JIS G3127 SL3N440 Steel Plate
What is JIS G 3127 SL3N440 plate?
We produce and export JIS G 3127 SL3N440 as nickel steel plate for low-temperature pressure vessels and storage equipment. SL3N440 is a 3.5 % nickel grade with a heat-analysis nickel range of 3.25–3.75 %. Typical service includes higher-strength 3.5 % nickel vessels and tanks that specify quenched-and-tempered plate and toughness at −110 °C.
JIS G 3127:2013 lists eight official symbols. This page specifies only SL3N440. Heat-treatment letters such as N, NT, TMC, TMCT, NNT and Q are marking symbols for the treatment actually given to the plate or test piece; they are not extra official kinds.
Composition, tensile properties, impact energy and heat-treatment conditions on this page follow JIS G 3127:2013. Specify the edition required on the purchase order.
SHH STEEL produces and exports JIS G 3127 SL3N440 plate to the ordered edition, delivery condition, dimensions and extra tests written on the enquiry.
Material specification for JIS G 3127 SL3N440
The items below follow JIS G 3127:2013. Thickness, width, length and the inspection document are stated on the enquiry rather than listed here as stock or capacity ranges.
| Parameter | Detail |
|---|---|
| Standard | JIS G 3127:2013, Nickel steel plates for pressure vessels for low temperature services |
| Official symbol | SL3N440 |
| Product form | Hot-rolled steel plate |
| How designations are listed | Eight official symbols in JIS G 3127:2013 Table 1 |
| Steelmaking | Killed steel |
| Applicable thickness | 6–50 mm (Table 1) |
| Minimum usable temperature listed in Table 1 | −110 °C |
| Usual heat treatment | Quenched and tempered. An intermediate heat treatment, cooling from the austenite-plus-ferrite two-phase region before tempering, may be added to improve toughness. |
| Heat-treatment marking | Q (quenching and tempering). Test-piece symbols TN, TNT, T2NT and SR may be added when specimen heat treatment is ordered |
| Chemical analysis | Heat analysis to JIS G 3127:2013 Table 3. Product analysis, when required, uses the permitted variations in JIS G 0321 Table 4 |
| Tensile and bend properties | JIS G 3127:2013 Table 4 (1 N/mm² = 1 MPa) |
| Impact properties | JIS G 3127:2013 Table 5, Charpy V-notch, rolling direction unless otherwise agreed |
| Dimensions | JIS G 3193, except thickness tolerances in JIS G 3127:2013 Table 6. Minus thickness tolerance is 0.25 mm unless a 0 mm minus tolerance is agreed |
| Appearance | JIS G 3193 clause 7. Weld repair only with prior purchaser approval |
| Marking | Official symbol and heat-treatment symbol, heat or inspection number, dimensions, and manufacturer name or abbreviation |
| Inspection document | When no document type is named, JIS G 3127:2013 refers to JIS G 0415 inspection document 2.3 or inspection certificate 3.1.B |
| Our supply | We produce and export SL3N440 plate to the ordered edition, delivery condition, dimensions and extra tests |
Chemical composition of JIS G 3127 SL3N440
JIS G 3127:2013 Table 3 is heat analysis. Other alloying elements may be added as needed; if they are added, their contents are reported on the inspection document.
| Element | SL3N440 heat analysis, JIS G 3127:2013 Table 3 (wt. %) |
|---|---|
| Carbon (C) | 0.15 max |
| Silicon (Si) | 0.30 max |
| Manganese (Mn) | 0.70 max |
| Phosphorus (P) | 0.015 max |
| Sulfur (S) | 0.015 max |
| Nickel (Ni) | 3.25–3.75 |
Tensile, bend and impact properties for JIS G 3127 SL3N440
JIS G 3127:2013 specifies tensile, bend and Charpy impact properties. Table 4 values are in N/mm², which the standard notes are equal to MPa.
| Mechanical property (JIS G 3127:2013 Table 4) | SL3N440 |
|---|---|
| Yield strength or proof strength, MPa | 440 min |
| Tensile strength, MPa | 540–690 |
| Elongation, % | 21 min (No. 5 specimen, 6–16 mm. Table 4 also gives 25 % min (No. 5, over 16 mm) and 21 % min (No. 4, over 20 mm).) |
| Bend test | 180°; inside radius 1.0× thickness at 25 mm and below, 1.5× thickness above 25 mm; No. 1 specimen; no crack on the outer surface |
Charpy V-notch impact values below are JIS G 3127:2013 Table 5 at −110 °C. By agreement, testing may be carried out at a lower temperature in place of the listed temperature. Transverse testing may be agreed; with purchaser approval the rolling-direction test may then be omitted.
| Charpy V-notch (JIS G 3127:2013 Table 5) | SL3N440 |
|---|---|
| Test temperature, °C | −110 |
| Average of three 10×10 mm specimens, J | 27 min |
| Individual 10×10 mm specimen, J | 21 min |
| Subsize specimens | For smaller specimens Table 5 requires averages of 14 J (10×5 mm) and 22 J (10×7.5 mm), with individual minima of 11 J and 17 J. |
Delivery conditions for JIS G 3127 SL3N440
JIS G 3127:2013 Table 2 sets the heat treatment for SL3N440: Quenched and tempered. An intermediate heat treatment, cooling from the austenite-plus-ferrite two-phase region before tempering, may be added to improve toughness.
