The tables below are a typographical common-size subset with theoretical masses from the EN 10219-2 Annex A formulae, using the same cold-formed calculation radii as the S235JRH page (2.0T/1.0T, 2.5T/1.5T or 3.0T/2.0T by thickness band). They are not a complete EN 10219-2 list, not a stock list, and not the Hybox 355 programme. A 100 × 100 × 5 section is 14.4 kg/m under these rules.
Square hollow sections (128 sizes).
Swipe horizontally to view all dimensions.
| Designation (mm) |
Side B (mm) |
Wall t (mm) |
Area (cm²) |
Mass M (kg/m) |
| 40 × 40 × 3 |
40 |
3 |
4.21 |
3.303 |
| 40 × 40 × 4 |
40 |
4 |
5.35 |
4.198 |
| 40 × 40 × 5 |
40 |
5 |
6.36 |
4.99 |
| 40 × 40 × 6 |
40 |
6 |
7.23 |
5.678 |
| 40 × 40 × 8 |
40 |
8 |
8.04 |
6.313 |
| 40 × 40 × 10 |
40 |
10 |
8.57 |
6.725 |
| 40 × 40 × 12 |
40 |
12 |
7.26 |
5.699 |
| 40 × 40 × 12.5 |
40 |
12.5 |
7.04 |
5.529 |
| 50 × 50 × 3 |
50 |
3 |
5.41 |
4.245 |
| 50 × 50 × 4 |
50 |
4 |
6.95 |
5.454 |
| 50 × 50 × 5 |
50 |
5 |
8.36 |
6.56 |
| 50 × 50 × 6 |
50 |
6 |
9.63 |
7.562 |
| 50 × 50 × 8 |
50 |
8 |
11.24 |
8.825 |
| 50 × 50 × 10 |
50 |
10 |
12.57 |
9.865 |
| 50 × 50 × 12 |
50 |
12 |
12.06 |
9.467 |
| 50 × 50 × 12.5 |
50 |
12.5 |
12.04 |
9.454 |
| 60 × 60 × 3 |
60 |
3 |
6.61 |
5.187 |
| 60 × 60 × 4 |
60 |
4 |
8.55 |
6.71 |
| 60 × 60 × 5 |
60 |
5 |
10.36 |
8.13 |
| 60 × 60 × 6 |
60 |
6 |
12.03 |
9.446 |
| 60 × 60 × 8 |
60 |
8 |
14.44 |
11.34 |
| 60 × 60 × 10 |
60 |
10 |
16.57 |
13 |
| 60 × 60 × 12 |
60 |
12 |
16.86 |
13.23 |
| 60 × 60 × 12.5 |
60 |
12.5 |
17.04 |
13.38 |
| 70 × 70 × 3 |
70 |
3 |
7.81 |
6.129 |
| 70 × 70 × 4 |
70 |
4 |
10.15 |
7.966 |
| 70 × 70 × 5 |
70 |
5 |
12.36 |
9.7 |
| 70 × 70 × 6 |
70 |
6 |
14.43 |
11.33 |
| 70 × 70 × 8 |
70 |
8 |
17.64 |
13.85 |
| 70 × 70 × 10 |
70 |
10 |
20.57 |
16.14 |
| 70 × 70 × 12 |
70 |
12 |
21.66 |
17 |
| 70 × 70 × 12.5 |
70 |
12.5 |
22.04 |
17.3 |
| 80 × 80 × 3 |
80 |
3 |
9.01 |
7.071 |
| 80 × 80 × 4 |
80 |
4 |
11.75 |
9.222 |
| 80 × 80 × 5 |
80 |
5 |
14.36 |
11.27 |
| 80 × 80 × 6 |
80 |
6 |
16.83 |
13.21 |
| 80 × 80 × 8 |
80 |
8 |
20.84 |
16.36 |
| 80 × 80 × 10 |
