JIS G 3101 SS400 Steel I-Beam
What is a JIS G 3101 SS400 Steel I-Beam?
JIS G 3101 SS400 steel I-beam is a hot-rolled taper-flange I-section in rolled steel for general structure. The material standard is JIS G 3101; this page uses the 2024 edition for chemistry and tensile values, and the edition named on the order governs acceptance. Dimensions, mass and tolerances for the section itself are those of JIS G 3192:2024 Table 11. The “400” in the grade name is the lower end of the specified tensile range, 400–510 N/mm². It is not a 400 N/mm² yield. Up to 16 mm at the test-piece location, the minimum yield point or proof stress is 245 N/mm²; it steps down as that thickness increases.
This page is the I-beam. The same grade as a rolled H-section is a separate listing, JIS G 3101 SS400 H-Beam, and the plate form is a plate data sheet. Do not use either of those pages as an I-beam table, and do not treat an IPE, an IPN or a GB/T 706 I-beam of similar depth as a JIS I-section.
SS400 I-beams are used in general industrial framing, light building work and duties such as crane-runway members where a taper-flange I-section is still specified. JIS G 3101 does not specify a Charpy test for SS400. The grade is not a pressure-vessel material, and it is not a substitute for JIS G 3106 SM490 when a welded-structure grade and a defined impact quality are what the order requires.
Material, Dimensions and Tolerances for JIS G 3101 SS400 I-Sections
The order and the inspection certificate should keep material, dimensions and tolerances distinct:
- JIS G 3101 is the material standard. Heat-analysis and tensile values on this page are those for SS400 sections in JIS G 3101:2024.
- JIS G 3192 is the dimensional standard for hot-rolled sections. The size table lists the 20 standard I-sections in Table 11, with designation dimensions, radii, area and theoretical mass. Those rows are reference dimensions, not a mill rolling list.
A documented special combination — for example SS400 on an IPE, or a JIS I-section certified to a different material standard — is only valid if every requirement of each named standard is met. Matching a nominal 200 mm or 8 in depth is not a substitution.
JIS G 3101 SS400 I-Beam Sizes: JIS G 3192 Table 11
The table lists all 20 standard I-sections in JIS G 3192:2024 Table 11, from I-100×75×5×8 to I-600×190×16×35. Columns are the published designation dimensions: height H, flange width B, web thickness t1, flange thickness t2 (taken at B/4), root radii r1 and r2, cross-sectional area and theoretical mass. These are representative (standard) dimensions. JIS G 3192 allows other sections by agreement; those extra sizes are not invented here. The rows are a dimensional reference, not a rolling programme and not a claim that every size is produced in SS400.
An I-section in this table is not a JIS G 3192 Table 15 H-section of the same nominal depth, and it is not an IPE, IPN or GB/T 706 I-beam. The inner flange surfaces are tapered; that is the usual distinction from a parallel-flange H-beam. Section moduli and moments of inertia are omitted because a second engineering table disagrees with the official scan on some of those reference properties, and those values are not invented here.
Theoretical mass is the tabulated reference value. Settlement should follow the contract and, when the purchaser requires a mass check, the mass tolerances of JIS G 3192 Table 7. Dimensional acceptance follows Table 3 of the ordered JIS G 3192 edition, not ASTM A6/A6M or EN 10034.
JIS G 3192 Table 11 I-sections (20 sizes)
Swipe horizontally to view all dimensions.
