DIN 17100 St37-2 Steel Angles | DIN 17100 Steel Angles - SHH STEEL

DIN 17100 St37-2 Steel Angles

DIN 17100 St37-2 (1.0037) is a withdrawn general structural steel (DIN 17100:1980). This page covers equal and unequal angles. Minimum yield is 235 MPa up to 16 mm; tensile strength is 340–470 MPa for 3–100 mm. The grade is superseded by EN 10025-2 S235JR. A St37-2 certificate is not an S235JR certificate. Size tables are an EN 10056 typographical cross-reference.
Keywords
DIN 17100 St37-2 steel angle, St37-2 equal unequal angle, DIN 17100 1.0037 angle, withdrawn St37-2 angle, St37-2 superseded S235JR
Equivalent Grades:
Near-equivalents only, not automatic substitutes.
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Size Chart
Applications
Comparison
Equivalent Grades
Sourcing
FAQ
Conclusion

What are DIN 17100 St37-2 Steel Angles?

DIN 17100 St37-2, also written St 37-2, is a general structural steel in the withdrawn German standard DIN 17100, last issued in 1980. The steel number for St37-2 is 1.0037. This page is for hot-rolled equal-leg and unequal-leg angles, not for a plate, a bar sold as a merchant bar only, a U-section, or an I or H section.

DIN 17100 covered steel sections, including angles, as well as bars, flats and other product forms delivered in the hot-formed or normalized condition. The standard is not current. New structural work should be specified to a living standard, ordinarily EN 10025-2 for this strength class. The live successor angle page on this site is EN 10025-2 S235JR Equal and Unequal Steel Angles.

DIN 17100 is Withdrawn and is Superseded by EN 10025-2 S235JR

DIN 17100, steels for general structural purposes, was withdrawn in the mid-1990s when DIN EN 10025 was adopted. The current European material standard for this class of non-alloy structural steel is EN 10025-2. The usual successor grade named for St37-2 is S235JR (steel number 1.0038).

That mapping is a successor relationship, not an identity of certificates. EN 10025-2 S235JR Equal and Unequal Steel Angles has its own EN 10025-2 chemistry, a 360–510 MPa tensile window for the usual long-product thicknesses, and a 27 J impact requirement at +20 °C across the tabulated thicknesses. A St37-2 inspection document is not an S235JR document, and an S235JR document is not automatically a DIN 17100 St37-2 document.

Do not confuse St37-2 (1.0037) with RSt37-2 (1.0038). RSt37-2 is a related, killed DIN 17100 designation that later shares a steel number with S235JR; it is not this page. USt37-2 (1.0036) is the rimmed companion and is also not this page. St37-3 is a higher DIN 17100 quality and is not this product.

DIN 17100 St37-2 Chemical Composition for Angles (Ladle Analysis)

The table recites the DIN 17100:1980 Table 1 ladle-analysis limits for St37-2 from two independent public recitations of that edition. Product (sample) analysis variations are wider and are not rewritten here as shop maxima. The edition actually named on a legacy order governs if one is cited.

Swipe horizontally to view all dimensions.

Element Ladle-analysis limit used on this page (St37-2) Notes
C, max, t ≤ 16 mm (%) 0.17 DIN 17100:1980 Table 1, St37-2 (1.0037).
C, max, thicker Table 1 bands through 100 mm (%) 0.20 The first step after 16 mm is 0.20 % in the recitations compared for this page; St37-2 stays at 0.20 % in the remaining Table 1 bands through 100 mm.
P, max (%) 0.050 Ladle analysis.
S, max (%) 0.050 Ladle analysis.
N, max (%) 0.009 Ladle analysis for St37-2.
Si, Mn No maxima in the St37-2 Table 1 row used here Do not copy the St52-3 silicon or manganese footnote onto St37-2.

DIN 17100 St37-2 Mechanical Properties: Yield and Tensile Strength

Table 2 of DIN 17100:1980 gives St37-2 a tensile range of 340–470 N/mm² for product thicknesses from 3 mm to 100 mm, and 360–510 N/mm² below 3 mm. Minimum upper yield point is 235 N/mm² at t ≤ 16 mm, then 225, 215, 205 and 195 N/mm² in the 16–40, 40–63, 63–80 and 80–100 mm bands. RSt37-2 holds 215 N/mm² in the two thickest of those bands; that is not the St37-2 row used here.

DIN 17100 Table 2 also specifies minimum elongation at rupture, which depends on specimen position, thickness and gauge length. Two public recitations of that elongation column do not agree closely enough, after layout reconstruction, for this page to reprint a single elongation table. Confirm elongation against the named edition, or specify the successor EN 10025-2 grade if a current elongation table is required.