80 |
10 |
24.57 |
19.28 |
| 80 × 80 × 12 |
80 |
12 |
26.46 |
20.77 |
| 80 × 80 × 12.5 |
80 |
12.5 |
27.04 |
21.23 |
| 90 × 90 × 3 |
90 |
3 |
10.21 |
8.013 |
| 90 × 90 × 4 |
90 |
4 |
13.35 |
10.48 |
| 90 × 90 × 5 |
90 |
5 |
16.36 |
12.84 |
| 90 × 90 × 6 |
90 |
6 |
19.23 |
15.1 |
| 90 × 90 × 8 |
90 |
8 |
24.04 |
18.87 |
| 90 × 90 × 10 |
90 |
10 |
28.57 |
22.42 |
| 90 × 90 × 12 |
90 |
12 |
31.26 |
24.54 |
| 90 × 90 × 12.5 |
90 |
12.5 |
32.04 |
25.15 |
| 100 × 100 × 3 |
100 |
3 |
11.41 |
8.955 |
| 100 × 100 × 4 |
100 |
4 |
14.95 |
11.73 |
| 100 × 100 × 5 |
100 |
5 |
18.36 |
14.41 |
| 100 × 100 × 6 |
100 |
6 |
21.63 |
16.98 |
| 100 × 100 × 8 |
100 |
8 |
27.24 |
21.39 |
| 100 × 100 × 10 |
100 |
10 |
32.57 |
25.56 |
| 100 × 100 × 12 |
100 |
12 |
36.06 |
28.31 |
| 100 × 100 × 12.5 |
100 |
12.5 |
37.04 |
29.08 |
| 120 × 120 × 3 |
120 |
3 |
13.81 |
10.84 |
| 120 × 120 × 4 |
120 |
4 |
18.15 |
14.25 |
| 120 × 120 × 5 |
120 |
5 |
22.36 |
17.55 |
| 120 × 120 × 6 |
120 |
6 |
26.43 |
20.75 |
| 120 × 120 × 8 |
120 |
8 |
33.64 |
26.41 |
| 120 × 120 × 10 |
120 |
10 |
40.57 |
31.84 |
| 120 × 120 × 12 |
120 |
12 |
45.66 |
35.84 |
| 120 × 120 × 12.5 |
120 |
12.5 |
47.04 |
36.93 |
| 140 × 140 × 3 |
140 |
3 |
16.21 |
12.72 |
| 140 × 140 × 4 |
140 |
4 |
21.35 |
16.76 |
| 140 × 140 × 5 |
140 |
5 |
26.36 |
20.69 |
| 140 × 140 × 6 |
140 |
6 |
31.23 |
24.52 |
| 140 × 140 × 8 |
140 |
8 |
40.04 |
31.43 |
| 140 × 140 × 10 |
140 |
10 |
48.57 |
38.12 |
| 140 × 140 × 12 |
140 |
12 |
55.26 |
43.38 |
| 140 × 140 × 12.5 |
140 |
12.5 |
57.04 |
44.78 |
| 150 × 150 × 3 |
150 |
3 |
17.41 |
13.67 |
| 150 × 150 × 4 |
150 |
4 |
22.95 |
18.01 |
| 150 × 150 × 5 |
150 |
5 |
28.36 |
22.26 |
| 150 × 150 × 6 |
150 |
6 |
33.63 |
26.4 |
| 150 × 150 × 8 |
150 |
8 |
43.24 |
33.95 |
| 150 × 150 × 10 |
150 |
10 |
52.57 |
41.26 |
| 150 × 150 × 12 |
150 |
12 |
60.06 |
47.15 |
| 150 × 150 × 12.5 |
150 |
12.5 |
62.04 |
48.7 |
| 160 × 160 × 3 |
160 |
3 |
18.61 |
14.61 |
| 160 × 160 × 4 |
160 |
4 |
24.55 |
19.27 |
| 160 × 160 × 5 |
160 |
5 |
30.36 |
23.83 |
| 160 × 160 × 6 |
160 |
6 |
36.03 |
28.29 |
| 160 × 160 × 8 |
