ASTM A572 Grade 50 C and MC Steel Channels

ASTM A572 Grade 50 C and MC steel channels are high-strength low-alloy C-shapes or MC-shapes with 50 ksi minimum yield and 65 ksi minimum tensile strength. Dimensions follow the ASTM A6/A6M C and MC series. This page covers Grade 50 channels only, not plates or W-shapes. SHH STEEL reviews grade, type, edition and certificate requirements before quoting.
Keywords
ASTM A572 Grade 50 C and MC Steel Channels, ASTM A572 Grade 50 Steel Channel, A572 Gr.50 C channel, A572 Grade 50 MC, ASTM A6 channel
Equivalent Grades:
Near-equivalents only, not automatic substitutes: A36 channel uses the same C/MC series at lower yield; A572 Grade 50 plate is the same grade, not the same product form; Q355B; S355JR; SM490.
Share:
General Description
Material Specification
Available Sizes of A572 Grade 50 C and MC Steel Channels
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why Source A572 Grade 50 Steel Channels from SHH STEEL
FAQ
Conclusion

What are ASTM A572 Grade 50 C and MC Steel Channels?

ASTM A572 Grade 50 steel channel is a hot-rolled C-shape or MC-shape in high-strength low-alloy structural steel Grade 50. The material standard is ASTM A572/A572M. Dimensions, mass and general requirements for the rolled section are those of ASTM A6/A6M. The 50 ksi [345 MPa] minimum yield is the same figure used for Grade 50 plates and for Grade 50 W-shapes, but this page is for the channel, not for a W-shape, an angle, or a plate.

American Standard channels are designated C, for example C 8×11.5 or C 15×50, where the second number is theoretical mass in pounds per foot. Miscellaneous channels are designated MC, for example MC 10×8.4 or MC 18×58. An MC is not a C of the same depth, and neither series is a European UPN or UPE or a Chinese or Japanese channel of a similar millimetre depth. Grade 50 can use the same C and MC series as A36; the difference is the material, not a second set of designations.

These channels are filed under ASTM A572 steel channel profiles in the steel channel profiles category of steel structural profiles. The same grade in plate form is listed separately as A572 Gr.50 structural steel plate. Do not use that plate page as a channel data sheet, and do not copy plate-width chemistry columns onto a C or MC certificate.

Grade 50 channels are used for building frames, bracing and general industrial work when the specification names this high-strength low-alloy grade in a C or MC section. The grade is not a pressure-vessel or nuclear safety material, and an A36 channel certificate does not fulfil a Grade 50 order.

This page covers C and MC Steel Channels in ASTM A572 Grade 50. The American Standard (C) and miscellaneous (MC) series follow ASTM A6/A6M; the material specification does not by itself define the dimensions.

Material, Dimensions and Tolerances for A572 Grade 50 Channels

The order and the inspection certificate should keep material, dimensions and tolerances distinct:

  • ASTM A572/A572M is the material standard. This article uses chemistry and tensile values for Grade 50 shapes from ASTM A572/A572M-21ε1. The edition named on the order governs acceptance.
  • ASTM A6/A6M is the general-requirements and dimensional standard for these rolled channels. The size tables below are reference dimensions and theoretical masses for the standard C and MC series, not a mill rolling list. The edition of A6/A6M named on the order governs dimensional acceptance.

Grade 50 steel shall be killed. Types 1, 2, 3 and 5 are the types listed for this grade; the type actually supplied should be the one named on the order or agreed with the mill. A documented special combination — for example Grade 50 on a UPN, or a C-shape certified to a different material standard — is only valid if every requirement of each named standard is met.

A572 Grade 50 Channel Sizes: Standard C and MC Series

The tables list designation, depth, flange width, web and flange thickness, and theoretical mass, in inch-pound and SI units, for the standard American Standard (C) and miscellaneous (MC) series under ASTM A6/A6M. The series is the same one used for A36 channels; Grade 50 does not invent a second size list. Use the tables to identify and estimate, not as a rolling programme for Grade 50. Mid-range C 6 to C 12 sizes are the usual enquiry core; the lightest C 3 rows and the MC 18 range should be confirmed size by size.

C 8×11.5 and C 8×18.75 share an 8 in depth but not a web or a mass. MC 10×8.4 is a miscellaneous 10 in channel, not a C 10×15.3. C 15×50, the heaviest standard C, has a 0.65 in flange, still well below the 3 in flange or leg thickness at which the Grade 50 silicon rule changes.

