ASTM B265 Grade 25 Titanium Plate | Ti-6Al-4V with Ni and Pd (UNS R56403)
What is ASTM B265 Grade 25 titanium plate?
ASTM B265 Grade 25 titanium plate is made to ASTM B265, the ASTM specification for titanium and titanium alloy strip, sheet and plate. It carries the UNS number R56403. Grade 25 is Ti-6Al-4V with 0.3–0.8% nickel and 0.04–0.08% palladium. It is aimed at high-strength parts that must resist crevice corrosion in hot brines.
This is an alpha-beta titanium alloy. Aluminium strengthens the alpha phase and vanadium or molybdenum stabilises the beta phase, so the structure and properties depend on hot working and heat treatment. Plate is normally supplied mill annealed, giving high strength, good fatigue performance and a strength-to-weight ratio well above that of steels.
Its typical density of about 4.43 g/cm³ is a little over half that of carbon steel, which is one reason titanium plate is chosen where weight matters.
ASTM B265 groups its grades into unalloyed titanium, corrosion-resistant grades with small additions of palladium, ruthenium, nickel or molybdenum, and structural alloys such as Ti-3Al-2.5V and Ti-6Al-4V. Each grade has its own UNS number, and the H grades add a higher guaranteed tensile strength for pressure vessel use.
SHH STEEL handles Grade 25 plate enquiries within its range of titanium alloy plates and sheets, checking the ordered ASTM B265 edition, product form and certificate type before confirming supply. Related designations covered on this site include ASME SB-265 Grade 25, ASTM B265 Grade 24.
Material specification for ASTM B265 Grade 25
ASTM B265 classifies flat titanium products by thickness and width. The same chemistry and tensile requirements apply to strip, sheet and plate, but dimensional tolerances and bend testing differ by product form.
| Ordering item | ASTM B265 basis |
|---|---|
| Standard | ASTM B265, Titanium and Titanium Alloy Strip, Sheet, and Plate; state the edition on the order |
| Grade / UNS | Grade 25, Ti-6Al-4V with Ni and Pd, UNS R56403 |
| Plate | Over 0.187 in (4.75 mm) thick and over 10 in (254 mm) wide |
| Sheet | 0.187 in (4.75 mm) and under, 24 in (610 mm) wide or more; state cold or hot rolled |
| Strip | 0.187 in (4.75 mm) and under, less than 24 in (610 mm) wide |
| Condition | Annealed |
| Certificate | Manufacturer’s report with chemical analysis, tensile results and other required tests |
Order information listed by the specification includes grade, product limitations, special mechanical properties, marking, finish, packaging, any additional reports and the disposition of rejected material. For ASME Code construction, order to ASME SB-265 Grade 25 and state any dual certification on the purchase order.
Chemical composition of ASTM B265 Grade 25 (UNS R56403)
Single values are maximums; ranges are shown where an element is added. Titanium is determined by difference. Product analysis tolerances cover variation between laboratories and do not broaden the heat analysis limits.
| Element | Heat analysis, % | Permissible variation in product analysis, % |
|---|---|---|
| Nitrogen (N) | 0.05 | +0.02 |
| Carbon (C) | 0.08 | +0.02 |
| Hydrogen (H) | 0.015 | +0.002 |
| Iron (Fe) | 0.40 | +0.15 |
| Oxygen (O) | 0.20 | +0.03 |
| Aluminium (Al) | 5.5–6.75 | ±0.40 |
| Vanadium (V) | 3.5–4.5 | ±0.15 |
| Nickel (Ni) | 0.3–0.8 | ±0.05 |
| Palladium (Pd) | 0.04–0.08 | ±0.005 |
| Other elements, each | 0.1 | +0.02 |
| Other elements, total | 0.4 | — |
| Titanium (Ti) | Balance | — |
Ingot top and bottom are analysed for the listed elements. Hydrogen is tested and reported on at least one final product sample, and a lower hydrogen limit may be negotiated. Other elements need not be reported unless they exceed 0.10% each or 0.40% total, and they may not be added intentionally.
Mechanical properties of ASTM B265 Grade 25
The values below are the requirements for Grade 25 plate in the annealed condition.
| Property | Requirement |
|---|---|
| Tensile strength, min | 130 ksi (895 MPa) |
| Yield strength, 0.2% offset | 120 ksi (828 MPa) min |
| Elongation in 2 in or 50 mm, min | 10% |
| Bend test, under 0.070 in (1.8 mm) | Mandrel radius 4.5T, bent 105° without outside fracture |
| Bend test, 0.070–0.187 in (1.8–4.75 mm) | Mandrel radius 5T |
| Bend test, over 0.187 in (4.75 mm) | Not applicable to material over 4.75 mm |
Tensile tests are made at room temperature. Only a minimum yield strength is set for this grade. Bend tests apply to sheet and strip up to 0.187 in (4.75 mm); plate over that thickness is not bend tested under the specification.
