EN 10219-1 S235JRH Steel Hollow Sections (HSS)
What are EN 10219-1 S235JRH Steel Hollow Sections?
EN 10219-1 S235JRH is a cold-formed welded structural hollow section in non-alloy quality steel number 1.0039. The product may be square, rectangular or circular. The 235 MPa yield class is the lowest non-alloy grade in Annex A of EN 10219-1:2006, and the JR quality verifies impact at +20 °C, and only when Option 1.3 is specified. This page is not the live EN 10219-1 S355J2H page, and it is not a hot-finished EN 10210 section.
Because S235JRH is a milder grade than S355J2H, it must not inherit a mill programme written only for S355. The size tables on this page are a typographical common subset with theoretical masses from the EN 10219-2 formulae, not the Tata Hybox 355 programme used on the S355J2H page.
Material, Manufacture and Scope for EN 10219-1 S235JRH Hollow Sections
EN 10219-1:2006 is the technical delivery standard for cold-formed welded hollow sections. Dimensions and tolerances are those of EN 10219-2. Annex A of Part 1 covers non-alloy grades up to 40 mm thickness. S235JRH is fully killed (FF). JR and J0 qualities are supplied with non-specific inspection unless Option 1.6 is specified. J2 quality, by contrast, is always specific inspection.
The product is formed and welded from strip or plate and is delivered in the cold-formed condition unless a later heat treatment is agreed. It is not a hot-finished EN 10210 hollow section and is not a fluid-conveyance pipe under EN 10255 or EN 10216-1.
EN 10219-1 S235JRH Chemical Composition and Carbon Equivalent
Table A.1 of EN 10219-1:2006, for product thickness ≤ 40 mm, sets these maximum cast-analysis limits for S235JRH, in percent: carbon 0.17, manganese 1.40, phosphorus 0.040, sulphur 0.040 and nitrogen 0.009. Silicon is not specified in that table for this grade. The nitrogen maximum does not apply if total aluminium is at least 0.020 % with an Al/N ratio of at least 2:1, or if sufficient other nitrogen-binding elements are present and recorded.
Table A.2 sets a single maximum CEV of 0.35 % for S235JRH at nominal thicknesses ≤ 40 mm. That figure is tighter than the 0.45 % cap used for S355J0H and S355J2H in the same table, and it is also not the thickness-banded CEV used for S235JRH in EN 10210-1. Do not copy an EN 10210 CEV row onto an EN 10219 certificate.
Swipe horizontally to view all dimensions.
EN 10219-1 S235JRH Mechanical Properties: Yield, Tensile, Elongation and Impact
Table A.3 of EN 10219-1:2006 requires, for S235JRH, a minimum yield ReH of 235 MPa for t ≤ 16 mm and 225 MPa for 16 mm < t ≤ 40 mm. Tensile strength Rm is 360–510 MPa in both the t < 3 mm and the 3 mm ≤ t ≤ 40 mm columns. Minimum elongation A is 24 %, with the notes in the table: for thicknesses > 3 mm and slender sections (D/T < 15 for circular, or (B+H)/2T < 12.5 for square and rectangular) the minimum is reduced by 2; for thicknesses ≤ 3 mm the minimum elongation is 17 %. Transverse values and tests below 3 mm follow the standard’s own rules.
Impact energy is 27 J at +20 °C. Footnote a states that the impact properties of S235JRH are verified only when Option 1.3 is specified. An S235JRH certificate without that option does not automatically carry a verified +20 °C Charpy result. That is a different inspection choice from S355J2H, where 27 J at −20 °C is mandatory.
Swipe horizontally to view all dimensions.
EN 10219-1 S235JRH Common Sizes: Typographical Subset with EN 10219-2 Masses
The tables below are a typographical common-size subset, not a complete EN 10219-2 list and not a mill stock list. They are also not copied from the Tata Hybox 355 programme used on the S355J2H page. Masses are theoretical values computed with the EN 10219-2 Annex A formulae: for circular sections M = 0.785A; for square and rectangular sections the calculation radii are 2.0T / 1.0T for t ≤ 6 mm, 2.5T / 1.5T for 6 mm < t ≤ 10 mm, and 3.0T / 2.0T for t > 10 mm. A 100 × 100 × 5 section is 14.4 kg/m under these rules, not the 14.7 kg/m hot-finished figure. Availability of any one size remains a mill question.
Square hollow sections (128 sizes).
Swipe horizontally to view all dimensions.
Rectangular hollow sections (143 sizes).
Swipe horizontally to view all dimensions.
Circular hollow sections (91 sizes).
CHS up to 168.3 mm (73 sizes).
Swipe horizontally to view all dimensions.
CHS over 168.3 mm up to 406.4 mm (18 sizes).
Swipe horizontally to view all dimensions.
Applications and Service Limits for EN 10219-1 S235JRH Hollow Sections
S235JRH hollow sections are used in general building frames, light columns, trusses and fabrications where a 235 MPa cold-formed hollow section is named and a colder impact quality is not required. The grade is not a substitute for S355J2H where the design needs 355 MPa or a −20 °C Charpy result. It is also not a pressure pipe and not a hot-finished EN 10210 section.
Near-Equivalents for EN 10219-1 S235JRH Hollow Sections: Not Automatic Substitutes
EN 10219-1 S355J2H and S355J0H are higher-strength grades in the same Part 1, with different chemistry, CEV and impact rules. EN 10210-1 S235JRH is hot-finished and uses a different CEV table and a thickness range beyond 40 mm. ASTM A500 Grade A or B, and GB/T 6728 Q235B sections, follow different specifications and must not be restamped as S235JRH.
Sourcing EN 10219-1 S235JRH Steel Hollow Sections from SHH STEEL
Send the shape, the designated size and thickness, the length, the EN 10219-1 edition, and whether Option 1.3 impact testing or a Declaration of Performance is required. Name S235JRH explicitly. SHH STEEL reviews the grade, size and certificate before quoting. The size tables are a typographical reference, not a warehouse list.
EN 10219-1 S235JRH Hollow Section FAQs
-
Is S235JRH the same product as the live S355J2H page?
- No. S235JRH is the 235 MPa JR quality. S355J2H is a 355 MPa grade with mandatory −20 °C impact testing. They do not share a mill programme on this site, and they should be ordered under the grade the design names.
-
Is the +20 °C impact test always done?
- Only when Option 1.3 is specified. EN 10219-1:2006 footnote a to Table A.3 says the impact properties of S235JRH are verified only under that option.
-
Why are the masses different from EN 10210?
- Cold-formed and hot-finished square or rectangular sections use different calculation corner radii. A 100 × 100 × 5 section is about 14.4 kg/m under EN 10219-2 and 14.7 kg/m under EN 10210-2.
-
Are these tables the Hybox 355 range?
- No. Hybox 355 is an S355J2H mill programme. These tables are a typographical common subset with EN 10219-2 theoretical masses.
Conclusion
EN 10219-1 S235JRH is the cold-formed 235 MPa hollow section of steel number 1.0039. Impact at +20 °C is verified only when Option 1.3 is specified. The size tables are a typographical common subset with EN 10219-2 masses, not a Hybox 355 list and not a stock list. Confirm the grade, the options, the size and the certificate on the order.