160 |
8 |
46.44 |
36.46 |
| 160 × 160 × 10 |
160 |
10 |
56.57 |
44.4 |
| 160 × 160 × 12 |
160 |
12 |
64.86 |
50.91 |
| 160 × 160 × 12.5 |
160 |
12.5 |
67.04 |
52.63 |
| 180 × 180 × 3 |
180 |
3 |
21.01 |
16.49 |
| 180 × 180 × 4 |
180 |
4 |
27.75 |
21.78 |
| 180 × 180 × 5 |
180 |
5 |
34.36 |
26.97 |
| 180 × 180 × 6 |
180 |
6 |
40.83 |
32.05 |
| 180 × 180 × 8 |
180 |
8 |
52.84 |
41.48 |
| 180 × 180 × 10 |
180 |
10 |
64.57 |
50.68 |
| 180 × 180 × 12 |
180 |
12 |
74.46 |
58.45 |
| 180 × 180 × 12.5 |
180 |
12.5 |
77.04 |
60.48 |
| 200 × 200 × 3 |
200 |
3 |
23.41 |
18.38 |
| 200 × 200 × 4 |
200 |
4 |
30.95 |
24.29 |
| 200 × 200 × 5 |
200 |
5 |
38.36 |
30.11 |
| 200 × 200 × 6 |
200 |
6 |
45.63 |
35.82 |
| 200 × 200 × 8 |
200 |
8 |
59.24 |
46.51 |
| 200 × 200 × 10 |
200 |
10 |
72.57 |
56.96 |
| 200 × 200 × 12 |
200 |
12 |
84.06 |
65.99 |
| 200 × 200 × 12.5 |
200 |
12.5 |
87.04 |
68.33 |
| 250 × 250 × 5 |
250 |
5 |
48.36 |
37.96 |
| 250 × 250 × 6 |
250 |
6 |
57.63 |
45.24 |
| 250 × 250 × 8 |
250 |
8 |
75.24 |
59.07 |
| 250 × 250 × 10 |
250 |
10 |
92.57 |
72.66 |
| 250 × 250 × 12 |
250 |
12 |
108.06 |
84.83 |
| 250 × 250 × 12.5 |
250 |
12.5 |
112.04 |
87.95 |
| 300 × 300 × 5 |
300 |
5 |
58.36 |
45.81 |
| 300 × 300 × 6 |
300 |
6 |
69.63 |
54.66 |
| 300 × 300 × 8 |
300 |
8 |
91.24 |
71.63 |
| 300 × 300 × 10 |
300 |
10 |
112.57 |
88.36 |
| 300 × 300 × 12 |
300 |
12 |
132.06 |
103.67 |
| 300 × 300 × 12.5 |
300 |
12.5 |
137.04 |
107.58 |
| 350 × 350 × 5 |
350 |
5 |
68.36 |
53.66 |
| 350 × 350 × 6 |
350 |
6 |
81.63 |
64.08 |
| 350 × 350 × 8 |
350 |
8 |
107.24 |
84.19 |
| 350 × 350 × 10 |
350 |
10 |
132.57 |
104.06 |
| 350 × 350 × 12 |
350 |
12 |
156.06 |
122.51 |
| 350 × 350 × 12.5 |
350 |
12.5 |
162.04 |
127.2 |
| 400 × 400 × 5 |
400 |
5 |
78.36 |
61.51 |
| 400 × 400 × 6 |
400 |
6 |
93.63 |
73.5 |
| 400 × 400 × 8 |
400 |
8 |
123.24 |
96.75 |
| 400 × 400 × 10 |
400 |
10 |
152.57 |
119.76 |
| 400 × 400 × 12 |
400 |
12 |
180.06 |
141.35 |
| 400 × 400 × 12.5 |
400 |
12.5 |
187.04 |
146.83 |
Rectangular hollow sections (143 sizes).
Swipe horizontally to view all dimensions.
