ASTM A588 Grade A C and MC Steel Channels
What are ASTM A588 Grade A C and MC Steel Channels?
ASTM A588 Grade A C and MC steel channels are hot-rolled C-shapes or MC-shapes in high-strength low-alloy structural steel Grade A, furnished for the atmospheric corrosion resistance that the specification is written around. The material standard is ASTM A588/A588M. Dimensions, mass and general requirements for the rolled section are those of ASTM A6/A6M. SHH STEEL supplies these channels to the grade letter, C or MC designation, edition and certificate named on the order.
This page is written for Grade A only. Grades B and K are other A588 grades with their own chemistry, and they are not this data sheet. Do not use ASTM A588 Grade A steel plate, or the Grade B or Grade K plate pages, as a channel data sheet, and do not treat this page as a substitute for ASTM A572 Grade 50 steel channel when weathering performance is not what the order requires.
American Standard channels are designated C, for example C 6×8.2 or C 15×50. Miscellaneous channels are designated MC, for example MC 12×10.6 or MC 18×58. An MC is not a C of the same depth. Neither series is a European UPN or UPE, and neither is a Chinese or Japanese channel of a similar millimetre depth.
The official scope of A588/A588M-24 covers high-strength low-alloy structural steel shapes, plates and bars for welded, riveted or bolted construction, intended primarily for welded bridges and buildings where savings in weight or added durability are important. The atmospheric corrosion resistance of this steel in most environments is substantially better than that of carbon structural steels with or without copper. When properly exposed to the atmosphere, the steel is suitable for many applications in the bare (unpainted) condition. The specification is limited to material up to 8 in [200 mm] inclusive. These channels are filed under ASTM A588 Grade A steel channel profiles in the steel channel profiles category of steel structural profiles.
This page covers C and MC Steel Channels in ASTM A588 Grade A. The American Standard (C) and miscellaneous (MC) series follow ASTM A6/A6M; the material standard does not by itself define the dimensions.
Material, Dimensions and Tolerances for A588 Grade A Channels
Keep the material specification, the grade letter and the dimensional standard distinct:
ASTM A588/A588M is the material standard, and Grade A is the grade on this page. The current ASTM listing used for the official public scope is A588/A588M-24. Grade A heat-analysis limits and the structural-shapes tensile row on this page follow the figures commonly tabulated for that specification. The edition named on the order governs acceptance.
ASTM A6/A6M is the general-requirements and dimensional standard for these rolled C and MC channels. The size tables below are the standard C and MC series used as a reference, not a mill rolling list. The edition of A6/A6M named on the order governs dimensional acceptance.
The specification points to Guide G101 for methods of estimating atmospheric corrosion resistance. That guide is not a substitute for naming Grade A, and it does not turn a painted carbon channel into an A588 channel.
A588 Grade A Channel Sizes: Standard C and MC Series
The tables list designation, depth, flange width, web and flange thickness, and theoretical mass, in inch-pound and SI units, for the standard American Standard (C) and miscellaneous (MC) series under ASTM A6/A6M. Use them to identify and estimate, not as a rolling programme for A588 Grade A. Mid-range C 6 to C 12 sizes are the usual enquiry core; the lightest C 3 rows and the MC 18 range should be confirmed size by size.
C 6×8.2 and C 6×13 share a 6 in depth but not a web or a mass. MC 12×10.6 is a miscellaneous 12 in channel, not a C 12×20.7. The specification is limited to material up to 8 in [200 mm] inclusive; every standard C and MC row tabulated here is far below that cap, and far below the plate-and-bar thickness bands that use a lower yield.
American Standard channels (C series)
32 sizes, from C 3×3.5 to C 15×50.
Swipe horizontally to view all dimensions.
Miscellaneous channels (MC series)
40 sizes, from MC 3×7.1 to MC 18×58.
Swipe horizontally to view all dimensions.
S-shapes and other bar-size or special channels can be reviewed when they are named on the enquiry. Complete tables for those series are not reproduced here. European UPN or UPE, and Chinese or Japanese channel designations, belong to their own dimensional standards, not to these C and MC rows.
