GB/T 1591 Q355B Steel Hollow Sections (GB/T 6728-2025) | GB/T 1591 Steel Hollow Sections - SHH STEEL

GB/T 1591 Q355B Steel Hollow Sections (GB/T 6728-2025)

GB/T 1591 Q355B hollow sections are cold-formed square, rectangular and circular sections to GB/T 6728-2025. Chemistry and CEV follow as-rolled Q355B in GB/T 1591-2018. Table 25 class 355 requires 355 MPa yield; 470–680 MPa tensile is not the 470–630 MPa GB/T 1591 band. Size tables are a formula-checked 2025 Tables 1–3 subset, not every row. SHH STEEL reviews certificates before quoting.
Keywords
Q355B hollow section, GB/T 1591 Q355B SHS, Q355B RHS, Q355B CHS, GB/T 6728-2025
Equivalent Grades:
Near-equivalents only, not automatic substitutes.
Share:
General Description
Material Specification
Available Sizes of GB/T 1591 Q355B Steel Hollow Sections (625 verified sizes)
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Sourcing GB/T 1591 Q355B Steel Hollow Sections from SHH STEEL
FAQ
Conclusion

What is a GB/T 1591 Q355B Steel Hollow Section (GB/T 6728-2025)?

A GB/T 1591 Q355B steel hollow section on this page is a cold-formed closed square, rectangular or circular section whose steel is as-rolled quality B of GB/T 1591-2018, and whose dimensions, mass and technical delivery follow GB/T 6728-2025. The 2025 section standard, published 29 August 2025 and implemented 1 March 2026, replaces GB/T 6728-2017 and GB/T 6723-2017. It does not replace GB/T 1591. Q355B remains a low-alloy high-strength structural steel with a 355 MPa first-band yield and a +20 °C impact quality; the formed section also has to meet product yield class 355 in GB/T 6728-2025 Table 25.

Closed sections are normally continuously roll-formed from plate or strip and welded (longitudinal HFW, longitudinal SAW or spiral SAW). Thickness 18 mm and above may use a two-stage forming route. Continuous hot-dip galvanized closed sections are included; sections formed and welded from already-galvanized sheet or strip are not. Open cold-formed sections now sit in the same 2025 document, but they are outside this hollow-section page.

Material, Manufacture and Why GB/T 1591 and GB/T 6728 Must Both Be Named

Write both documents on the contract. GB/T 1591-2018 is the grade standard: Table 1 chemistry, Table 2 CEV, Table 7 and 8 mechanicals, and Table 11 impact for quality B. Delivery condition 7.3 allows as-rolled, normalized, normalizing-rolled or TMCP starting product; this page is the as-rolled Q355B route. GB/T 6728-2025 is the section standard: Tables 1–3 and Annex A for size and mass, Annex B for wall-thickness deviation, and Table 25 for the product yield class of the cold-formed hollow section. Confusing those roles is how a 470–630 MPa tensile band gets copied into a Table 25 discussion, or how a 2017 size list gets dated 2025.

Usual closed-section length is 4000–12000 mm, with Table 21 cut-length tolerances (ordinary +50/0 mm; precision +5/0 mm to 6000 mm and +10/0 mm above). Straightness is not more than 2 mm per metre and not more than 0.15 % of total length. Theoretical-mass lot tolerances in clause 6.4 are −6 % to +10 % when the total of the side lengths is not more than 1600 mm, and −4 % to +6 % above that.

GB/T 1591 Q355B Hollow-Section Sizes: Verified Common Subset of GB/T 6728-2025 Tables 1–3

The dimensional list is the same verified 2025 subset used on the sister Q235B page: 625 closed-section rows (216 square, 321 rectangular and 88 circular). Area is recomputed with Annex A, and only typographical sizes with a preferred wall whose published area matches that formula are shown. Mass is the Annex A theoretical value M = 0.785A. The list is not every row of Tables 1–3, and it is not a 2017 chart with a 2025 label.

The size tables below are a formula-checked subset of GB/T 6728-2025 Tables 1 (square), 2 (rectangular) and 3 (circular). Each listed size uses a typographical designation and a preferred wall thickness whose published area matches the Annex A formula. Theoretical mass is computed as M = 0.785A (kg/m, with A in cm²). These tables are not a complete recitation of every row in the 2025 standard. Order against the edition on the contract, and do not treat a withdrawn 2017 table as a 2025 size list.

Verified common square sizes from GB/T 6728-2025 Table 1 (formula-checked subset, not every published row)

216 verified SHS rows are listed below, grouped by size.

20–90 mm square (66 sizes)

Swipe horizontally to view all dimensions.

Designation (B×B×t) B (mm) t (mm) A (cm²) Mass (kg/m)
20×20×1.2 20 1.2 0.865 0.679
20×20×1.5 20 1.5 1.052 0.826
20×20×1.7 20 1.7 1.170 0.918
20×20×2 20 2 1.337 1.050
25×25×1.2 25 1.2 1.105 0.868
25×25×1.7 25 1.7 1.510 1.185
25×25×2 25 2 1.737 1.364
30×30×1.5 30 1.5 1.652 1.297
30×30×1.7 30 1.7 1.850 1.452
30×30×1.8 30 1.8 1.947 1.528
30×30×2 30 2 2.137 1.678
30×30×2.2 30 2.2 2.322 1.823
30×30×2.5 30 2.5 2.589 2.032
30×30×2.75 30 2.75 2.803 2.200
30×30×3 30 3 3.008 2.361
40×40×1.8 40 1.8 2.667 2.094
40×40×2 40 2 2.937 2.306
40×40×2.2 40 2.2 3.202 2.513
40×40×2.5 40 2.5 3.589 2.817
40×40×2.75 40 2.75 3.903 3.064
40×40×3 40 3 4.208 3.303
40×40×3.5 40 3.5 4.795 3.764
50×50×1.5 50 1.5 2.852 2.239
50×50×1.7 50 1.7 3.210 2.520
50×50×1.8 50 1.8 3.387 2.659
50×50×2 50 2 3.737 2.934
50×50×2.2 50 2.2 4.082 3.204
50×50×3 50 3 5.408 4.245
50×50×4 50 4 6.948 5.454
50×50×4.75 50 4.75 8.016 6.293
60×60×2 60 2 4.537 3.562
60×60×2.2 60 2.2 4.962 3.895
60×60×2.75 60 2.75 6.103 4.791
60×60×3 60 3 6.608 5.187
60×60×3.75 60 3.75 8.075 6.339
60×60×4 60 4 8.548 6.710
60×60×4.5 60 4.5 9.469 7.433
60×60×4.75 60 4.75 9.916 7.784
60×60×5 60 5 10.356 8.130
65×65×4 65 4 9.348 7.338
70×70×2.75 70 2.75 7.203 5.654
70×70×3 70 3 7.808 6.129
70×70×3.5 70 3.5 8.995 7.061
70×70×3.75 70 3.75 9.575 7.517
70×70×4 70 4 10.148 7.966
70×70×4.5 70 4.5 11.269 8.846
70×70×4.75 70 4.75 11.816 9.276
70×70×5 70 5 12.356 9.700
75×75×3 75 3 8.408 6.600
75×75×4 75 4 10.948 8.594
80×80×2.5 80 2.5 7.589 5.957
80×80×2.75 80 2.75 8.303 6.518
80×80×3 80 3 9.008 7.071
80×80×3.5 80 3.5 10.395 8.160
80×80×3.75 80 3.75 11.075 8.694
80×80×4 80 4 11.748 9.222
80×80×4.5 80 4.5 13.069 10.259
80×80×4.75 80 4.75 13.716 10.767
80×80×5 80 5 14.356 11.270
80×80×5.5 80 5.5 15.611 12.255
80×80×6 80 6 16.833 13.214
90×90×3 90 3 10.208 8.013
90×90×4 90 4 13.348 10.478
90×90×5 90 5 16.356 12.840
90×90×6 90 6 19.233 15.098
90×90×8 90 8 24.042 18.873