| Designation (mm) |
H (mm) |
B (mm) |
Wall t (mm) |
Area (cm²) |
Mass M (kg/m) |
| 50 × 30 × 3 |
50 |
30 |
3 |
4.21 |
3.303 |
| 50 × 30 × 4 |
50 |
30 |
4 |
5.35 |
4.198 |
| 50 × 30 × 5 |
50 |
30 |
5 |
6.36 |
4.99 |
| 50 × 30 × 6 |
50 |
30 |
6 |
7.23 |
5.678 |
| 50 × 30 × 8 |
50 |
30 |
8 |
8.04 |
6.313 |
| 60 × 40 × 3 |
60 |
40 |
3 |
5.41 |
4.245 |
| 60 × 40 × 4 |
60 |
40 |
4 |
6.95 |
5.454 |
| 60 × 40 × 5 |
60 |
40 |
5 |
8.36 |
6.56 |
| 60 × 40 × 6 |
60 |
40 |
6 |
9.63 |
7.562 |
| 60 × 40 × 8 |
60 |
40 |
8 |
11.24 |
8.825 |
| 60 × 40 × 10 |
60 |
40 |
10 |
12.57 |
9.865 |
| 60 × 40 × 12 |
60 |
40 |
12 |
12.06 |
9.467 |
| 60 × 40 × 12.5 |
60 |
40 |
12.5 |
12.04 |
9.454 |
| 80 × 40 × 3 |
80 |
40 |
3 |
6.61 |
5.187 |
| 80 × 40 × 4 |
80 |
40 |
4 |
8.55 |
6.71 |
| 80 × 40 × 5 |
80 |
40 |
5 |
10.36 |
8.13 |
| 80 × 40 × 6 |
80 |
40 |
6 |
12.03 |
9.446 |
| 80 × 40 × 8 |
80 |
40 |
8 |
14.44 |
11.34 |
| 80 × 40 × 10 |
80 |
40 |
10 |
16.57 |
13 |
| 80 × 40 × 12 |
80 |
40 |
12 |
16.86 |
13.23 |
| 80 × 40 × 12.5 |
80 |
40 |
12.5 |
17.04 |
13.38 |
| 80 × 60 × 3 |
80 |
60 |
3 |
7.81 |
6.129 |
| 80 × 60 × 4 |
80 |
60 |
4 |
10.15 |
7.966 |
| 80 × 60 × 5 |
80 |
60 |
5 |
12.36 |
9.7 |
| 80 × 60 × 6 |
80 |
60 |
6 |
14.43 |
11.33 |
| 80 × 60 × 8 |
80 |
60 |
8 |
17.64 |
13.85 |
| 80 × 60 × 10 |
80 |
60 |
10 |
20.57 |
16.14 |
| 80 × 60 × 12 |
80 |
60 |
12 |
21.66 |
17 |
| 80 × 60 × 12.5 |
80 |
60 |
12.5 |
22.04 |
17.3 |
| 100 × 50 × 3 |
100 |
50 |
3 |
8.41 |
6.6 |
| 100 × 50 × 4 |
100 |
50 |
4 |
10.95 |
8.594 |
| 100 × 50 × 5 |
100 |
50 |
5 |
13.36 |
10.48 |
| 100 × 50 × 6 |
100 |
50 |
6 |
15.63 |
12.27 |
| 100 × 50 × 8 |
100 |
50 |
8 |
19.24 |
15.11 |
| 100 × 50 × 10 |
100 |
50 |
10 |
22.57 |
17.71 |
| 100 × 50 × 12 |
100 |
50 |
12 |
24.06 |
18.89 |
| 100 × 50 × 12.5 |
100 |
50 |
12.5 |
24.54 |
19.27 |
| 100 × 60 × 3 |
100 |
60 |
3 |
9.01 |
7.071 |
| 100 × 60 × 4 |
100 |
60 |
4 |
11.75 |
9.222 |
| 100 × 60 × 5 |
100 |
60 |
5 |
14.36 |
11.27 |
| 100 × 60 × 6 |
100 |
60 |
6 |
16.83 |
13.21 |
| 100 × 60 × 8 |
100 |
60 |
8 |
20.84 |
16.36 |
| 100 × 60 × 10 |
100 |
60 |
10 |
24.57 |
19.28 |
| 100 × 60 × 12 |
100 |
60 |
12 |
26.46 |
20.77 |
| 100 × 60 × 12.5 |
100 |
60 |
12.5 |
27.04 |
21.23 |
| 100 × 80 × 3 |
100 |
80 |
3 |
10.21 |
8.013 |
| 100 × 80 × 4 |
100 |
80 |
4 |
13.35 |
10.48 |
| 100 × 80 × 5 |
100 |
80 |
5 |
16.36 |
12.84 |
| 100 × 80 × 6 |
100 |
80 |
6 |
19.23 |
15.1 |