American Standard channels (C series)

32 sizes, from C 3×3.5 to C 15×50.

Swipe horizontally to view all dimensions.

Designation d (in) bf (in) tw (in) tf (in) d (mm) bf (mm) tw (mm) tf (mm) Mass (lb/ft) Mass (kg/m)
C 3×3.5 3 1.37 0.132 0.273 76.2 34.8 3.35 6.93 3.5 5.2
C 3×4.1 3 1.41 0.17 0.273 76.2 35.8 4.32 6.93 4.1 6.1
C 3×5 3 1.5 0.258 0.273 76.2 38.1 6.55 6.93 5 7.4
C 3×6 3 1.6 0.356 0.273 76.2 40.6 9.04 6.93 6 8.9
C 4×4.5 4 1.52 0.125 0.296 102 38.6 3.18 7.52 4.5 6.7
C 4×5.4 4 1.58 0.184 0.296 102 40.1 4.67 7.52 5.4 8
C 4×6.25 4 1.65 0.247 0.296 102 41.9 6.27 7.52 6.25 9.3
C 4×7.25 4 1.72 0.321 0.296 102 43.7 8.15 7.52 7.25 10.8
C 5×6.7 5 1.75 0.19 0.32 127 44.5 4.83 8.13 6.7 10.4
C 5×9 5 1.89 0.325 0.32 127 48 8.26 8.13 9 13
C 6×8.2 6 1.92 0.2 0.343 152 48.8 5.08 8.71 8.2 12.2
C 6×10.5 6 2.03 0.314 0.343 152 51.6 7.98 8.71 10.5 15.6
C 6×13 6 2.16 0.437 0.343 152 54.9 11.1 8.71 13 19.3
C 7×9.8 7 2.09 0.21 0.366 178 53.1 5.33 9.3 9.8 14.6
C 7×12.25 7 2.19 0.314 0.366 178 55.6 7.98 9.3 12.25 18.2
C 7×14.75 7 2.3 0.419 0.366 178 58.4 10.6 9.3 14.75 22
C 8×11.5 8 2.26 0.22 0.39 203 57.4 5.59 9.91 11.5 17.1
C 8×13.75 8 2.34 0.303 0.39 203 59.4 7.7 9.91 13.75 20.5
C 8×18.75 8 2.53 0.487 0.39 203 64.3 12.4 9.91 18.75 27.9
C 9×13.4 9 2.43 0.233 0.413 229 61.7 5.92 10.5 13.4 19.9
C 9×15 9 2.49 0.285 0.413 229 63.2 7.24 10.5 15 22
C 9×20 9 2.65 0.448 0.413 229 67.3 11.4 10.5 20 30
C 10×15.3 10 2.6 0.24 0.436 254 66 6.1 11.1 15.3 22.8
C 10×20 10 2.74 0.379 0.436 254 69.6 9.63 11.1 20 30
C 10×25 10 2.89 0.526 0.436 254 73.4 13.4 11.1 25 37
C 10×30 10 3.03 0.673 0.436 254 77 17.1 11.1 30 45
C 12×20.7 12 2.94 0.282 0.501 305 74.7 7.16 12.7 20.7 30.8
C 12×25 12 3.05 0.387 0.501 305 77.5 9.83 12.7 25 37
C 12×30 12 3.17 0.51 0.501 305 80.5 13 12.7 30 45
C 15×33.9 15 3.4 0.4 0.65 381 86.4 10.2 16.5 33.9 50.4
C 15×40 15 3.52 0.52 0.65 381 89.4 13.2 16.5 40 60
C 15×50 15 3.72 0.716 0.65 381 94.5 18.2 16.5 50 74

Miscellaneous channels (MC series)

40 sizes, from MC 3×7.1 to MC 18×58.

Swipe horizontally to view all dimensions.

