ISO 630-1 Structural Steel Plate | Hot-Rolled General Technical Delivery Conditions | ISO 630-1 Structural Steel - SHH STEEL

ISO 630-1 Structural Steel Plate | Hot-Rolled General Technical Delivery Conditions

ISO 630-1 steel plate is supplied under ISO 630-1:2021 (Edition 2), the international standard that specifies the general technical delivery conditions for hot-rolled steel flat and long products (plates, sections, wide flats and bars) used principally for general-purpose structural steels and intended for use in welded or bolted structures. ISO 630-1 is not itself a steel-grade specification and does not tabulate grade chemistry or tensile values. The specific requirements for structural steels are given in the individual parts of ISO 630, for example ISO 630-2 for general-purpose grades and ISO 630-5 for steels with improved atmospheric corrosion resistance. Continuous-mill sheet and strip, and tubular products, are outside the Scope. This page is written to ISO 630-1:2021; confirm that this is the edition on the order. Clauses 8.3, 9 and 10, Table 1 and Annex A were not in the portion of the document inspected for this page; confirm those against the official text.
Standard
ISO 630-1:2021 (Edition 2)
Role
General technical delivery conditions (not a steel grade)
Product forms (Scope)
Plates, sections, wide flats and bars
Grade requirements
In the individual parts of ISO 630
CEV (clause 6.3.3)
IIW Formula (1); Pcm Formula (2) by agreement
Nominal density (clause 6.7.2)
7 850 kg/m³
Inspection (clause 7.1)
Specific or non-specific (ISO 404); document type per ISO 10474
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why choose Us
Our Service
FAQ
Conclusion

General Description of ISO 630-1 Structural Steel Plate

ISO 630-1 steel plate is supplied under ISO 630-1:2021 (Edition 2), the international standard that specifies the general technical delivery conditions for hot-rolled steel flat and long products (plates, sections, wide flats and bars) used principally for general-purpose structural steels and intended for use in welded or bolted structures. ISO 630-1 is not itself a steel-grade specification and does not tabulate grade chemistry or tensile values. The specific requirements for structural steels are given in the individual parts of ISO 630, for example ISO 630-2 for general-purpose grades and ISO 630-5 for steels with improved atmospheric corrosion resistance. Continuous-mill sheet and strip, and tubular products, are outside the Scope. This page is written to ISO 630-1:2021; confirm that this is the edition on the order. Clauses 8.3, 9 and 10, Table 1 and Annex A were not in the portion of the document inspected for this page; confirm those against the official text.

Part 1 is the general technical delivery conditions for the ISO 630 series. It is not the part that specifies weldable fine-grain structural steels (that is ISO 630-3), quenched and tempered high yield strength plates (ISO 630-4), or seismic-improved structural steels (ISO 630-6). This page does not treat E295 or E355, or any other commercial grade name, as an ISO 630-1 grade. General technical delivery conditions on this page are those of ISO 630-1:2021; grade requirements are taken from the relevant part stated on the order. Confirm the official texts of both ISO 630-1 and that part.

ISO 630-1 Structural Steel Plate Material Specification

As of 12 November 2026, ISO 630-1:2021 (Edition 2, April 2021) remains published. It cancels and replaces the first edition (ISO 630-1:2011), which was technically revised, and is the edition used on this page. A systematic review of the 2021 edition closed on 3 September 2026; this page does not treat that close as a withdrawal, as a confirmation step that changes the text, or as the publication of a replacement edition. Buyers should confirm that ISO 630-1:2021 is the edition stated on the order. This page does not tabulate any later edition.

ISO 630-1 Structural Steel Plate is described by ISO 630-1:2021, whose title is “Structural steels — Part 1: General technical delivery conditions for hot-rolled products.” The Scope covers steel flat and long products (plates, sections, wide flats and bars) used principally for general-purpose structural steels, intended for use in welded or bolted structures. The specific requirements for structural steels are given in the individual parts of ISO 630. Sheet and strip (ISO/TC 17/SC 12) and tubular products (ISO/TC 5/SC 1) are outside the document. In every part of ISO 630, “thickness” means nominal thickness unless otherwise stated.

