ASTM B265 Grade 21 Titanium Plate | TIMETAL 21S (UNS R58210)

ASTM B265 Grade 21 titanium plate is TIMETAL 21S titanium alloy (UNS R58210) supplied solution treated. It is specified for 793 MPa minimum tensile strength, 759 MPa yield and 15% minimum elongation. Typical uses include aerospace sheet structures and engine nacelle parts. SHH STEEL reviews size, finish and certificate requirements before quoting.
Keywords
ASTM B265 Grade 21 titanium plate, Grade 21 titanium plate, UNS R58210 plate, TIMETAL 21S titanium alloy plate, ASTM B265 titanium sheet
Equivalent Grades:
UNS R58210, ASME SB-265 Gr.21
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why choose Us
Our Service
FAQ
Conclusion

What is ASTM B265 Grade 21 titanium plate?

ASTM B265 Grade 21 titanium plate is made to ASTM B265, the ASTM specification for titanium and titanium alloy strip, sheet and plate. It carries the UNS number R58210. Grade 21 is Ti-15Mo-3Al-2.7Nb-0.25Si, a metastable beta alloy known commercially as Beta 21S. It was developed as an oxidation-resistant, cold-rollable beta sheet alloy and resists hydraulic fluids and many acids.

This is a beta or metastable beta titanium alloy. Large additions of beta-stabilising elements such as vanadium, molybdenum, chromium or niobium keep a body-centred cubic structure after solution treatment. That structure is cold formable, and many beta alloys can then be aged to very high strength.

Its typical density of about 4.94 g/cm³ is a little over half that of carbon steel, which is one reason titanium plate is chosen where weight matters.

ASTM B265 groups its grades into unalloyed titanium, corrosion-resistant grades with small additions of palladium, ruthenium, nickel or molybdenum, and structural alloys such as Ti-3Al-2.5V and Ti-6Al-4V. Each grade has its own UNS number, and the H grades add a higher guaranteed tensile strength for pressure vessel use.

SHH STEEL handles Grade 21 plate enquiries within its range of titanium alloy plates and sheets, checking the ordered ASTM B265 edition, product form and certificate type before confirming supply. Related designations covered on this site include ASME SB-265 Grade 21.

Material specification for ASTM B265 Grade 21

ASTM B265 classifies flat titanium products by thickness and width. The same chemistry and tensile requirements apply to strip, sheet and plate, but dimensional tolerances and bend testing differ by product form.

Ordering item ASTM B265 basis
Standard ASTM B265, Titanium and Titanium Alloy Strip, Sheet, and Plate; state the edition on the order
Grade / UNS Grade 21, TIMETAL 21S, UNS R58210
Plate Over 0.187 in (4.75 mm) thick and over 10 in (254 mm) wide
Sheet 0.187 in (4.75 mm) and under, 24 in (610 mm) wide or more; state cold or hot rolled
Strip 0.187 in (4.75 mm) and under, less than 24 in (610 mm) wide
Condition Solution treated, as required for this beta grade; aged properties by agreement
Certificate Manufacturer’s report with chemical analysis, tensile results and other required tests

Order information listed by the specification includes grade, product limitations, special mechanical properties, marking, finish, packaging, any additional reports and the disposition of rejected material. For ASME Code construction, order to ASME SB-265 Grade 21 and state any dual certification on the purchase order.

Chemical composition of ASTM B265 Grade 21 (UNS R58210)

Single values are maximums; ranges are shown where an element is added. Titanium is determined by difference. Product analysis tolerances cover variation between laboratories and do not broaden the heat analysis limits.

Element Heat analysis, % Permissible variation in product analysis, %
Nitrogen (N) 0.03 +0.02
Carbon (C) 0.05 +0.02
Hydrogen (H) 0.015 +0.002
Iron (Fe) 0.40 +0.15
Oxygen (O) 0.17 +0.03
Aluminium (Al) 2.5–3.5 ±0.40
Molybdenum (Mo) 14.0–16.0 ±0.50
Niobium (Nb) 2.2–3.2 ±0.15
Silicon (Si) 0.15–0.25 ±0.02
Other elements, each 0.15 +0.02
Other elements, total 0.4 —
Titanium (Ti) Balance —

Ingot top and bottom are analysed for the listed elements. Hydrogen is tested and reported on at least one final product sample, and a lower hydrogen limit may be negotiated. Other elements need not be reported unless they exceed 0.10% each or 0.40% total, and they may not be added intentionally.