A588 Grade A Chemical Composition for Channels
The figures below are the Grade A heat-analysis limits commonly tabulated for ASTM A588/A588M. They are limits, not typical heat results, and they are not the Grade B or Grade K rows. The 0.04% phosphorus and 0.05% sulfur maxima are the limits used on this page for structural shapes. A tighter phosphorus or sulfur figure sometimes shown for plate is not applied to these C or MC shapes. Product analysis, when required, shall conform to those same heat-analysis limits, subject to the numeric permitted variations below, taken from Table A of ASTM A6/A6M-19. Where Table A shows no under-minimum or over-maximum figure, none is applied on this page.
The following product-analysis variations apply to those heat-analysis limits.
Table A footnote A gives a different manganese variation for bars and bar-size shapes: ±0.03% up to 0.90% inclusive, and ±0.06% over 0.90% to 2.20% inclusive. Where a heat-analysis limit is a maximum only, the over-maximum variation is the figure that raises the product-analysis ceiling. The A6/A6M edition named on the order governs.
Do not copy a Grade B or Grade K chemistry row onto a Grade A channel, and do not copy a plate-width exception onto this C-shape or MC-shape unless the ordered edition actually requires it.
A588 Grade A Channel Mechanical Properties: Yield, Tensile and Elongation
For structural shapes, the tensile requirements commonly tabulated for ASTM A588/A588M apply to all thicknesses in the specification: 70 ksi [485 MPa] minimum tensile strength, 50 ksi [345 MPa] minimum yield, 18% minimum elongation in 8 in [200 mm] and 21% minimum elongation in 2 in [50 mm]. The reductions that appear for plates and bars thicker than 4 in [100 mm] are plate-and-bar rules. They are not applied to these C or MC shapes.
A footnote that lowers the 2 in elongation to 18% applies to wide-flange shapes with flange thickness over 3 in [75 mm], not to these C or MC shapes. None of the standard C or MC rows tabulated here has a thickness over 3 in. Charpy testing is not treated here as a default A588 requirement; if an impact supplementary is needed, it must be named on the order. Tension-test orientation follows A6/A6M.
Delivery, Inspection and Identification of A588 Grade A Channels
A588 Grade A channels are commonly supplied as-rolled. The inspection document should identify ASTM A588/A588M and its edition, Grade A (not merely “A588”), the A6/A6M C or MC designation, the heat number, the heat analysis and the tensile results. An EN 10204 type 3.1 document, or the mill’s equivalent inspection certificate, is the usual export request. A Grade A plate certificate does not identify an C-shape or MC-shape, and a Grade B certificate does not satisfy a Grade A line. Length is a matter for the rolling programme and the order, often in the region of 20–40 ft or 6–12 m; those lengths are enquiry ranges, not a stock list.
Weldability, Exposure and Surface Condition of A588 Grade A Channels
A588 Grade A is intended for welded, riveted or bolted construction. The specification requires a welding procedure suitable for the grade and the intended use or service, and points to Appendix X3 of A6/A6M for weldability information. This page does not prescribe a procedure or a preheat chart. Procedure should be set from the certificate analysis and the applicable welding specification.
Bare weathering service depends on proper exposure so that the surface can develop and hold its oxide. The as-rolled surface is mill scale; blast cleaning, painting or another coating system is an order option when the design is not a bare application. Cutting, punching, forming or coating can be reviewed when that specification is sent with the enquiry.
A6/A6M Shape Tolerances and Theoretical Mass
Dimensional and mass tolerances for these C or MC shapes are those of ASTM A6/A6M, not of A588/A588M itself. This article does not reproduce the inch or millimetre tolerance tables; acceptance is against the edition of A6/A6M named on the order. Out-of-square at the heel and variation of the two legs matter for connections. Settlement on theoretical or weighed mass should follow the contract.
Applications and Service Limits
A588 Grade A steel channels are used where a 50 ksi HSLA C-shape or MC-shape and the atmospheric corrosion resistance of this specification are what the order names: bridge and building work, exposed frames, bracing and details that are intended to stand bare when the exposure is suitable, or to be coated when the design requires it. The 50 ksi yield is the same figure used for A572 Grade 50 steel channel, but that grade is not a weathering specification.
Bare use is not automatic in every climate or in every detail. Sheltered, wet, or chloride-rich exposures, and details that trap moisture, can be poor places to assume an unpainted A588 surface. The grade is not specified here as a pressure-vessel or nuclear-safety material, and it is not a stainless steel. Durability in a coated design comes from the coating system as well as from the grade.