| 100 × 80 × 8 |
100 |
80 |
8 |
24.04 |
18.87 |
| 100 × 80 × 10 |
100 |
80 |
10 |
28.57 |
22.42 |
| 100 × 80 × 12 |
100 |
80 |
12 |
31.26 |
24.54 |
| 100 × 80 × 12.5 |
100 |
80 |
12.5 |
32.04 |
25.15 |
| 120 × 60 × 3 |
120 |
60 |
3 |
10.21 |
8.013 |
| 120 × 60 × 4 |
120 |
60 |
4 |
13.35 |
10.48 |
| 120 × 60 × 5 |
120 |
60 |
5 |
16.36 |
12.84 |
| 120 × 60 × 6 |
120 |
60 |
6 |
19.23 |
15.1 |
| 120 × 60 × 8 |
120 |
60 |
8 |
24.04 |
18.87 |
| 120 × 60 × 10 |
120 |
60 |
10 |
28.57 |
22.42 |
| 120 × 60 × 12 |
120 |
60 |
12 |
31.26 |
24.54 |
| 120 × 60 × 12.5 |
120 |
60 |
12.5 |
32.04 |
25.15 |
| 120 × 80 × 3 |
120 |
80 |
3 |
11.41 |
8.955 |
| 120 × 80 × 4 |
120 |
80 |
4 |
14.95 |
11.73 |
| 120 × 80 × 5 |
120 |
80 |
5 |
18.36 |
14.41 |
| 120 × 80 × 6 |
120 |
80 |
6 |
21.63 |
16.98 |
| 120 × 80 × 8 |
120 |
80 |
8 |
27.24 |
21.39 |
| 120 × 80 × 10 |
120 |
80 |
10 |
32.57 |
25.56 |
| 120 × 80 × 12 |
120 |
80 |
12 |
36.06 |
28.31 |
| 120 × 80 × 12.5 |
120 |
80 |
12.5 |
37.04 |
29.08 |
| 140 × 80 × 3 |
140 |
80 |
3 |
12.61 |
9.897 |
| 140 × 80 × 4 |
140 |
80 |
4 |
16.55 |
12.99 |
| 140 × 80 × 5 |
140 |
80 |
5 |
20.36 |
15.98 |
| 140 × 80 × 6 |
140 |
80 |
6 |
24.03 |
18.87 |
| 140 × 80 × 8 |
140 |
80 |
8 |
30.44 |
23.9 |
| 140 × 80 × 10 |
140 |
80 |
10 |
36.57 |
28.7 |
| 140 × 80 × 12 |
140 |
80 |
12 |
40.86 |
32.07 |
| 140 × 80 × 12.5 |
140 |
80 |
12.5 |
42.04 |
33 |
| 150 × 100 × 3 |
150 |
100 |
3 |
14.41 |
11.31 |
| 150 × 100 × 4 |
150 |
100 |
4 |
18.95 |
14.87 |
| 150 × 100 × 5 |
150 |
100 |
5 |
23.36 |
18.33 |
| 150 × 100 × 6 |
150 |
100 |
6 |
27.63 |
21.69 |
| 150 × 100 × 8 |
150 |
100 |
8 |
35.24 |
27.67 |
| 150 × 100 × 10 |
150 |
100 |
10 |
42.57 |
33.41 |
| 150 × 100 × 12 |
150 |
100 |
12 |
48.06 |
37.73 |
| 150 × 100 × 12.5 |
150 |
100 |
12.5 |
49.54 |
38.89 |
| 160 × 80 × 3 |
160 |
80 |
3 |
13.81 |
10.84 |
| 160 × 80 × 4 |
160 |
80 |
4 |
18.15 |
14.25 |
| 160 × 80 × 5 |
160 |
80 |
5 |
22.36 |
17.55 |
| 160 × 80 × 6 |
160 |
80 |
6 |
26.43 |
20.75 |
| 160 × 80 × 8 |
160 |
80 |
8 |
33.64 |
26.41 |
| 160 × 80 × 10 |
160 |
80 |
10 |
40.57 |
31.84 |
| 160 × 80 × 12 |
160 |
80 |
12 |
45.66 |
35.84 |
| 160 × 80 × 12.5 |
160 |
80 |
12.5 |
47.04 |
36.93 |
| 180 × 100 × 3 |
180 |
100 |
3 |
16.21 |
12.72 |
| 180 × 100 × 4 |
180 |
100 |
4 |
21.35 |
16.76 |
| 180 × 100 × 5 |
180 |
100 |
5 |
26.36 |
20.69 |
| 180 × 100 × 6 |
180 |
100 |
6 |
31.23 |
24.52 |
| 180 × 100 × 8 |