The normative references of ISO 630-1:2021 include the other parts of the series then published: ISO 630-2 (structural steels for general purposes), ISO 630-3 (fine-grain structural steels), ISO 630-4 (high yield strength quenched and tempered structural steel plates), ISO 630-5 (structural steels with improved atmospheric corrosion resistance) and ISO 630-6 (seismic-improved structural steels for building). ISO 630-3, ISO 630-4 and ISO 630-6 are named here and are not linked, because those product-family pages are not published on this site. This page does not treat those parts as interchangeable with each other or with Part 1.

Clause 4.1 states that classification of the steel grades in accordance with ISO 4948-1 and ISO 4948-2 is given in the individual parts, depending on the steel-grade chemical composition and treatment condition. Clause 4.2 designates the steels with steel names in accordance with ISO/TS 4949, and defines quality letters by impact-test temperature: quality A, no impact testing; B, 20 °C; C, 0 °C; D, −20 °C; E, −40 °C; L, −50 °C; F, −60 °C. Which of those qualities exists for a given grade is specified in the relevant part, not by Part 1 alone. Do not assume that every part uses every quality letter.

ISO 630-1 Structural Steel Plate Chemical Composition

ISO 630-1:2021 does not itself tabulate a grade-by-grade chemical composition. Clause 6.3.1 requires the heat analysis reported by the steel producer to comply with the requirements of the individual parts of ISO 630 and to be included in the relevant inspection document. If CEV or Pcm is applied, the heat analyses of all elements needed to calculate CEV and Pcm shall be reported.

Clause 6.3.2: product analysis shall be carried out when agreed and specified at enquiry and order. The permissible product-analysis tolerances on the heat-analysis limiting values are specified in the individual parts of ISO 630, not in Part 1 itself.

Clause 6.3.3 requires the carbon equivalent value (CEV) to be determined with the following IIW (International Institute for Welding) Formula (1), which was clearly legible in the inspected text:

CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15

A note to clause 6.3.3 allows other formulae for CEV, and the weld-crack sensitivity composition (Pcm), if agreed at enquiry and order (option 5.2 d). The following Formula (2) for Pcm, which was also clearly legible, is given:

Pcm = C + Si/30 + Mn/20 + Cu/20 + Ni/60 + Cr/20 + Mo/15 + V/10 + 5B

Those formulae are as published in clause 6.3.3. Confirm the official symbols, grouping and coefficients against the official text before use on an order. A listed CEV formula is not a welding procedure. Grade maxima for CEV, where they exist, are specified in the individual parts (for example Table A.3 of ISO 630-2) and are not restated as Part 1 limits on this page.

ISO 630-1 Structural Steel Plate Mechanical Properties

Clause 6.4.1 requires the mechanical properties, under the inspection and testing conditions of clauses 7, 8 and 9 and in the delivery condition specified in clause 6.2, to conform with the relevant requirements given in the individual parts of ISO 630. ISO 630-1 itself does not tabulate yield strength, tensile strength, elongation or impact energy. This page does not invent those figures and does not borrow them from a related European or other standard. Confirm the official tables of the part stated on the order.

Clause 6.4.2 (tensile properties) and clause 6.4.3 (Charpy V-notch impact properties) both refer those requirements to the individual parts. Clause 6.4.1 also requires agreement, where appropriate, at enquiry and order about the mechanical properties to be adhered to after additional heat treatment such as stress relief (option 5.2 e). Clause 6.4.4: by agreement, products of the grades and qualities specified in the individual parts shall comply with one of the improved deformation properties perpendicular to the product surface as specified in ISO 7778 (option 5.2 f, special classes for the reduction of area).

Clauses 8.3 and 9 (selection and preparation of samples and test pieces, and test methods) were not in the portion of ISO 630-1:2021 inspected for this page (the inspected text ends in clause 8.2). They are not restated here. Confirm those clauses, including any specimen orientation or temperature rules, against the official text and against the relevant part.

ISO 630-1 Structural Steel Plate Delivery Conditions

Clause 6.1.1: unless a special steelmaking process has been agreed at enquiry and order, the steelmaking process is at the manufacturer’s discretion. If a special steelmaking process has been specified, it shall be reported in the inspection document. Clause 6.1.2: the method of deoxidation shall be as given in the individual parts of ISO 630. Clause 6.2: the delivery conditions are given in the individual parts. Option 5.2 b allows a required delivery condition to be agreed, and is written as applicable for ISO 630-2 and ISO 630-5.

