GB/T 1299 3Cr2Mo Tool Steel Plate
What is GB/T 1299 3Cr2Mo tooling plate?
GB/T 1299 3Cr2Mo Tool Steel Plate identifies formal grade 3Cr2Mo, unified numeric code T22020, Table 1 row 6-1 of GB/T 1299-2000. The historical table does not give a numerical delivery hardness or specimen cycle for this row; prehardened supply is an order option rather than an invented standard hardness band.
This is an edition-specific historical technical draft. The officially current standard is GB/T 1299-2025, effective 2026-05-01; its complete chemistry tables have not been verified for this article. Do not treat the historical values below as a current-edition certificate. The 2014 edition had already replaced the earlier GB/T 1298-2008 carbon-tool standard; the 2025 edition also absorbs GB/T 33811-2017 plate requirements. Neither later merger expands the old 2000 bar/flat acceptance scope by implication. [S1, S2]
The 2000 scope covers hot-rolled, forged, cold-drawn and bright bars; its chemistry also applies to ingots, billets and products. Hot-rolled and forged flat bars are addressed separately in the dimensional clauses. A commercial plate enquiry therefore needs a stated flat-bar or independently agreed plate acceptance basis: the bar specimen response is not an arbitrary plate-thickness guarantee. [S1 §1, §4]
SHH STEEL produces and exports 3Cr2Mo tooling stock to an agreed specification and documented inspection basis. The existing GB/T 1299 hub is a navigation reference, not a new grade classification.
For plate supply, use this historical grade chemistry together with an expressly agreed product and inspection specification; bar and flat-steel provisions do not automatically establish rolled-plate conformity.
Material specification for 3Cr2Mo
| Item | Source-qualified requirement |
|---|---|
| Grade / edition | 3Cr2Mo; GB/T1299-2000 Table1 6-1 |
| Code | T22020 |
| Family | Plastic mould steel |
| Delivery condition | Annealed under §5.2; prehardened when expressly ordered |
| Delivery hardness | No numerical Table3 entry; specify applicable condition/order basis |
| Specimen response | No numerical Table3 entry or cycle; none invented |
| Form | Historical bar/flat provisions do not automatically establish general plate conformity |
Cast-analysis composition of 3Cr2Mo
Table 1 gives melting/cast-analysis requirements, mass percent. Residual copper and combined copper-plus-nickel requirements are added from §5.1.3, not omitted because their cells are outside the named alloy row. [S1 printed pp4–5]
| Element / residual condition | Mass % |
|---|---|
| Carbon (C) | 0.28–0.40 |
| Silicon (Si) | 0.20–0.80 |
| Manganese (Mn) | 0.60–1.00 |
| Phosphorus (P) | ≤0.030 |
| Sulfur (S) | ≤0.030 |
| Chromium (Cr) | 1.40–2.00 |
| Molybdenum (Mo) | 0.30–0.55 |
| Residual copper (Cu) | ≤0.30 |
| Residual Cu + Ni | ≤0.55 |
Unquoted alloy cells are not zero-residual guarantees. Product-analysis permissible deviations are referred by §5.1.4 to GB/T 222-1984 Table 2; no unverified numeric deviation is added to these cast-analysis limits. A certificate must identify cast versus product analysis. The special reduced-molybdenum agreement in §5.1.2 applies to 5CrNiMo, not this grade.
AmendmentNo.1 item4 assigns Ni0.85–1.15 only to3Cr2MnNiMo, not this3Cr2Mo row. No mandatory nickel range is copied into this grade. [S6]
Delivery hardness and specimen response for 3Cr2Mo
Delivery hardness and specimen-test response apply in the historical source’s stated product and test context. For plate orders, agree the supplied condition, hardness, dimensions, surface quality, decarburization, sampling and inspection separately; specimen results do not guarantee full-section plate or finished-tool hardness.
Table3 does not specify a numerical deliveryHBW entry for this grade. Do not invent a prehardened hardness band, a maximum copied from another mould grade or a conversion from specimenHRC. The supplied condition and acceptance must be stated in the order. [S1 §5.2/Table3]
Delivery condition for 3Cr2Mo
Annealed under §5.2; prehardened when expressly ordered. The Table3 row has no hardening cycle, quench medium, HRC minimum or numerical delivery hardness for this plastic-mould grade. None is inferred from the informative foreign association. Production treatment and supplied-condition acceptance require agreement. [S1 §5.2/Table3]
Welding and surface processing 3Cr2Mo
3Cr2Mo is tooling stock rather than a generic weldable structural plate. Repair welding needs a qualified procedure addressing carbon/alloy content, prior treatment, restraint, crack risk and subsequent inspection. No unsupported preheat, interpass or post-weld temperature is prescribed.
Thermal cutting, grinding and EDM may alter the working surface. Specify cleanup allowance, edge preparation and inspection of critical tool features; a conforming heat analysis alone does not prove an undamaged finished edge.
Flat/plate dimensions and surface acceptance
Clauses 4.1–4.5 refer the respective hot-rolled, forged, cold-drawn and flat-bar forms to their named dimensional standards and agreed groups. Clause 4.6 sends other materials/products to the relevant national/industry standard, or supplier/purchaser agreement where none applies. Do not relabel a bar tolerance as a plate tolerance. [S1 printed p2]
Flat-steel surface quality is agreed under §5.8.4. Flat-steel decarburization, and round/side-size stock above 150 mm, are agreement matters under §5.6.1; the round/side-size formulas in Table 5 are not plate-thickness guarantees. Agree flatness, surface, edge quality and cleanup material for the actual form. No unverified plate capacity range or mill stock availability is asserted.