The same recitations list an ISO-V longitudinal average of 27 J at +20 °C for St37-2 in the 10–16 mm band, in the U or N condition, with thicker-band impact cells left blank. That is not the same impact coverage as EN 10025-2 S235JR. Do not treat a St37-2 document as a silent 27 J guarantee at +20 °C for every thickness.

Swipe horizontally to view all dimensions.

Nominal thickness (mm) Minimum upper yield ReH (N/mm²) Tensile strength Rm (N/mm²)
< 3 — 360–510
3–100, t ≤ 16 235 340–470
> 16–40 225 340–470
> 40–63 215 340–470
> 63–80 205 340–470
> 80–100 195 340–470

DIN 17100 St37-2 Angle Sizes: EN 10056 Cross-Reference (DIN 1028 / 1029 Historical)

Historical German equal-leg and unequal-leg angle dimensions were tabulated in DIN 1028 and DIN 1029. Those dimensional standards have been replaced in current European practice by EN 10056-1, with tolerances in EN 10056-2. This page does not transcribe an unverified DIN 1028 or DIN 1029 annex.

The tables below are therefore a typographical cross-reference: the same verified EN 10056-1:2017 subset already published on EN 10025-2 S235JR Equal and Unequal Steel Angles (71 equal-leg sizes, from L 80×80×8 to L 300×300×35, and five unequal-leg sizes in the L 200×100 family). They are for identification and estimating on a withdrawn-grade enquiry, not a rolling programme, not a warehouse list, and not a claim that every EN 10056-1 or every historical DIN 1028/1029 size is shown.

L 200×200×16 is a 200 mm equal angle, 16 mm thick, at the boundary of the first DIN 17100 St37-2 yield band (235 MPa). L 200×200×20 is 20 mm thick, so the St37-2 minimum yield in Table 2 is 225 MPa, not 235 MPa. L 200×100×12 is an unequal 200 mm by 100 mm angle and is not L 200×200×12. American L-shapes, and Chinese or Japanese angle designations, belong to their own dimensional standards, not to these EN 10056 rows.

Equal-leg angles (71 verified sizes, L 80×80×8 to L 300×300×35)

L 80 to L 150 equal (15 sizes)

Swipe horizontally to view all dimensions.

Designation Leg h = b (mm) t (mm) A (cm²) Mass (kg/m)
L 80×80×8 80 8 12.3 9.63
L 90×90×6 90 6 10.6 8.3
L 130×130×10 130 10 25.2 19.8
L 130×130×11 130 11 27.6 21.7
L 130×130×12 130 12 30 23.6
L 130×130×13 130 13 32.3 25.4
L 130×130×14 130 14 34.7 27.2
L 150×150×10 150 10 29.3 23
L 150×150×12 150 12 34.8 27.3
L 150×150×13 150 13 37.6 29.5
L 150×150×14 150 14 40.3 31.6
L 150×150×15 150 15 43 33.8
L 150×150×16 150 16 45.7 35.9
L 150×150×18 150 18 51 40.1
L 150×150×20 150 20 56.3 44.2

L 160 to L 200 equal (28 sizes)

Swipe horizontally to view all dimensions.

Designation Leg h = b (mm) t (mm) A (cm²) Mass (kg/m)
L 160×160×14 160 14 43.2 33.9
L 160×160×15 160 15 46.1 36.2
L 160×160×16 160 16 49 38.4
L 160×160×17 160 17 51.8 40.7
L 160×160×18 160 18 54.7 42.9
L 160×160×19 160 19 57.5 45.1
L 160×160×20 160 20 60.3 47.3
L 180×180×13 180 13 45.5 35.7
L 180×180×14 180 14 48.8 38.3
L 180×180×15 180 15 52.1 40.9
L 180×180×16 180 16 55.4 43.5
L 180×180×17 180 17 58.7 46
L 180×180×18 180 18 61.9 48.6
L 180×180×19 180 19 65.1 51.1
L 180×180×20 180 20 68.3 53.7
L 180×180×22 180 22 74.9 58.6
L 200×200×15 200 15 58.1 45.6
L 200×200×16 200 16 61.8 48.5
L 200×200×17 200 17 65.5 51.4
L 200×200×18 200 18 69.1 54.2
L 200×200×19 200 19 72.7 57.1
L 200×200×20 200 20 76.3 59.9
L 200×200×21 200 21 79.9 62.8
L 200×200×22 200 22 83.5 65.6
L 200×200×23 200 23 87.1 68.3
L 200×200×24 200 24 90.6 71.1
L 200×200×25 200 25 94.1 73.9
L 200×200×26 200 26 97.6 76.6

L 250 to L 300 equal (28 sizes)

Swipe horizontally to view all dimensions.

