ASTM A500 Grade C Steel Hollow Sections (HSS) | ASTM A500 Steel Hollow Sections - SHH STEEL

ASTM A500 Grade C Steel Hollow Sections (HSS)

ASTM A500 Grade C steel hollow sections are cold-formed welded or seamless carbon steel square, rectangular and round HSS to ASTM A500/A500M-23. Yield is 50 ksi [345 MPa] and tensile strength 62 ksi [425 MPa] for all those shapes. The tables list 516 AISC v15.0 HSS designations. This page is Grade C only. SHH STEEL reviews grade and certificate before quoting.
Keywords
ASTM A500 Grade C HSS, A500-C square tube, A500-C rectangular HSS, A500-C round HSS, A500/A500M-23 Grade C
Equivalent Grades:
Near-equivalents only, not automatic substitutes.
Share:
General Description
Material Specification
Available Sizes of ASTM A500 Grade C Steel Hollow Sections
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Sourcing ASTM A500 Grade C Steel Hollow Sections from SHH STEEL
FAQ
Conclusion

What are ASTM A500 Grade C Steel Hollow Sections?

ASTM A500 Grade C steel hollow sections are the higher-strength cold-formed carbon steel grade in A500/A500M-23: 50 ksi [345 MPa] minimum yield and 62 ksi [425 MPa] minimum tensile strength, for round, square, rectangular and agreed special shapes, welded or seamless. The same scope limits apply as for Grade B — periphery 88 in [2235 mm] or less, specified wall 1.000 in [25.4 mm] or less — and the same 1 November 2023 edition text is used on this page.

Grade C is now specified with those minima for rounds as well as for shaped tubes. Under editions before the 2021 revision, round Grade C was 46 ksi. That older split should not be used when the order names A500/A500M-21, 21a or 23. This page is Grade C only. It is not Grade B, not Grade D, and not ASTM A1085.

Industry practice in the United States often treats Grade C as the default structural HSS grade, and many mills issue dual Grade B and Grade C certificates when both sets of requirements are met. That is a production practice, not a reason to accept a Grade B-only paper against a Grade C specification, and not a statement about any particular inventory.

Material, Manufacture and Scope for ASTM A500 Grade C HSS

Like Grade B, Grade C is cold-formed carbon steel, welded or seamless, formed into square, rectangular, round or agreed special sections. The order should name Grade C, the A500/A500M edition, the outside size and specified wall, the manufacturing method if it matters, and any extras such as copper-containing steel or additional tests.

Grade C chemistry is not identical to Grade B: the carbon maximum is lower (0.23 % heat analysis, 0.27 % product analysis). A dual-grade certificate has to live inside the tighter of the two limits where they differ. Dimensional acceptance follows the ordered A500/A500M edition, not ASTM A6/A6M.

ASTM A500 Grade C HSS Sizes: Square, Rectangular and Round (AISC Manual, 15th Edition)

The same 516 AISC Manual, 15th Edition, HSS designations appear here as on the Grade B companion page — 107 square, 281 rectangular and 128 round — because Grade B and Grade C share the AISC geometry file, not because the two grades are interchangeable certificates. Each row joins the inch-pound and SI companion records. The list is a reference for identification and estimating. It is not a rolling programme and not a promise that every designation is produced in ASTM A500 Grade C. All 516 rows sit inside the A500/A500M-23 envelope of 88 in [2235 mm] periphery and 1.000 in [25.4 mm] specified wall.

Order by the specified (nominal) wall. The published design wall, tdes, is about 0.93 of the nominal wall on these electric-resistance-welded rows and is the thickness many design specifications use for A500 HSS; it is not a substitute for the ordered wall on the mill certificate. Corner radii are not invented. Masses are theoretical reference values; tolerance and settlement follow the ordered A500/A500M edition, not ASTM A6/A6M.

Do not read an HSS 6×6 as an EN 100×100 square, or a round HSS as an AISC Pipe or ASTM A53 line. Those are different product standards, even when the outside dimensions look close.

Square HSS (SHS)

107 square designations, grouped by outside size. The first group is the larger squares, from HSS 22×22 down through HSS 10×10.