| Designation | H (mm) | B (mm) | t1 (mm) | t2 (mm) | r1 (mm) | r2 (mm) | A (cm²) | Mass (kg/m) |
|---|---|---|---|---|---|---|---|---|
| I-100×75×5×8 | 100 | 75 | 5 | 8 | 7 | 3.5 | 16.43 | 12.9 |
| I-125×75×5.5×9.5 | 125 | 75 | 5.5 | 9.5 | 9 | 4.5 | 20.45 | 16.1 |
| I-150×75×5.5×9.5 | 150 | 75 | 5.5 | 9.5 | 9 | 4.5 | 21.83 | 17.1 |
| I-150×125×8.5×14 | 150 | 125 | 8.5 | 14 | 13 | 6.5 | 46.15 | 36.2 |
| I-180×100×6×10 | 180 | 100 | 6 | 10 | 10 | 5 | 30.06 | 23.6 |
| I-200×100×7×10 | 200 | 100 | 7 | 10 | 10 | 5 | 33.06 | 26.0 |
| I-200×150×9×16 | 200 | 150 | 9 | 16 | 15 | 7.5 | 64.16 | 50.4 |
| I-250×125×7.5×12.5 | 250 | 125 | 7.5 | 12.5 | 12 | 6 | 48.79 | 38.3 |
| I-250×125×10×19 | 250 | 125 | 10 | 19 | 21 | 10.5 | 70.73 | 55.5 |
| I-300×150×8×13 | 300 | 150 | 8 | 13 | 12 | 6 | 61.58 | 48.3 |
| I-300×150×10×18.5 | 300 | 150 | 10 | 18.5 | 19 | 9.5 | 83.47 | 65.5 |
| I-300×150×11.5×22 | 300 | 150 | 11.5 | 22 | 23 | 11.5 | 97.88 | 76.8 |
| I-350×150×9×15 | 350 | 150 | 9 | 15 | 13 | 6.5 | 74.58 | 58.5 |
| I-350×150×12×24 | 350 | 150 | 12 | 24 | 25 | 12.5 | 111.1 | 87.2 |
| I-400×150×10×18 | 400 | 150 | 10 | 18 | 17 | 8.5 | 91.73 | 72.0 |
| I-400×150×12.5×25 | 400 | 150 | 12.5 | 25 | 27 | 13.5 | 122.1 | 95.8 |
| I-450×175×11×20 | 450 | 175 | 11 | 20 | 19 | 9.5 | 116.8 | 91.7 |
| I-450×175×13×26 | 450 | 175 | 13 | 26 | 27 | 13.5 | 146.1 | 115 |
| I-600×190×13×25 | 600 | 190 | 13 | 25 | 25 | 12.5 | 169.4 | 133 |
| I-600×190×16×35 | 600 | 190 | 16 | 35 | 38 | 19 | 224.5 | 176 |
JIS G 3101 SS400 Chemical Composition (Heat Analysis)
The figures below are heat-analysis limits for SS400 in JIS G 3101:2024. They should not be copied from SS540, which does have carbon and manganese maxima, or from a Chinese or European 235 MPa table that publishes carbon and manganese limits SS400 does not. They are limits, not typical heat results.
JIS G 3101 SS400 Mechanical Properties: Yield, Tensile, Elongation and Bend
Tensile properties of SS400 sections follow Table 3 of JIS G 3101:2024 (plates, strips, flats and sections). Thickness is that at the test-piece location. Unless otherwise specified, the yield value is the upper yield point (ReH); if no yield point appears, 0.2% proof stress (Rp0.2) is determined. Annex JA, which applies to sections with a leg length under 40 mm, is not used for the standard I-sections in the size table above, whose flange widths are 75 mm or more.
Elongation uses the test pieces named in the same table. For No. 4 test pieces on plates thicker than 90 mm, the standard reduces the tabulated elongation by 1 for each 25 mm or fraction of thickness, with a maximum reduction of 3; that reduction is a plate rule and is not extended here to invent a section value.
The specified bend is 180° with an inner radius of 1.5 times the thickness, using a No. 1 test piece (a No. 3 piece may be used at 5 mm and under). The bend test may be omitted unless the purchaser specifies it, but the steel still has to satisfy the bendability requirement. JIS G 3101 does not specify a Charpy test for SS400; a toughness value must not be inferred from the grade name. If the specification needs a defined impact test, a JIS G 3106 quality such as SM490B or SM490C, or another standard that actually tables that test, should be nominated.
Delivery, Inspection and Identification of JIS G 3101 SS400 I-Beams
SS400 I-beams are delivered as hot-rolled sections unless a further treatment is ordered. The mill certificate should name JIS G 3101, the edition, grade SS400, and the JIS G 3192 I-section designation (H×B×t1×t2), so the beam can be traced to both the material and the dimensional standard. A certificate that only says “SS400” or only “I-beam”, without the section designation, is not complete identification.
The default inspection document, if not otherwise specified, is a JIS G 0415 inspection certificate 3.1 in the 2024 revision of G 3101. Do not infer a Charpy result from the grade name; if toughness has to be demonstrated, write the test on the order or nominate a standard that actually tables it.
Weldability and Surface Condition of JIS G 3101 SS400 I-Beams
SS400 is a general-structure carbon steel and is routinely welded, provided the procedure matches the flange and web thickness and any coating. Because the standard does not table a carbon maximum, the actual heat analysis on the certificate is the right input to a welding procedure, not a borrowed CEV from S235JR or Q235B. The as-rolled surface, including mill scale on the tapered inner flanges, is part of the product unless the order requires a prepared finish.