Mechanical properties of ASTM B265 Grade 21

The values below are the requirements for Grade 21 plate in the solution treated condition.

Property Requirement
Tensile strength, min 115 ksi (793 MPa)
Yield strength, 0.2% offset 110 ksi (759 MPa) min
Elongation in 2 in or 50 mm, min 15%
Bend test, under 0.070 in (1.8 mm) Mandrel radius 3T, bent 105° without outside fracture
Bend test, 0.070–0.187 in (1.8–4.75 mm) Mandrel radius 3T
Bend test, over 0.187 in (4.75 mm) Not applicable to material over 4.75 mm

Tensile tests are made at room temperature. Only a minimum yield strength is set for this grade. Bend tests apply to sheet and strip up to 0.187 in (4.75 mm); plate over that thickness is not bend tested under the specification.

Elevated-temperature design values are not part of the plate specification. They come from the design code, such as ASME Section II, Part D where the grade is listed.

Delivery condition, finish and marking

ASTM B265 covers material in the annealed condition, or for this beta alloy normally solution treated. Plate must be free of injurious external and internal imperfections. Annealed product may be furnished descaled, sandblasted, ground, or sandblasted and ground; state the finish on the order.

  • Condition: Solution treated, as required for this beta grade; aged properties by agreement
  • Surface: descaled, sandblasted or ground, as ordered; minor spot grinding is permitted within the thickness tolerance
  • Marking: specification, grade, heat number, manufacturer’s identification and nominal thickness, in rows that can be removed with hot alkaline cleaning
  • Packaging: boxed, crated, boarded or as the manufacturer’s standard practice unless the order states otherwise

Material is normally purchased solution treated. Aged properties are not fixed by the plate specification and must be agreed between purchaser and manufacturer. If the plate will be formed or welded in your shop, say so at enquiry so the finish and protective packing suit the next process.

Welding and fabrication of Grade 21 titanium plate

Grade 21 can be welded by gas tungsten arc, electron beam or laser with full inert-gas shielding, but weld properties depend strongly on the heat treatment that follows.

  • Shield the weld, heat-affected zone and root until below about 400 °C
  • Agree the post-weld heat treatment with the designer, since ageing response differs between weld and base metal
  • Use qualified procedures and approved filler metal
  • Keep joints clean and free of iron contamination

In the solution-treated condition beta alloys can be cold formed more easily than alpha-beta alloys. Forming is normally done before ageing.

Beta alloys are machined with sharp carbide tools, low speeds and generous coolant, and tool wear is higher in the aged condition, so heavy machining is often done before ageing. Keep fine chips away from ignition sources.

These are general practices, not a qualified procedure. The fabricator must qualify the welding procedure, filler metal and inspection to the applicable code.

Dimensional tolerances and flatness

Dimensional tolerances are set in the specification’s tables for thickness, width, length, weight and flatness. Plate flatness has its own table for annealed plate. For sheet, cold-rolled tolerances apply unless hot-rolled sheet is ordered.

State the nominal thickness, width, length, quantity and any cutting drawing at enquiry. If a project needs tighter flatness, a specific edge condition or cut-to-size pieces, write it on the order rather than relying on the default tables. No stock sizes are implied by this page.

Titanium plate can be cut by waterjet, abrasive saw, plasma or machining. Thermal cutting leaves an oxygen-enriched edge that should be removed by machining or grinding before welding or forming, so agree the cut-edge condition and any machining allowance on the order.

Applications and service limits of Grade 21 titanium plate

Typical uses of Grade 21 plate include:

  • Aerospace sheet structures and engine nacelle parts
  • Metal-matrix composite foil and sheet
  • Parts exposed to hydraulic fluids at elevated temperature
  • High-strength formed sheet components

Aged properties are not fixed by B265 and must be agreed. Beta alloys have good resistance to many media, but they are not suited to hydrofluoric acid, fluoride-bearing media or dry chlorine. They are denser than Ti-6Al-4V, and aged properties, toughness and service temperature limits must be agreed for the part.

When selecting Grade 21, compare it with Grade 19, Grade 20, Grade 36. The choice usually turns on the balance of strength, formability, corrosion behaviour in the actual medium and cost, and on which standard the drawing or design code names.

Compare Grade 21 with other ASTM B265 grades

The grades below are the closest neighbours of Grade 21 in ASTM B265. Values are tensile strength, 0.2% yield or proof strength and minimum elongation, as set by the standard.