Designation d (in) bf (in) tw (in) tf (in) d (mm) bf (mm) tw (mm) tf (mm) Mass (lb/ft) Mass (kg/m)
MC 3×7.1 3 1.94 0.312 0.351 76.2 49.3 7.92 8.92 7.1 10.6
MC 4×13.8 4 2.5 0.5 0.5 102 63.5 12.7 12.7 13.8 20.5
MC 6×6.5 6 1.85 0.155 0.291 152 47 3.94 7.39 6.5 9.7
MC 6×7 6 1.88 0.179 0.291 152 47.8 4.55 7.39 7 10.4
MC 6×12 6 2.5 0.31 0.375 152 63.5 7.87 9.53 12 17.9
MC 6×15.1 6 2.94 0.316 0.475 152 74.7 8.03 12.1 15.1 22.5
MC 6×15.3 6 3.5 0.34 0.385 152 88.9 8.64 9.78 15.3 22.8
MC 6×16.3 6 3 0.375 0.475 152 76.2 9.53 12.1 16.3 24.3
MC 6×18 6 3.5 0.379 0.475 152 88.9 9.63 12.1 18 26.8
MC 7×19.1 7 3.45 0.352 0.5 178 87.6 8.94 12.7 19.1 28.4
MC 7×22.7 7 3.6 0.503 0.5 178 91.4 12.8 12.7 22.7 33.8
MC 8×8.5 8 1.87 0.179 0.311 203 47.5 4.55 7.9 8.5 12.6
MC 8×18.7 8 2.98 0.353 0.5 203 75.7 8.97 12.7 18.7 27.8
MC 8×20 8 3.03 0.4 0.5 203 77 10.2 12.7 20 29.8
MC 8×21.4 8 3.45 0.375 0.525 203 87.6 9.53 13.3 21.4 31.8
MC 8×22.8 8 3.5 0.427 0.525 203 88.9 10.8 13.3 22.8 33.9
MC 9×23.9 9 3.45 0.4 0.55 229 87.6 10.2 14 23.9 35.6
MC 9×25.4 9 3.5 0.45 0.55 229 88.9 11.4 14 25.4 37.8
MC 10×6.5 10 1.17 0.152 0.202 254 29.7 3.86 5.13 6.5 9.7
MC 10×8.4 10 1.5 0.17 0.28 254 38.1 4.32 7.11 8.4 12.5
MC 10×22 10 3.32 0.29 0.575 254 84.3 7.37 14.6 22 33
MC 10×25 10 3.41 0.38 0.575 254 86.6 9.65 14.6 25 37
MC 10×28.5 10 3.95 0.425 0.575 254 100 10.8 14.6 28.5 42.4
MC 10×33.6 10 4.1 0.575 0.575 254 104 14.6 14.6 33.6 50
MC 10×41.1 10 4.32 0.796 0.575 254 110 20.2 14.6 41.1 61.2
MC 12×10.6 12 1.5 0.19 0.309 305 38.1 4.83 7.85 10.6 15.8
MC 12×14.3 12 2.12 0.25 0.313 305 53.8 6.35 7.95 14.3 21.3
MC 12×31 12 3.67 0.37 0.7 305 93.2 9.4 17.8 31 46
MC 12×35 12 3.77 0.465 0.7 305 95.8 11.8 17.8 35 52
MC 12×40 12 3.89 0.59 0.7 305 98.8 15 17.8 40 60
MC 12×45 12 4.01 0.71 0.7 305 102 18 17.8 45 67
MC 12×50 12 4.14 0.835 0.7 305 105 21.2 17.8 50 74
MC 13×31.8 13 4 0.375 0.61 330 102 9.53 15.5 31.8 47.3
MC 13×35 13 4.07 0.447 0.61 330 103 11.4 15.5 35 52
MC 13×40 13 4.19 0.56 0.61 330 106 14.2 15.5 40 60
MC 13×50 13 4.41 0.787 0.61 330 112 20 15.5 50 74
MC 18×42.7 18 3.95 0.45 0.625 457 100 11.4 15.9 42.7 63.5
MC 18×45.8 18 4 0.5 0.625 457 102 12.7 15.9 45.8 68.2
MC 18×51.9 18 4.1 0.6 0.625 457 104 15.2 15.9 51.9 77.2
MC 18×58 18 4.2 0.7 0.625 457 107 17.8 15.9 58 86

S-shapes and other bar-size or special channels can be reviewed when they are named on the enquiry. Complete tables for those series are not reproduced here. European UPN or UPE, and Chinese or Japanese channel designations, belong to their own dimensional standards, not to these C and MC rows.

A572 Grade 50 Chemical Composition for Channels

The figures below are heat-analysis limits for Grade 50 shapes from ASTM A572/A572M-21ε1. They apply to these C and MC channels as structural shapes. They must not be copied from a plate-width column, and they are limits, not typical heat results.

