EN 10219-1 S355J2H Steel Hollow Sections (HSS) | EN 10219-1 Steel Hollow Sections - SHH STEEL

EN 10219-1 S355J2H Steel Hollow Sections (HSS)

EN 10219-1 S355J2H steel hollow sections are cold-formed welded structural hollow sections in steel 1.0576. The 16 mm and under band is 355 MPa minimum yield, with 27 J impact at −20 °C. The size tables are common mill-programme sizes, not the full EN 10219-2 list, with masses from the EN 10219-2 formulae.
Keywords
EN 10219-1 S355J2H, S355J2H SHS, S355J2H RHS, S355J2H CHS, cold formed hollow section
Equivalent Grades:
Near-equivalents only, not automatic substitutes.
Share:
General Description
Material Specification
Available Sizes of EN 10219-1 S355J2H Steel Hollow Sections
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Sourcing EN 10219-1 S355J2H Steel Hollow Sections from SHH STEEL
FAQ
Conclusion

What are EN 10219-1 S355J2H Steel Hollow Sections?

EN 10219-1 S355J2H is a killed, fine-grain, cold-formed welded structural hollow section in steel number 1.0576. The J2 quality requires a 27 J Charpy result at −20 °C, which is a colder verification than S355JRH or S355J0H. In the thickness band most often supplied, the specified minimum yield is 355 MPa. The product is a cold-formed hollow section under EN 10219, not a hot-finished hollow section under EN 10210, and the two families must not be mixed on the same certificate.

Square, rectangular and circular sections are all part of the same grade. Corner-radius rules, and therefore calculated mass, follow EN 10219-2 rather than EN 10210-2.

Material, Manufacture and Scope for EN 10219-1 S355J2H Hollow Sections

EN 10219-1 sets the technical delivery conditions for cold-formed welded structural hollow sections of non-alloy and fine-grain steels. EN 10219-2 sets the dimensions, tolerances and sectional properties, including the mass formulae used on this page. S355J2H is supplied fully killed. The values quoted below follow EN 10219-1 as restated in manufacturer declarations for Hybox 355 S355J2H (including the Tata Steel UK Declaration of Performance) and in consistent technical data for steel 1.0576. The edition named on the order governs.

Typical manufacture is continuous cold forming from flat product with a longitudinal electric-resistance weld. This page does not treat the product as EN 10210-1 S355J2H, as ASTM A500 Grade C, or as a Chinese Q355 hollow section to GB/T 6728. Those documents use different process routes, different tolerance sets and, in some cases, different tensile ranges.

EN 10219-1 S355J2H Common Sizes: Square, Rectangular and Circular (Hybox 355 Programme)

The tables below list common cold-formed sizes from the Tata Steel Hybox 355 programme for EN 10219 S355J2H. They are a mill programme, not the complete EN 10219-2 standard list, and they are not a stock list. Masses are calculated from the EN 10219-2 Annex B formulae (see the notes under each table) and are shown to three significant figures. Each row was cross-checked against the mass published in the Hybox 355 technical guide, which states that masses are according to EN 10219.

Common square hollow sections (SHS)

Cold-formed square sizes in the Hybox 355 S355J2H programme. 96 common sizes in this table.

Swipe horizontally to view all dimensions.

