JIS G 3454 STPG370 Seamless Steel Pipe

JIS G 3454 STPG370 is carbon steel pipe for pressure service, with a 370 MPa tensile minimum and 215 MPa yield. Cast analysis limits carbon to 0.25 % and phosphorus and sulphur to 0.040 %. The size table is a common JIS Schedule 40 subset with formula-checked masses. This page is seamless STPG370 only. SHH STEEL reviews the certificate before quoting.
Keywords
JIS G 3454 STPG370, STPG370 seamless pipe, JIS pressure pipe, STPG370 Sch40, G 3454 carbon steel pipe
Equivalent Grades:
Near-equivalents only, not automatic substitutes.
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Size Chart (19 common Schedule 40 sizes)
Applications
Equivalent Grades
Sourcing
FAQ
Conclusion

What is JIS G 3454 STPG370 Seamless Steel Pipe?

JIS G 3454 specifies carbon steel pipes for pressure service. STPG370 is the usual lower-strength grade in that standard, with a 370 N/mm² tensile minimum and a 215 N/mm² yield or proof-stress minimum. The standard allows seamless and electric-resistance-welded manufacture, with finish symbols such as S-H (hot-finished seamless), S-C (cold-finished seamless), E-H, E-C and E-G. This page is filed under seamless steel pipes and is confined to seamless STPG370 (S-H or S-C). An ERW enquiry is a different product and must not be published on this leaf.

The pipe is usually delivered as manufactured; cold-finished pipe is annealed after manufacture. Ends may be plain or, when required, bevelled.

Material, Manufacture and Scope for JIS G 3454 STPG370 Seamless Pipe

STPG410 is a higher-strength grade in the same standard and is not this page. Hydrostatic test pressures vary with schedule number; a Schedule 40 listing, for example, is commonly associated with a 6.0 MPa test pressure in mill tables, but the ordered schedule and the standard’s own test clause govern the certificate. Dimensional tolerances differ for hot-finished seamless pipe and for cold-finished seamless pipe, and they must not be taken from a welded-pipe table.

JIS G 3454 STPG370 Chemical Composition

Cast analysis for STPG370 is carbon 0.25 % maximum, silicon 0.35 % maximum, manganese 0.30–0.90 %, phosphorus 0.040 % maximum and sulphur 0.040 % maximum. Other alloying elements may be added if necessary. These phosphorus and sulphur limits are 0.040 %, not 0.40 %; a missing zero in a secondary table should not be copied onto the certificate.

Swipe horizontally to view all dimensions.

Element STPG370, %
Carbon, max 0.25
Silicon, max 0.35
Manganese 0.30–0.90
Phosphorus, max 0.040
Sulphur, max 0.040

JIS G 3454 STPG370 Mechanical Properties

STPG370 requires a tensile strength of at least 370 N/mm² and a yield point or proof stress of at least 215 N/mm². Minimum elongation is 30 % for a No. 11 or No. 12 piece taken parallel to the pipe axis, 25 % for a No. 5 piece taken perpendicular to the axis, and 28 % / 23 % for No. 4 pieces in the two directions. When the wall is thinner than 8 mm, the elongation is reduced by 1.5 % for each 1 mm reduction in wall thickness, using the banded table in the standard. Flattening and bending tests also apply as specified.

Swipe horizontally to view all dimensions.

Property STPG370
Tensile strength, min 370 N/mm² (MPa)
Yield point or proof stress, min 215 N/mm² (MPa)
Elongation, No. 11 or No. 12, parallel to the axis, min 30 %
Elongation, No. 5, perpendicular, min 25 %
Elongation, No. 4, parallel / perpendicular, min 28 % / 23 %

JIS G 3454 STPG370 Common Sizes: JIS Schedule 40 Subset

The table below is a common JIS Schedule 40 typographical subset from 6A to 350A, with published masses that have been checked with W = 0.0246615(D − t)t. Japanese outside diameters (21.7 mm at 15A, 34.0 mm at 25A, and so on) are used. This is not a complete JIS G 3454 size range: other schedules, including 20, 60 and 80, exist and must be named if they are wanted. It is also not a stock list. Masses are for plain ends.

Swipe horizontally to view all dimensions.

Nominal size B (in) Outside diameter D (mm) Wall t (mm) Mass (kg/m)
6A 1/8 10.5 1.7 0.369
8A 1/4 13.8 2.2 0.629
10A 3/8 17.3 2.3 0.851
15A 1/2 21.7 2.8 1.31
20A 3/4 27.2 2.9 1.74
25A 1 34 3.4 2.57
32A 1 1/4 42.7 3.6 3.47
40A 1 1/2 48.6 3.7 4.1
50A 2 60.5 3.9 5.44
65A 2 1/2 76.3 5.2 9.12
80A 3 89.1 5.5 11.3
90A 3 1/2 101.6 5.7 13.5
100A 4 114.3 6 16
125A 5 139.8 6.6 21.7
150A 6 165.2 7.1 27.7
200A 8 216.3 8.2 42.1
250A 10 267.4 9.3 59.2
300A 12 318.5 10.3 78.3
350A 14 355.6 11.1 94.3

Applications and Service Limits for JIS G 3454 STPG370 Seamless Pipe

STPG370 is used for ordinary pressure piping in plant and building work where JIS G 3454 is named. It is not JIS G 3452 SGP ordinary piping, not JIS G 3455 high-pressure pipe, and not ASTM A106 Grade B. Those products have different chemistry, test and size rules.

Near-Equivalents for JIS G 3454 STPG370 Seamless Pipe: Not Automatic Substitutes

ASTM A106 Grade B and GB/T 8163 Grade 20 are often compared in export enquiries, but the tensile minima, yield values and chemistry ranges differ. EN 10216-1 P235TR1 is a European pressure-tube grade, not a restamp of STPG370. JIS G 3452 SGP has no carbon limit and a 290 MPa tensile minimum, and it is not a pressure-pipe standard.

Sourcing JIS G 3454 STPG370 Seamless Steel Pipe from SHH STEEL

Send the nominal size or outside diameter, the schedule or wall, hot-finished or cold-finished seamless process, length, end finish, and the JIS G 3454 edition. Name STPG370 and the seamless process explicitly. Do not tick a welded-pipe term for this page. SHH STEEL reviews the process, the grade and the certificate before quoting.

JIS G 3454 STPG370 Seamless Pipe FAQs

Can STPG370 be electric-resistance welded?
The standard allows ERW as well as seamless manufacture. This page is confined to seamless STPG370 under the seamless-pipe category. An ERW enquiry is a different product.
Is Schedule 40 the only available wall?
No. The table is a common Schedule 40 subset. Other schedules exist and must be named if they are required.
How does STPG370 differ from SGP?
SGP under JIS G 3452 is ordinary piping with no carbon limit and a 290 MPa tensile minimum. STPG370 is a pressure-pipe grade with specified carbon, manganese and a 370/215 MPa tensile/yield pair.
Are phosphorus and sulphur 0.40 %?
No. The limits are 0.040 % maximum. A missing zero in a secondary table is an error.

Conclusion

JIS G 3454 STPG370 is carbon steel pressure pipe with a 370 MPa tensile minimum and 215 MPa yield. This page covers the seamless product and a common Schedule 40 size subset with formula-checked masses, not a stock list and not an ERW page. Confirm the process, the schedule and the certificate on the order.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X