Elevated-temperature design values are not part of the plate specification. They come from the design code, such as ASME Section II, Part D where the grade is listed.
Delivery condition, finish and marking
ASTM B265 covers material in the annealed condition. Plate must be free of injurious external and internal imperfections. Annealed product may be furnished descaled, sandblasted, ground, or sandblasted and ground; state the finish on the order.
- Condition: Annealed
- Surface: descaled, sandblasted or ground, as ordered; minor spot grinding is permitted within the thickness tolerance
- Marking: specification, grade, heat number, manufacturer’s identification and nominal thickness, in rows that can be removed with hot alkaline cleaning
- Packaging: boxed, crated, boarded or as the manufacturer’s standard practice unless the order states otherwise
Plate is supplied annealed. Solution treating and ageing, where wanted, is normally done on the part and its properties are agreed separately. If the plate will be formed or welded in your shop, say so at enquiry so the finish and protective packing suit the next process.
Welding and fabrication of Grade 25 titanium plate
Grade 25 can be welded by gas tungsten arc, plasma arc, electron beam and laser processes, but it needs more control than CP titanium.
- Shield the weld, heat-affected zone and root with inert gas until below about 400 °C
- Use qualified procedures and matching or engineer-approved filler metal
- Expect lower weld-zone ductility than in the base plate; stress relief after welding is common
- Clean joints thoroughly and avoid iron contamination
Cold formability is limited. Most forming of alpha-beta plate is done hot or by creep forming, and machining needs sharp tools, rigid set-ups and generous coolant.
Plan machining around the low thermal conductivity of the alloy: heat stays at the tool edge, so cutting speeds are low and coolant flow is high. Avoid interrupted light cuts that work-harden the surface, and keep fine chips away from ignition sources.
These are general practices, not a qualified procedure. The fabricator must qualify the welding procedure, filler metal and inspection to the applicable code.
Dimensional tolerances and flatness
Dimensional tolerances are set in the specification’s tables for thickness, width, length, weight and flatness. Plate flatness has its own table for annealed plate. For sheet, cold-rolled tolerances apply unless hot-rolled sheet is ordered.
State the nominal thickness, width, length, quantity and any cutting drawing at enquiry. If a project needs tighter flatness, a specific edge condition or cut-to-size pieces, write it on the order rather than relying on the default tables. No stock sizes are implied by this page.
Titanium plate can be cut by waterjet, abrasive saw, plasma or machining. Thermal cutting leaves an oxygen-enriched edge that should be removed by machining or grinding before welding or forming, so agree the cut-edge condition and any machining allowance on the order.
Applications and service limits of Grade 25 titanium plate
Typical uses of Grade 25 plate include:
- Geothermal and oil and gas parts in hot brine
- High-strength chemical process equipment
- Marine and subsea components
- Fastener blanks and structural parts in crevice-prone service
Alpha-beta alloys resist seawater and many oxidizing media well, but they are less resistant than CP titanium in hot reducing acids. They are not suited to hydrofluoric acid, fluoride-bearing media, dry chlorine or red fuming nitric acid. Maximum service temperature and fatigue design values come from the applicable design code, not from the plate specification.
When selecting Grade 25, compare it with Grade 5, Grade 23, Grade 24. The choice usually turns on the balance of strength, formability, corrosion behaviour in the actual medium and cost, and on which standard the drawing or design code names.
Compare Grade 25 with other ASTM B265 grades
The grades below are the closest neighbours of Grade 25 in ASTM B265. Values are tensile strength, 0.2% yield or proof strength and minimum elongation, as set by the standard.
| Grade | Tensile strength | Yield / proof strength | Elongation, min | Typical role |
|---|---|---|---|---|
| Grade 5 (R56400) | 130 ksi (895 MPa) | 120 ksi (828 MPa) min | 10% | Workhorse alpha-beta alloy |
| Grade 23 (R56407) | 120 ksi (828 MPa) | 110 ksi (759 MPa) min | 10% | Ti-6Al-4V ELI, damage-tolerant |
| Grade 24 (R56405) | 130 ksi (895 MPa) | 120 ksi (828 MPa) min | 10% | Ti-6Al-4V with Pd |
| Grade 25 (R56403) | 130 ksi (895 MPa) | 120 ksi (828 MPa) min | 10% | Ti-6Al-4V with Ni and Pd |
| Grade 29 (R56404) | 120 ksi (828 MPa) | 110 ksi (759 MPa) min | 10% | Ti-6Al-4V ELI with Ru |
| Grade 35 (R56340) | 130 ksi (895 MPa) | 120 ksi (828 MPa) min | 5% | Ti-4.5Al-2Mo-1.6V-0.5Fe-0.3Si alpha-beta alloy |
| Grade 38 (R54250) | 130 ksi (895 MPa) | 115 ksi (794 MPa) min | 10% | Ti-4Al-2.5V-1.5Fe alpha-beta alloy |
A higher strength level is not automatically better. Interstitial limits, toughness, bend radius and fatigue behaviour differ between grades, so changes need engineer approval.