95–160 mm square (53 sizes)

Swipe horizontally to view all dimensions.

Designation (B×B×t) B (mm) t (mm) A (cm²) Mass (kg/m)
100×100×3.75 100 3.75 14.075 11.049
100×100×4 100 4 14.948 11.734
100×100×4.5 100 4.5 16.669 13.085
100×100×4.75 100 4.75 17.516 13.750
100×100×5 100 5 18.356 14.410
100×100×5.5 100 5.5 20.011 15.709
100×100×6 100 6 21.633 16.982
100×100×8 100 8 27.242 21.385
100×100×10 100 10 32.566 25.565
105×105×10 105 10 34.566 27.135
110×110×4 110 4 16.548 12.990
110×110×5 110 5 20.356 15.980
110×110×6 110 6 24.033 18.866
110×110×8 110 8 30.442 23.897
120×120×3.5 120 3.5 15.995 12.556
120×120×3.75 120 3.75 17.075 13.404
120×120×4 120 4 18.148 14.246
120×120×4.5 120 4.5 20.269 15.911
120×120×4.75 120 4.75 21.316 16.733
120×120×5 120 5 22.356 17.550
120×120×5.5 120 5.5 24.411 19.163
120×120×6 120 6 26.433 20.750
120×120×8 120 8 33.642 26.409
130×130×4 130 4 19.748 15.502
130×130×5 130 5 24.356 19.120
130×130×6 130 6 28.833 22.634
130×130×8 130 8 36.842 28.921
130×130×10 130 10 44.566 34.985
140×140×3.5 140 3.5 18.795 14.754
140×140×3.75 140 3.75 20.075 15.759
140×140×4 140 4 21.348 16.758
140×140×4.5 140 4.5 23.869 18.737
140×140×5 140 5 26.356 20.690
140×140×5.5 140 5.5 28.811 22.617
140×140×6 140 6 31.233 24.518
140×140×8 140 8 40.042 31.433
150×150×3.75 150 3.75 21.575 16.937
150×150×4 150 4 22.948 18.014
150×150×4.5 150 4.5 25.669 20.150
150×150×4.75 150 4.75 27.016 21.208
150×150×5 150 5 28.356 22.260
150×150×5.5 150 5.5 31.011 24.344
150×150×6 150 6 33.633 26.402
150×150×8 150 8 43.242 33.945
150×150×12 150 12 60.059 47.147
160×160×3.75 160 3.75 23.075 18.114
160×160×4 160 4 24.548 19.270
160×160×4.5 160 4.5 27.469 21.563
160×160×4.75 160 4.75 28.916 22.699
160×160×5 160 5 30.356 23.830
160×160×5.5 160 5.5 33.211 26.071
160×160×8 160 8 46.442 36.457
160×160×12 160 12 64.859 50.915

170–300 mm square (49 sizes)

Swipe horizontally to view all dimensions.

Designation (B×B×t) B (mm) t (mm) A (cm²) Mass (kg/m)
170×170×2 170 2 13.337 10.470
170×170×4 170 4 26.148 20.526
170×170×5 170 5 32.356 25.400
170×170×6 170 6 38.433 30.170
170×170×8 170 8 49.642 38.969
170×170×10 170 10 60.566 47.545
170×170×12 170 12 69.659 54.683
180×180×3.75 180 3.75 26.075 20.469
180×180×4 180 4 27.748 21.782
180×180×4.75 180 4.75 32.716 25.682
180×180×5 180 5 34.356 26.970
180×180×5.5 180 5.5 37.611 29.525
180×180×6 180 6 40.833 32.054
180×180×10 180 10 64.566 50.685
180×180×12 180 12 74.459 58.451
190×190×4 190 4 29.348 23.038
190×190×4.75 190 4.75 34.616 27.174
190×190×5 190 5 36.356 28.540
190×190×6 190 6 43.233 33.938
190×190×10 190 10 68.566 53.825
190×190×12 190 12 79.259 62.219
200×200×3.75 200 3.75 29.075 22.824
200×200×4 200 4 30.948 24.294
200×200×4.75 200 4.75 36.516 28.665
200×200×5 200 5 38.356 30.110
200×200×5.5 200 5.5 42.011 32.979
200×200×6 200 6 45.633 35.822
200×200×10 200 10 72.566 56.965
200×200×12 200 12 84.059 65.987
220×220×5 220 5 42.356 33.250
220×220×5.5 220 5.5 46.411 36.433
220×220×10 220 10 80.566 63.245
220×220×12 220 12 93.659 73.523
240×240×8 240 8 72.042 56.553
240×240×10 240 10 88.566 69.525
240×240×12 240 12 103.259 81.059
250×250×4.75 250 4.75 46.016 36.123
250×250×12 250 12 108.059 84.827
260×260×6 260 6 60.033 47.126
260×260×8 260 8 78.442 61.577
260×260×12 260 12 112.859 88.595
280×280×6 280 6 64.833 50.894
280×280×8 280 8 84.842 66.601
280×280×10 280 10 104.566 82.085
280×280×12 280 12 122.459 96.131
300×300×6 300 6 69.633 54.662
300×300×8 300 8 91.242 71.625
300×300×10 300 10 112.566 88.365
300×300×12 300 12 132.059 103.667

320–1200 mm square (48 sizes)

Swipe horizontally to view all dimensions.

