304TP. Heat treatment (Table 2): 1010 °C min, rapid cool. Elongation reductions apply for walls under 8 mm; elongation is not mandatory below 40 mm OD (record unless agreed). Note: hot-finished SUS321TP / SUS321HTP may use 460 / 180 N/mm² by agreement.

Manufacture of JIS G3459 SUS304TP Pipe (Seamless and Welded)

JIS G3459 manufactures SUS304TP by seamless (symbol S) or welded routes — automatic arc (A), laser (L), or electric-resistance (E) — then applies the ordered finish: hot finish H, cold finish C, weld-bead worked B, or ERW-as-welded G. SHH STEEL confirms the Table 1 symbol string on the acknowledgement before rolling or welding starts.

After forming, SUS304TP receives Table 2 treatment — 1010 °C min, rapid cool. Austenitic heats take solution annealing with rapid cooling; hot-finished seamless may omit separate solution treatment when hot-worked and rapidly cooled in-line under the Table 2 note, unless the purchaser forbids it. Use thread: plant utility water, food and beverage transfer, HVAC condensate, fire-protection headers, and general process lines that still say “304 pipe”.

Marking carries the grade symbol SUS304TP, process/finish marks, manufacturer ID, and other clause-15 items. Size hint: schedule 5S–40 / 10S–80 OD×wall across 15A–300A is the usual enquiry band; seamless S or welded A/L/E per Table 1. Weld thread: 308/308L-class fillers; control heat input on non-L heats when the joint stays in a corrosive medium.

Dimensions and Tolerances for JIS G3459 SUS304TP

Dimensional order lines for SUS304TP should state OD × wall (or schedule 5S/10S/20S/40/80/…), length type, and end finish. Tolerances follow clause 10 by process route. Use: plant utility water, food and beverage transfer, HVAC condensate, fire-protection headers, and general process lines that still say “304 pipe”. Tolerance class follows the process route ordered for SUS304TP, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Weld-shop note tied to SUS304TP: 308/308L-class fillers; control heat input on non-L heats when the joint stays in a corrosive medium.

OD and wall tolerances differ for hot-finished seamless versus cold-finished / welded routes — quote the process symbol with the size. Caution: as-welded intergranular attack risk rises when cast carbon sits near the 0.08% ceiling — prefer SUS304LTP or a stabilised sister for corrosive welded joints. Fixed lengths and multiple cut lengths for SUS304TP are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Size practice for SUS304TP remains schedule 5S–40 / 10S–80 OD×wall across 15A–300A is the usual enquiry band; seamless S or welded A/L/E per Table 1.

Equivalent Grades for JIS G3459 SUS304TP

SUS304TP is the JIS G3459 designation. Alias 304 / UNS S30400 appears only as a cross-walk. Compare sisters SUS304LTP, SUS316TP, SUS321TP, SUS304HTP when the medium or temperature outgrows this mark. Hook: lock SUS304TP on the PO. When a dual-cert path is required, list both JIS G3459 SUS304TP and the ASTM mark with separate test scopes instead of assuming one chemistry line clears both files. Keep the SUS304TP caution visible here: as-welded intergranular attack risk rises when cast carbon sits near the 0.08% ceiling — prefer SUS304LTP or a stabilised sister for corrosive welded joints.

Heat Treatment and Delivery Condition for JIS G3459 SUS304TP

Mill heat treatment for SUS304TP: 1010 °C min, rapid cool. Bright annealing may omit pickling when the surface is scale-free. Delivery label: solution annealed. Recorded furnace charts for SUS304TP should support the Table 2 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Weld-shop note tied to SUS304TP: 308/308L-class fillers; control heat input on non-L heats when the joint stays in a corrosive medium.

Certificate wording for SUS304TP should show the heat-treatment condition actually performed, not a generic “annealed” stamp that hides temperature. Use: plant utility water, food and beverage transfer, HVAC condensate, fire-protection headers, and general process lines that still say “304 pipe”. Field heat treatment of SUS304TP after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Weld-shop note tied to SUS304TP: 308/308L-class fillers; control heat input on non-L heats when the joint stays in a corrosive medium.