Clause 5.1 requires the purchaser, at enquiry and order, to supply: (a) the quantity; (b) the type of product; (c) the nominal dimensions and the tolerances on dimensions and shape; (d) the number of the relevant part of ISO 630; (e) the steel name (grade) or designation; (f) all required options (see 5.2); and (g) the inspection document to be issued (see 7.1). If the purchaser does not specify any of the clause 5.2 options at enquiry and order, the products shall be supplied in accordance with the basic specification (see 5.1).

The options listed in clause 5.2 are: (a) specification of the steelmaking process (6.1); (b) required delivery condition (6.2), applicable for ISO 630-2 and ISO 630-5; (c) product analysis (6.3.2); (d) alternative weldability formula (6.3.3); (e) mechanical properties after additional heat treatment (6.4.1); (f) special classes for the reduction of area (6.4.4); (g) a deviating surface-condition standard (6.5); (h) a deviating frequency of testing (8.2); (i) specification of an analytical method (9.1); (j) a deviating testing temperature for the impact test (9.3); (k) testing of impact properties in the transverse direction (9.3); (l) ultrasonic testing upon agreement with a referenced standard (9.5); (m) marking method (clause 10); (n) information to be given by marking (Table 1); and (o) suitability for hot-dip galvanizing upon agreement with a referenced standard, applicable for ISO 630-2, ISO 630-3, ISO 630-4 and ISO 630-6. Table 1 and clauses 9 and 10 were not in the inspected text and are not tabulated here; confirm those against the official document.

ISO 630-1 Structural Steel Plate Weldability

Weldability is supported by the CEV requirement of clause 6.3.3. The IIW Formula (1) given there is CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15. An agreed alternative formula, or the Pcm Formula (2), may be used under option 5.2 d. A listed formula is not a welding procedure, a preheat schedule or a qualified joint. The fabricator shall qualify welding to the project specification and to the official edition and part on the order. This page does not tabulate preheat, heat-input or hydrogen controls.

Grade CEV maxima, silicon-control options and copper options, where they exist, are specified in the individual parts and are not default Part 1 limits. For atmospheric-corrosion-resistant (weathering) structural steels, see ISO 630-5, not Part 1 alone. Option 5.2 o (suitability for hot-dip galvanizing, upon agreement with a referenced standard) is written as applicable for ISO 630-2, ISO 630-3, ISO 630-4 and ISO 630-6; it is an agreed option, not a default.

ISO 630-1 Structural Steel Plate Tolerances

Clause 6.5 requires the surface-condition requirements to be agreed at enquiry and order in accordance with ISO 7788 for plates and wide flats, ISO 20723 for sections, and ISO 9443 for bars (a deviating standard may be agreed under option 5.2 g). Clause 6.6: ultrasonic requirements, together with the conditions of their verification, shall be specified by agreement (see 9.5; clause 9.5 itself was not in the inspected text).

Clause 6.7.1 requires the nominal dimensions and the tolerances on dimensions and shape to be agreed at enquiry and order, with reference to: ISO 7452 for plates and ISO 9034 for wide flats; and, for hot-rolled long products, ISO 657-1, ISO 657-2, ISO 657-5, ISO 657-11, ISO 657-15, ISO 657-19 and ISO 657-21 for sections, or ISO 1035-1, ISO 1035-2, ISO 1035-3 and ISO 1035-4 for bars. A note to 6.7.1 allows the relevant standards shown in Annex A to be used by agreement. Annex A (informative) was not in the inspected portion of the document (Contents places it at document page 10) and is not tabulated here. Confirm Annex A against the official text if it is to be used.

Clause 6.7.2: a density of 7 850 kg/m³ shall be used as the basis for the calculation of the nominal mass from the nominal dimensions of all steels in the individual parts of ISO 630. Actual mass may be used by agreement.

ISO 630-1 Structural Steel Plate Applications and service limits

ISO 630-1:2021 applies to hot-rolled plates, sections, wide flats and bars used principally for general-purpose structural steels in welded or bolted structures, in the Scope of that document. It does not by itself assign a steel grade, a minimum design temperature, a pressure-equipment duty, a fire rating or a fatigue class. Selection of the ISO 630 part, the grade and quality, the thickness, the delivery condition and any agreed option is a design decision for the project engineer. Confirm fitness for the intended service against the official Part 1, the relevant part, the project specification and the quality document.