Designation (B×B×t) B (mm) t (mm) A (cm²) Mass (kg/m)
320×320×6 320 6 74.433 58.430
320×320×8 320 8 97.642 76.649
320×320×10 320 10 120.566 94.645
320×320×12 320 12 141.659 111.203
330×330×8 330 8 100.842 79.161
340×340×8 340 8 104.042 81.673
350×350×6 350 6 81.633 64.082
350×350×8 350 8 107.242 84.185
350×350×10 350 10 132.566 104.065
350×350×12 350 12 156.059 122.507
370×370×6.3 370 6.3 90.290 70.877
390×390×2 390 2 30.937 24.286
400×400×6.3 400 6.3 97.850 76.812
400×400×8 400 8 123.242 96.745
400×400×10 400 10 152.566 119.765
400×400×12 400 12 180.059 141.347
400×400×14 400 14 207.748 163.082
450×450×8 450 8 139.242 109.305
450×450×10 450 10 172.566 135.465
450×450×12 450 12 204.059 160.187
450×450×14 450 14 235.748 185.062
500×500×8 500 8 155.242 121.865
500×500×10 500 10 192.566 151.165
500×500×12 500 12 228.059 179.027
500×500×14 500 14 263.748 207.042
500×500×16 500 16 298.772 234.536
500×500×18 500 18 333.134 261.510
500×500×20 500 20 366.832 287.963
500×500×25 500 25 448.175 351.817
600×600×16 600 16 362.772 284.776
600×600×18 600 18 405.134 318.030
600×600×20 600 20 446.832 350.763
700×700×16 700 16 426.772 335.016
700×700×18 700 18 477.134 374.550
700×700×25 700 25 648.175 508.817
800×800×16 800 16 490.772 385.256
800×800×20 800 20 606.832 476.363
800×800×25 800 25 748.175 587.317
900×900×20 900 20 686.832 539.163
900×900×25 900 25 848.175 665.817
900×900×30 900 30 1005.372 789.217
900×900×36 900 36 1188.535 933.000
900×900×40 900 40 1307.327 1026.252
1000×1000×25 1000 25 948.175 744.317
1000×1000×30 1000 30 1125.372 883.417
1000×1000×36 1000 36 1332.535 1046.040
1000×1000×40 1000 40 1467.327 1151.852
1200×1200×20 1200 20 926.832 727.563

Verified common rectangular sizes from GB/T 6728-2025 Table 2 (formula-checked subset, not every published row)

321 verified RHS rows are listed below, grouped by size.

H 30–80 mm rectangular (74 sizes)

Swipe horizontally to view all dimensions.

Designation (H×B×t) H (mm) B (mm) t (mm) A (cm²) Mass (kg/m)
30×20×1.5 30 20 1.5 1.352 1.061
30×20×1.7 30 20 1.7 1.510 1.185
30×20×1.8 30 20 1.8 1.587 1.246
30×20×2 30 20 2 1.737 1.364
30×20×2.2 30 20 2.2 1.882 1.477
30×20×2.5 30 20 2.5 2.089 1.640
40×20×1.5 40 20 1.5 1.652 1.297
40×20×1.7 40 20 1.7 1.850 1.452
40×20×1.8 40 20 1.8 1.947 1.528
40×20×2 40 20 2 2.137 1.678
40×20×2.2 40 20 2.2 2.322 1.823
40×20×2.5 40 20 2.5 2.589 2.032
40×20×2.75 40 20 2.75 2.803 2.200
40×20×3 40 20 3 3.008 2.361
40×25×1.5 40 25 1.5 1.802 1.415
40×25×1.7 40 25 1.7 2.020 1.586
40×25×1.8 40 25 1.8 2.127 1.670
40×25×2 40 25 2 2.337 1.835
40×25×2.75 40 25 2.75 3.078 2.416
40×25×3 40 25 3 3.308 2.597
40×30×1.5 40 30 1.5 1.952 1.532
40×30×1.7 40 30 1.7 2.190 1.719
40×30×1.8 40 30 1.8 2.307 1.811
40×30×2.2 40 30 2.2 2.762 2.168
40×30×2.5 40 30 2.5 3.089 2.425
40×30×3 40 30 3 3.608 2.832
50×30×1.8 50 30 1.8 2.667 2.094
50×30×2 50 30 2 2.937 2.306
50×30×2.2 50 30 2.2 3.202 2.513
50×30×2.75 50 30 2.75 3.903 3.064
50×30×3 50 30 3 4.208 3.303
50×40×1.7 50 40 1.7 2.870 2.253
50×40×1.8 50 40 1.8 3.027 2.376
50×40×2 50 40 2 3.337 2.620
50×40×2.2 50 40 2.2 3.642 2.859
50×40×2.75 50 40 2.75 4.453 3.495
50×40×3 50 40 3 4.808 3.774
50×40×4 50 40 4 6.148 4.826
55×40×1.5 55 40 1.5 2.702 2.121
55×40×1.7 55 40 1.7 3.040 2.386
60×30×2.2 60 30 2.2 3.642 2.859
60×30×2.5 60 30 2.5 4.089 3.210
60×30×2.75 60 30 2.75 4.453 3.495
60×30×3 60 30 3 4.808 3.774
60×30×4 60 30 4 6.148 4.826
60×40×2 60 40 2 3.737 2.934
60×40×2.2 60 40 2.2 4.082 3.204
60×40×2.5 60 40 2.5 4.589 3.602
60×40×3 60 40 3 5.408 4.245
60×40×3.5 60 40 3.5 6.195 4.863
70×50×2.75 70 50 2.75 6.103 4.791
70×50×3 70 50 3 6.608 5.187
70×50×3.75 70 50 3.75 8.075 6.339
70×50×4 70 50 4 8.548 6.710
70×50×4.75 70 50 4.75 9.916 7.784
80×40×2 80 40 2 4.537 3.562
80×40×2.2 80 40 2.2 4.962 3.895
80×40×2.75 80 40 2.75 6.103 4.791
80×40×3 80 40 3 6.608 5.187
80×40×3.75 80 40 3.75 8.075 6.339
80×40×4 80 40 4 8.548 6.710
80×40×4.5 80 40 4.5 9.469 7.433
80×40×4.75 80 40 4.75 9.916 7.784
80×40×5 80 40 5 10.356 8.130
80×50×2.75 80 50 2.75 6.653 5.222
80×50×3 80 50 3 7.208 5.658
80×50×3.75 80 50 3.75 8.825 6.928
80×50×4 80 50 4 9.348 7.338
80×50×4.75 80 50 4.75 10.866 8.530
80×60×3 80 60 3 7.808 6.129
80×60×3.5 80 60 3.5 8.995 7.061
80×60×4 80 60 4 10.148 7.966
80×60×4.5 80 60 4.5 11.269 8.846
80×60×4.75 80 60 4.75 11.816 9.276

