GB/T 1591 Q355B Round, Square and Flat Steel Bars

GB/T 1591-2018 Q355B bars follow as-rolled quality B chemistry and the thickness-dependent yield, tensile and elongation bands in GB/T 1591 Tables 7, 8 and 11. For sections and bars, phosphorus and sulfur may be raised to 0.040 %. These bars are not GB/T 6728 hollow sections and not GB/T 706 Q355B angles. Size tables are typographical sizes, not a warehouse list.
Keywords
GB/T 1591 Q355B bars, Q355B round steel bar, Q355B flat bar, GB/T 1591-2018 quality B bars, Q355B square bar
Equivalent Grades:
Near-equivalents only, not automatic substitutes.
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Size Chart
Applications
Comparison
Equivalent Grades
Sourcing
FAQ
Conclusion

What are GB/T 1591 Q355B Round, Square and Flat Steel Bars?

GB/T 1591-2018 Q355B is a high-strength low-alloy structural steel, quality B, used here for as-rolled round, square and flat bars. Chemistry, CEV and the thickness-dependent yield, tensile and elongation bands follow GB/T 1591-2018 Tables 2, 7, 8 and 11 as already used on this site for Q355B hollow-section material. The edition named on the purchase order governs delivery.

These bars are not GB/T 1591 Q355B Steel Hollow Sections (GB/T 6728-2025). That page is a GB/T 6728-2025 hollow section with a GB/T 1591 Q355B material grade. They are also not GB/T 706 Q355B Equal and Unequal Steel Angles, which is a GB/T 706 angle. A hollow-section or angle certificate is not a bar certificate.

Material and Scope for GB/T 1591-2018 Q355B Bars

The material standard is GB/T 1591-2018, quality B, as-rolled. This page uses the section-and-bar footnotes in that standard: phosphorus and sulfur may be raised by 0.005 % to 0.040 %, and the maximum CEV for sections and bars may be 0.54 % in the thicker band where that footnote applies. Do not apply the GB/T 6728-2025 Table 25 hollow-section class 355 tensile band (470–680 MPa) to these bars; bar mechanicals follow GB/T 1591 Tables 7, 8 and 11, including the 470–630 MPa tensile band used here.

GB/T 1591 Q355B Chemical Composition and CEV (As-Rolled, Heat Analysis)

The tables list the as-rolled Q355B heat-analysis limits and CEV bands used on this site, with the section-and-bar footnotes called out for phosphorus, sulfur and CEV.

Swipe horizontally to view all dimensions.

Element Heat-analysis limit (mass %) Notes for as-rolled Q355B bars
C, max 0.24 For t > 30 mm, C ≤ 0.22 %. For sections with t > 100 mm, carbon may be agreed.
Si, max 0.55 See the controlled-silicon CEV note in GB/T 1591.
Mn, max 1.60 —
P, max 0.035 For sections and bars, P and S may be raised by 0.005 % to 0.040 %.
S, max 0.035 Same section and bar footnote as phosphorus.
Nb, V, Ti Dash (no specified requirement) Not a mandated microalloy addition for as-rolled Q355B.
Cr, max 0.30 —
Ni, max 0.30 —
Cu, max 0.40 —
N, max 0.012 An Als/Alt or other nitrogen-binding waiver may apply as in GB/T 1591.

Swipe horizontally to view all dimensions.

Nominal thickness (mm) Maximum CEV (%) for Q355 B/C/D Notes
≤ 30 0.45 Applies to most common bar sizes on this page.
> 30–63 0.47 —
> 63–150 0.47 —
> 150–250 0.49 For sections and bars the maximum CEV may be 0.54 %.
> 250–400 Dash for quality B and C 0.49 is tabulated only for quality D plate, which is not this product.

GB/T 1591-2018 Q355B Bar Mechanical Properties (Tables 7, 8 and 11)

Yield, tensile and elongation depend on nominal thickness. For quality B, minimum yield is 355 MPa at t ≤ 16 mm and then steps down through the Table 7 bands shown below. Tensile strength in the Table 8 band used here is 470–630 MPa through 100 mm, with longitudinal elongation 22 %, 21 % and 20 % in the three thickness rows tabulated. Do not use a single 355 MPa yield for every bar thickness, and do not use the GB/T 6728 Table 25 470–680 MPa class 355 tensile range as if it were this bar table.

Swipe horizontally to view all dimensions.

Nominal thickness (mm) Minimum yield ReH (MPa), Q355 B and C
≤ 16 355
> 16–40 345
> 40–63 335
> 63–80 325
> 80–100 315
> 100–150 295
> 150–200 285
> 200–250 275
> 250–400 Dash (quality D plate only, not this product)

Swipe horizontally to view all dimensions.