Clause 7.1 requires products to be delivered either with specific or non-specific inspection (see ISO 404) as specified in the individual parts of ISO 630, to confirm compliance with the order and with ISO 630-1. In the case of specific inspection, the purchaser shall state the required type of inspection document in accordance with ISO 10474. If the purchaser requires the presence of an authorized representative or an inspector designated by official regulations, the purchaser shall notify the manufacturer of the name and address of the organization or person who is to carry out the inspection and produce the inspection document.

Clause 7.2.1 requires the following tests, according to the individual parts, and reporting on the relevant inspection document: heat analysis; tensile test; impact test, if specified; visual examination of the surface condition; and dimensional inspection. Clause 7.2.2: if agreed at enquiry and order, product analysis and an ultrasonic test for internal soundness shall also be carried out and reported. Clause 7.3: retests shall be in accordance with ISO 404. Clause 8.1 requires samples and test pieces to be marked so that the product is traceable and the position of the samples in the product is unambiguously known. Clause 8.2.1: verification of the heat analysis shall be one per heat; for product analysis, if specified and unless otherwise agreed, one test piece per heat shall be taken to determine the elements indicated with numerical values for that steel grade in the relevant part. Verification of mechanical properties, the test unit, and the tests for specific inspection (8.2.2 and 8.2.3) shall be as specified in the individual parts.

Compare ISO 630-1 with the other ISO 630 parts

ISO 630-1 is the general technical delivery conditions for the series. It is not a substitute for the grade requirements of any other part, and the parts are not interchangeable with each other on the basis of a similar name.

  • ISO 630-2 specifies technical delivery conditions for structural steels for general purposes (Annex A grades such as S235, S275 and S355 in the qualities listed in that part). Those grade pages are not yet published on this site and are named, not linked. Grade chemistry, CEV maxima and mechanical tables are in Part 2, not in Part 1.
  • ISO 630-5 specifies technical delivery conditions for structural steels with improved atmospheric corrosion resistance, including ISO 630-5 S235W, ISO 630-5 S355W and ISO 630-5 S355WP. Those are Part 5 designations, not Part 1 grades.
  • ISO 630-3 (fine-grain structural steels), ISO 630-4 (high yield strength quenched and tempered structural steel plates) and ISO 630-6 (seismic-improved structural steels for building) are other parts named in the normative references of ISO 630-1:2021. Their product-family pages are not published on this site and are not linked. They are not substitutes for Part 1 or for Part 2.

This page does not treat EN 10025-2 designations (including E295 and E355), or any other foreign standard, as ISO 630-1 grades or as automatic equivalents of a Part 1 delivery. Official correspondence tables were not inspected. Engineer approval is required before any substitution. The four ISO 630-2 Annex B grades SG205, SG250, SG285 and SG345 are not tabulated here; their Annex B tables were not in the portion of ISO 630-2 inspected for those pages, and those product pages are held.

ISO 630-1 Structural Steel Plate Equivalent Material Grade

The heading identifies a comparison topic, not a declaration of interchangeable material. ISO 630-1 is a general technical delivery condition, not a steel grade, and no automatic foreign equivalent or dual certification is offered for a “Part 1 grade.” A similar product-form description, or a similar number in another standard, is not interchangeability.

Standard Country-Region Equivalent Grade Note
ISO 630-1:2021 International (ISO) ISO 630-1 (this page) General technical delivery conditions for hot-rolled structural flat and long products. Not a steel grade. Not interchangeable with any individual part of ISO 630.
ISO 630-2 International (ISO) S235, S275, S355 (Part 2 Annex A) Related part: general-purpose structural steels. Grade requirements are in ISO 630-2, not in Part 1. Those product pages are not yet published and are named, not linked. Not a Part 1 grade and not an automatic equivalent.
ISO 630-5 International (ISO) S235W, S355W, S355WP Related part: structural steels with improved atmospheric corrosion resistance. These are Part 5 designations, not Part 1 grades. Not automatic equivalents of a Part 1 delivery. Engineer approval is required before any substitution.

None of those relationships is interchangeability. Confirm every requirement against the official text of each standard named on the order, and obtain engineer approval before any substitution.