H 90–150 mm rectangular (75 sizes)

Swipe horizontally to view all dimensions.

Designation (H×B×t) H (mm) B (mm) t (mm) A (cm²) Mass (kg/m)
90×40×3 90 40 3 7.208 5.658
90×40×4 90 40 4 9.348 7.338
90×40×5 90 40 5 11.356 8.915
90×50×3 90 50 3 7.808 6.129
90×50×4 90 50 4 10.148 7.966
90×60×3 90 60 3 8.408 6.600
90×60×3.25 90 60 3.25 9.055 7.109
90×60×3.5 90 60 3.5 9.695 7.610
90×60×3.75 90 60 3.75 10.325 8.105
90×60×4 90 60 4 10.948 8.594
90×60×4.5 90 60 4.5 12.169 9.552
90×60×4.75 90 60 4.75 12.766 10.022
100×40×2.5 100 40 2.5 6.589 5.172
100×40×3 100 40 3 7.808 6.129
100×40×4 100 40 4 10.148 7.966
100×40×5 100 40 5 12.356 9.700
100×50×2.75 100 50 2.75 7.753 6.086
100×50×3 100 50 3 8.408 6.600
100×50×3.75 100 50 3.75 10.325 8.105
100×50×4 100 50 4 10.948 8.594
100×50×4.75 100 50 4.75 12.766 10.022
100×60×2.75 100 60 2.75 8.303 6.518
100×60×3 100 60 3 9.008 7.071
100×60×3.5 100 60 3.5 10.395 8.160
100×60×3.75 100 60 3.75 11.075 8.694
100×60×4 100 60 4 11.748 9.222
100×60×4.5 100 60 4.5 13.069 10.259
100×60×4.75 100 60 4.75 13.716 10.767
100×60×5 100 60 5 14.356 11.270
100×80×2.5 100 80 2.5 8.589 6.742
100×80×2.75 100 80 2.75 9.403 7.381
100×80×3 100 80 3 10.208 8.013
100×80×3.5 100 80 3.5 11.795 9.259
100×80×3.75 100 80 3.75 12.575 9.872
100×80×4 100 80 4 13.348 10.478
100×80×4.5 100 80 4.5 14.869 11.672
100×80×4.75 100 80 4.75 15.616 12.259
100×80×5 100 80 5 16.356 12.840
120×50×3 120 50 3 9.608 7.542
120×60×2.75 120 60 2.75 9.403 7.381
120×60×3 120 60 3 10.208 8.013
120×60×3.5 120 60 3.5 11.795 9.259
120×60×3.75 120 60 3.75 12.575 9.872
120×60×4 120 60 4 13.348 10.478
120×60×4.5 120 60 4.5 14.869 11.672
120×60×4.75 120 60 4.75 15.616 12.259
120×60×5 120 60 5 16.356 12.840
120×60×5.5 120 60 5.5 17.811 13.982
120×80×2.5 120 80 2.5 9.589 7.527
120×80×2.75 120 80 2.75 10.503 8.245
120×80×3 120 80 3 11.408 8.955
120×80×3.5 120 80 3.5 13.195 10.358
120×80×3.75 120 80 3.75 14.075 11.049
120×80×4 120 80 4 14.948 11.734
120×80×4.5 120 80 4.5 16.669 13.085
120×80×4.75 120 80 4.75 17.516 13.750
120×80×5 120 80 5 18.356 14.410
120×80×5.5 120 80 5.5 20.011 15.709
120×80×6 120 80 6 21.633 16.982
140×80×3.75 140 80 3.75 15.575 12.227
140×80×4 140 80 4 16.548 12.990
140×80×4.5 140 80 4.5 18.469 14.498
140×80×4.75 140 80 4.75 19.416 15.242
140×80×5 140 80 5 20.356 15.980
140×80×5.5 140 80 5.5 22.211 17.436
150×50×4 150 50 4 14.948 11.734
150×50×6 150 50 6 21.633 16.982
150×50×8 150 50 8 27.242 21.385
150×70×6 150 70 6 24.033 18.866
150×100×3.75 150 100 3.75 17.825 13.993
150×100×4 150 100 4 18.948 14.874
150×100×4.5 150 100 4.5 21.169 16.617
150×100×4.75 150 100 4.75 22.266 17.479
150×100×5 150 100 5 23.356 18.335
150×100×6 150 100 6 27.633 21.692

H 160–250 mm rectangular (59 sizes)

Swipe horizontally to view all dimensions.