JIS G 3192 Shape Tolerances and Theoretical Mass for JIS G 3101 SS400 I-Beams
Height, flange width, thickness, length, out-of-square and straightness are accepted to JIS G 3192 Table 3, which covers I-sections together with angles, channels, bulb flats and T-sections. Those limits are not the H-section rules in the same standard’s later tables, and they are not EN 10034 or ASTM A6/A6M. Root radii in Table 11 are representative dimensions used to calculate area and mass; JIS G 3192 does not put a separate tolerance on those radii.
When the purchaser requires a mass check, Table 7 applies to a lot of the same size (1 t or more, or at least 10 bars if the lot is lighter): ±5 % when the thicker of t1 and t2 is under 10 mm, and ±4 % at 10 mm and above. Theoretical masses in the table are the published three-significant-figure values, not a weighed-mass guarantee.
Applications and Service Limits for JIS G 3101 SS400 Steel I-Beams
SS400 I-beams are used where a Japanese general-structure grade and a taper-flange I-section are what the drawing calls for — light frames, platforms, machinery supports and some crane-runway members. In current building practice the parallel-flange H-section has taken much of that work; this page does not treat the H-beam as a silent replacement, or the I-beam as a silent replacement for the H-beam.
The thickest flange in the standard Table 11 series is 35 mm (I-600×190×16×35), which falls in the 16 mm to 40 mm yield band (235 N/mm²). The 40 mm and 100 mm yield steps in G 3101 are not used by these standard I-sections. SS400 remains without a specified Charpy test.
JIS G 3101 SS400 I-Beams Compared with SS400 H-Beams, IPE and GB/T 706
The SS400 H-beam listing uses the same material standard and a different JIS G 3192 table (Table 15). An I-300×150 is not an H 300×150. SS490 and SS540 are higher tensile grades in JIS G 3101, with their own chemistry and yield tables; they are not automatic upgrades of an SS400 I-beam certificate. JIS G 3106 SM490 is a welded-structure grade and is not SS400 under another name.
IPE and IPN (EN 10365, material usually EN 10025-2) and GB/T 706 I-beams are different dimensional series. A similar nominal depth does not make them interchangeable with a JIS Table 11 I-section, in geometry or in the material certificate.
Near-Equivalents for JIS G 3101 SS400 Steel I-Beams: Not Automatic Substitutes
Engineers sometimes place SS400 next to Q235B or S235JR because the tensile and thinner-section yield bands sit in a similar neighbourhood. Those comparisons are a starting point for a substitution study, not a licence to restamp the beam. SS400 has no tabulated carbon or manganese maximum, no default impact test, and a different elongation-and-bend package. Any substitution has to be accepted by the purchaser against the editions named on the order.
Sourcing JIS G 3101 SS400 Steel I-Beams from SHH STEEL
SHH STEEL reviews enquiries for JIS G 3101 SS400 I-beams against the grade, the JIS G 3192 Table 11 designation, and the certificate that will accompany the sections. The 20-row table is a standard-section reference, not a catalogue of guaranteed mill items. Lengths and any additional tests should be written on the enquiry so they can be checked before a quotation is prepared.
JIS G 3101 SS400 I-Beam FAQs
-
Is a JIS SS400 I-beam the same as an SS400 H-beam?
- No. Both can be certified to JIS G 3101 SS400, but they are different JIS G 3192 series. Table 11 I-sections have tapered inner flange surfaces. Table 15 H-sections are parallel-flange. An I-300×150 is not an H 300×150.
-
Does “SS400” mean a 400 N/mm² yield?
- No. The 400 in the grade name is the lower end of the 400–510 N/mm² tensile range. The minimum yield is 245 N/mm² up to 16 mm at the test-piece location, and 235 N/mm² from 16 mm to 40 mm.
-
How many standard I-beam sizes does JIS G 3192 Table 11 list?
- Twenty, from I-100×75×5×8 to I-600×190×16×35. Other dimensions may be agreed, but they are not tabulated on this page.
-
Can an IPE or a GB/T 706 I-beam be used as a JIS SS400 I-beam?
- Not as an automatic substitute. Those are different dimensional standards and usually different material standards. A similar nominal depth is not a substitution.
-
Does SS400 include a Charpy test?
- No. JIS G 3101 does not specify a Charpy test for SS400. If toughness has to be demonstrated, the test must be written on the order, or a standard that actually tables it — such as a JIS G 3106 quality — should be nominated.
Conclusion
JIS G 3101 SS400 steel I-beam is a general-structure taper-flange I-section whose “400” is a tensile minimum, not a yield. The size table lists the 20 standard sections in JIS G 3192:2024 Table 11, from I-100×75×5×8 to I-600×190×16×35, as a dimensional reference and not as a stock list. Confirm the grade, the Table 11 designation and the certificate before the beams are released to the job, and do not treat the SS400 H-beam listing as the same product.