GB/T 1299 3Cr2MnNiMo Tool Steel Plate | GB/T 1299 Tool Steel - SHH STEEL

GB/T 1299 3Cr2MnNiMo Tool Steel Plate

GB/T 1299 3Cr2MnNiMo is a chromium-manganese-nickel-molybdenum plastic mould steel for plastic mould blanks, mould inserts and supported tooling components. This page uses the finalized historical alloy tool steel edition, not an unverified current chemistry table. Plate enquiries need an explicit product form agreement because the cited specification principally covers bar and flat stock. Delivery condition, specimen hardening response and finished tool requirements remain separate acceptance matters. SHH STEEL produces and exports 3Cr2MnNiMo tooling stock against the agreed edition, form and inspection requirements.
Equivalent Grades:
Country differences require full-source review; no automatic equivalent.
Heat Treatment
Annealed; prehardened when specified.
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why choose Us
Our Service
Conclusion

What is GB/T 1299 3Cr2MnNiMo tooling plate?

GB/T 1299 3Cr2MnNiMo Tool Steel Plate identifies formal grade 3Cr2MnNiMo, unified numeric code T22024, Table 1 row 6-2 of GB/T 1299-2000. Amendment No.1 assigns the nickel window only to this mould grade; the informative trade association does not create an additional formal ASTM grade or a guaranteed prehardened hardness.

The technical basis is GB/T 1299-2000 with its published amendment. Grade chemistry is discussed separately from the product-form acceptance agreed for plate or flat-stock supply.

The 2000 scope covers hot-rolled, forged, cold-drawn and bright bars; its chemistry also applies to ingots, billets and products. Hot-rolled and forged flat bars are addressed separately in the dimensional clauses. A commercial plate enquiry therefore needs a stated flat-bar or independently agreed plate acceptance basis: the bar specimen response is not an arbitrary plate-thickness guarantee. [S1 §1, §4]

SHH STEEL produces and exports 3Cr2MnNiMo tooling stock to an agreed specification and documented inspection basis. The existing GB/T 1299 hub is a navigation reference, not a new grade classification.

For plate supply, use this historical grade chemistry together with an expressly agreed product and inspection specification; bar and flat-steel provisions do not automatically establish rolled-plate conformity.

Material specification for 3Cr2MnNiMo

Item Source-qualified requirement
Grade / edition 3Cr2MnNiMo; GB/T1299-2000 Table1 6-2
Code T22024
Family Plastic mould steel
Delivery condition Annealed under §5.2; prehardened when expressly ordered
Delivery hardness No numerical Table3 entry; specify applicable condition/order basis
Specimen response No numerical Table3 entry or cycle; none invented
Form Historical bar/flat provisions do not automatically establish general plate conformity

Cast-analysis composition of 3Cr2MnNiMo

Table1 cast-analysis chemistry, mass percent, with AmendmentNo.1 item4 assigning Ni0.85–1.15 exclusively to this row. [S1,S6]

Element / condition Mass%
Carbon (C) 0.32–0.40
Silicon (Si) 0.20–0.40
Manganese (Mn) 1.10–1.50
Phosphorus (P) ≤0.030
Sulfur (S) ≤0.030
Chromium (Cr) 1.70–2.00
Molybdenum (Mo) 0.25–0.40
Nickel (Ni) 0.85–1.15
Residual copper (Cu) ≤0.30

Specify intentional alloy nickel and residual-element acceptance separately in the purchase specification. Identify cast analysis versus product analysis on the inspection documents and define the applicable product-analysis deviation basis.

Delivery hardness and specimen response for 3Cr2MnNiMo

Delivery hardness and specimen-test response apply in the historical source’s stated product and test context. For plate orders, agree the supplied condition, hardness, dimensions, surface quality, decarburization, sampling and inspection separately; specimen results do not guarantee full-section plate or finished-tool hardness.

Table3 does not specify a numerical deliveryHBW entry for this grade. Do not invent a prehardened hardness band, a maximum copied from another mould grade or a conversion from specimenHRC. The supplied condition and acceptance must be stated in the order. [S1 §5.2/Table3]

Delivery condition for 3Cr2MnNiMo

Annealed under §5.2; prehardened when expressly ordered. The Table3 row has no hardening cycle, quench medium, HRC minimum or numerical delivery hardness for this plastic-mould grade. None is inferred from the informative foreign association. Production treatment and supplied-condition acceptance require agreement. [S1 §5.2/Table3]

Welding and surface processing 3Cr2MnNiMo

3Cr2MnNiMo is tooling stock rather than a generic weldable structural plate. Repair welding needs a qualified procedure addressing carbon/alloy content, prior treatment, restraint, crack risk and subsequent inspection. No unsupported preheat, interpass or post-weld temperature is prescribed.

Thermal cutting, grinding and EDM may alter the working surface. Specify cleanup allowance, edge preparation and inspection of critical tool features; a conforming heat analysis alone does not prove an undamaged finished edge.

Flat/plate dimensions and surface acceptance

Clauses 4.1–4.5 refer the respective hot-rolled, forged, cold-drawn and flat-bar forms to their named dimensional standards and agreed groups. Clause 4.6 sends other materials/products to the relevant national/industry standard, or supplier/purchaser agreement where none applies. Do not relabel a bar tolerance as a plate tolerance. [S1 printed p2]

Flat-steel surface quality is agreed under §5.8.4. Flat-steel decarburization, and round/side-size stock above 150 mm, are agreement matters under §5.6.1; the round/side-size formulas in Table 5 are not plate-thickness guarantees. Agree flatness, surface, edge quality and cleanup material for the actual form. No unverified plate capacity range or mill stock availability is asserted.