180 |
100 |
8 |
40.04 |
31.43 |
| 180 × 100 × 10 |
180 |
100 |
10 |
48.57 |
38.12 |
| 180 × 100 × 12 |
180 |
100 |
12 |
55.26 |
43.38 |
| 180 × 100 × 12.5 |
180 |
100 |
12.5 |
57.04 |
44.78 |
| 200 × 100 × 3 |
200 |
100 |
3 |
17.41 |
13.67 |
| 200 × 100 × 4 |
200 |
100 |
4 |
22.95 |
18.01 |
| 200 × 100 × 5 |
200 |
100 |
5 |
28.36 |
22.26 |
| 200 × 100 × 6 |
200 |
100 |
6 |
33.63 |
26.4 |
| 200 × 100 × 8 |
200 |
100 |
8 |
43.24 |
33.95 |
| 200 × 100 × 10 |
200 |
100 |
10 |
52.57 |
41.26 |
| 200 × 100 × 12 |
200 |
100 |
12 |
60.06 |
47.15 |
| 200 × 100 × 12.5 |
200 |
100 |
12.5 |
62.04 |
48.7 |
| 200 × 120 × 3 |
200 |
120 |
3 |
18.61 |
14.61 |
| 200 × 120 × 4 |
200 |
120 |
4 |
24.55 |
19.27 |
| 200 × 120 × 5 |
200 |
120 |
5 |
30.36 |
23.83 |
| 200 × 120 × 6 |
200 |
120 |
6 |
36.03 |
28.29 |
| 200 × 120 × 8 |
200 |
120 |
8 |
46.44 |
36.46 |
| 200 × 120 × 10 |
200 |
120 |
10 |
56.57 |
44.4 |
| 200 × 120 × 12 |
200 |
120 |
12 |
64.86 |
50.91 |
| 200 × 120 × 12.5 |
200 |
120 |
12.5 |
67.04 |
52.63 |
| 200 × 150 × 3 |
200 |
150 |
3 |
20.41 |
16.02 |
| 200 × 150 × 4 |
200 |
150 |
4 |
26.95 |
21.15 |
| 200 × 150 × 5 |
200 |
150 |
5 |
33.36 |
26.18 |
| 200 × 150 × 6 |
200 |
150 |
6 |
39.63 |
31.11 |
| 200 × 150 × 8 |
200 |
150 |
8 |
51.24 |
40.23 |
| 200 × 150 × 10 |
200 |
150 |
10 |
62.57 |
49.11 |
| 200 × 150 × 12 |
200 |
150 |
12 |
72.06 |
56.57 |
| 200 × 150 × 12.5 |
200 |
150 |
12.5 |
74.54 |
58.52 |
| 250 × 150 × 5 |
250 |
150 |
5 |
38.36 |
30.11 |
| 250 × 150 × 6 |
250 |
150 |
6 |
45.63 |
35.82 |
| 250 × 150 × 8 |
250 |
150 |
8 |
59.24 |
46.51 |
| 250 × 150 × 10 |
250 |
150 |
10 |
72.57 |
56.96 |
| 250 × 150 × 12 |
250 |
150 |
12 |
84.06 |
65.99 |
| 250 × 150 × 12.5 |
250 |
150 |
12.5 |
87.04 |
68.33 |
| 300 × 200 × 5 |
300 |
200 |
5 |
48.36 |
37.96 |
| 300 × 200 × 6 |
300 |
200 |
6 |
57.63 |
45.24 |
| 300 × 200 × 8 |
300 |
200 |
8 |
75.24 |
59.07 |
| 300 × 200 × 10 |
300 |
200 |
10 |
92.57 |
72.66 |
| 300 × 200 × 12 |
300 |
200 |
12 |
108.06 |
84.83 |
| 300 × 200 × 12.5 |
300 |
200 |
12.5 |
112.04 |
87.95 |
| 400 × 200 × 5 |
400 |
200 |
5 |
58.36 |
45.81 |
| 400 × 200 × 6 |
400 |
200 |
6 |
69.63 |
54.66 |
| 400 × 200 × 8 |
400 |
200 |
8 |
91.24 |
71.63 |
| 400 × 200 × 10 |
400 |
200 |
10 |
112.57 |
88.36 |
| 400 × 200 × 12 |
400 |
200 |
12 |
132.06 |
103.67 |
| 400 × 200 × 12.5 |
400 |
200 |
12.5 |
137.04 |
107.58 |
Circular hollow sections (91 sizes).