Size H × B (mm) Thickness T (mm) Area A (cm²) Mass (kg/m), EN 10219-2 formula Hybox 355 published mass (kg/m)
25 × 25 2 1.74 1.36 1.36
25 × 25 2.5 2.09 1.64 1.64
30 × 30 2 2.14 1.68 1.68
30 × 30 2.5 2.59 2.03 2.03
30 × 30 3 3.01 2.36 2.36
40 × 40 2 2.94 2.31 2.31
40 × 40 2.5 3.59 2.82 2.82
40 × 40 3 4.21 3.3 3.3
40 × 40 4 5.35 4.2 4.2
50 × 50 2.5 4.59 3.6 3.6
50 × 50 3 5.41 4.25 4.25
50 × 50 4 6.95 5.45 5.45
50 × 50 5 8.36 6.56 6.56
60 × 60 3 6.61 5.19 5.19
60 × 60 4 8.55 6.71 6.71
60 × 60 5 10.4 8.13 8.13
60 × 60 6 12 9.45 9.45
70 × 70 3 7.81 6.13 6.13
70 × 70 3.5 8.99 7.06 7.06
70 × 70 4 10.1 7.97 7.97
70 × 70 5 12.4 9.7 9.7
70 × 70 6 14.4 11.3 11.3
80 × 80 3 9.01 7.07 7.07
80 × 80 3.5 10.4 8.16 8.16
80 × 80 4 11.7 9.22 9.22
80 × 80 5 14.4 11.3 11.3
80 × 80 6 16.8 13.2 13.2
90 × 90 3 10.2 8.01 8.01
90 × 90 3.5 11.8 9.26 9.26
90 × 90 4 13.3 10.5 10.5
90 × 90 5 16.4 12.8 12.8
90 × 90 6 19.2 15.1 15.1
100 × 100 3 11.4 8.96 8.96
100 × 100 4 14.9 11.7 11.7
100 × 100 5 18.4 14.4 14.4
100 × 100 6 21.6 17 17
100 × 100 8 27.2 21.4 21.4
120 × 120 3 13.8 10.8 10.8
120 × 120 4 18.1 14.2 14.2
120 × 120 5 22.4 17.5 17.5
120 × 120 6 26.4 20.7 20.7
120 × 120 8 33.6 26.4 26.4
120 × 120 10 40.6 31.8 31.8
140 × 140 4 21.3 16.8 16.8
140 × 140 5 26.4 20.7 20.7
140 × 140 6 31.2 24.5 24.5
140 × 140 8 40 31.4 31.4
140 × 140 10 48.6 38.1 38.1
150 × 150 4 22.9 18 18
150 × 150 5 28.4 22.3 22.3
150 × 150 6 33.6 26.4 26.4
150 × 150 8 43.2 33.9 33.9
150 × 150 10 52.6 41.3 41.3
160 × 160 4 24.5 19.3 19.3
160 × 160 5 30.4 23.8 23.8
160 × 160 6 36 28.3 28.3
160 × 160 8 46.4 36.5 36.5
160 × 160 10 56.6 44.4 44.4
180 × 180 5 34.4 27 27
180 × 180 6 40.8 32.1 32.1
180 × 180 6.3 42.4 33.3 33.3
180 × 180 8 52.8 41.5 41.5
180 × 180 10 64.6 50.7 50.7
180 × 180 12 74.5 58.5 58.5
180 × 180 12.5 77 60.5 60.5
200 × 200 5 38.4 30.1 30.1
200 × 200 6 45.6 35.8 35.8
200 × 200 6.3 47.4 37.2 37.2
200 × 200 8 59.2 46.5 46.5
200 × 200 10 72.6 57 57
200 × 200 12 84.1 66 66
200 × 200 12.5 87 68.3 68.3
250 × 250 6 57.6 45.2 45.2
250 × 250 6.3 60 47.1 47.1
250 × 250 8 75.2 59.1 59.1
250 × 250 10 92.6 72.7 72.7
250 × 250 12 108 84.8 84.8
250 × 250 12.5 112 88 88
300 × 300 6 69.6 54.7 54.7
300 × 300 6.3 72.6 57 57
300 × 300 8 91.2 71.6 71.6
300 × 300 10 113 88.4 88.4
300 × 300 12 132 104 104
300 × 300 12.5 137 108 108
350 × 350 6 81.6 64.1 64.1
350 × 350 6.3 85.2 66.9 66.9
350 × 350 8 107 84.2 84.2
350 × 350 10 133 104 104
350 × 350 12 156 123 123
350 × 350 12.5 162 127 127
400 × 400 6 93.6 73.5 73.5
400 × 400 6.3 97.8 76.8 76.8
400 × 400 8 123 96.7 96.7
400 × 400 10 153 120 120
400 × 400 12 180 141 141
400 × 400 12.5 187 147 147

Common rectangular hollow sections (RHS)

Cold-formed rectangular sizes in the Hybox 355 S355J2H programme. The first dimension is the size as printed in that guide. 137 common sizes in this table.

