JIS G 3455 STS370 Seamless Steel Pipe

JIS G 3455:2024 STS370 is seamless carbon steel pipe for high-pressure service at temperatures not exceeding 350 °C. Heat analysis limits carbon to 0.25 %, silicon 0.10–0.35 %, manganese 0.30–1.10 %, and phosphorus and sulfur to 0.035 %. Minimum tensile strength is 370 N/mm² and minimum yield is 215 N/mm². Size tables are a typographical Schedule 40 subset.
Keywords
JIS G 3455 STS370, STS370 seamless pipe, JIS G3455 high-pressure pipe, STS370 carbon steel pipe, G 3455 STS370 sizes
Equivalent Grades:
Near-equivalents only, not automatic substitutes.
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Size Chart
Applications
Equivalent Grades
Sourcing
FAQ
Conclusion

What is JIS G 3455 STS370 Seamless Steel Pipe?

JIS G 3455 STS370 is seamless carbon steel pipe intended for high-pressure service at a temperature not exceeding 350 °C. The values on this page follow JIS G 3455:2024, cross-checked against a JISC-verified public recitation and against the 2020 English text where those sources agree on the STS370 limits. The edition named on the purchase order governs delivery.

STS370 is one grade in G 3455; higher-strength grades in the same standard are not this product. Do not treat this pipe as JIS G 3454 STPG370 Seamless Steel Pipe. G 3454 is a different specification with a different service statement, even where some chemical or tensile figures look close.

Material, Manufacture and Scope for JIS G 3455 STS370 Seamless Pipe

The product is seamless pipe. Welded pipe is outside the scope of this page. G 3455 is a carbon steel pipe specification for high-pressure service, with a temperature ceiling of 350 °C in the edition used here. Design pressure, joint design and any required non-destructive tests remain the responsibility of the purchaser’s design standard; this page does not convert the 350 °C statement into a boiler Code listing.

A corresponding international note sometimes links JIS G 3455 with ISO 9329-2 (elevated-temperature or high-pressure quality), not with ISO 9329-1. Existing ISO 9329-4 stainless tube pages on this site are a different product family and are not substitutes for STS370.

JIS G 3455 STS370 Chemical Composition (Heat Analysis)

The table lists the STS370 heat-analysis limits used on this page. Silicon and manganese are ranges. Do not apply a STPG370, STS410 or STS480 row to this grade.

Swipe horizontally to view all dimensions.

Element Heat-analysis limit (mass %) Notes
C, max 0.25 STS370 heat analysis in JIS G 3455:2024, cross-checked to the 2020 English text where the two agree.
Si 0.10–0.35 A range, not a maximum only.
Mn 0.30–1.10 A range, not a maximum only.
P, max 0.035 —
S, max 0.035 —

JIS G 3455 STS370 Mechanical Properties

Minimum tensile strength is 370 N/mm² and minimum yield strength is 215 N/mm². Elongation depends on the test piece: 30 % on No. 11 or No. 12, 25 % on No. 5, and 28 % longitudinal or 23 % transverse on No. 4. The test piece actually used must be the one reported on the certificate.

Swipe horizontally to view all dimensions.

Property Requirement for STS370
Tensile strength, min 370 N/mm²
Yield strength, min 215 N/mm²
Elongation, min, No. 11 or No. 12 test piece 30 %
Elongation, min, No. 5 test piece 25 %
Elongation, min, No. 4 test piece, longitudinal / transverse 28 % / 23 %

JIS G 3455 STS370 Common Sizes: JIS Schedule 40 Typographical Subset

The table below is a common typographical JIS Schedule 40 subset from 6A to 350A, shown here for JIS G 3455:2024 STS370 seamless pipe. Published masses have been checked with W = 0.0246615(D − t)t. Japanese outside diameters (21.7 mm at 15A, 34.0 mm at 25A, and so on) are used. This is not a complete JIS G 3455 size range: other schedules exist and must be named if they are wanted. It is also not a stock list. Masses are for plain ends. The same typographical subset appears on JIS G 3454 STPG370 Seamless Steel Pipe; that product is G 3454 STPG370, a different specification, and the two certificates are not interchangeable.

Swipe horizontally to view all dimensions.

Nominal size B (in) Outside diameter D (mm) Wall t (mm) Mass (kg/m)
6A 1/8 10.5 1.7 0.369
8A 1/4 13.8 2.2 0.629
10A 3/8 17.3 2.3 0.851
15A 1/2 21.7 2.8 1.31
20A 3/4 27.2 2.9 1.74
25A 1 34 3.4 2.57
32A 1 1/4 42.7 3.6 3.47
40A 1 1/2 48.6 3.7 4.1
50A 2 60.5 3.9 5.44
65A 2 1/2 76.3 5.2 9.12
80A 3 89.1 5.5 11.3
90A 3 1/2 101.6 5.7 13.5
100A 4 114.3 6 16
125A 5 139.8 6.6 21.7
150A 6 165.2 7.1 27.7
200A 8 216.3 8.2 42.1
250A 10 267.4 9.3 59.2
300A 12 318.5 10.3 78.3
350A 14 355.6 11.1 94.3

Applications and Service Limits for JIS G 3455 STS370 Seamless Pipe

STS370 is used for high-pressure carbon steel piping within the 350 °C ceiling of G 3455 and the purchaser’s design standard. It is not automatically a substitute for G 3454 STPG370, for ASTM A106 Grade B, or for a listed ASME SA-106 product. End finish, length and any required tests must be stated on the order.

Near-Equivalents for JIS G 3455 STS370 Seamless Pipe: Not Automatic Substitutes

Near-equivalents only, not automatic substitutes. JIS G 3454 STPG370, ASTM A106 Grade B, ASME SA-106 Grade B and related ISO 9329-2 grades have their own chemistry, tests and service statements. Do not treat a certificate from those specifications as STS370, and do not use an ISO 9329-4 stainless tube page as a carbon-steel stand-in.

Sourcing JIS G 3455 STS370 Seamless Steel Pipe from SHH STEEL

SHH STEEL reviews the named JIS G 3455 edition, the STS370 certificate and the ordered size and schedule before quoting. The typographical Schedule 40 subset on this page is not a warehouse list. Name the A-size or outside diameter, the schedule or wall, and the end finish on the enquiry.

FAQ: JIS G 3455 STS370 Seamless Steel Pipe

Is STS370 the same as JIS G 3454 STPG370?
No. G 3455 STS370 is a high-pressure specification with a 350 °C service ceiling in the 2024 edition used here. G 3454 STPG370 is a different standard. The typographical Schedule 40 subset may look similar; the certificates are not interchangeable.
Which edition is used on this page?
JIS G 3455:2024, cross-checked against a JISC-verified recitation and the 2020 English text where those sources agree on the STS370 limits. The edition named on the order governs delivery.
Is this ISO 9329-1 pipe?
No. Correspondence notes for G 3455 point toward ISO 9329-2, not ISO 9329-1. Existing ISO 9329-4 stainless tube pages on this site are also not this product.

Conclusion

Specify JIS G 3455 STS370 as seamless high-pressure carbon steel pipe to the named edition, with the STS370 chemistry and the 370 / 215 N/mm² mechanical minima. Do not substitute G 3454 STPG370 or an ISO 9329-1 or 9329-4 document without a written agreement.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X