Nominal thickness (mm) Tensile strength Rm (MPa) Minimum longitudinal elongation A (%)
≤ 40 470–630 (through 100 mm in the GB/T 1591 Table 8 band used here) 22
> 40–63 470–630 21
> 63–100 470–630 20

GB/T 1591 Q355B Round, Square and Flat Bar Sizes (Common Typographical Metric Sizes, Theoretical Mass)

GB/T 1591 does not itself tabulate a closed list of bar diameters and flat widths. The tables below are common typographical metric merchant-bar rounds, squares and flats, with theoretical mass at 7.85 g/cm³: rounds M = 0.006165 d² kg/m and squares or flats M = 0.00785 a b kg/m. They are labeled as common sizes, not as every bar size that can be ordered, and they are not a warehouse list. Do not use a GB/T 6728 hollow-section table or a GB/T 706 angle table as a bar table.

Common typographical round bars

Swipe horizontally to view all dimensions.

Diameter d (mm) Theoretical mass (kg/m)
10 0.617
12 0.888
16 1.578
18 1.997
20 2.466
22 2.984
25 3.853
28 4.833
30 5.548
32 6.313
36 7.99
40 9.86
45 12.48
50 15.41
56 19.33
60 22.19
63 24.47
70 30.21
80 39.46
90 49.94
100 61.65
110 74.6
120 88.78
130 104.19
140 120.83
150 138.71
160 157.82
180 199.75
200 246.6

Common typographical square bars

Swipe horizontally to view all dimensions.

Side a (mm) Theoretical mass (kg/m)
10 0.785
12 1.13
16 2.01
20 3.14
25 4.906
30 7.065
40 12.56
50 19.62
60 28.26
70 38.46
80 50.24
100 78.5

Common typographical flat bars

Swipe horizontally to view all dimensions.

Thickness x width (mm) Theoretical mass (kg/m)
5 x 20 0.785
5 x 30 1.177
5 x 40 1.57
5 x 50 1.962
6 x 20 0.942
6 x 30 1.413
6 x 40 1.884
6 x 50 2.355
6 x 60 2.826
8 x 20 1.256
8 x 30 1.884
8 x 40 2.512
8 x 50 3.14
8 x 80 5.024
10 x 20 1.57
10 x 30 2.355
10 x 40 3.14
10 x 50 3.925
10 x 80 6.28
10 x 100 7.85
12 x 30 2.826
12 x 40 3.768
12 x 50 4.71
12 x 80 7.536
12 x 100 9.42
16 x 40 5.024
16 x 50 6.28
16 x 80 10.05
16 x 100 12.56
20 x 40 6.28
20 x 50 7.85
20 x 80 12.56
20 x 100 15.7
25 x 50 9.812
25 x 80 15.7
25 x 100 19.62

Applications and Service Limits for GB/T 1591 Q355B Bars

Q355B bars are used in general structural and fabrication work where GB/T 1591 quality B is specified. Impact testing is not a quality-B requirement in the same way as qualities C, D or E; if a temperature or impact value is needed, it must be agreed and may point to a different quality. Name the bar form, the size and the required certificate on the order.

GB/T 1591 Q355B Bars Compared with GB/T 6728 Hollows and GB/T 706 Angles

GB/T 1591 Q355B Steel Hollow Sections (GB/T 6728-2025) uses GB/T 1591 Q355B chemistry in a GB/T 6728-2025 hollow section, including the Table 25 class 355 discussion on that page. GB/T 706 Q355B Equal and Unequal Steel Angles is a GB/T 706 rolled angle. Neither product form is a substitute for these bars, even though the material grade name is the same.

Near-Equivalents for GB/T 1591 Q355B Bars: Not Automatic Substitutes

Near-equivalents only, not automatic substitutes. EN 10025-2 S355JR bars, ASTM A572 Grade 50 bars and other 355 MPa class bar specifications have their own chemistry, CEV and thickness bands. Do not treat a Q355B angle or hollow-section certificate as a bar certificate.

Sourcing GB/T 1591 Q355B Steel Bars from SHH STEEL

SHH STEEL reviews the named GB/T 1591 edition, the Q355B quality-B certificate and the ordered bar size before quoting. The typographical metric size tables on this page are not a warehouse list. State the form, the diameter or thickness and width, and the length on the enquiry.

FAQ: GB/T 1591 Q355B Steel Bars

Are these the same product as GB/T 1591 Q355B hollow sections?
No. The hollow-section page is a GB/T 6728-2025 product that uses Q355B as the material grade. These are bars. The tensile table on this page follows GB/T 1591, not GB/T 6728 Table 25.
May phosphorus and sulfur be 0.040 %?
Yes, for sections and bars GB/T 1591 allows P and S to be raised by 0.005 % to 0.040 %. The heat-analysis table still shows the 0.035 % base maxima with that footnote.
Is yield always 355 MPa?
No. Minimum yield is 355 MPa only at t ≤ 16 mm and then follows the Table 7 thickness bands.

Conclusion

Specify GB/T 1591-2018 Q355B bars with as-rolled quality B chemistry and the thickness-dependent mechanical bands in Tables 7, 8 and 11. Do not substitute a GB/T 6728 hollow section or a GB/T 706 angle certificate for a bar certificate.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X