HSS 22×22 to HSS 10×10

36 designations in this group.

Swipe horizontally to view all dimensions.

Designation SI designation B (in) B (mm) tnom (in) tnom (mm) tdes (in) tdes (mm) A (in²) A (mm²) Mass (lb/ft) Mass (kg/m)
HSS 22×22×7/8 HSS 558.8×558.8×22.2 22 559 0.875 22.2 0.814 20.7 67.3 43400 244.88 364
HSS 22×22×3/4 HSS 558.8×558.8×19 22 559 0.75 19.1 0.698 17.7 58.2 37600 212 315
HSS 20×20×7/8 HSS 508×508×22.2 20 508 0.875 22.2 0.814 20.7 60.8 39200 221.06 329
HSS 20×20×3/4 HSS 508×508×19 20 508 0.75 19.1 0.698 17.7 52.6 33900 191.58 285
HSS 20×20×5/8 HSS 508×508×15.9 20 508 0.625 15.9 0.581 14.8 44.3 28600 161.4 240
HSS 20×20×1/2 HSS 508×508×12.7 20 508 0.5 12.7 0.465 11.8 35.8 23100 130.52 194
HSS 18×18×7/8 HSS 457.2×457.2×22.2 18 457 0.875 22.2 0.814 20.7 54.3 35000 197.24 293
HSS 18×18×3/4 HSS 457.2×457.2×19 18 457 0.75 19.1 0.698 17.7 47.1 30400 171.16 255
HSS 18×18×5/8 HSS 457.2×457.2×15.9 18 457 0.625 15.9 0.581 14.8 39.6 25500 144.39 215
HSS 18×18×1/2 HSS 457.2×457.2×12.7 18 457 0.5 12.7 0.465 11.8 32.1 20700 116.91 174
HSS 16×16×7/8 HSS 406.4×406.4×22.2 16 406 0.875 22.2 0.814 20.7 47.7 30800 173.43 258
HSS 16×16×3/4 HSS 406.4×406.4×19.0 16 406 0.75 19.1 0.698 17.7 41.5 26800 150.75 224
HSS 16×16×5/8 HSS 406.4×406.4×15.9 16 406 0.625 15.9 0.581 14.8 35 22600 127.37 189
HSS 16×16×1/2 HSS 406.4×406.4×12.7 16 406 0.5 12.7 0.465 11.8 28.3 18300 103.3 153
HSS 16×16×3/8 HSS 406.4×406.4×9.5 16 406 0.375 9.53 0.349 8.86 21.5 13900 78.52 117
HSS 16×16×5/16 HSS 406.4×406.4×7.9 16 406 0.3125 7.94 0.291 7.39 18.1 11700 65.87 97.9
HSS 14×14×7/8 HSS 355.6×355.6×22.2 14 356 0.875 22.2 0.814 20.7 41.2 26600 149.61 223