Designation (H×B×t) H (mm) B (mm) t (mm) A (cm²) Mass (kg/m)
160×60×3 160 60 3 12.608 9.897
160×60×4.5 160 60 4.5 18.469 14.498
160×80×3.5 160 80 3.5 15.995 12.556
160×80×3.75 160 80 3.75 17.075 13.404
160×80×4 160 80 4 18.148 14.246
160×80×4.5 160 80 4.5 20.269 15.911
160×80×4.75 160 80 4.75 21.316 16.733
160×80×5 160 80 5 22.356 17.550
160×80×5.5 160 80 5.5 24.411 19.163
160×80×6 160 80 6 26.433 20.750
180×65×3 180 65 3 14.108 11.075
180×65×4.5 180 65 4.5 20.719 16.264
180×100×4 180 100 4 21.348 16.758
180×100×5 180 100 5 26.356 20.690
180×100×6 180 100 6 31.233 24.518
180×100×8 180 100 8 40.042 31.433
180×160×3.5 180 160 3.5 22.995 18.051
180×160×4 180 160 4 26.148 20.526
180×160×5 180 160 5 32.356 25.400
180×160×6 180 160 6 38.433 30.170
180×160×8 180 160 8 49.642 38.969
200×100×4.5 200 100 4.5 25.669 20.150
200×100×4.75 200 100 4.75 27.016 21.208
200×100×5 200 100 5 28.356 22.260
200×100×5.5 200 100 5.5 31.011 24.344
200×100×6 200 100 6 33.633 26.402
200×100×8 200 100 8 43.242 33.945
200×120×4 200 120 4 24.548 19.270
200×120×5 200 120 5 30.356 23.830
200×120×6 200 120 6 36.033 28.286
200×120×8 200 120 8 46.442 36.457
200×150×3.5 200 150 3.5 23.695 18.600
200×150×4 200 150 4 26.948 21.154
200×150×4.5 200 150 4.5 30.169 23.682
200×150×4.75 200 150 4.75 31.766 24.937
200×150×5 200 150 5 33.356 26.185
200×150×5.5 200 150 5.5 36.511 28.661
200×150×6 200 150 6 39.633 31.112
200×150×10 200 150 10 62.566 49.115
220×140×4 220 140 4 27.748 21.782
220×140×5 220 140 5 34.356 26.970
220×140×6 220 140 6 40.833 32.054
220×140×10 220 140 10 64.566 50.685
220×140×12 220 140 12 74.459 58.451
250×150×4.5 250 150 4.5 34.669 27.215
250×150×4.75 250 150 4.75 36.516 28.665
250×150×5 250 150 5 38.356 30.110
250×150×5.5 250 150 5.5 42.011 32.979
250×150×6 250 150 6 45.633 35.822
250×180×4 250 180 4 33.348 26.178
250×180×5 250 180 5 41.356 32.465
250×180×6 250 180 6 49.233 38.648
250×180×8 250 180 8 64.042 50.273
250×180×10 250 180 10 78.566 61.675
250×180×12 250 180 12 91.259 71.639
250×200×5 250 200 5 43.356 34.035
250×200×8 250 200 8 67.242 52.785
250×200×10 250 200 10 82.566 64.815
250×200×12 250 200 12 96.059 75.407

H 260–400 mm rectangular (53 sizes)

Swipe horizontally to view all dimensions.

Designation (H×B×t) H (mm) B (mm) t (mm) A (cm²) Mass (kg/m)
260×180×5 260 180 5 42.356 33.250
260×180×10 260 180 10 80.566 63.245
260×180×12 260 180 12 93.659 73.523
280×180×5 280 180 5 44.356 34.820
280×180×8 280 180 8 68.842 54.041
280×180×10 280 180 10 84.566 66.385
280×200×5 280 200 5 46.356 36.390
280×200×8 280 200 8 72.042 56.553
280×200×10 280 200 10 88.566 69.525
280×200×12 280 200 12 103.259 81.059
300×100×5 300 100 5 38.356 30.110
300×100×6 300 100 6 45.633 35.822
300×100×10 300 100 10 72.566 56.965
300×100×12 300 100 12 84.059 65.987
300×150×4.75 300 150 4.75 41.266 32.394
300×150×5 300 150 5 43.356 34.035
300×150×5.5 300 150 5.5 47.511 37.296
300×150×8 300 150 8 67.242 52.785
300×150×10 300 150 10 82.566 64.815
300×150×12 300 150 12 96.059 75.407
300×160×5 300 160 5 44.356 34.820
300×160×8 300 160 8 68.842 54.041
300×160×10 300 160 10 84.566 66.385
300×160×12 300 160 12 98.459 77.291
300×200×5 300 200 5 48.356 37.960
300×200×12 300 200 12 108.059 84.827
300×250×6 300 250 6 63.633 49.952
300×250×8 300 250 8 83.242 65.345
300×250×10 300 250 10 102.566 80.515
300×250×12 300 250 12 120.059 94.247
360×200×6 360 200 6 64.833 50.894
360×200×8 360 200 8 84.842 66.601
360×200×10 360 200 10 104.566 82.085
390×220×8 390 220 8 92.842 72.881
390×250×7 390 250 7 85.958 67.477
400×160×6 400 160 6 64.833 50.894
400×160×8 400 160 8 84.842 66.601
400×160×10 400 160 10 104.566 82.085
400×200×5.5 400 200 5.5 64.011 50.249
400×200×6 400 200 6 69.633 54.662
400×200×8 400 200 8 91.242 71.625
400×200×10 400 200 10 112.566 88.365
400×200×12 400 200 12 132.059 103.667
400×250×5 400 250 5 63.356 49.735
400×250×8 400 250 8 99.242 77.905
400×250×10 400 250 10 122.566 96.215
400×250×12 400 250 12 144.059 113.087
400×300×5 400 300 5 68.356 53.660
400×300×6 400 300 6 81.633 64.082
400×300×8 400 300 8 107.242 84.185
400×300×10 400 300 10 132.566 104.065
400×300×12 400 300 12 156.059 122.507
400×390×4.75 400 390 4.75 73.566 57.750

H 450–1000 mm rectangular (60 sizes)

Swipe horizontally to view all dimensions.