Element Heat analysis, Grade 50 shapes Notes for A572 Grade 50 channels
C, max (%) 0.23 See also the manganese trade-off below.
Mn, max (%) 1.35 (may be 1.60) For each 0.01 percentage point decrease below the specified carbon maximum, manganese may be increased 0.06 percentage points above 1.35, to a maximum of 1.60.
Mn, min (%) 0.50 Minimum heat-analysis manganese for shapes (and for plates 3/8 in [10 mm] and under). The ratio of manganese to carbon shall be not less than 2.
P, max (%) / S, max (%) 0.04 / 0.05 for these shapes The tabulated limits are 0.030%. Footnote I permits 0.04% phosphorus and 0.05% sulfur for structural shapes, sheet piling, bars, and plates with widths up to and including 15 in [380 mm]. C and MC channels are structural shapes, so those 0.04 / 0.05 values apply here.
Si, max (%) 0.40 0.40% maximum for shapes with flange or leg thickness 3 in [75 mm] and under; 0.15–0.40% when flange thickness exceeds 3 in. None of the standard C or MC rows below has a flange over 3 in, so 0.40% max applies to this list.

A572 Grade 50 Channel Mechanical Properties

Tensile properties of Grade 50 channels follow the Grade 50 requirements in ASTM A572/A572M-21ε1. There is a 50 ksi [345 MPa] minimum yield and a 65 ksi [450 MPa] minimum tensile strength. The specification does not set a maximum yield for this grade. Those minima are higher than the A36 shapes table, and there is no 80 ksi tensile cap of the kind used for ordinary A36 shapes. The 19% elongation in 2 in that applies to wide-flange shapes over 426 lb/ft [634 kg/m] does not apply to these C or MC channels.

Property Requirement for A572 Grade 50 shapes
Minimum yield point 50 ksi [345 MPa]
Minimum tensile strength 65 ksi [450 MPa]
Yield maximum None specified
Minimum elongation in 8 in [200 mm] 18%
Minimum elongation in 2 in [50 mm] 21%

Charpy V-notch testing is not a default Grade 50 requirement. Supplementary requirements such as S5 or S30 apply only when they are named on the order. Do not treat Grade 50 as a weathering steel unless a weathering specification is also named.

Delivery Conditions, Inspection and Identification

A572 Grade 50 channels are commonly supplied as-rolled, in killed steel of the type agreed for the order. The inspection document should show ASTM A572/A572M and its edition, Grade 50, the type where it is required, the A6/A6M designation (C or MC), the heat number, the heat analysis, and the tensile results. If a Charpy supplementary or a particular A6/A6M finish is required, that must appear on the order and on the certificate. An A36 channel certificate, or a Grade 50 plate or W-shape certificate, does not, by itself, identify these channels.

An EN 10204 type 3.1 document, or the mill’s equivalent inspection certificate, is the usual export request; type 3.2 or nominated third-party attendance can be added when the specification requires it. Identification follows the mill’s marking practice. Length is a matter for the rolling programme and the order, often in the region of 20–40 ft or 6–12 m.

Weldability and Surface Condition of A572 Grade 50 Channels

Grade 50 is a weldable high-strength low-alloy structural steel when thickness, joint design and hydrogen control are taken into account. Procedure should be set from the certificate analysis, the type actually supplied, and the applicable welding specification. This page does not prescribe a procedure or a preheat chart, and it does not invent a carbon-equivalent limit that the specification does not table for these as-rolled channels.

The as-rolled surface is mill scale. Blast, paint or galvanizing is an order option. Cutting, punching, forming or coating can be reviewed when that specification is sent with the enquiry. They are not assumed for every size.

A6/A6M Shape Tolerances and Theoretical Mass

Dimensional and mass tolerances for these C and MC sections are those of ASTM A6/A6M, not of A572/A572M itself. This article does not reproduce the inch or millimetre tolerance tables; acceptance is against the edition named on the order.

A delivered C 8×18.75 will measure close to the tabulated depth, flange and thicknesses within those tolerances, not as a set of exact advertised inches. Out-of-square and flange tilt matter for connections. Settlement on theoretical or weighed mass should follow the contract.

Applications and Service Limits

A572 Grade 50 steel channels are used where a 50 ksi high-strength low-alloy grade and a C or MC section are specified:

  • Building and industrial frames, bracing and general fabrications whose specification names Grade 50 channel rather than A36 or a non-American channel series.
  • Export packages that compare the grade with Q355B or with S355JR, provided each line keeps its own material standard, toughness rule and shape system.

It is not specified here for pressure equipment, for nuclear safety-related components, or for members that actually require a tabulated impact test or a weathering specification that has not been named. Durability comes from the coating or fire-protection system, not from the Grade 50 designation alone.