HSS 14×14×3/4 HSS 355.6×355.6×19 14 356 0.75 19.1 0.698 17.7 35.9 23200 130.33 194
HSS 14×14×5/8 HSS 355.6×355.6×15.9 14 356 0.625 15.9 0.581 14.8 30.3 19500 110.36 164
HSS 14×14×1/2 HSS 355.6×355.6×12.7 14 356 0.5 12.7 0.465 11.8 24.6 15900 89.68 133
HSS 14×14×3/8 HSS 355.6×355.6×9.5 14 356 0.375 9.53 0.349 8.86 18.7 12100 68.31 102
HSS 14×14×5/16 HSS 355.6×355.6×7.9 14 356 0.3125 7.94 0.291 7.39 15.7 10100 57.36 85.3
HSS 12×12×3/4 HSS 304.8×304.8×19 12 305 0.75 19.1 0.698 17.7 30.3 19500 109.91 164
HSS 12×12×5/8 HSS 304.8×304.8×15.9 12 305 0.625 15.9 0.581 14.8 25.7 16600 93.34 139
HSS 12×12×1/2 HSS 304.8×304.8×12.7 12 305 0.5 12.7 0.465 11.8 20.9 13500 76.07 113
HSS 12×12×3/8 HSS 304.8×304.8×9.5 12 305 0.375 9.53 0.349 8.86 16 10300 58.1 86.3
HSS 12×12×5/16 HSS 304.8×304.8×7.9 12 305 0.3125 7.94 0.291 7.39 13.4 8650 48.86 72.6
HSS 12×12×1/4 HSS 304.8×304.8×6.4 12 305 0.25 6.35 0.233 5.92 10.8 6970 39.43 58.6
HSS 12×12×3/16 HSS 304.8×304.8×4.8 12 305 0.1875 4.76 0.174 4.42 8.15 5260 29.84 44.4
HSS 10×10×3/4 HSS 254×254×19 10 254 0.75 19.1 0.698 17.7 24.7 15900 89.5 133
HSS 10×10×5/8 HSS 254×254×15.9 10 254 0.625 15.9 0.581 14.8 21 13500 76.33 113
HSS 10×10×1/2 HSS 254×254×12.7 10 254 0.5 12.7 0.465 11.8 17.2 11100 62.46 92.7
HSS 10×10×3/8 HSS 254×254×9.5 10 254 0.375 9.53 0.349 8.86 13.2 8520 47.9 71.2
HSS 10×10×5/16 HSS 254×254×7.9 10 254 0.3125 7.94 0.291 7.39 11.1 7160 40.35 60
HSS 10×10×1/4 HSS 254×254×6.4 10 254 0.25 6.35 0.233 5.92 8.96 5780 32.63 48.5
HSS 10×10×3/16 HSS 254×254×4.8 10 254 0.1875 4.76 0.174 4.42 6.76 4360 24.73 36.8