Designation (H×B×t) H (mm) B (mm) t (mm) A (cm²) Mass (kg/m)
450×250×6 450 250 6 81.633 64.082
450×250×8 450 250 8 107.242 84.185
450×250×10 450 250 10 132.566 104.065
450×250×12 450 250 12 156.059 122.507
600×400×10 600 400 10 192.566 151.165
600×400×12 600 400 12 228.059 179.027
600×400×14 600 400 14 263.748 207.042
700×300×12 700 300 12 228.059 179.027
700×300×14 700 300 14 263.748 207.042
700×300×16 700 300 16 298.772 234.536
700×300×18 700 300 18 333.134 261.510
700×300×20 700 300 20 366.832 287.963
700×400×12 700 400 12 252.059 197.867
700×400×14 700 400 14 291.748 229.022
700×400×16 700 400 16 330.772 259.656
700×400×18 700 400 18 369.134 289.770
700×400×20 700 400 20 406.832 319.363
700×500×16 700 500 16 362.772 284.776
700×500×18 700 500 18 405.134 318.030
700×500×20 700 500 20 446.832 350.763
700×600×20 700 600 20 486.832 382.163
700×600×30 700 600 30 705.372 553.717
800×400×30 800 400 30 645.372 506.617
800×400×40 800 400 40 827.327 649.452
800×500×20 800 500 20 486.832 382.163
800×500×30 800 500 30 705.372 553.717
800×500×36 800 500 36 828.535 650.400
800×500×40 800 500 40 907.327 712.252
800×600×36 800 600 36 900.535 706.920
800×600×40 800 600 40 987.327 775.052
800×700×40 800 700 40 1067.327 837.852
900×200×3.75 900 200 3.75 81.575 64.037
900×390×7 900 390 7 176.958 138.912
900×400×30 900 400 30 705.372 553.717
900×400×36 900 400 36 828.535 650.400
900×400×40 900 400 40 907.327 712.252
900×600×30 900 600 30 825.372 647.917
900×600×32 900 600 32 875.090 686.945
900×600×36 900 600 36 972.535 763.440
900×600×40 900 600 40 1067.327 837.852
900×700×20 900 700 20 606.832 476.363
900×700×30 900 700 30 885.372 695.017
900×700×36 900 700 36 1044.535 819.960
900×700×40 900 700 40 1147.327 900.652
1000×400×30 1000 400 30 765.372 600.817
1000×400×36 1000 400 36 900.535 706.920
1000×400×40 1000 400 40 987.327 775.052
1000×600×20 1000 600 20 606.832 476.363
1000×600×30 1000 600 30 885.372 695.017
1000×600×36 1000 600 36 1044.535 819.960
1000×600×40 1000 600 40 1147.327 900.652
1000×700×20 1000 700 20 646.832 507.763
1000×700×30 1000 700 30 945.372 742.117
1000×700×36 1000 700 36 1116.535 876.480
1000×700×40 1000 700 40 1227.327 963.452
1000×800×20 1000 800 20 686.832 539.163
1000×800×30 1000 800 30 1005.372 789.217
1000×800×32 1000 800 32 1067.090 837.665
1000×800×36 1000 800 36 1188.535 933.000
1000×800×40 1000 800 40 1307.327 1026.252

Verified common circular sizes from GB/T 6728-2025 Table 3 (formula-checked subset, not every published row)

88 verified CHS rows are listed below, grouped by size.

Outside diameter up to 165 mm (31 sizes)

Swipe horizontally to view all dimensions.

Designation (D×t) D (mm) t (mm) A (cm²) Mass (kg/m)
21.3×1.2 21.3 1.2 0.758 0.595
21.3×1.5 21.3 1.5 0.933 0.732
21.3×2 21.3 2 1.213 0.952
21.3×2.5 21.3 2.5 1.477 1.159
21.3×3 21.3 3 1.725 1.354
26.8×1.2 26.8 1.2 0.965 0.758
26.8×1.5 26.8 1.5 1.192 0.936
26.8×3 26.8 3 2.243 1.761
42.4×1.5 42.4 1.5 1.927 1.513
42.4×2.5 42.4 2.5 3.134 2.460
42.4×3 42.4 3 3.713 2.915
42.4×4 42.4 4 4.825 3.788
48×1.5 48 1.5 2.191 1.720
48×2 48 2 2.890 2.269
48×3 48 3 4.241 3.329
48.3×5 48.3 5 6.802 5.339
48.3×9 48.3 9 11.112 8.723
60×2 60 2 3.644 2.861
60×2.5 60 2.5 4.516 3.545
60×4 60 4 7.037 5.524
76×4 76 4 9.048 7.103
88.9×3 88.9 3 8.096 6.355
88.9×6 88.9 6 15.626 12.267
114×4 114 4 13.823 10.851
114×6 114 6 20.358 15.981
114.3×5 114.3 5 17.169 13.478
139.7×5 139.7 5 21.159 16.610
140×4 140 4 17.090 13.416
165×4 165 4 20.232 15.882
165×6 165 6 29.971 23.527
165×8 165 8 39.458 30.975

Outside diameter 219.1–1219 mm (57 sizes)

Swipe horizontally to view all dimensions.

Designation (D×t) D (mm) t (mm) A (cm²) Mass (kg/m)
219.1×5 219.1 5 33.631 26.400
219.1×6 219.1 6 40.168 31.532
219.1×10 219.1 10 65.691 51.567
273×5 273 5 42.097 33.046
273×8 273 8 66.602 52.282
273×10 273 10 82.624 64.860
325×6 325 6 60.130 47.202
325×8 325 8 79.671 62.542
325×10 325 10 98.960 77.684
325×12 325 12 117.998 92.629
355.6×6 355.6 6 65.898 51.730
355.6×8 355.6 8 87.361 68.579
355.6×10 355.6 10 108.573 85.230
406.4×8 406.4 8 100.129 78.601
406.4×10 406.4 10 124.533 97.758
406.4×12 406.4 12 148.685 116.718
457×8 457 8 112.846 88.584
457×10 457 10 140.429 110.237
457×12 457 12 167.761 131.692
508×8 508 8 125.664 98.646
508×10 508 10 156.451 122.814
508×12 508 12 186.988 146.785
610×8 610 8 151.299 118.770
610×10 610 10 188.496 147.969
610×12.5 610 12.5 234.638 184.191
610×16 610 16 298.577 234.383
610×20 610 20 370.708 291.006
630×10 630 10 194.779 152.901
630×12 630 12 232.981 182.890
630×16 630 16 308.630 242.275
630×20 630 20 383.274 300.870
630×25 630 25 475.166 373.005
660×12 660 12 244.290 191.768
660×14 660 14 284.126 223.039
660×16 660 16 323.710 254.112
660×20 660 20 402.124 315.667
660×25 660 25 498.728 391.501
711×16 711 16 349.345 274.236
711×20 711 20 434.168 340.822
711×30 711 30 641.827 503.834
813×16 813 16 400.616 314.483
813×20 813 20 498.257 391.131
813×25 813 25 618.894 485.832
813×30 813 30 737.960 579.299
914×16 914 16 451.384 354.336
914×25 914 25 698.219 548.102
914×30 914 30 833.150 654.023
1067×20 1067 20 657.850 516.412
1067×25 1067 25 818.385 642.432
1067×30 1067 30 977.349 767.219
1118×20 1118 20 689.894 541.567
1118×25 1118 25 858.440 673.876
1118×30 1118 30 1025.416 804.951
1219×16 1219 16 604.694 474.685
1219×20 1219 20 753.354 591.383
1219×25 1219 25 937.765 736.146
1219×30 1219 30 1120.606 879.676

GB/T 1591 Q355B Chemical Composition and CEV (As-Rolled, Heat Analysis)

This product is as-rolled Q355B under GB/T 1591-2018 (published 14 May 2018, implemented 1 February 2019, replacing GB/T 1591-2008). Chemistry is Table 1 for the as-rolled route. Q355N and Q355M have separate chemistry and CEV tables and are not this page. Qualities C and D are 0 °C and −20 °C grades, not quality B. GB/T 6728-2025 clause 6.5 points the section back to that material standard; 6728 itself is not the grade certificate.