Designation Leg h = b (mm) t (mm) A (cm²) Mass (kg/m)
L 250×250×17 250 17 82.1 64.4
L 250×250×18 250 18 86.7 68.1
L 250×250×19 250 19 91.4 71.7
L 250×250×20 250 20 96 75.3
L 250×250×21 250 21 101 78.9
L 250×250×22 250 22 105 82.5
L 250×250×23 250 23 110 86.1
L 250×250×24 250 24 114 89.7
L 250×250×25 250 25 119 93.2
L 250×250×26 250 26 123 96.7
L 250×250×27 250 27 128 101
L 250×250×28 250 28 133 104
L 250×250×29 250 29 137 107
L 250×250×30 250 30 141 111
L 250×250×31 250 31 145 114
L 250×250×32 250 32 150 118
L 250×250×33 250 33 154 121
L 250×250×34 250 34 158 124
L 250×250×35 250 35 163 128
L 300×300×27 300 27 154 121
L 300×300×28 300 28 159 125
L 300×300×29 300 29 165 129
L 300×300×30 300 30 170 133
L 300×300×31 300 31 175 138
L 300×300×32 300 32 181 142
L 300×300×33 300 33 186 146
L 300×300×34 300 34 191 150
L 300×300×35 300 35 197 154

Unequal-leg angles (5 verified sizes, L 200×100×10 to L 200×100×16)

Swipe horizontally to view all dimensions.

Designation Long leg h (mm) Short leg b (mm) t (mm) A (cm²) Mass (kg/m)
L 200×100×10 200 100 10 29.2 23
L 200×100×12 200 100 12 34.8 27.3
L 200×100×14 200 100 14 40.3 31.6
L 200×100×15 200 100 15 43 33.7
L 200×100×16 200 100 16 45.7 35.9

Applications and Service Limits for DIN 17100 St37-2 Angles

St37-2 angles still appear on older drawings, bills of materials and maintenance enquiries. For new design, specify a current standard and grade, ordinarily EN 10025-2 S235JR with an EN 10056 designation, unless the contract truly requires a legacy DIN 17100 document. Weldability, coating and inspection must be stated on the order. This page does not convert a withdrawn grade into a design code listing.

DIN 17100 St37-2 Angles Compared with EN 10025-2 S235JR and Related DIN Grades

EN 10025-2 S235JR Equal and Unequal Steel Angles is the live successor page for this strength class. Read the two pages together when a legacy enquiry uses the St37-2 name. The tensile window, phosphorus and sulfur maxima, and the impact coverage are not the same.

USt37-2 and RSt37-2 remain different DIN 17100 designations. St52-3 is a higher-strength DIN 17100 grade and has its own companion page, not this one.

Near-Equivalents for DIN 17100 St37-2 Steel Angles: Not Automatic Substitutes

Near-equivalents only, not automatic substitutes. EN 10025-2 S235JR is the usual successor grade, not a drop-in certificate. S235J0 and S235J2 are colder impact qualities in EN 10025-2 and are not implied by St37-2. ASTM A36, GB/T 706 Q235B and JIS G 3101 SS400 angles use different chemistry and different shape standards. Do not treat any of those certificates as DIN 17100 St37-2, or the reverse.

Sourcing DIN 17100 St37-2 Steel Angles from SHH STEEL

SHH STEEL reviews whether the enquiry truly requires a withdrawn DIN 17100 document or can be fulfilled as EN 10025-2 S235JR Equal and Unequal Steel Angles under EN 10025-2. State the designation (for example L 200×200×16 or the historical DIN size), the length, and the certificate required. These angles are filed under Steel Angles. The typographical size tables on this page are not a warehouse list.

FAQ: DIN 17100 St37-2 Steel Angles

Is DIN 17100 still a current standard?
No. DIN 17100 was withdrawn after DIN EN 10025 was adopted. The last edition used on this page is DIN 17100:1980. The usual successor grade for St37-2 angles is EN 10025-2 S235JR.
Can a St37-2 certificate be used as S235JR?
No. The mapping is a successor relationship, not an identity of certificates. Chemistry, tensile window and impact coverage differ. Specify the standard actually required on the order.
Which size standard is used on this page?
Historical German angle sizes were in DIN 1028 (equal) and DIN 1029 (unequal). This page does not transcribe an unverified annex of those standards. The tables are the verified EN 10056-1 subset already used on the live S235JR angle page, as a typographical cross-reference, not a warehouse list.

Conclusion

Treat DIN 17100 St37-2 as a withdrawn grade for equal and unequal angles, with the 1.0037 chemistry and the Table 2 yield and tensile bands recited here. For current supply, prefer EN 10025-2 S235JR unless the contract truly requires a legacy DIN 17100 document. The two certificates are not interchangeable.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X