JIS G3455

Product Showcase

JIS G3455 Steel Structural Profiles

SHH STEEL offers JIS G3455 carbon steel seamless pipes. JIS G3455 specifies STS370/STS410 pipes for high-pressure service in steam and water lines. High-strength, certified quality, competitive prices, customizable. Trust SHH STEEL!

JIS G 3455 STS370 Seamless Steel Pipe

JIS G 3455:2024 STS370 is seamless carbon steel pipe for high-pressure service at temperatures not exceeding 350 °C. Heat analysis limits carbon to 0.25 %, silicon 0.10–0.35 %, manganese 0.30–1.10 %, and phosphorus and sulfur to 0.035 %. Minimum tensile strength is 370 N/mm² and minimum yield is 215 N/mm². Size tables are a typographical Schedule 40 subset.
View More

JIS G3455 Steel Structural Profiles

Seamless Steel Pipes

SHH STEEL, a leading Steel Seamless Pipes exporter, produces and exports steel seamless pipes for high-pressure and structural applications. Our products, like ASTM A106, offer strength and reliability. With a 5,000-ton inventory, we deliver in 3–5 days, backed by SGS/TUV inspections and mill certificates. Trust SHH STEEL for ASTM A106 seamless pipes and custom solutions.

Buyers also search this range as seamless steel pipe, seamless steel tube and hot-rolled or cold-drawn seamless pipe. The applicable standard, grade, size and test requirements are confirmed per inquiry.