Swipe horizontally to view all dimensions.

Size H × B (mm) Thickness T (mm) Area A (cm²) Mass (kg/m), EN 10219-2 formula Hybox 355 published mass (kg/m)
50 × 25 2 2.74 2.15 2.15
50 × 25 2.5 3.34 2.62 2.62
50 × 25 3 3.91 3.07 3.07
50 × 30 2 2.94 2.31 2.31
50 × 30 2.5 3.59 2.82 2.82
50 × 30 3 4.21 3.3 3.3
50 × 30 4 5.35 4.2 4.2
60 × 40 2.5 4.59 3.6 3.6
60 × 40 3 5.41 4.25 4.25
60 × 40 4 6.95 5.45 5.45
60 × 40 5 8.36 6.56 6.56
70 × 40 3 6.01 4.72 4.72
70 × 40 4 7.75 6.08 6.08
70 × 40 5 9.36 7.34 7.34
70 × 50 3 6.61 5.19 5.19
70 × 50 4 8.55 6.71 6.71
70 × 50 5 10.4 8.13 8.13
80 × 40 3 6.61 5.19 5.19
80 × 40 4 8.55 6.71 6.71
80 × 40 5 10.4 8.13 8.13
80 × 50 3 7.21 5.66 5.66
80 × 50 4 9.35 7.34 7.34
80 × 50 5 11.4 8.91 8.91
80 × 60 3 7.81 6.13 6.13
80 × 60 3.5 8.99 7.06 7.06
80 × 60 4 10.1 7.97 7.97
80 × 60 5 12.4 9.7 9.7
90 × 50 3 7.81 6.13 6.13
90 × 50 4 10.1 7.97 7.97
90 × 50 5 12.4 9.7 9.7
100 × 40 3 7.81 6.13 6.13
100 × 40 4 10.1 7.97 7.97
100 × 40 5 12.4 9.7 9.7
100 × 50 3 8.41 6.6 6.6
100 × 50 4 10.9 8.59 8.59
100 × 50 5 13.4 10.5 10.5
100 × 50 6 15.6 12.3 12.3
100 × 60 3 9.01 7.07 7.07
100 × 60 3.5 10.4 8.16 8.16
100 × 60 4 11.7 9.22 9.22
100 × 60 5 14.4 11.3 11.3
100 × 60 6 16.8 13.2 13.2
100 × 80 3 10.2 8.01 8.01
100 × 80 4 13.3 10.5 10.5
100 × 80 5 16.4 12.8 12.8
100 × 80 6 19.2 15.1 15.1
120 × 40 3 9.01 7.07 7.07
120 × 40 4 11.7 9.22 9.22
120 × 40 5 14.4 11.3 11.3
120 × 60 3 10.2 8.01 8.01
120 × 60 3.5 11.8 9.26 9.26
120 × 60 4 13.3 10.5 10.5
120 × 60 5 16.4 12.8 12.8
120 × 60 6 19.2 15.1 15.1
120 × 80 3 11.4 8.96 8.96
120 × 80 4 14.9 11.7 11.7
120 × 80 5 18.4 14.4 14.4
120 × 80 6 21.6 17 17
120 × 80 8 27.2 21.4 21.4
140 × 80 3 12.6 9.9 9.9
140 × 80 4 16.5 13 13
140 × 80 5 20.4 16 16
140 × 80 6 24 18.9 18.9
140 × 80 8 30.4 23.9 23.9
140 × 80 10 36.6 28.7 28.7
150 × 100 3 14.4 11.3 11.3
150 × 100 4 18.9 14.9 14.9
