JIS G 3101 SS540 Steel I-Beam

JIS G 3101 SS540 I-beam is named for a 540 N/mm2 tensile minimum, not a 540 N/mm2 yield. Yield is 400 N/mm2 up to 16 mm; mechanicals stop at 40 mm. All 20 JIS G 3192 Table 11 I-sections have flanges at or under 35 mm, inside that cap. SHH STEEL reviews grade and certificate before quoting.
Keywords
JIS G 3101 SS540 I-Beam, SS540 I-beam, JIS G 3192 Table 11, SS540 steel I-section, I-600x190x16x35
Equivalent Grades:
Near-equivalents only, not automatic substitutes.
Share:
General Description
Material Specification
Available Sizes of JIS G 3101 SS540 Steel I-Beam
Chemical Composition
Mechanical Properties
Applications
Equivalent Grades
Sourcing
FAQ
Conclusion

What is a JIS G 3101 SS540 Steel I-Beam?

A JIS G 3101 SS540 I-beam is a general-structure rolled I-section whose material conforms to JIS G 3101 and whose standard sizes follow JIS G 3192 Table 11. The grade is named for a 540 N/mm2 tensile minimum, not for a 540 N/mm2 yield. Yield is 400 N/mm2 up to 16 mm and 390 N/mm2 between 16 mm and 40 mm, based on flange thickness. Mechanical properties stop at 40 mm. This page is SS540 only, and only the I-section. It is not the SS400 or SS490 I-beam, and not the SS540 H-beam.

Material, Dimensions and Tolerances for JIS G 3101 SS540 I-Sections

JIS G 3101 is the material standard. JIS G 3192 Table 11 is the I-section series used here, not Table 15 H-sections. The 40 mm mechanical cap is part of the grade, not a rolling limit invented for this page. The largest flange thickness in the 20 typographical Table 11 rows is 35 mm on I-600x190x16x35, so every row in that table sits inside the cap. The editions named on the order govern acceptance.

JIS G 3101 SS540 I-Beam Sizes: JIS G 3192 Table 11

The table lists the same 20 typographical I-sections already verified on the SS400 I-beam page, from I-100x75x5x8 to I-600x190x16x35. It is not a mill rolling list and not an H-beam table. Because the maximum tabulated flange is 35 mm, the SS540 40 mm mechanical limit covers this series. A thicker special I-section would have to be agreed separately; it is not implied here.

Swipe horizontally to view all dimensions.

Designation H (mm) B (mm) t1 (mm) t2 (mm) r1 (mm) r2 (mm) A (cm²) Mass (kg/m)
I-100×75×5×8 100 75 5 8 7 3.5 16.43 12.9
I-125×75×5.5×9.5 125 75 5.5 9.5 9 4.5 20.45 16.1
I-150×75×5.5×9.5 150 75 5.5 9.5 9 4.5 21.83 17.1
I-150×125×8.5×14 150 125 8.5 14 13 6.5 46.15 36.2
I-180×100×6×10 180 100 6 10 10 5 30.06 23.6
I-200×100×7×10 200 100 7 10 10 5 33.06 26.0
I-200×150×9×16 200 150 9 16 15 7.5 64.16 50.4
I-250×125×7.5×12.5 250 125 7.5 12.5 12 6 48.79 38.3
I-250×125×10×19 250 125 10 19 21 10.5 70.73 55.5
I-300×150×8×13 300 150 8 13 12 6 61.58 48.3
I-300×150×10×18.5 300 150 10 18.5 19 9.5 83.47 65.5
I-300×150×11.5×22 300 150 11.5 22 23 11.5 97.88 76.8
I-350×150×9×15 350 150 9 15 13 6.5 74.58 58.5
I-350×150×12×24 350 150 12 24 25 12.5 111.1 87.2
I-400×150×10×18 400 150 10 18 17 8.5 91.73 72.0
I-400×150×12.5×25 400 150 12.5 25 27 13.5 122.1 95.8
I-450×175×11×20 450 175 11 20 19 9.5 116.8 91.7
I-450×175×13×26 450 175 13 26 27 13.5 146.1 115
I-600×190×13×25 600 190 13 25 25 12.5 169.4 133
I-600×190×16×35 600 190 16 35 38 19 224.5 176

JIS G 3101 SS540 Chemical Composition (Heat Analysis)

SS540 heat analysis is carbon 0.30 % maximum, manganese 1.60 % maximum, phosphorus 0.040 % maximum and sulphur 0.040 % maximum. Unlike SS400 and SS490, carbon and manganese are specified for this grade. Do not drop those limits when copying a table from a lower-tensile sister page.

