GB/T 1299 5CrNiMo Tool Steel Plate | GB/T 1299 Tool Steel - SHH STEEL

GB/T 1299 5CrNiMo Tool Steel Plate

GB/T 1299 5CrNiMo is a chromium-nickel-molybdenum hot-work die steel for hot-work die blanks, forming dies and supported tooling components. This page uses the finalized historical alloy tool steel edition, not an unverified current chemistry table. Plate enquiries need an explicit product form agreement because the cited specification principally covers bar and flat stock. Delivery condition, specimen hardening response and finished tool requirements remain separate acceptance matters. SHH STEEL produces and exports 5CrNiMo tooling stock against the agreed edition, form and inspection requirements.
Equivalent Grades:
Country differences require full-source review; no automatic equivalent.
Heat Treatment
Annealed.
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why choose Us
Our Service
Conclusion

What is GB/T 1299 5CrNiMo tooling plate?

GB/T 1299 5CrNiMo Tool Steel Plate identifies formal grade 5CrNiMo, unified numeric code T20103, Table 1 row 4-2 of GB/T 1299-2000. Its nickel window and negotiated molybdenum provision belong to this grade only; a historical L6 association does not supply an unprinted Chinese specimen-hardness minimum.

The technical basis is GB/T 1299-2000 with its published amendment. Grade chemistry is discussed separately from the product-form acceptance agreed for plate or flat-stock supply.

The 2000 scope covers hot-rolled, forged, cold-drawn and bright bars; its chemistry also applies to ingots, billets and products. Hot-rolled and forged flat bars are addressed separately in the dimensional clauses. A commercial plate enquiry therefore needs a stated flat-bar or independently agreed plate acceptance basis: the bar specimen response is not an arbitrary plate-thickness guarantee. [S1 §1, §4]

SHH STEEL produces and exports 5CrNiMo tooling stock to an agreed specification and documented inspection basis. The existing GB/T 1299 hub is a navigation reference, not a new grade classification.

For plate supply, use this historical grade chemistry together with an expressly agreed product and inspection specification; bar and flat-steel provisions do not automatically establish rolled-plate conformity.

Material specification for 5CrNiMo

Item Historical source / qualification
Grade / edition 5CrNiMo; GB/T 1299-2000, Table 1 row 4-2
Unified code T20103; code for this grade, not a separate grade
Source family Hot-work die steel
Default delivery Annealed under §5.2; do not infer prehardened delivery
Delivery hardness 197–241 HBW 10/3000; Table 3
Specimen response No HRC minimum printed; §5.4.3 excludes hot-work specimen-hardness inspection
Form Bar/flat-bar requirements are not automatic rolled-plate acceptance
Edition status Historical 2000 basis; not complete current 2025 requirements

Cast-analysis composition of 5CrNiMo

Table 1 cast-analysis requirements, mass percent, with Amendment No. 1 allocating Ni 1.40–1.80 % only to 5CrNiMo. This is deliberate alloy nickel, not a new grade or residual-nickel guarantee. [S1, S6]

Element / residual condition Mass %
Carbon (C) 0.50–0.60
Silicon (Si) ≤0.40
Manganese (Mn) 0.50–0.80
Phosphorus (P) ≤0.030
Sulfur (S) ≤0.030
Chromium (Cr) 0.50–0.80
Molybdenum (Mo) 0.15–0.30
Nickel (Ni) 1.40–1.80
Residual copper (Cu) ≤0.30

Clause 5.1.2 expressly permits, by supplier/purchaser agreement, molybdenum content below 0.20 %. The ordinary Table 1 Mo window remains 0.15–0.30 %; the clause is not converted into a new lower limit, an unlimited Mo waiver, or a different grade. Product-analysis deviations remain the referenced GB/T 222-1984 Table 2 basis.

Specify intentional alloy nickel and residual-element acceptance separately in the purchase specification. Identify cast analysis versus product analysis on the inspection documents and define the applicable product-analysis deviation basis.

Delivery hardness and specimen response for 5CrNiMo

Delivery hardness and specimen-test response apply in the historical source’s stated product and test context. For plate orders, agree the supplied condition, hardness, dimensions, surface quality, decarburization, sampling and inspection separately; specimen results do not guarantee full-section plate or finished-tool hardness.

Table 3 gives annealed delivery hardness 197–241 HBW 10/3000, a range, not a maximum-only limit. The specimen-HRC column is blank for this hot-work row. Clause 5.4.3 expressly states that hot-work die steels are not inspected for specimen quench hardness. No HRC minimum, finished-tool hardness or tensile strength is invented. [S1 printed pp6–7]

Delivery condition and reference hardening test for 5CrNiMo

Annealed delivery is the §5.2 default. Table 3 nevertheless prints a reference hardening range of 830–860 °C with oil cooling for this hot-work row; its HRC cell is blank and §5.4.3 excludes specimen-hardness inspection. Do not infer a hardness acceptance from that temperature entry. No row-specific preheat, temper or production soak is printed. [S1 printed p7]

Welding and surface processing 5CrNiMo

5CrNiMo is tooling stock rather than a generic weldable structural plate. Repair welding needs a qualified procedure addressing carbon/alloy content, prior treatment, restraint, crack risk and subsequent inspection. No unsupported preheat, interpass or post-weld temperature is prescribed.

Thermal cutting, grinding and EDM may alter the working surface. Specify cleanup allowance, edge preparation and inspection of critical tool features; a conforming heat analysis alone does not prove an undamaged finished edge.