150 × 100 5 23.4 18.3 18.3
150 × 100 6 27.6 21.7 21.7
150 × 100 8 35.2 27.7 27.7
150 × 100 10 42.6 33.4 33.4
160 × 80 3 13.8 10.8 10.8
160 × 80 4 18.1 14.2 14.2
160 × 80 5 22.4 17.5 17.5
160 × 80 6 26.4 20.7 20.7
160 × 80 8 33.6 26.4 26.4
160 × 80 10 40.6 31.8 31.8
180 × 80 3 15 11.8 11.8
180 × 80 4 19.7 15.5 15.5
180 × 80 5 24.4 19.1 19.1
180 × 80 6 28.8 22.6 22.6
180 × 80 8 36.8 28.9 28.9
180 × 80 10 44.6 35 35
180 × 100 4 21.3 16.8 16.8
180 × 100 5 26.4 20.7 20.7
180 × 100 6 31.2 24.5 24.5
180 × 100 8 40 31.4 31.4
180 × 100 10 48.6 38.1 38.1
200 × 100 4 22.9 18 18
200 × 100 5 28.4 22.3 22.3
200 × 100 6 33.6 26.4 26.4
200 × 100 8 43.2 33.9 33.9
200 × 100 10 52.6 41.3 41.3
200 × 120 4 24.5 19.3 19.3
200 × 120 5 30.4 23.8 23.8
200 × 120 6 36 28.3 28.3
200 × 120 8 46.4 36.5 36.5
200 × 120 10 56.6 44.4 44.4
200 × 150 4 26.9 21.2 21.2
200 × 150 5 33.4 26.2 26.2
200 × 150 6 39.6 31.1 31.1
200 × 150 8 51.2 40.2 40.2
200 × 150 10 62.6 49.1 49.1
250 × 150 5 38.4 30.1 30.1
250 × 150 6 45.6 35.8 35.8
250 × 150 6.3 47.4 37.2 37.2
250 × 150 8 59.2 46.5 46.5
250 × 150 10 72.6 57 57
250 × 150 12 84.1 66 66
250 × 150 12.5 87 68.3 68.3
300 × 100 6 45.6 35.8 35.8
300 × 100 8 59.2 46.5 46.5
300 × 100 10 72.6 57 57
300 × 200 6 57.6 45.2 45.2
300 × 200 6.3 60 47.1 47.1
300 × 200 8 75.2 59.1 59.1
300 × 200 10 92.6 72.7 72.7
300 × 200 12 108 84.8 84.8
300 × 200 12.5 112 88 88
400 × 200 6 69.6 54.7 54.7
400 × 200 6.3 72.6 57 57
400 × 200 8 91.2 71.6 71.6
400 × 200 10 113 88.4 88.4
400 × 200 12 132 104 104
400 × 200 12.5 137 108 108
450 × 250 6 81.6 64.1 64.1
450 × 250 6.3 85.2 66.9 66.9
450 × 250 8 107 84.2 84.2
450 × 250 10 133 104 104
450 × 250 12 156 123 123
450 × 250 12.5 162 127 127
500 × 300 6 93.6 73.5 73.5
500 × 300 6.3 97.8 76.8 76.8
500 × 300 8 123 96.7 96.7
500 × 300 10 153 120 120
500 × 300 12 180 141 141
500 × 300 12.5 187 147 147