Corrosion Resistance of JIS G3459 SUS304TP

chromium-nickel passive film handles aqueous and mild chemical media; outdoor chloride pitting is usually the first limiter Special quality annex tests are available by agreement; they are not a blanket warranty for every process medium. Family filing: austenitic. Coupon orientation, weld condition, and surface finish for SUS304TP belong in the corrosion test order so annex results can be compared to the installed spool honestly. Keep the SUS304TP caution visible here: as-welded intergranular attack risk rises when cast carbon sits near the 0.08% ceiling — prefer SUS304LTP or a stabilised sister for corrosive welded joints.

Do not market invented PREN digits. Bring medium chemistry and SHH STEEL will map SUS304TP honestly against SUS304LTP, SUS316TP, SUS321TP, SUS304HTP. Role: everyday 18-8 austenitic piping grade for corrosion-resistant, low-temperature and utility services where molybdenum is not justified. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for SUS304TP rather than relying on schedule thickness alone. This paragraph is locked to SUS304TP duty: everyday 18-8 austenitic piping grade for corrosion-resistant, low-temperature and utility services where molybdenum is not justified.

Applications of JIS G3459 SUS304TP Pipe

Typical BOM language pairs JIS G3459 SUS304TP with OD × wall (or schedule), process/finish symbols, and heat-treatment condition. Primary sketch: plant utility water, food and beverage transfer, HVAC condensate, fire-protection headers, and general process lines that still say “304 pipe”. Spool fabricators should copy SUS304TP onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Corrosion framing beside SUS304TP: chromium-nickel passive film handles aqueous and mild chemical media; outdoor chloride pitting is usually the first limiter.

Spell SUS304TP on isometrics, spool sheets and valve specs alike. Sister options when the medium hardens: SUS304LTP, SUS316TP, SUS321TP, SUS304HTP. Commissioning teams benefit when the as-built dossier repeats SUS304TP beside heat numbers, linking isometric revisions to the same mill certificates. Keep the SUS304TP caution visible here: as-welded intergranular attack risk rises when cast carbon sits near the 0.08% ceiling — prefer SUS304LTP or a stabilised sister for corrosive welded joints.

Weldability of JIS G3459 SUS304TP

Weldability of SUS304TP follows austenitic practice. Filler/shop note: 308/308L-class fillers; control heat input on non-L heats when the joint stays in a corrosive medium. Caution: as-welded intergranular attack risk rises when cast carbon sits near the 0.08% ceiling — prefer SUS304LTP or a stabilised sister for corrosive welded joints. Procedure qualification for SUS304TP should use the same product form and wall class as production, including any bead-worked or as-welded finish that will ship. Corrosion framing beside SUS304TP: chromium-nickel passive film handles aqueous and mild chemical media; outdoor chloride pitting is usually the first limiter.

For welded G3459 pipe, confirm whether bead working (B) or as-welded ERW (G) finish is acceptable to the corrosion owner. Shop note: 308/308L-class fillers; control heat input on non-L heats when the joint stays in a corrosive medium. Consumable lot control and shielding-gas notes for SUS304TP stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. This paragraph is locked to SUS304TP duty: everyday 18-8 austenitic piping grade for corrosion-resistant, low-temperature and utility services where molybdenum is not justified.

Surface Finishes for JIS G3459 SUS304TP

Pickled mill finish covers most piping RFQs for SUS304TP. Bright anneal, grind, or polish only when the enquiry writes a measurable target. Use: plant utility water, food and beverage transfer, HVAC condensate, fire-protection headers, and general process lines that still say “304 pipe”. Roughness or polish callouts for SUS304TP must name OD, ID, or both; ambiguous “bright pipe” language is clarified before finishing slots are booked. Weld-shop note tied to SUS304TP: 308/308L-class fillers; control heat input on non-L heats when the joint stays in a corrosive medium.

Sanitary-lean duties may add ID polish; chemical lines may prefer a clean pickle only. State the need on the SUS304TP order. Final visual standards for SUS304TP reject grinding burns, embedded free iron, and unrepaired weld undercut before bundles are closed. Keep the SUS304TP caution visible here: as-welded intergranular attack risk rises when cast carbon sits near the 0.08% ceiling — prefer SUS304LTP or a stabilised sister for corrosive welded joints.