HSS 9×9 to HSS 6×6

28 designations in this group.

Swipe horizontally to view all dimensions.

Designation SI designation B (in) B (mm) tnom (in) tnom (mm) tdes (in) tdes (mm) A (in²) A (mm²) Mass (lb/ft) Mass (kg/m)
HSS 9×9×5/8 HSS 228.6×228.6×15.9 9 229 0.625 15.9 0.581 14.8 18.7 12100 67.82 101
HSS 9×9×1/2 HSS 228.6×228.6×12.7 9 229 0.5 12.7 0.465 11.8 15.3 9870 55.66 82.6
HSS 9×9×3/8 HSS 228.6×228.6×9.5 9 229 0.375 9.53 0.349 8.86 11.8 7610 42.79 63.6
HSS 9×9×5/16 HSS 228.6×228.6×7.9 9 229 0.3125 7.94 0.291 7.39 9.92 6400 36.1 53.6
HSS 9×9×1/4 HSS 228.6×228.6×6.4 9 229 0.25 6.35 0.233 5.92 8.03 5180 29.23 43.4
HSS 9×9×3/16 HSS 228.6×228.6×74.8 9 229 0.1875 4.76 0.174 4.42 6.06 3910 22.18 33
HSS 9×9×1/8 HSS 228.6×228.6×3.2 9 229 0.125 3.18 0.116 2.95 4.09 2640 14.96 22.3
HSS 8×8×5/8 HSS 203.2×203.2×15.9 8 203 0.625 15.9 0.581 14.8 16.4 10600 59.32 88
HSS 8×8×1/2 HSS 203.2×203.2×12.7 8 203 0.5 12.7 0.465 11.8 13.5 8710 48.85 72.5
HSS 8×8×3/8 HSS 203.2×203.2×9.5 8 203 0.375 9.53 0.349 8.86 10.4 6710 37.69 56
HSS 8×8×5/16 HSS 203.2×203.2×7.9 8 203 0.3125 7.94 0.291 7.39 8.76 5650 31.84 47.3
HSS 8×8×1/4 HSS 203.2×203.2×6.4 8 203 0.25 6.35 0.233 5.92 7.1 4580 25.82 38.4
HSS 8×8×3/16 HSS 203.2×203.2×4.8 8 203 0.1875 4.76 0.174 4.42 5.37 3460 19.63 29.2
HSS 8×8×1/8 HSS 203.2×203.2×3.2 8 203 0.125 3.18 0.116 2.95 3.62 2340 13.26 19.7
HSS 7×7×5/8 HSS 177.8×177.8×15.9 7 178 0.625 15.9 0.581 14.8 14 9030 50.81 75.3
HSS 7×7×1/2 HSS 177.8×177.8×12.7 7 178 0.5 12.7 0.465 11.8 11.6 7480 42.05 62.4
HSS 7×7×3/8 HSS 177.8×177.8×9.5 7 178 0.375 9.53 0.349 8.86 8.97 5790 32.58 48.4
HSS 7×7×5/16 HSS 177.8×177.8×7.9 7 178 0.3125 7.94 0.291 7.39 7.59 4900 27.59 41
HSS 7×7×1/4 HSS 177.8×177.8×6.4 7 178 0.25 6.35 0.233 5.92 6.17 3980 22.42 33.3
HSS 7×7×3/16 HSS 177.8×177.8×4.8 7 178 0.1875 4.76 0.174 4.42 4.67 3010 17.08 25.4
HSS 7×7×1/8 HSS 177.8×177.8×3.2 7 178 0.125 3.18 0.116 2.95 3.16 2040 11.56 17.2
HSS 6×6×5/8 HSS 152.4×152.4×15.9 6 152 0.625 15.9 0.581 14.8 11.7 7550 42.3 62.6
HSS 6×6×1/2 HSS 152.4×152.4×12.7 6 152 0.5 12.7 0.465 11.8 9.74 6280 35.24 52.2
HSS 6×6×3/8 HSS 152.4×152.4×9.5 6 152 0.375 9.53 0.349 8.86 7.58 4890 27.48 40.8
HSS 6×6×5/16 HSS 152.4×152.4×7.9 6 152 0.3125 7.94 0.291 7.39 6.43 4150 23.34 34.6
HSS 6×6×1/4 HSS 152.4×152.4×6.4 6 152 0.25 6.35 0.233 5.92 5.24 3380 19.02 28.3
HSS 6×6×3/16 HSS 152.4×152.4×4.8 6 152 0.1875 4.76 0.174 4.42 3.98 2570 14.53 21.6
HSS 6×6×1/8 HSS 152.4×152.4×3.2 6 152 0.125 3.18 0.116 2.95 2.7 1740 9.86 14.7

HSS 5.5×5.5 to HSS 2×2

43 designations in this group.

Swipe horizontally to view all dimensions.