Common circular hollow sections (CHS)

Cold-formed circular sizes in the Hybox 355 S355J2H programme.

Swipe horizontally to view all dimensions.

Outside diameter D (mm) Thickness T (mm) Area A (cm²) Mass (kg/m), EN 10219-2 formula Hybox 355 published mass (kg/m)
33.7 3 2.89 2.27 2.27
42.4 3 3.71 2.91 2.91
48.3 3 4.27 3.35 3.35
48.3 4 5.57 4.37 4.37
60.3 3 5.4 4.24 4.24
60.3 4 7.07 5.55 5.55
76.1 3 6.89 5.41 5.41
76.1 4 9.06 7.11 7.11
88.9 3 8.1 6.36 6.36
88.9 3.5 9.39 7.37 7.37
88.9 4 10.7 8.38 8.38
88.9 5 13.2 10.3 10.3
88.9 6.3 16.3 12.8 12.8
114.3 3 10.5 8.23 8.23
114.3 3.5 12.2 9.56 9.56
114.3 4 13.9 10.9 10.9
114.3 5 17.2 13.5 13.5
114.3 6 20.4 16 16
114.3 6.3 21.4 16.8 16.8
139.7 3 12.9 10.1 10.1
139.7 4 17.1 13.4 13.4
139.7 5 21.2 16.6 16.6
139.7 6 25.2 19.8 19.8
139.7 6.3 26.4 20.7 20.7
139.7 8 33.1 26 26
139.7 10 40.7 32 32
168.3 4 20.6 16.2 16.2
168.3 4.5 23.2 18.2 18.2
168.3 5 25.7 20.1 20.1
168.3 6 30.6 24 24
168.3 6.3 32.1 25.2 25.2
168.3 8 40.3 31.6 31.6
168.3 10 49.7 39 39
168.3 12.5 61.2 48 48
193.7 4 23.8 18.7 18.7
193.7 4.5 26.7 21 21
193.7 5 29.6 23.3 23.3
193.7 6 35.4 27.8 27.8
193.7 6.3 37.1 29.1 29.1
193.7 8 46.7 36.6 36.6
193.7 10 57.7 45.3 45.3
193.7 12.5 71.2 55.9 55.9
219.1 4.5 30.3 23.8 23.8
219.1 5 33.6 26.4 26.4
219.1 6 40.2 31.5 31.5
219.1 6.3 42.1 33.1 33.1
219.1 8 53.1 41.6 41.6
219.1 10 65.7 51.6 51.6
219.1 12 78.1 61.3 61.3
219.1 12.5 81.1 63.7 63.7
219.1 16 102 80.1 80.1
244.5 5 37.6 29.5 29.5
244.5 6 45 35.3 35.3
244.5 6.3 47.1 37 37
244.5 8 59.4 46.7 46.7
244.5 10 73.7 57.8 57.8
244.5 12 87.7 68.8 68.8
244.5 12.5 91.1 71.5 71.5
244.5 16 115 90.2 90.2
273 4 33.8 26.5 26.5
273 4.5 38 29.8 29.8
273 5 42.1 33 33
273 6 50.3 39.5 39.5
273 6.3 52.8 41.4 41.4
273 8 66.6 52.3 52.3
273 10 82.6 64.9 64.9
273 12 98.4 77.2 77.2
273 12.5 102 80.3 80.3
273 16 129 101 101
323.9 5 50.1 39.3 39.3
323.9 6 59.9 47 47
323.9 6.3 62.9 49.3 49.3
323.9 8 79.4 62.3 62.3
323.9 10 98.6 77.4 77.4
323.9 12 118 92.3 92.3
323.9 12.5 122 96 96
323.9 16 155 121 121
355.6 5 55.1 43.2 43.2
355.6 6 65.9 51.7 51.7
355.6 6.3 69.1 54.3 54.3
355.6 8 87.4 68.6 68.6
355.6 10 109 85.2 85.2
355.6 12 130 102 102
355.6 12.5 135 106 106
355.6 16 171 134 134
406.4 6 75.5 59.2 59.2
406.4 6.3 79.2 62.2 62.2
406.4 8 100 78.6 78.6
406.4 10 125 97.8 97.8
406.4 12 149 117 117
406.4 12.5 155 121 121
406.4 16 196 154 154
457 6 85 66.7 66.7
457 6.3 89.2 70 70
457 8 113 88.6 88.6
457 10 140 110 110
457 12 168 132 132
457 12.5 175 137 137
457 16 222 174 174
508 6 94.6 74.3 74.3
508 6.3 99.3 77.9 77.9
508 8 126 98.6 98.6
508 10 156 123 123
508 12 187 147 147
508 12.5 195 153 153
508 16 247 194 194