If the purchaser will heat-treat the plate, the plate may be supplied as-rolled by agreement, and the purchase order must state that fact and the heat-treatment conditions.
The usual marking addition for this treatment is Q (quenching and tempering). Examples in clause 4.5 include SL2N255N, SL3N275NT, SL3N255TMC, SL7N590TMCT, SL9N520NNT and SL9N590Q. Those suffixes record the treatment; they do not create extra official symbols beyond the eight kinds in Table 1.
The purchase order should name the official symbol, the heat-treatment symbol, thickness, width and length, any extra specimen heat treatment (including PWHT simulation, marked SR), and the inspection document required.
This page does not offer heat-treatment or fabrication services.
Welding and thermal cutting4403
JIS G 3127:2013 does not specify a welding procedure. SL3N440 is a 3.5 % nickel pressure-vessel plate, not a general structural plate. Welding and thermal cutting should be qualified for the nickel content, thickness, delivery condition and the minimum temperature of the equipment.
Higher-nickel grades, especially the 9 % nickel symbols, are commonly welded with matching high-nickel filler metals and controlled heat input. Thermal cutting can harden the adjacent material; that zone should be considered, and removed where later forming or welding requires it.
Form, appearance, dimensions and thickness tolerances
Shape, dimensions, mass and most tolerances follow JIS G 3193. Length and cut-edge width tolerances are tolerance A unless otherwise specified. Thickness tolerances are JIS G 3127:2013 Table 6. The minus thickness tolerance is 0.25 mm; if a 0 mm minus tolerance is agreed, 0.25 mm is added to the plus side.
Appearance follows JIS G 3193 clause 7. Weld repair requires prior purchaser approval. Numeric thickness, width, length and flatness limits should be stated on the purchase order.
Applications and specificat3o440imits
We produce and export SL3N440 plate for higher-strength 3.5 % nickel vessels and tanks that specify quenched-and-tempered plate and toughness at −110 °C. JIS G 3127:2013 Table 1 lists a minimum usable temperature of −110 °C for this symbol and an applicable thickness of 6–50 mm.
If the design temperature moves into a colder nickel class, or if a different official symbol, should be treated as a new material selection. Strength after a later heat treatment that is not the Table 2 condition is not assumed from the symbol alone.
JIS G 3127 is a nickel steel plate standard for low-temperature pressure vessels. It is not a carbon low-temperature plate standard such as JIS G 3126, and it is not an ASTM A353 or A553 order unless those specifications are written on the enquiry.
Compare JIS G 3127 SL3N440 with other steel plates
SL3N440 is a 3.5 % nickel low-temperature vessel plate. The comparison below is for selection only; these materials are not equivalents.
| Material | Alloy / type | Delivery condition | Mechanical requirements | Typical service | Substitution limit |
|---|---|---|---|---|---|
| JIS G 3127 SL3N440 (this plate) | 3.5 % nickel vessel plate, heat-analysis nickel 3.25–3.75 % | Quenched and tempered. | JIS G 3127:2013: yield 440 MPa minimum, tensile 540–690 MPa; Charpy average 27 J minimum at −110 °C on a 10×10 mm specimen | Typical service includes higher-strength 3.5 % nickel vessels and tanks that specify quenched-and-tempered plate and toughness at −110 °C | A different nickel class, heat treatment or specification is not an automatic substitute |
| JIS G 3127 SL3N275 steel plate | 3.5 % nickel vessel plate, heat-analysis nickel 3.25–3.75 % | Normalized. Normalizing and tempering may be applied if needed. By agreement the manufacturer may use TMCP or another appropriate heat treatment. | JIS G 3127:2013: yield 275 MPa minimum, tensile 480–620 MPa; Charpy average 21 J minimum at −101 °C on a 10×10 mm specimen | Typical service includes low-temperature pressure vessels that need toughness at −101 °C and the higher 275 MPa yield of this 3.5 % nickel symbol | A different official symbol from SL3N440, not an automatic substitute |
| ASTM A203 Grade F | Quenched-and-tempered 3.5 % nickel vessel plate | Quenched and tempered | Tensile 550–690 MPa | Higher-strength 3.5 % nickel vessel service | Related QT 3.5 % nickel plate under ASTM A203, not an automatic substitute |
| GB/T 713.4 08Ni3DR | Chinese 3.5 % nickel low-temperature vessel plate | As specified in GB/T 713.4-2023 | Yield 320 MPa, tensile 490–620 MPa, service about −100 °C | 3.5 % nickel low-temperature vessels and tanks | A different standard and strength window from this JIS symbol, not an automatic substitute |
| ASME SA203 Grade E | Nickel-alloy pressure-vessel plate in the normalized SA203 family. | Normalized. | Use its own ordered specification, thickness and delivery condition; no strength or toughness value is transferred to this grade. | Low-temperature process vessels and refrigerated containment. | A normalized nickel-vessel comparison, not automatic equivalence to the JIS symbol. Its Code edition, strength, impact temperature and certification must be selected separately. |
Equivalent and related grades by country
The designations below are near names, not automatic substitutes. Confirm chemistry, heat treatment, tensile properties, impact temperature and product form before any substitution.