Swipe horizontally to view all dimensions.

Element Heat-analysis limit (mass %) Notes for as-rolled Q355B hollow sections
C, max 0.24 For t > 30 mm, C ≤ 0.22 %. For sections with t > 100 mm, carbon may be agreed.
Si, max 0.55 See the controlled-silicon CEV increment in the notes under Table 2.
Mn, max 1.60 —
P, max 0.035 For sections and bars, P and S may be raised by 0.005 % to 0.040 %.
S, max 0.035 Same section and bar footnote as phosphorus.
Nb, V, Ti Dash (no specified requirement) Not a mandated microalloy addition for as-rolled Q355B.
Cr, max 0.30 —
Ni, max 0.30 —
Cu, max 0.40 —
Mo Dash —
N, max 0.012 An Als/Alt or other nitrogen-binding waiver may apply as in GB/T 1591.
B Dash —

Table 2 carbon equivalent (IIW ladle analysis): CEV = C + Mn/6 + (Cr+Mo+V)/5 + (Ni+Cu)/15. If silicon is held down and carbon or manganese are raised to meet tensile requirements, CEV may be increased by 0.02 % when Si ≤ 0.030 %, or by 0.01 % when Si ≤ 0.25 %.

Swipe horizontally to view all dimensions.

Nominal thickness (mm) Maximum CEV (%) for Q355 B/C/D Notes
≤ 30 0.45 Applies to most common hollow-section walls on this page.
> 30–63 0.47 —
> 63–150 0.47 —
> 150–250 0.49 For sections and bars the maximum CEV may be 0.54 %.
> 250–400 Dash for quality B and C 0.49 is tabulated only for quality D plate, which is not this product.

Mechanical Properties: GB/T 6728-2025 Table 25 Class 355 versus GB/T 1591 Tables 7, 8 and 11

For the cold-formed section, Table 25 class 355 is 355 MPa minimum yield, 470–680 MPa tensile, and 20 % minimum elongation. That tensile band is wider at the top than the 470–630 MPa range in GB/T 1591-2018 Table 7 for t ≤ 100 mm. A product ordered as GB/T 1591 Q355B in a GB/T 6728-2025 section has to be checked against both documents. Do not treat them as interchangeable, and do not replace the 2025 table with a plate quotation.

Table 25 footnote: for sections not larger than 60 mm × 60 mm (including equal-perimeter circular and rectangular sections), or with a flat-width to thickness ratio not greater than 14, the elongation on a 12.5 mm wide tensile specimen may be 3 percentage points lower. When yield is not clearly pronounced, Rp0.2 may replace ReH in the material standard.

Swipe horizontally to view all dimensions.

Product yield class ReH min (MPa) Rm (MPa) A min (%)
235 235 370–560 24
355 355 470–680 20
390 390 490–700 18
420 420 520–730 By agreement
460 460 550–770 By agreement
500 500 610–820 By agreement
550 550 670–880 By agreement
620 620 710–940 By agreement
690 690 770–1000 By agreement
750 750 750–1010 By agreement

GB/T 1591-2018 Table 7 and Table 8 remain the starting-steel mechanicals for as-rolled Q355 B and C. Yield steps down through 250 mm; the >250–400 mm yield is a dash for B and C (265 MPa is tabulated only for quality D plate). Tensile strength is 470–630 MPa up to 100 mm and 450–600 MPa from above 100 mm to 250 mm. Longitudinal elongation is 22 / 21 / 20 / 18 / 17 % in the bands t ≤ 40, >40–63, >63–100, >100–150 and >150–250 mm. Transverse elongation values are for plate and are not used as the default for these sections.

Swipe horizontally to view all dimensions.

Nominal thickness (mm) Minimum yield ReH (MPa), Q355 B and C
≤ 16 355
> 16–40 345
> 40–63 335
> 63–80 325
> 80–100 315
> 100–150 295
> 150–200 285
> 200–250 275
> 250–400 Dash (quality D plate only, not this product)

Swipe horizontally to view all dimensions.

Nominal thickness (mm) Tensile strength Rm (MPa) Minimum longitudinal elongation A (%)
≤ 40 470–630 (through 100 mm) 22
> 40–63 470–630 21
> 63–100 470–630 20
> 100–150 450–600 18
> 150–250 450–600 17

Impact testing of 6728 sections 6 mm and thicker is optional by agreement; when required, results follow GB/T 1591. Table 11 for Q355B is 34 J longitudinal and 27 J transverse at +20 °C. Default specimens are longitudinal; transverse is by agreement. Under 7.2.2, steels with nominal thickness not less than 6 mm, or nominal diameter not less than 12 mm, shall be impact tested when that clause applies. That is not the GB/T 700 Q235B inspection waiver for thickness under 25 mm, and that waiver must not be invented here. Subsize 10×7.5×55 or 10×5×55 specimens, at 75 % or 50 % of Table 11, may be used when a standard 10×10×55 specimen cannot be prepared; the larger size is preferred.

Delivery, Inspection and Identification of Q355B GB/T 6728-2025 Hollow Sections

Name GB/T 1591-2018 quality B, the delivery condition if it is not as-rolled, GB/T 6728-2025, the shape and designation, length and cutting class, weld process where it matters, and theoretical or actual mass. If a zinc coating is required, state the mass; unless otherwise agreed, closed galvanized sections have a hot-dip coating of not less than 200 g/m² on each of the inner and outer surfaces. Inspection follows 6728 clauses 7 and 8, including the retest rules added for coating mass. The certificate should identify both the 2018 material edition and the 2025 section edition when those are the ordered documents.

Weldability, CEV and Surface Condition of Q355B Cold-Formed Hollow Sections

Unlike Q235B, as-rolled Q355B carries published CEV caps in GB/T 1591 Table 2. Those caps, and the controlled-silicon increment, should be on the mill certificate when welding procedure is part of the order. The product is still a cold-formed, usually welded, closed section, so qualification has to include the longitudinal weld and the cold-formed corners where the application requires it. Surface and weld quality follow 6728 clauses 6.9 and 6.10. Laser or plasma cutting, where used, follows the 2025 clause 6.3 provisions. Galvanizing is only part of the supply when it is specified.