Formula notes. For circular sections the calculation diameter is d = D − 2T, the area is A (cm²) = π(D² − d²)/(4 × 10²), and the mass is M (kg/m) = 0.785 × A. For square and rectangular sections the calculation corner radii are ro = 2.0T and ri = 1.0T when T ≤ 6 mm, ro = 2.5T and ri = 1.5T when 6 mm < T ≤ 10 mm, and ro = 3.0T and ri = 2.0T when T > 10 mm. The area is A (cm²) = [2T(B + H − 2T) − (4 − π)(ro² − ri²)] / 10², and M = 0.785 × A. A worked check is 100 × 100 × 5: A = 18.4 cm² and M = 14.4 kg/m, which matches both the formula and the Hybox guide. Across the 339 common sizes listed here, every calculated mass agrees with the published Hybox mass once both figures are expressed to three significant figures (absolute differences stay within 0.06 kg/m below 100 kg/m; at and above 100 kg/m the published guide already rounds to the nearest integer).

EN 10219-1 S355J2H Chemical Composition and Carbon Equivalent

The ladle-analysis maxima below are the EN 10219-1 values used for S355J2H in the manufacturer declarations cited above. Product analysis, where required, follows the permitted deviations in EN 10219-1. Nitrogen is controlled through the killed, fine-grain practice rather than a separate JR-style nitrogen maximum.

Swipe horizontally to view all dimensions.

Element (cast analysis) Maximum, % (mass)
Carbon, max 0.22
Silicon, max 0.55
Manganese, max 1.60
Phosphorus, max 0.030
Sulfur, max 0.030
CEV, max (t ≤ 16 mm) 0.45
CEV, max (16 mm < t ≤ 40 mm) 0.47

EN 10219-1 S355J2H Mechanical Properties: Yield, Tensile, Elongation and Impact

Specified mechanical properties for EN 10219-1 S355J2H, as used in the declarations cited above, are thickness-dependent. The impact requirement is 27 J at −20 °C; it is not a room-temperature JR test and it is not a 0 °C J0 test.

Swipe horizontally to view all dimensions.

Property Requirement
Yield strength ReH, min, t ≤ 16 mm 355 MPa
Yield strength ReH, min, 16 mm < t ≤ 40 mm 345 MPa
Tensile strength Rm, t < 3 mm 510–680 MPa
Tensile strength Rm, 3 mm ≤ t ≤ 40 mm 470–630 MPa
Elongation A, min, t ≤ 40 mm A 20 %
Charpy V-notch, min 27 J at −20 °C

A EN 10219-1 Table A.3 footnote c reduces the elongation minimum to 18 % for some section sizes; apply that footnote when it is part of the ordered edition. Properties for thicknesses above 40 mm, where offered, follow the ordered edition of EN 10219-1 and are not restated here from another standard.

Delivery, Inspection and Identification of EN 10219-1 S355J2H Hollow Sections

The inspection document should name EN 10219-1 and EN 10219-2, the grade S355J2H or steel number 1.0576, the edition, the size, the wall thickness, and the impact temperature. A Declaration of Performance under the Construction Products Regulation, where applicable, is a different document from a mill test report and should be asked for if the order needs it. Do not accept an EN 10210-1 certificate, an S355JRH or S355J0H certificate, or a hot-finished mass table as a substitute for S355J2H to EN 10219.

Weldability and Surface Condition of EN 10219-1 S355J2H Hollow Sections

The 0.45 CEV cap in the 16 mm and under band, and 0.47 up to 40 mm, is the weldability control published for this grade. Welding procedure, consumable and preheat still depend on thickness, heat analysis and the project welding specification. The longitudinal weld is part of the product; any additional fabrication welding is outside the mill production weld and has to be specified separately. Surface condition follows EN 10219 unless the order names a coating or a tighter finish.

Dimensional Tolerances and Theoretical Mass for EN 10219-1 S355J2H Hollow Sections

Outside dimensions, wall thickness, out-of-roundness, straightness and mass tolerance are those of EN 10219-2 for the ordered type and thickness. Calculated masses on this page use the EN 10219-2 Annex B corner-radius assumptions for cold-formed sections. Those radii differ from the hot-finished radii in EN 10210-2, so a Celsius or other EN 10210 mass must not be used in place of the figures above. Mass tolerance is applied to the theoretical mass of the ordered length, not to a stock-list figure.