Inspection and Testing for JIS G3459 SUS304TP

SHH STEEL reports the tests actually performed for SUS304TP — no surrogate NDT lines. Hydrostatic vs eddy-current/ultrasonic choice belongs on the PO. Caution: as-welded intergranular attack risk rises when cast carbon sits near the 0.08% ceiling — prefer SUS304LTP or a stabilised sister for corrosive welded joints. Sampling plans for SUS304TP keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Corrosion framing beside SUS304TP: chromium-nickel passive film handles aqueous and mild chemical media; outdoor chloride pitting is usually the first limiter.

NDT sensitivity levels and hydrostatic pressures follow the standard tables unless the purchaser specifies higher. Size context: schedule 5S–40 / 10S–80 OD×wall across 15A–300A is the usual enquiry band; seamless S or welded A/L/E per Table 1. Non-conforming SUS304TP lengths are segregated and retested or rejected under clause 14 rather than reworked into unmarked stock. This paragraph is locked to SUS304TP duty: everyday 18-8 austenitic piping grade for corrosion-resistant, low-temperature and utility services where molybdenum is not justified.

Packaging and Shipping for JIS G3459 SUS304TP

Export packing for JIS G3459 SUS304TP is built around rust prevention and transit abrasion control. Bundle tickets repeat the grade symbol and heat number. Duty: everyday 18-8 austenitic piping grade for corrosion-resistant, low-temperature and utility services where molybdenum is not justified. Bundle tickets for SUS304TP repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Corrosion framing beside SUS304TP: chromium-nickel passive film handles aqueous and mild chemical media; outdoor chloride pitting is usually the first limiter.

Marking paint and ink stickers stay chloride-lean. Heat numbers on tags match the MTC for SUS304TP. Desiccant and wrap choices for SUS304TP follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Weld-shop note tied to SUS304TP: 308/308L-class fillers; control heat input on non-L heats when the joint stays in a corrosive medium.

Photographic packing records are available on request for project QA files on SUS304TP. Claims handling for SUS304TP starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. This paragraph is locked to SUS304TP duty: everyday 18-8 austenitic piping grade for corrosion-resistant, low-temperature and utility services where molybdenum is not justified.

Why Choose SHH STEEL

SHH STEEL can produce and supply JIS G3459 SUS304TP. Buyers choose SHH STEEL for SUS304TP because the paperwork matches the stencil: Table 3 chemistry, Table 4 tensile, Table 2 heat treatment, and honest S/A/L/E marking. Application fit: plant utility water, food and beverage transfer, HVAC condensate, fire-protection headers, and general process lines that still say “304 pipe”.

SHH STEEL will not invent PREN posters or warehouse tonnages. Bring OD × wall, medium notes, and test scope — we will quote SUS304TP cleanly. Ask for a written acknowledgement that names SUS304TP, the Table 1 process/finish marks, and the Table 2 heat-treatment condition before melt. SHH STEEL can make SUS304TP to that written scope.

Supply Capability

Supply capability for SUS304TP covers process/finish symbols in Table 1, heat treatment in Table 2, and mechanical acceptance in Table 4. SHH STEEL can make the sizes on your list when the mill slot fits. Role: everyday 18-8 austenitic piping grade for corrosion-resistant, low-temperature and utility services where molybdenum is not justified.

Item Capability
Standard JIS G3459:2021 stainless steel pipes
Grade symbol SUS304TP
Product form Seamless (S) and welded (A / L / E) pipe; finishes H / C / B / G
Delivery condition solution annealed
Documents Mill test certificate (JIS G 0415 / EN 10204 3.1 style as ordered)
Typical OD practice 10.5–660.4 mm (6A–650A) per standard Note 1; other by agreement
Wall / schedule Schedule 5S–160 class and measured wall within family practice

Stock / Available sizes

SHH STEEL can produce and supply JIS G3459 SUS304TP. Stock / Available sizes for SUS304TP: common A-number bores with schedule or measured wall as the project uses. Seamless and welded availability varies by diameter — confirm route with the RFQ. Hint: schedule 5S–40 / 10S–80 OD×wall across 15A–300A is the usual enquiry band; seamless S or welded A/L/E per Table 1.