| Country / region | Standard | Grade or designation | Similarity and key differences | Substitution caveat |
|---|---|---|---|---|
| Japan | JIS G 3127:2013 | SL3N440 | This plate. Heat-analysis nickel 3.25–3.75 %, yield 440 MPa minimum, tensile 540–690 MPa, Charpy at −110 °C. Quenched and tempered. | This product |
| United States | ASTM A203/A203M | Grade F | A quenched-and-tempered 3.5 % nickel vessel plate. Tensile strength is 550–690 MPa, close to this 540–690 MPa window, but yield and impact rules remain those of ASTM A203. | Near name only. |
| China | GB/T 713.4-2023 | 08Ni3DR | The closest Chinese 3.5 % nickel vessel plate is 08Ni3DR. It is not a 440 MPa quenched-and-tempered grade of this type. | Related nickel class only. |
| Europe | EN 10028-4 | No direct counterpart specified | No verified one-to-one European counterpart was established for this quenched-and-tempered 3.5 % nickel symbol. | Confirm chemistry, heat treatment and toughness before any substitution. |
| International | ISO 9328-1 and ISO 9328-4 | No single ISO symbol specified | JIS G 3127:2013 is based on ISO 9328-1:2011 and ISO 9328-4:2011 with modifications (MOD). The 2013 comparison notes that JIS lists eight kinds and treats SL7N590 as its own kind. | Use the JIS symbol on the order unless an ISO designation is separately specified. |
Why choose SHH STEEL for JIS G 3127 SL3N440
- We produce and export JIS G 3127 SL3N440 nickel steel plate
- We review the enquiry for edition, symbol, heat-treatment mark, dimensions and extra tests
- We keep the eight official symbols distinct, including the N, Q and NNT delivery routes
- We match documentation to what the purchase order requires
How to enquire for JIS G 3127 SL3N440 plate
| Item | What to specify |
|---|---|
| Standard and symbol | JIS G 3127 SL3N440 and the edition required |
| Heat-treatment mark | Q (quenching and tempering) |
| Dimensions | Required thickness (6–50 mm in Table 1), width and length |
| Chemistry | Heat analysis to JIS G 3127:2013 Table 3, or to another edition if specified |
| Mechanical tests | Tensile and bend properties to Table 4; Charpy tests to Table 5 unless a lower test temperature is agreed |
| Other tests | Ultrasonic examination or other extra tests only when written on the order |
| Documentation | State the inspection document type required by the project |
| Processing | Cutting or other processing only when requested |
Thickness, width and length are taken from the enquiry. This page does not list stock sizes, mill capacity or fabrication services.
FAQ
-
Does JIS G 3127 cover only 9 % nickel plate?
- No. JIS G 3127:2013 lists eight official symbols: SL2N255, SL3N255, SL3N275, SL3N440, SL5N590, SL7N590, SL9N520 and SL9N590. This page is SL3N440.
-
Which edition do the tables on this page follow?
- They follow JIS G 3127:2013. Specify the edition required on the purchase order.
-
What do suffixes such as N, Q or NNT mean?
- They are official heat-treatment marking symbols in JIS G 3127:2013 clause 4.5, not extra kinds. For SL3N440 the usual mark is Q (quenching and tempering). Test-piece letters such as SR can be added when specimen heat treatment is ordered.
-
Can another nickel vessel plate be used in place of SL3N440?
- Only after a project review. Related names in other specifications may share a nickel class but differ in yield, tensile range, heat treatment or impact temperature.
-
What should a quotation enquiry include?
- JIS G 3127 SL3N440, the edition required, the heat-treatment mark, plate thickness by width by length, quantity, any extra tests or specimen heat treatment, and the inspection document required by the project.
Request a quotation
Contact SHH STEEL for a quotation for JIS G 3127 SL3N440 nickel steel plate. Please include your required quantity, plate thickness, width and length, delivery destination and preferred delivery schedule so we can review your production and export requirements.
Specify the heat-treatment condition and marking symbol, and say if specimen heat treatment or a PWHT simulation is required. If your project requires a stated impact temperature below the Table 5 value, ultrasonic examination or another extra test, include the acceptance criteria and the inspection document required.
If you are considering a related designation, send the applicable standard and project specification with your enquiry so we can review chemistry, heat treatment and toughness.
For a detailed quotation, email your material specification, quantity and delivery requirements to our team.