Flat/plate dimensions and surface acceptance

Clauses 4.1–4.5 refer the respective hot-rolled, forged, cold-drawn and flat-bar forms to their named dimensional standards and agreed groups. Clause 4.6 sends other materials/products to the relevant national/industry standard, or supplier/purchaser agreement where none applies. Do not relabel a bar tolerance as a plate tolerance. [S1 printed p2]

Flat-steel surface quality is agreed under §5.8.4. Flat-steel decarburization, and round/side-size stock above 150 mm, are agreement matters under §5.6.1; the round/side-size formulas in Table 5 are not plate-thickness guarantees. Agree flatness, surface, edge quality and cleanup material for the actual form. No unverified plate capacity range or mill stock availability is asserted.

Applications and selection limits for 5CrNiMo

Qualitative engineering selection for 5CrNiMo can include hot-work die blanks, forming dies and supported tooling components. Its nickel window and negotiated molybdenum provision belong to this grade only; a historical L6 association does not supply an unprinted Chinese specimen-hardness minimum. These application suggestions do not add normative tool-life, impact-energy or load ratings to the specification.

Match working-edge support, wear mechanism, section, processing route and inspection to the actual tool. No specimen HRC minimum is specified for this grade in the cited historical row. Its absence does not imply a finished-tool or full-section plate hardness guarantee; any additional response test and acceptance criterion must be stated in the order.

Compare 5CrNiMo with three live own product pages

These three own product pages were verified live for this batch. They are explicit material-selection contrasts, not unpublished drafts or asserted equivalents.

Published own product Material distinction Acceptance distinction Selection caution
JIS G4401 SK105 Tool Steel Plate Carbon tool steel contrast, not a certified counterpart Published JIS product/condition basis; do not import this GB bar test Review carbon, alloying, supplied condition and actual plate scope
JIS G4401 SK120 Tool Steel Plate Carbon tool steel contrast, not a certified counterpart Published JIS product/condition basis; do not import this GB bar test Review carbon, alloying, supplied condition and actual plate scope
ASTM A829 4140 Alloy Steel Plate Engineering alloy plate contrast Chemistry-ordered plate, not this tool-steel specimen acceptance A readily compared plate page is not substitution approval

Country differences and substitution limits for 5CrNiMo

Country comparisons below deliberately distinguish actual source windows from unsupported trade-name substitutions. A comparison entry is not an automatic equivalent. [S1 Annex B; S4; S5]

Country / system Designation and verified difference Substitution limit
China 5CrNiMo, GB/T 1299-2000; cast C 0.50–0.60 %, delivery 197–241 HBW 10/3000 Current GB/T 1299-2025 requires separate full-table verification
Japan JIS G4401:2009 SK105 carbon-tool contrast: C 1.00–1.10 and Si 0.10–0.35 %, versus GB C 0.50–0.60 and Si ≤0.40 %. No corresponding JIS alloy grade established here; JIS decarburization HV is not this hardening-test HRC
United States GB2000 informative Annex B associates this row with ASTM A681-1994 L6. Separately verified A681-08 L6 C0.65–0.75 and Ni1.25–2.00 % differ from GB C0.50–0.60 and Ni1.40–1.80 %. No ASTM hardness minimum or specimen cycle is transferred. Informative association or selected window overlap is not identical chemistry, form, delivery condition or specimen acceptance
Germany / ISO-based procurement No exact DIN/EN/ISO counterpart established by the cited GB table; specify the actual national adoption and edition Do not inherit an ISO steel number or a later national chemistry window from a commercial cross-reference

Why choose SHH STEEL for 5CrNiMo

SHH STEEL produces and exports 5CrNiMo tooling stock with an explicit edition and product-form agreement. We distinguish cast chemistry, delivery hardness and reference specimen response rather than advertising a universal final-tool hardness.

  • Review the actual plate or flat manufacturing and acceptance basis.
  • Maintain heat identification and agreed inspection reporting.
  • Review substitutions against complete source editions.
  • Agree any optional condition or supplementary testing before confirmation.

Inspection and enquiry planning for 5CrNiMo

Enquiry item Required detail
Grade and standard 5CrNiMo; state the governing edition rather than only GB/T 1299
Product form Flat bar or independently specified plate; manufacturing route and finish
Dimensions Thickness × width × length, quantity and machining allowance
Condition and hardness Annealed; 197–241 HBW 10/3000 on the historical basis, or expressly agreed different requirement
Test verification Cast/product analysis, delivery hardness, specimen-test guarantee/report requirement and sampling basis
Inspection Certificate type, heat traceability, surface/decarburization and any additional agreed quality checks
Final tooling / logistics Duty, final-tool acceptance, treatment responsibility, packing, destination and timing

Requested sizes and processes are reviewed for feasibility; this draft is not an unconditional stock or production-performance commitment.

Agree the applicable chemistry, condition and inspection criteria before supply. Treatment responsibility and final-tool acceptance should be defined for the actual application rather than inferred from a trade-name comparison.

Request a quotation

Request a quotation for GB/T 1299 5CrNiMo tooling plate or flat stock by email. State the governing edition, actual product form and manufacturing route, quantity, dimensions, drawing, finish and machining allowance. For ordinary rolled plate, identify the separate applicable plate acceptance basis rather than relying only on the historical bar specification.

Confirm the supplied condition and hardness acceptance: this historical annealed row gives 197–241 HBW 10/3000. Specify cast versus product analysis, inspection-document type, traceability, sampling and whether a hardening-test report or an agreed supplier conformity guarantee is required. No specimen HRC minimum is printed for this hot-work row; §5.4.3 excludes that inspection. Define final tooling acceptance separately.

Include surface and decarburization acceptance, flatness and dimensional tolerances, critical edge preparation, cutting requirements and any supplementary NDT or microstructure checks with agreed methods and criteria. Describe tool duty, final properties and production-treatment responsibility separately. For a proposed substitute, attach its complete governing specification and drawing for review. Provide packing, delivery destination and target timing; feasibility and any optional condition are confirmed before acceptance.

Email only: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response