ASTM B265 Grade 25 equivalent grades
The designations below are commonly compared with ASTM B265 Grade 25. They are close in composition and role, but limits, tests and product forms are set by each standard, so they are not automatically interchangeable.
| Standard / system | Designation | Relationship to ASTM B265 Grade 25 |
|---|---|---|
| ASME SB-265 | Grade 25 | ASME Code adoption of B265; ordered for pressure equipment |
| ASTM B265 | Grade 24 | Base grade: same chemistry, lower minimum tensile strength; H material may be dual certified |
| UNS | R56403 | Same unified number as ASTM Grade 25 |
Where a drawing names one designation and the supplier offers another, agree in writing which standard governs chemistry, tensile values, testing and marking. Dual or multiple certification is possible only when the material meets every cited standard in full, and the certificate must show the results against each one.
Why choose SHH STEEL for Grade 25 titanium plate
SHH STEEL supports specification-led purchasing of titanium plate and sheet.
- We quote to the ASTM B265 edition, grade and product form you name, and keep B265 and SB-265 requirements distinct
- Certificates are checked against the Grade 25 chemistry and tensile limits
- Sizes, quantities, testing and delivery are confirmed in the quotation, not assumed
- Finish, marking and packing are agreed before production
Questions on equivalents, dual certification or edition changes are answered before an order is placed.
How to enquire for ASTM B265 Grade 25 plate
Send the material schedule with the details below. We review the enquiry and raise any open points before confirming the supply route.
| Enquiry item | Information required |
|---|---|
| Material | ASTM B265 Grade 25 (UNS R56403), edition; add ASME SB-265 if Code use |
| Product form | Plate, sheet or strip; for sheet, cold or hot rolled |
| Dimensions | Thickness, width, length, quantity and any cutting drawing |
| Finish | Descaled, sandblasted, ground or other agreed surface |
| Testing | Any special mechanical properties, extra analysis or reports |
| Documents | Certificate type and any third-party inspection |
| Destination | Delivery place and packing requirements |
FAQ
-
Is ASTM B265 Grade 25 the same as ASME SB-265 Grade 25?
- SB-265 is the ASME Code adoption of B265, so Grade 25 requirements normally match. They are separate documents, and ASME may adopt a different edition. For Code work, order SB-265 Grade 25 or dual certification.
-
What is the tensile strength of ASTM B265 Grade 25 titanium plate?
- The requirement is 130 ksi (895 MPa) minimum. The 0.2% proof or yield strength is 120 ksi (828 MPa) minimum. Minimum elongation is 10%. Values apply to the condition and thickness range stated in the standard.
-
What is Grade 25 mainly used for?
- Typical uses include geothermal and oil and gas parts in hot brine, high-strength chemical process equipment and marine and subsea components. The design engineer should confirm the grade for the actual service.
-
When is a titanium product classed as plate under B265?
- Plate is over 0.187 in (4.75 mm) thick and over 10 in (254 mm) wide. Thinner product is sheet if 24 in (610 mm) wide or more, otherwise strip.
-
What should I send for a quotation?
- Send ASTM B265 Grade 25, the edition, product form, thickness, width, length and quantity, the finish, any special testing, the certificate type and the destination. Add ASME SB-265 if the plate is for Code construction.
Request a quotation for ASTM B265 Grade 25 titanium plate
ASTM B265 Grade 25 is Ti-6Al-4V with Ni and Pd titanium alloy, UNS R56403, specified for 130 ksi (895 MPa) minimum tensile strength, 120 ksi (828 MPa) minimum yield or proof strength and 10% minimum elongation in the annealed condition. Typical uses include geothermal and oil and gas parts in hot brine and high-strength chemical process equipment.
Send the product form, sizes, quantity, finish, certificate type and destination to SHH STEEL. Compare other grades on the ASTM B265 page or browse all titanium alloy plates and sheets. Availability, testing and delivery are confirmed against each enquiry.
Contact: admin@steelspecs.com