Grade 50 Channel Compared with A36, Plates and S355JR

An A36 channel can use the same C and MC series at a 36 ksi yield and with a different chemistry table; it does not fulfil a Grade 50 requirement. A572 Gr.50 plate is the same grade in plate form, not a channel, and plate-width chemistry must not be used for these sections. S355JR and Q355B are useful 355 MPa-class comparisons only if chemistry, toughness and the shape standard are also satisfied.

Dual certification requires every requirement of each named standard to be met on the delivered piece. An A572 Grade 50 W-beam or angle page in this series will be linked here once it is published; those product URLs are not pre-linked.

Near-Equivalents: Not Automatic Substitutes

The comparisons below are for orientation. They are not a licence to substitute one grade or one shape for another on a contract or an inspection certificate.

Grade / designation Standard Relationship to A572 Grade 50 channel Caution
A36 channel ASTM A36/A36M; dimensions ASTM A6/A6M A carbon structural channel that can use the same C and MC series at a lower yield. A36 is 36 ksi yield with a 58–80 ksi tensile range. It is not a Grade 50 certificate.
A572 Grade 50 W-shape or plate ASTM A572/A572M The same grade in a different product form. A W-shape or a plate certificate does not identify a C or MC section. Plate chemistry columns must not be used for these channels.
Q355B / S355JR / SM490 GB/T 1591 or EN 10025-2 or JIS G 3106; different shape standards Common 50 ksi or 355 MPa-class comparisons in export enquiries. Each has its own chemistry, toughness and shape system. A shared 50 ksi or 345 MPa discussion is not a substitution method.

Sourcing A572 Grade 50 Steel Channels from SHH STEEL

SHH STEEL supplies A572 Grade 50 steel channels as an export trading house, coordinating mill production and project procurement. For this product the useful work is to keep Grade 50 from being fulfilled with an A36 certificate, to keep C and MC designations from being mixed, and to align type, killed-steel practice, A6/A6M size and the inspection document before a rolling programme is committed.

Sections can be sourced from mills that SHH STEEL buys from, including Masteel, Rizhao Steel, Laiwu (Shandong Steel Laiwu) and Tung Ho Steel, among others when the programme matches the order. Those mills do not each roll every C or MC size in Grade 50. Mid-range C sizes are the usual core; MC 18 rows and uncommon light C 3 variants are confirmed per line.

The same enquiry can also cover W-shapes, angles, or Chinese, Japanese or European designations, provided each line states its material standard, shape standard and size. If cutting, punching, forming or a coating system is required, include that specification for review. Export packing and container loading can be arranged to the packing list agreed for the shipment.

A572 Grade 50 C and MC Steel Channel FAQs

Can an A36 channel be supplied against an A572 Grade 50 channel order?
No, not as a substitute. A36 and Grade 50 can share the same C or MC designation, but Grade 50 has a 50 ksi minimum yield, a different chemistry table, and killed-steel practice. An A36 certificate does not fulfil a Grade 50 requirement.
Is there a maximum yield for A572 Grade 50 channel?
ASTM A572/A572M does not set a maximum yield for Grade 50. The specified values are a 50 ksi [345 MPa] minimum yield and a 65 ksi [450 MPa] minimum tensile strength.
Which phosphorus and sulfur limits apply to these channels?
For structural shapes, including C and MC channels, footnote I of the Grade 50 chemistry table allows 0.04% phosphorus and 0.05% sulfur, rather than the 0.030% figures that remain tabulated for other product forms.
Is a Charpy test required for Grade 50 channel?
Not by default. Charpy supplementary requirements such as S5 or S30 apply only when they are named on the order.
Which standards should appear on the inspection document?
At least ASTM A572/A572M and its edition, Grade 50, the type where it is required, the C or MC designation to A6/A6M, the heat number, heat analysis, and tensile results. Any impact supplementary should also appear if it was ordered.

Request a Quotation for ASTM A572 Grade 50 C and MC Steel Channels

ASTM A572 Grade 50 C and MC steel channels are high-strength low-alloy C-shapes or MC-shapes with 50 ksi [345 MPa] minimum yield. Nominate the C or MC size to ASTM A6/A6M and the material to ASTM A572/A572M-21ε1 (or the edition on the order). The tables are reference dimensions, not a rolling list. Send the designation list, type, edition, certificate type and any processing notes; SHH STEEL will review the package and quote accordingly.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X