CHS up to 168.3 mm (73 sizes).
Swipe horizontally to view all dimensions.
| D × t (mm) |
Outside diameter D (mm) |
Wall t (mm) |
Area (cm²) |
Mass M (kg/m) |
| 21.3 × 3 |
21.3 |
3 |
1.72 |
1.354 |
| 21.3 × 4 |
21.3 |
4 |
2.17 |
1.707 |
| 21.3 × 5 |
21.3 |
5 |
2.56 |
2.01 |
| 26.9 × 3 |
26.9 |
3 |
2.25 |
1.768 |
| 26.9 × 4 |
26.9 |
4 |
2.88 |
2.259 |
| 26.9 × 5 |
26.9 |
5 |
3.44 |
2.7 |
| 26.9 × 6 |
26.9 |
6 |
3.94 |
3.093 |
| 33.7 × 3 |
33.7 |
3 |
2.89 |
2.271 |
| 33.7 × 4 |
33.7 |
4 |
3.73 |
2.93 |
| 33.7 × 5 |
33.7 |
5 |
4.51 |
3.539 |
| 33.7 × 6 |
33.7 |
6 |
5.22 |
4.099 |
| 33.7 × 8 |
33.7 |
8 |
6.46 |
5.07 |
| 42.4 × 3 |
42.4 |
3 |
3.71 |
2.915 |
| 42.4 × 4 |
42.4 |
4 |
4.83 |
3.788 |
| 42.4 × 5 |
42.4 |
5 |
5.87 |
4.612 |
| 42.4 × 6 |
42.4 |
6 |
6.86 |
5.386 |
| 42.4 × 8 |
42.4 |
8 |
8.65 |
6.787 |
| 42.4 × 10 |
42.4 |
10 |
10.18 |
7.99 |
| 48.3 × 3 |
48.3 |
3 |
4.27 |
3.351 |
| 48.3 × 4 |
48.3 |
4 |
5.57 |
4.37 |
| 48.3 × 5 |
48.3 |
5 |
6.8 |
5.339 |
| 48.3 × 6 |
48.3 |
6 |
7.97 |
6.259 |
| 48.3 × 8 |
48.3 |
8 |
10.13 |
7.951 |
| 48.3 × 10 |
48.3 |
10 |
12.03 |
9.445 |
| 48.3 × 12 |
48.3 |
12 |
13.68 |
10.74 |
| 60.3 × 3 |
60.3 |
3 |
5.4 |
4.239 |
| 60.3 × 4 |
60.3 |
4 |
7.07 |
5.554 |
| 60.3 × 5 |
60.3 |
5 |
8.69 |
6.819 |
| 60.3 × 6 |
60.3 |
6 |
10.24 |
8.035 |
| 60.3 × 8 |
60.3 |
8 |
13.14 |
10.32 |
| 60.3 × 10 |
60.3 |
10 |
15.8 |
12.4 |
| 60.3 × 12 |
60.3 |
12 |
18.21 |
14.29 |
| 60.3 × 12.5 |
60.3 |
12.5 |
18.77 |
14.74 |
| 76.1 × 3 |
76.1 |
3 |
6.89 |
5.408 |
| 76.1 × 4 |
76.1 |
4 |
9.06 |
7.112 |
| 76.1 × 5 |
76.1 |
5 |
11.17 |
8.767 |
| 76.1 × 6 |
76.1 |
6 |
13.21 |
10.37 |
| 76.1 × 8 |
76.1 |
8 |
17.12 |
13.44 |
| 76.1 × 10 |
76.1 |
10 |
20.77 |
16.3 |
| 76.1 × 12 |
76.1 |
12 |
24.17 |
18.97 |
| 76.1 × 12.5 |
76.1 |
12.5 |
24.98 |
19.61 |
| 88.9 × 3 |
88.9 |
3 |
8.1 |
6.355 |
| 88.9 × 4 |
88.9 |
4 |
10.67 |
8.375 |
| 88.9 × 5 |
88.9 |
5 |
13.18 |
10.35 |
| 88.9 × 6 |
88.9 |
6 |
15.63 |
12.27 |
| 88.9 × 8 |
88.9 |
8 |
20.33 |
15.96 |
| 88.9 × 10 |
88.9 |
10 |
24.79 |
19.46 |
| 88.9 × 12 |