Mill certificates, packing photos, and third-party witness can be bundled into the SUS304TP supply scope when the PO says so. Use: plant utility water, food and beverage transfer, HVAC condensate, fire-protection headers, and general process lines that still say “304 pipe”. SHH STEEL can produce trial lengths of SUS304TP for procedure qualification before the bulk release when the project calendar needs it.

FAQ

What is JIS G3459 SUS304TP stainless steel pipe used for?
JIS G3459 SUS304TP is stainless pipe for corrosion-resistant, low-temperature, high-temperature and fire-protection piping — plant utility water, food and beverage transfer, HVAC condensate, fire-protection headers, and general process lines that still say “304 pipe”. Role summary: everyday 18-8 austenitic piping grade for corrosion-resistant, low-temperature and utility services where molybdenum is not justified. It is a Japanese product standard mark, not an automatic ASTM A312 certificate.
Does JIS G3459 SUS304TP cover seamless and welded pipe?
Yes. Table 1 allows seamless (S) and welded automatic-arc (A), laser (L), or electric-resistance (E) routes with finish symbols H/C/B/G. SHH STEEL can produce and supply either route for SUS304TP when the mill can meet the ordered size and tests. The title omits Seamless/Welded because the standard itself covers both — the PO must still name the process symbol.
What heat treatment applies to SUS304TP?
SUS304TP is delivered solution annealed under JIS G3459. Table 2 reference: 1010 °C min, rapid cool. Stabilisation or other purchaser options, where allowed, must be written on the order. Certificate wording should match the treatment actually performed.
How does SUS304TP compare with sister grades SUS304LTP, SUS316TP, SUS321TP?
SUS304TP is filed as austenitic. Typical sisters on the same RFQ are SUS304LTP, SUS316TP, SUS321TP. Design caution: as-welded intergranular attack risk rises when cast carbon sits near the 0.08% ceiling — prefer SUS304LTP or a stabilised sister for corrosive welded joints Pick the sister when the medium or strength floor outgrows this symbol rather than stretching schedule alone.
What tests appear on the mill certificate for SUS304TP?
Expect cast analysis (Table 3), room-temperature tensile results (Table 4), dimensions, hydrostatic or NDT as ordered, and every special annex test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow JIS G 0415 or EN 10204 3.1 style when specified.
Is 304 / UNS S30400 the same as ordering SUS304TP?
No. 304 / UNS S30400 is a commercial / UNS cross-walk for body text. The purchase order should lock JIS G3459 and SUS304TP so cast limits, heat treatment, and process symbols are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for JIS G3459 SUS304TP?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for SUS304TP within the typical 10.5–660.4 mm OD practice, with schedules or measured walls by agreement. Size context: schedule 5S–40 / 10S–80 OD×wall across 15A–300A is the usual enquiry band; seamless S or welded A/L/E per Table 1. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
How should SUS304TP be welded?
Shop guidance: 308/308L-class fillers; control heat input on non-L heats when the joint stays in a corrosive medium. Mill heat treatment of seamless or welded pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or anneal practice as applicable. Caution: as-welded intergranular attack risk rises when cast carbon sits near the 0.08% ceiling — prefer SUS304LTP or a stabilised sister for corrosive welded joints
When should I choose a duplex or higher-Mo grade instead of SUS304TP?
Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: as-welded intergranular attack risk rises when cast carbon sits near the 0.08% ceiling — prefer SUS304LTP or a stabilised sister for corrosive welded joints Sister pointers: SUS304LTP, SUS316TP, SUS321TP. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify JIS G3459 SUS304TP with ASTM A312 or A789?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites JIS G3459 SUS304TP does not clear ASTM acceptance by default. State both standards, sizes, and test scopes before melt.
What surface finishes are available for SUS304TP?
Pickled after heat treatment is the usual piping supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for SUS304TP when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.

Conclusion

JIS G3459 SUS304TP is stainless steel pipe for corrosion-resistant, low-temperature, high-temperature and fire-protection piping — everyday 18-8 austenitic piping grade for corrosion-resistant, low-temperature and utility services where molybdenum is not justified. SHH STEEL can produce and supply it in seamless or welded routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include SUS304LTP, SUS316TP, SUS321TP. Related ASTM pages share chemistry families but not Japanese acceptance text. Email admin@steelspecs.com with OD × wall, process symbol, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X