Why choose Us

SHH STEEL produces and exports structural plate to the ISO 630 series, including supply under ISO 630-1 Structural Steel Plate. We review the ordered edition of ISO 630-1, the relevant part, the steel name and quality, thickness, delivery condition, inspection-document type and agreed options before production, and we state the actual results on the inspection document. We do not treat ISO 630-1 as a grade designation, and we do not treat a related EN 10025-2 name (including E295 or E355) as an ISO 630-1 grade.

Orders are accepted against ISO 630-1:2021 and the relevant part unless the order states a different edition. Enquiry details should include the mandatory information of clause 5.1 and any clause 5.2 options required. See the ISO 630-1 hub for the product family, and the ISO 630-2 and ISO 630-5 hubs for the grade parts.

Our Service

Supply covers production to the ordered ISO 630-1:2021 general technical delivery conditions together with the relevant part of ISO 630, mill documentation, and export packing and shipment. Inspection documents record the actual heat analysis, the delivery condition, and the mechanical results required by the official tables of the part and edition on the order. Agreed options are supplied when they are stated on the order, not by default.

To enquire, state ISO 630-1:2021, the relevant part of ISO 630, the steel name and quality, dimensions, quantity, the inspection-document type and any required options. SHH STEEL will confirm manufacturability and the inspection plan against that order. This page is a product description written to ISO 630-1:2021; the official standard of the edition on the order, the relevant part, and the inspection document, govern acceptance.

FAQ

What is ISO 630-1 steel plate?

ISO 630-1 Structural Steel Plate is plate supplied under the general technical delivery conditions of ISO 630-1:2021 for hot-rolled structural flat and long products. ISO 630-1 is not itself a steel grade and does not tabulate grade chemistry or tensile values. The specific grade requirements are given in the individual parts of ISO 630, which shall be stated on the order together with the steel name.

Is ISO 630-1:2021 the current edition?

Yes, as of 12 November 2026. ISO 630-1:2021 (Edition 2, April 2021) remains published and is the edition used on this page. It cancels and replaces ISO 630-1:2011, which was technically revised. A systematic review closed on 3 September 2026; this page does not treat that close as a withdrawal or as the publication of a replacement edition. State ISO 630-1:2021, together with the relevant part of ISO 630 and the steel name, on the order, and confirm that this is the edition that applies. This page does not tabulate any later edition.

Does ISO 630-1 specify grades such as E295, E355 or S355?

No. ISO 630-1:2021 is a general technical delivery condition. It does not tabulate those grade names as Part 1 designations. E295 and E355 are not treated on this page as ISO 630-1 grades. S355 and the other general-purpose grades are specified in ISO 630-2, and weathering grades such as ISO 630-5 S355W are specified in ISO 630-5. State the relevant part and the steel name on the order. Official correspondence with other standards was not inspected. Engineer approval is required before any substitution.

What information must be supplied on an ISO 630-1 order?

Clause 5.1 requires the purchaser to supply, at enquiry and order: the quantity; the type of product; the nominal dimensions and the tolerances on dimensions and shape; the number of the relevant part of ISO 630; the steel name (grade) or designation; all required options (clause 5.2); and the inspection document to be issued (clause 7.1). If no clause 5.2 option is specified, the products are supplied to the basic specification. Confirm the official wording of clauses 5.1 and 5.2 against ISO 630-1:2021.

How should ISO 630-1 steel plate be ordered?

State ISO 630-1:2021, the relevant part of ISO 630, the steel name and quality, the product form and dimensions, the quantity, and the type of inspection document (specific or non-specific, with the ISO 10474 type if specific inspection is required). State any required option (delivery condition, product analysis, alternative weldability formula, transverse impact test, ultrasonic test, special steelmaking, or other clause 5.2 options). The official texts of ISO 630-1 and of the relevant part govern acceptance.

Enquire about ISO 630-1 Structural Steel Plate

Enquire for ISO 630-1 Structural Steel Plate to ISO 630-1:2021. State the relevant part of ISO 630, the steel name and quality, the dimensions, the quantity, the delivery condition if a particular condition is required, the inspection-document type and any agreed options. SHH STEEL will confirm the inspection plan against the official tables of the edition and part on the order. The official standard and the inspection document govern acceptance.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X