Grade Tensile strength Yield / proof strength Elongation, min Typical role
Grade 19 (R58640) 115 ksi (793 MPa) 110 ksi (759 MPa) min 15% Beta C, heat-treatable beta alloy
Grade 20 (R58645) 115 ksi (793 MPa) 110 ksi (759 MPa) min 15% Beta C with Pd
Grade 21 (R58210) 115 ksi (793 MPa) 110 ksi (759 MPa) min 15% Ti-15Mo-3Al-2.7Nb-0.25Si beta alloy
Grade 36 (R58450) 65 ksi (450 MPa) 60–95 ksi (410–655 MPa) 10% Ti-45Nb beta alloy

Beta alloys are usually chosen for formability before ageing and for high aged strength, not for corrosion alone. Compare the agreed heat-treated properties before changing grade.

ASTM B265 Grade 21 equivalent grades

The designations below are commonly compared with ASTM B265 Grade 21. They are close in composition and role, but limits, tests and product forms are set by each standard, so they are not automatically interchangeable.

Standard / system Designation Relationship to ASTM B265 Grade 21
ASME SB-265 Grade 21 ASME Code adoption of B265; ordered for pressure equipment
UNS R58210 Same unified number as ASTM Grade 21
GB/T 3620.1 designation TB8 (Ti-15Mo-3Al-2.7Nb-0.25Si) Similar nominal composition

Where a drawing names one designation and the supplier offers another, agree in writing which standard governs chemistry, tensile values, testing and marking. Dual or multiple certification is possible only when the material meets every cited standard in full, and the certificate must show the results against each one.

Why choose SHH STEEL for Grade 21 titanium plate

SHH STEEL supports specification-led purchasing of titanium plate and sheet.

  • We quote to the ASTM B265 edition, grade and product form you name, and keep B265 and SB-265 requirements distinct
  • Certificates are checked against the Grade 21 chemistry and tensile limits
  • Sizes, quantities, testing and delivery are confirmed in the quotation, not assumed
  • Finish, marking and packing are agreed before production

Questions on equivalents, dual certification or edition changes are answered before an order is placed.

How to enquire for ASTM B265 Grade 21 plate

Send the material schedule with the details below. We review the enquiry and raise any open points before confirming the supply route.

Enquiry item Information required
Material ASTM B265 Grade 21 (UNS R58210), edition; add ASME SB-265 if Code use
Product form Plate, sheet or strip; for sheet, cold or hot rolled
Dimensions Thickness, width, length, quantity and any cutting drawing
Finish Descaled, sandblasted, ground or other agreed surface
Testing Any special mechanical properties, extra analysis or reports
Documents Certificate type and any third-party inspection
Destination Delivery place and packing requirements

FAQ

Is ASTM B265 Grade 21 the same as ASME SB-265 Grade 21?
SB-265 is the ASME Code adoption of B265, so Grade 21 requirements normally match. They are separate documents, and ASME may adopt a different edition. For Code work, order SB-265 Grade 21 or dual certification.
What is the tensile strength of ASTM B265 Grade 21 titanium plate?
The requirement is 115 ksi (793 MPa) minimum. The 0.2% proof or yield strength is 110 ksi (759 MPa) minimum. Minimum elongation is 15%. Values apply to the condition and thickness range stated in the standard.
What is Grade 21 mainly used for?
Typical uses include aerospace sheet structures and engine nacelle parts, metal-matrix composite foil and sheet and parts exposed to hydraulic fluids at elevated temperature. Aged properties are not fixed by B265 and must be agreed.
When is a titanium product classed as plate under B265?
Plate is over 0.187 in (4.75 mm) thick and over 10 in (254 mm) wide. Thinner product is sheet if 24 in (610 mm) wide or more, otherwise strip.
What should I send for a quotation?
Send ASTM B265 Grade 21, the edition, product form, thickness, width, length and quantity, the finish, any special testing, the certificate type and the destination. Add ASME SB-265 if the plate is for Code construction.

Request a quotation for ASTM B265 Grade 21 titanium plate

ASTM B265 Grade 21 is TIMETAL 21S titanium alloy, UNS R58210, specified for 115 ksi (793 MPa) minimum tensile strength, 110 ksi (759 MPa) minimum yield or proof strength and 15% minimum elongation in the solution treated condition. Typical uses include aerospace sheet structures and engine nacelle parts and metal-matrix composite foil and sheet.

Send the product form, sizes, quantity, finish, certificate type and destination to SHH STEEL. Compare other grades on the ASTM B265 page or browse all titanium alloy plates and sheets. Availability, testing and delivery are confirmed against each enquiry.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X