Swipe horizontally to view all dimensions.

Element SS540 ladle analysis, Table 2 (mass %)
Carbon, max 0.30
Manganese, max 1.60
Phosphorus, max 0.040
Sulphur, max 0.040

JIS G 3101 SS540 Mechanical Properties: Yield, Tensile, Elongation and Bend

Minimum yield is 400 N/mm2 up to 16 mm and 390 N/mm2 from 16 mm to 40 mm. Tensile strength is 540 N/mm2 minimum, with no tabulated maximum. Elongation and the 180-degree bend follow Table 3 as shown, and they stop at 40 mm with the rest of the mechanical table. JIS G 3101 does not specify a Charpy test for SS540.

Swipe horizontally to view all dimensions.

Property Table 3 requirement for SS540 sections
Minimum yield, t <= 16 mm 400 N/mm2
Minimum yield, 16 mm < t <= 40 mm 390 N/mm2
Tensile strength 540 N/mm2 minimum (no tabulated maximum)
Elongation, t <= 5 mm 16% min, test piece No. 5
Elongation, 5 mm < t <= 16 mm 13% min, test piece No. 1A
Elongation, 16 mm < t <= 40 mm 17% min, test piece No. 1A
Bend 180 degrees, inner radius 2.0 x thickness, test piece No. 1 (No. 3 may be used at 5 mm and under)

Applications and Service Limits for JIS G 3101 SS540 Steel I-Beams

SS540 I-sections are used in general building and fabrication where this tensile class is specified in an I-beam and the flange is within 40 mm. The grade is not a weathering grade, not a pressure-vessel material, and not an SM welded-structure grade. If a Charpy value or a flange over 40 mm is needed, that has to be a different enquiry.

Near-Equivalents for JIS G 3101 SS540 Steel I-Beams: Not Automatic Substitutes

SS400 and SS490 are lower-tensile grades in the same standard; SS490 also has no carbon or manganese cap. SM490 is JIS G 3106. S355JR and Q355B I-beams use different shape systems. An SS540 H-beam is the same grade in a different series and stays on its own page.

Sourcing JIS G 3101 SS540 Steel I-Beams from SHH STEEL

Send the Table 11 designation, the length, and the JIS G 3101 edition, and name SS540 explicitly. Do not use the SS400 I-beam term or the SS540 H-beam term for this page. SHH STEEL reviews the grade, the flange thickness and the certificate before quoting. The size table is a typographical reference, not a warehouse list.

JIS G 3101 SS540 I-Beam FAQs

Do mechanical properties apply above 40 mm?
No. SS540 mechanicals stop at 40 mm flange thickness. The typographical Table 11 series used here has a maximum flange of 35 mm, so those 20 rows sit inside the cap.
Is the yield 540 N/mm2?
No. 540 N/mm2 is the tensile minimum, with no tabulated maximum. Yield is 400 N/mm2 up to 16 mm and 390 N/mm2 from 16 mm to 40 mm.
Does SS540 specify carbon?
Yes. Carbon is 0.30 % maximum and manganese is 1.60 % maximum, with phosphorus and sulphur 0.040 % maximum. That is different from SS400 and SS490.
Is this the SS540 H-beam page?
No. This page is the I-section to Table 11. H-sections use Table 15 and stay on the H-beam page.

Conclusion

JIS G 3101 SS540 I-beams use the 20 typographical Table 11 I-sections, with a 540 N/mm2 tensile minimum and a 400 N/mm2 yield up to 16 mm. Mechanicals stop at 40 mm; the tabulated flanges in this series do not exceed 35 mm. Confirm the designation, the grade and the certificate on the order.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X