Applications and selection limits for 3Cr2Mo
Qualitative engineering selection for 3Cr2Mo can include plastic mould blanks, mould inserts and supported tooling components. The historical table does not give a numerical delivery hardness or specimen cycle for this row; prehardened supply is an order option rather than an invented standard hardness band. These application suggestions do not add normative tool-life, impact-energy or load ratings to the specification.
Match working-edge support, wear mechanism, section, processing route and inspection to the actual tool. No specimen HRC minimum is specified for this grade in the cited historical row. Its absence does not imply a finished-tool or full-section plate hardness guarantee; any additional response test and acceptance criterion must be stated in the order.
Compare 3Cr2Mo with three live own product pages
These three own product pages were verified live for this batch. They are explicit material-selection contrasts, not unpublished drafts or asserted equivalents.
| Published own product | Material distinction | Acceptance distinction | Selection caution |
|---|---|---|---|
| JIS G4401 SK105 Tool Steel Plate | Carbon tool steel contrast, not a certified counterpart | Published JIS product/condition basis; do not import this GB bar test | Review carbon, alloying, supplied condition and actual plate scope |
| JIS G4401 SK120 Tool Steel Plate | Carbon tool steel contrast, not a certified counterpart | Published JIS product/condition basis; do not import this GB bar test | Review carbon, alloying, supplied condition and actual plate scope |
| ASTM A829 4140 Alloy Steel Plate | Engineering alloy plate contrast | Chemistry-ordered plate, not this tool-steel specimen acceptance | A readily compared plate page is not substitution approval |
Country differences and substitution limits for 3Cr2Mo
Country comparisons below deliberately distinguish actual source windows from unsupported trade-name substitutions. A comparison entry is not an automatic equivalent. [S1 Annex B; S4; S5]
| Country / system | Designation and verified difference | Substitution limit |
|---|---|---|
| China | 3Cr2Mo, GB/T 1299-2000; cast C 0.28–0.40 %, no numerical delivery-hardness entry in Table3 | Current GB/T 1299-2025 requires separate full-table verification |
| Japan | JIS G4401:2009 SK105 carbon-tool contrast: C 1.00–1.10 and Si 0.10–0.35 %, versus GB C 0.28–0.40 and Si 0.20–0.80 %. | No corresponding JIS alloy grade established here; JIS decarburization HV is not GB delivery hardness or an invented blank-cell HRC |
| United States | GBAnnexB informatively associates A681-1994 P20. Actual A681-08 P20 C0.28–0.40,Cr1.40–2.00,Mo0.30–0.55 % match these selected GB windows; this does not supply a missing GB delivery-hardness band or test cycle. | Informative association or selected window overlap is not identical chemistry, form, delivery condition or specimen acceptance |
| Germany / ISO-based procurement | No exact DIN/EN/ISO counterpart established by the cited GB table; specify the actual national adoption and edition | Do not inherit an ISO steel number or a later national chemistry window from a commercial cross-reference |
Why choose SHH STEEL for 3Cr2Mo
SHH STEEL produces and exports 3Cr2Mo tooling stock with an explicit edition and product-form agreement. We distinguish cast chemistry, delivery hardness and reference specimen response rather than advertising a universal final-tool hardness.
- Review the actual plate or flat manufacturing and acceptance basis.
- Maintain heat identification and agreed inspection reporting.
- Review substitutions against complete source editions.
- Agree any optional condition or supplementary testing before confirmation.
Inspection and enquiry planning for 3Cr2Mo
| Enquiry item | Required detail |
|---|---|
| Grade and standard | 3Cr2Mo; state the governing edition rather than only GB/T 1299 |
| Product form | Flat bar or independently specified plate; manufacturing route and finish |
| Dimensions | Thickness × width × length, quantity and machining allowance |
| Condition and hardness | State annealed or agreed prehardened condition; numerical hardness acceptance must be specified in the order |
| Test verification | Cast/product analysis, delivery hardness, specimen-test guarantee/report requirement and sampling basis |
| Inspection | Certificate type, heat traceability, surface/decarburization and any additional agreed quality checks |
| Final tooling / logistics | Duty, final-tool acceptance, treatment responsibility, packing, destination and timing |
Requested sizes and processes are reviewed for feasibility; this draft is not an unconditional stock or production-performance commitment.
Request a quotation
Request a quotation for GB/T 1299 3Cr2Mo tooling plate or flat stock by email. State the governing edition, actual product form and manufacturing route, quantity, dimensions, drawing, finish and machining allowance. For ordinary rolled plate, identify the separate applicable plate acceptance basis rather than relying only on the historical bar specification.
Confirm the supplied condition and hardness acceptance: Table3 gives no numerical delivery-hardness entry for this grade; state the ordered condition and acceptance explicitly. Specify cast versus product analysis, inspection-document type, traceability, sampling and whether a hardening-test report or an agreed supplier conformity guarantee is required. No specimen-HRC minimum or cycle is printed for this mould row; define supplied-condition and final-tool acceptance separately.
Include surface and decarburization acceptance, flatness and dimensional tolerances, critical edge preparation, cutting requirements and any supplementary NDT or microstructure checks with agreed methods and criteria. Describe tool duty, final properties and production-treatment responsibility separately. For a proposed substitute, attach its complete governing specification and drawing for review. Provide packing, delivery destination and target timing; feasibility and any optional condition are confirmed before acceptance.
Email only: admin@steelspecs.com