88.9 |
12 |
28.99 |
22.76 |
| 88.9 × 12.5 |
88.9 |
12.5 |
30 |
23.55 |
| 114.3 × 3 |
114.3 |
3 |
10.49 |
8.234 |
| 114.3 × 4 |
114.3 |
4 |
13.86 |
10.88 |
| 114.3 × 5 |
114.3 |
5 |
17.17 |
13.48 |
| 114.3 × 6 |
114.3 |
6 |
20.41 |
16.03 |
| 114.3 × 8 |
114.3 |
8 |
26.72 |
20.97 |
| 114.3 × 10 |
114.3 |
10 |
32.77 |
25.72 |
| 114.3 × 12 |
114.3 |
12 |
38.57 |
30.27 |
| 114.3 × 12.5 |
114.3 |
12.5 |
39.98 |
31.38 |
| 139.7 × 3 |
139.7 |
3 |
12.88 |
10.11 |
| 139.7 × 4 |
139.7 |
4 |
17.05 |
13.39 |
| 139.7 × 5 |
139.7 |
5 |
21.16 |
16.61 |
| 139.7 × 6 |
139.7 |
6 |
25.2 |
19.78 |
| 139.7 × 8 |
139.7 |
8 |
33.1 |
25.98 |
| 139.7 × 10 |
139.7 |
10 |
40.75 |
31.99 |
| 139.7 × 12 |
139.7 |
12 |
48.14 |
37.79 |
| 139.7 × 12.5 |
139.7 |
12.5 |
49.95 |
39.21 |
| 168.3 × 3 |
168.3 |
3 |
15.58 |
12.23 |
| 168.3 × 4 |
168.3 |
4 |
20.65 |
16.21 |
| 168.3 × 5 |
168.3 |
5 |
25.65 |
20.14 |
| 168.3 × 6 |
168.3 |
6 |
30.59 |
24.02 |
| 168.3 × 8 |
168.3 |
8 |
40.29 |
31.63 |
| 168.3 × 10 |
168.3 |
10 |
49.73 |
39.04 |
| 168.3 × 12 |
168.3 |
12 |
58.92 |
46.26 |
| 168.3 × 12.5 |
168.3 |
12.5 |
61.18 |
48.03 |
CHS over 168.3 mm up to 406.4 mm (18 sizes).
Swipe horizontally to view all dimensions.
| D × t (mm) |
Outside diameter D (mm) |
Wall t (mm) |
Area (cm²) |
Mass M (kg/m) |
| 219.1 × 5 |
219.1 |
5 |
33.63 |
26.4 |
| 219.1 × 6 |
219.1 |
6 |
40.17 |
31.53 |
| 219.1 × 8 |
219.1 |
8 |
53.06 |
41.65 |
| 219.1 × 10 |
219.1 |
10 |
65.69 |
51.57 |
| 219.1 × 12 |
219.1 |
12 |
78.07 |
61.29 |
| 219.1 × 12.5 |
219.1 |
12.5 |
81.13 |
63.69 |
| 273 × 5 |
273 |
5 |
42.1 |
33.05 |
| 273 × 6 |
273 |
6 |
50.33 |
39.51 |
| 273 × 8 |
273 |
8 |
66.6 |
52.28 |
| 273 × 10 |
273 |
10 |
82.62 |
64.86 |
| 273 × 12 |
273 |
12 |
98.39 |
77.24 |
| 273 × 12.5 |
273 |
12.5 |
102.3 |
80.3 |
| 323.9 × 5 |
323.9 |
5 |
50.09 |
39.32 |
| 323.9 × 6 |
323.9 |
6 |
59.92 |
47.04 |
| 323.9 × 8 |
323.9 |
8 |
79.39 |
62.32 |
| 323.9 × 10 |
323.9 |
10 |
98.61 |
77.41 |
| 323.9 × 12 |
323.9 |
12 |
117.58 |
92.3 |
| 323.9 × 12.5 |
323.9 |
12.5 |
122.29 |
95.99 |