Applications and Service Limits for EN 10219-1 S355J2H Steel Hollow Sections

S355J2H is commonly specified for building frames, trusses, columns, machinery supports and general structural work in which a 355 MPa yield class and a −20 °C impact test are required. It is not automatically suitable for pressure equipment, fire-protected members without a further assessment, or low-temperature service below the verified impact temperature. Cold forming strain and the presence of a weld seam remain part of the product condition when later fabrication or fatigue is assessed.

EN 10219-1 S355J2H Compared with S355J0H, EN 10210-1 S355J2H and ASTM A500

S355J0H uses the same 355 MPa yield class but verifies impact at 0 °C, not at −20 °C. S355JRH is a still milder quality with a room-temperature impact test and a different chemistry table. EN 10210-1 S355J2H is hot-finished. It can have a different mass for the same designated size because of different corner-radius rules, and it is a different specification family. ASTM A500 Grade C is a 50 ksi [345 MPa] cold-formed HSS specification with its own tensile range, periphery limit and design-wall convention; it is not a one-for-one substitute. GB/T 6728 is a dimensional standard for cold-formed Chinese sections and must be paired with the actual material standard named on the order.

Near-Equivalents for EN 10219-1 S355J2H Hollow Sections: Not Automatic Substitutes

Designers sometimes compare S355J2H with EN 10210-1 S355J2H, ASTM A500 Grade C, or GB/T 1591 Q355B used in a GB/T 6728 hollow section. Those comparisons are starting points only. Process route, impact temperature, tensile range, corner radii, tolerances and certificate wording all have to be checked against the order. None of those products is an automatic substitute for EN 10219-1 S355J2H.

Sourcing EN 10219-1 S355J2H Steel Hollow Sections from SHH STEEL

Send the shape (SHS, RHS or CHS), the designated size and thickness, the length, the EN 10219-1 edition, and whether a Declaration of Performance is required. Name S355J2H explicitly if the −20 °C impact quality is needed; do not assume that an S355J0H or S355JRH offer meets the same enquiry. SHH STEEL reviews the grade, size and certificate wording before quoting. The tables above are a common-size programme, not a claim of warehouse stock.

EN 10219-1 S355J2H Hollow Section FAQs

Is this the same product as EN 10210-1 S355J2H?
No. EN 10219-1 S355J2H is cold-formed. EN 10210-1 S355J2H is hot-finished. Corner-radius rules, calculated mass and some tolerances differ. A 10210 certificate or a hot-finished mass table should not be used in place of EN 10219.
Are the size tables the complete EN 10219-2 list?
No. They are common sizes from the Tata Hybox 355 programme for S355J2H, labelled as a mill programme. Masses are calculated from the EN 10219-2 Annex B formulae and were cross-checked against that guide. Other sizes may be available by agreement, but they are not tabulated here.
Why is the impact test at −20 °C?
J2H is the EN 10219-1 quality that requires a minimum 27 J Charpy result at −20 °C. J0H is verified at 0 °C and JRH at room temperature. Those qualities are not interchangeable with S355J2H without a review of the order.
What mass should be used for 100 × 100 × 5?
The EN 10219-2 formula gives 14.4 kg/m, and the Hybox 355 guide publishes the same figure. Do not replace it with an EN 10210-2 mass for the same designated size.
Can ASTM A500 Grade C be substituted?
Only if the delivered piece and certificate also meet every requirement of the order, including EN 10219-1 S355J2H impact testing where that is specified. A500 Grade C is a different specification with its own tensile range and design-wall rules. It is not an automatic substitute.

Conclusion

EN 10219-1 S355J2H is a killed, cold-formed structural hollow section in steel 1.0576, with a 355 MPa minimum yield in the 16 mm and under band and a 27 J impact requirement at −20 °C. The tables list common Hybox 355 programme sizes, not the full EN 10219-2 list, with masses from the EN 10219-2 formulae. Name the shape, size, thickness, edition and any Declaration of Performance on the enquiry; SHH STEEL will review the package before quoting. This page does not treat the product as EN 10210-1 or as a stock list.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X