Applications and selection limits for 3Cr2MnNiMo

Qualitative engineering selection for 3Cr2MnNiMo can include plastic mould blanks, mould inserts and supported tooling components. Amendment No.1 assigns the nickel window only to this mould grade; the informative trade association does not create an additional formal ASTM grade or a guaranteed prehardened hardness. These application suggestions do not add normative tool-life, impact-energy or load ratings to the specification.

Match working-edge support, wear mechanism, section, processing route and inspection to the actual tool. No specimen HRC minimum is specified for this grade in the cited historical row. Its absence does not imply a finished-tool or full-section plate hardness guarantee; any additional response test and acceptance criterion must be stated in the order.

Compare 3Cr2MnNiMo with three live own product pages

These three own product pages were verified live for this batch. They are explicit material-selection contrasts, not unpublished drafts or asserted equivalents.

Published own product Material distinction Acceptance distinction Selection caution
JIS G4401 SK105 Tool Steel Plate Carbon tool steel contrast, not a certified counterpart Published JIS product/condition basis; do not import this GB bar test Review carbon, alloying, supplied condition and actual plate scope
JIS G4401 SK120 Tool Steel Plate Carbon tool steel contrast, not a certified counterpart Published JIS product/condition basis; do not import this GB bar test Review carbon, alloying, supplied condition and actual plate scope
ASTM A829 4140 Alloy Steel Plate Engineering alloy plate contrast Chemistry-ordered plate, not this tool-steel specimen acceptance A readily compared plate page is not substitution approval

Country differences and substitution limits for 3Cr2MnNiMo

Country comparisons below deliberately distinguish actual source windows from unsupported trade-name substitutions. A comparison entry is not an automatic equivalent. [S1 Annex B; S4; S5]

Country / system Designation and verified difference Substitution limit
China 3Cr2MnNiMo, GB/T 1299-2000; cast C 0.32–0.40 %, no numerical delivery-hardness entry in Table3 Current GB/T 1299-2025 requires separate full-table verification
Japan JIS G4401:2009 SK105 carbon-tool contrast: C 1.00–1.10 and Si 0.10–0.35 %, versus GB C 0.32–0.40 and Si 0.20–0.40 %. No corresponding JIS alloy grade established here; JIS decarburization HV is not GB delivery hardness or an invented blank-cell HRC
United States GBAnnexB prints 718 in the American comparison column, but no formal A681-08 type718 is established. Actual A681-08 P20 is only a contrast: Mn0.60–1.00,Mo0.30–0.55 % versus GB Mn1.10–1.50,Mo0.25–0.40 %, with GB Ni0.85–1.15 % explicitly required. No automatic P20/718 alias. Informative association or selected window overlap is not identical chemistry, form, delivery condition or specimen acceptance
Germany / ISO-based procurement No exact DIN/EN/ISO counterpart established by the cited GB table; specify the actual national adoption and edition Do not inherit an ISO steel number or a later national chemistry window from a commercial cross-reference

Why choose SHH STEEL for 3Cr2MnNiMo

SHH STEEL produces and exports 3Cr2MnNiMo tooling stock with an explicit edition and product-form agreement. We distinguish cast chemistry, delivery hardness and reference specimen response rather than advertising a universal final-tool hardness.

  • Review the actual plate or flat manufacturing and acceptance basis.
  • Maintain heat identification and agreed inspection reporting.
  • Review substitutions against complete source editions.
  • Agree any optional condition or supplementary testing before confirmation.

Inspection and enquiry planning for 3Cr2MnNiMo

Enquiry item Required detail
Grade and standard 3Cr2MnNiMo; state the governing edition rather than only GB/T 1299
Product form Flat bar or independently specified plate; manufacturing route and finish
Dimensions Thickness × width × length, quantity and machining allowance
Condition and hardness State annealed or agreed prehardened condition; numerical hardness acceptance must be specified in the order
Test verification Cast/product analysis, delivery hardness, specimen-test guarantee/report requirement and sampling basis
Inspection Certificate type, heat traceability, surface/decarburization and any additional agreed quality checks
Final tooling / logistics Duty, final-tool acceptance, treatment responsibility, packing, destination and timing

Requested sizes and processes are reviewed for feasibility; this draft is not an unconditional stock or production-performance commitment.

Agree the applicable chemistry, condition and inspection criteria before supply. Treatment responsibility and final-tool acceptance should be defined for the actual application rather than inferred from a trade-name comparison.

Request a quotation

Request a quotation for GB/T 1299 3Cr2MnNiMo tooling plate or flat stock by email. State the governing edition, actual product form and manufacturing route, quantity, dimensions, drawing, finish and machining allowance. For ordinary rolled plate, identify the separate applicable plate acceptance basis rather than relying only on the historical bar specification.

Confirm the supplied condition and hardness acceptance: Table3 gives no numerical delivery-hardness entry for this grade; state the ordered condition and acceptance explicitly. Specify cast versus product analysis, inspection-document type, traceability, sampling and whether a hardening-test report or an agreed supplier conformity guarantee is required. No specimen-HRC minimum or cycle is printed for this mould row; define supplied-condition and final-tool acceptance separately.

Include surface and decarburization acceptance, flatness and dimensional tolerances, critical edge preparation, cutting requirements and any supplementary NDT or microstructure checks with agreed methods and criteria. Describe tool duty, final properties and production-treatment responsibility separately. For a proposed substitute, attach its complete governing specification and drawing for review. Provide packing, delivery destination and target timing; feasibility and any optional condition are confirmed before acceptance.

Email only: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X