A588 Grade A Channel Compared with A588 Plate, Grade B and Grade 50
ASTM A588 Grade A steel plate is the same grade letter in a different product form. The 46 ksi and 42 ksi yield figures that appear for plates and bars over 4 in are plate-and-bar rules. Structural shapes are commonly tabulated at 50 ksi yield and 70 ksi tensile for all thicknesses in the specification. A plate certificate does not identify a C or MC channel.
Grade B and Grade K are other A588 grades with their own chemistry rows. A Grade B or Grade K certificate does not satisfy a Grade A line unless the order is changed.
ASTM A572 Grade 50 C and MC steel channels can also be furnished as 50 ksi C or MC shapes, but A572 Grade 50 is not written for atmospheric corrosion resistance and does not share the Grade A copper, chromium and vanadium bands.
Near-Equivalents: Not Automatic Substitutes
Stock and Supply of A588 Grade A C and MC Steel Channels from SHH STEEL
SHH STEEL supplies ASTM A588 Grade A C and MC steel channels as an export trading house, coordinating mill production and project procurement. The useful work on this product is to keep Grade A distinct from Grade B, Grade K and from A572 Grade 50, to say whether the channel is for bare or coated service, to select the correct C or MC designation, and to align the inspection document with the edition named on the order.
Sizes, lengths and certificates are confirmed per enquiry. The tables are the standard A6/A6M C and MC series, not a list of pieces on the floor. Mid-range C 6 to C 12 sizes are the usual core; the lightest C 3 rows and the MC 18 range are confirmed per line.
Sections can be sourced from mills that SHH STEEL buys from, including Masteel, Rizhao Steel, Laiwu (Shandong Steel Laiwu) and Tung Ho Steel, among others when the programme matches the order. Those mills do not each roll every C or MC size in A588 Grade A. If cutting, punching, forming or a coating system is required, include that specification for review. Export packing and container loading can be arranged to the packing list agreed for the shipment.
A588 Grade A C and MC Steel Channel FAQs
-
Why does this page name Grade A instead of just A588?
- A588/A588M is a specification with more than one grade letter, and the chemistry rows are not the same. This article is written for Grade A, which is the grade commonly tabulated for A588 channels. A Grade B or Grade K certificate does not satisfy a Grade A line unless the order is changed.
-
Do these channels use the lower yield values listed for thick A588 plate?
- No. The 46 ksi and 42 ksi yield figures that appear for plates and bars over 4 in are plate-and-bar rules. Structural shapes are commonly tabulated at 50 ksi yield and 70 ksi tensile for all thicknesses in the specification. The standard C and MC series is far below those plate-thickness bands.
-
Can every A588 Grade A channel be left unpainted?
- Not automatically. The specification says that, when properly exposed to the atmosphere, the steel is suitable for many applications in the bare condition. Sheltered, wet or chloride-rich details, and surfaces that cannot dry, are poor places to assume a bare finish. The order should say whether the channel is for bare or coated service.
-
Is a C-shape the same as an MC of the same depth?
- No. C designations are American Standard channels; MC designations are miscellaneous channels. MC 12×10.6 is not a C 12, and the flange, web and mass are those of the MC series. The order should use the designation that the specification actually names.
-
Is A588 Grade A the same as A572 Grade 50?
- No. Both can be furnished as 50 ksi C or MC channels, but A588 Grade A is written for atmospheric corrosion resistance and has its own chemistry, including copper, chromium and vanadium bands that A572 Grade 50 does not share as this grade.
Request a Quotation for ASTM A588 Grade A C and MC Steel Channels
ASTM A588 Grade A C and MC steel channels are high-strength low-alloy C-shapes or MC-shapes written for atmospheric corrosion resistance, with 50 ksi [345 MPa] minimum yield and 70 ksi [485 MPa] minimum tensile for structural shapes. Nominate the C or MC size to ASTM A6/A6M, the material to ASTM A588/A588M Grade A (or the edition on the order), and whether the channel is for bare or coated service. The tables are reference dimensions, not a rolling list. Send the designation list, grade letter, edition, certificate type and any processing notes; SHH STEEL will review the package and quote accordingly.