Dimensional Tolerances and Theoretical Mass for Q355B GB/T 6728-2025 Hollow Sections

Use the 2025 Annex B wall-thickness deviations, not a 2017 table. Length, straightness and theoretical-mass lot tolerances are those already given above. Circular out-of-roundness is in Table 24. Masses in the size tables are Annex A theoretical values for a theoretical-mass order; they do not replace weighing when actual mass is specified.

Wall-thickness permitted deviations are taken from GB/T 6728-2025 Annex B Table B.1, as recovered from the 2025 text. Values are plus or minus, in millimetres. Arbitration measurement is 50 mm from the end. Square sections use five positions (Fig. B.1, average); rectangular sections use five positions (Fig. B.2, average); circular sections use three positions (Fig. B.3, average), excluding the weld and HAZ. The recovered table starts at the >1.50–2.00 mm band. A possible thinner first band was not recovered as clean text, so deviations for walls 1.50 mm and under are not stated here.

Swipe horizontally to view all dimensions.

Nominal wall thickness t (mm) Permitted deviation (± mm)
>1.50–2.00 0.23
>2.00–2.50 0.28
>2.50–3.00 0.29
>3.00–4.00 0.3
>4.00–5.00 0.32
>5.00–6.00 0.34
>6.00–8.00 0.39
>8.00–10.00 0.44
>10.00–12.50 0.47
>12.50–15.00 0.51
>15.00–18.00 0.55
>18.00–25.00 1.1
>25.00–40.00 1.2
>40.00–60.00 1.3

Applications and Service Limits for GB/T 1591 Q355B Steel Hollow Sections

Q355B hollow sections are used in building frames, trusses, columns, machinery supports and general fabricated structures where a 355 MPa yield class and quality B are specified. Quality B impact, when tested, is at +20 °C. It is not Q355C or Q355D, and it is not Q355N or Q355M. Weathering, stainless, fire-resistant and bridge steels, and low-temperature qualities, have to be ordered as themselves. A higher Table 25 class (390 and above) is a different product yield class, not a free upgrade from Q355B.

GB/T 1591 Q355B Hollow Sections Compared with Q235B, Former Q345B, S355 and A500

Q235B uses GB/T 700 and Table 25 class 235, with no CEV cap and a different impact rule. The older name Q345B maps to Q355B in the 2018 designation system, but a 2008 document is not the 2018 text. S355J0H and S355J2H under EN 10219-1 are the usual European comparisons, with the impact temperature written into the grade. ASTM A500 Grade C is a common US HSS comparison. None of those is an automatic substitute for a GB/T 1591 Q355B, GB/T 6728-2025 certificate.

Near-Equivalents for GB/T 1591 Q355B Hollow Sections: Not Automatic Substitutes

The keywords row keeps only a one-line caution. The comparisons are in this table.

Swipe horizontally to view all dimensions.

Grade / designation Standard Relationship to this Q355B hollow section Caution
Q235B hollow section GB/T 700-2006 with GB/T 6728-2025 The same 2025 dimensional family, in product yield class 235. A lower yield class is not a substitute for a Q355B order. Chemistry, CEV and Table 25 bands differ.
Former Q345B GB/T 1591-2008 name mapping Q355B is the 2018 designation that maps from the older Q345B name for this quality and yield class. Name mapping is not a licence to use a 2008 table or a 2008 certificate as if it were 2018/2025.
S355J0H or S355J2H EN 10219-1 European cold-formed hollow-section grades often compared with Q355B, with 0 °C or −20 °C impact in the J0 or J2 condition. EN 10219 chemistry, impact temperature and size lists are not GB/T documents. Dual certification has to be demonstrated.
ASTM A500 Grade C ASTM A500/A500M A frequent US HSS comparison at a 50 ksi yield class. A500 figures and AISC designations are a different system. A 6728/1591 certificate is not an A500 certificate.

Sourcing GB/T 1591 Q355B Steel Hollow Sections from SHH STEEL

SHH STEEL reviews the ordered quality, delivery condition, 6728-2025 size and wall, CEV if it is a purchase condition, length and any galvanizing requirement before quoting. Send the designation or the measured sides and thickness, the length, and the certificate wording you need. Sizes that exist in the 2025 standard but are not in this verified subset can still be discussed against the official table on the contract.

Q355B Hollow Section FAQs

Does Table 25 replace GB/T 1591 for a Q355B hollow section?
No. Table 25 is the 2025 product yield-class table for the cold-formed section (class 355: 355 MPa yield, 470–680 MPa tensile). Chemistry, CEV, thickness-dependent yield and the 34 J impact figure remain GB/T 1591-2018 subjects. Both documents apply when both are named.
Why is 470–680 MPa not the same as 470–630 MPa?
470–680 MPa is the Table 25 class 355 tensile range in GB/T 6728-2025. 470–630 MPa is the GB/T 1591 Table 7 band for t ≤ 100 mm. They come from different standards and must not be swapped or averaged.
Is Q355B the same as the old Q345B name?
Q355B is the 2018 designation that maps from the former Q345B name for this quality and yield class. That mapping does not authorise a 2008 size or chemistry table, or a 2008 certificate, on a 2018/2025 order.
Are these size tables complete?
No. They are a formula-checked subset of GB/T 6728-2025 Tables 1–3, not every published row. Unverified OCR rows were left out rather than guessed, including rectangular pages that did not yield typographical, area-matching sizes.
Can the Q235B impact inspection waiver be used on Q355B?
No. The under-25 mm inspection waiver is a GB/T 700 Q235B rule. For Q355B, when impact applies, GB/T 1591 7.2.2 and Table 11 (34 J longitudinal at +20 °C) govern. Under 6728-2025, impact of sections 6 mm and thicker is optional by agreement and then follows the material standard.

Conclusion

Order Q355B hollow sections to GB/T 1591-2018 and GB/T 6728-2025 together, and keep Table 25 class 355 (470–680 MPa) distinct from the 470–630 MPa band in GB/T 1591. The size list on this page is a verified common subset of the 2025 tables, not a complete recitation. SHH STEEL will check quality, CEV, shape, wall and certificate wording against the ordered editions before quoting.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X