Designation SI designation B (in) B (mm) tnom (in) tnom (mm) tdes (in) tdes (mm) A (in²) A (mm²) Mass (lb/ft) Mass (kg/m)
HSS 5-1/2×5-1/2×3/8 HSS 139.7×139.7×9.5 5.5 140 0.375 9.53 0.349 8.86 6.88 4440 24.93 37
HSS 5-1/2×5-1/2×5/16 HSS 139.7×139.7×7.9 5.5 140 0.3125 7.94 0.291 7.39 5.85 3770 21.21 31.5
HSS 5-1/2×5-1/2×1/4 HSS 139.7×139.7×6.4 5.5 140 0.25 6.35 0.233 5.92 4.77 3080 17.32 25.7
HSS 5-1/2×5-1/2×3/16 HSS 139.7×139.7×4.8 5.5 140 0.1875 4.76 0.174 4.42 3.63 2340 13.25 19.7
HSS 5-1/2×5-1/2×1/8 HSS 139.7×139.7×3.2 5.5 140 0.125 3.18 0.116 2.95 2.46 1590 9.01 13.4
HSS 5×5×1/2 HSS 127×127×12.7 5 127 0.5 12.7 0.465 11.8 7.88 5080 28.43 42.1
HSS 5×5×3/8 HSS 127×127×9.5 5 127 0.375 9.53 0.349 8.86 6.18 3990 22.37 33.2
HSS 5×5×5/16 HSS 127×127×7.9 5 127 0.3125 7.94 0.291 7.39 5.26 3390 19.08 28.3
HSS 5×5×1/4 HSS 127×127×6.4 5 127 0.25 6.35 0.233 5.92 4.3 2770 15.62 23.2
HSS 5×5×3/16 HSS 127×127×4.8 5 127 0.1875 4.76 0.174 4.42 3.28 2120 11.97 17.8
HSS 5×5×1/8 HSS 127×127×3.2 5 127 0.125 3.18 0.116 2.95 2.23 1440 8.16 12.1
HSS 4-1/2×4-1/2×1/2 HSS 114.3×114.3×12.7 4.5 114 0.5 12.7 0.465 11.8 6.95 4480 25.03 37.1
HSS 4-1/2×4-1/2×3/8 HSS 114.3×114.3×9.5 4.5 114 0.375 9.53 0.349 8.86 5.48 3540 19.82 29.4
HSS 4-1/2×4-1/2×5/16 HSS 114.3×114.3×7.9 4.5 114 0.3125 7.94 0.291 7.39 4.68 3020 16.96 25.2
HSS 4-1/2×4-1/2×1/4 HSS 114.3×114.3×6.4 4.5 114 0.25 6.35 0.233 5.92 3.84 2480 13.91 20.7
HSS 4-1/2×4-1/2×3/16 HSS 114.3×114.3×4.8 4.5 114 0.1875 4.76 0.174 4.42 2.93 1890 10.7 15.9
HSS 4-1/2×4-1/2×1/8 HSS 114.3×114.3×3.2 4.5 114 0.125 3.18 0.116 2.95 2 1290 7.31 10.9
HSS 4×4×1/2 HSS 101.6×101.6×12.7 4 102 0.5 12.7 0.465 11.8 6.02 3880 21.63 32
HSS 4×4×3/8 HSS 101.6×101.6×9.5 4 102 0.375 9.53 0.349 8.86 4.78 3080 17.27 25.6
HSS 4×4×5/16 HSS 101.6×101.6×7.9 4 102 0.3125 7.94 0.291 7.39 4.1 2650 14.83 22
HSS 4×4×1/4 HSS 101.6×101.6×6.4 4 102 0.25 6.35 0.233 5.92 3.37 2170 12.21 18.1
HSS 4×4×3/16 HSS 101.6×101.6×4.8 4 102 0.1875 4.76 0.174 4.42 2.58 1660 9.42 14
HSS 4×4×1/8 HSS 101.6×101.6×3.2 4 102 0.125 3.18 0.116 2.95 1.77 1140 6.46 9.59
HSS 3-1/2×3-1/2×3/8 HSS 88.9×88.9×9.5 3.5 88.9 0.375 9.53 0.349 8.86 4.09 2640 14.72 21.8
HSS 3-1/2×3-1/2×5/16 HSS 88.9×88.9×7.9 3.5 88.9 0.3125 7.94 0.291 7.39 3.52 2270 12.7 18.8
HSS 3-1/2×3-1/2×1/4 HSS 88.9×88.9×6.4 3.5 88.9 0.25 6.35 0.233 5.92 2.91 1880 10.51 15.6
HSS 3-1/2×3-1/2×3/16 HSS 88.9×88.9×4.8 3.5 88.9 0.1875 4.76 0.174 4.42 2.24 1450 8.15 12.1
HSS 3-1/2×3-1/2×1/8 HSS 88.9×88.9×3.2 3.5 88.9 0.125 3.18 0.116 2.95 1.54 994 5.61 8.33
HSS 3×3×3/8 HSS 76.2×76.2×9.5 3 76.2 0.375 9.53 0.349 8.86 3.39 2190 12.17 18
HSS 3×3×5/16 HSS 76.2×76.2×7.9 3 76.2 0.3125 7.94 0.291 7.39 2.94 1900 10.58 15.7
HSS 3×3×1/4 HSS 76.2×76.2×6.4 3 76.2 0.25 6.35 0.233 5.92 2.44 1570 8.81 13.1
HSS 3×3×3/16 HSS 76.2×76.2×4.8 3 76.2 0.1875 4.76 0.174 4.42 1.89 1220 6.87 10.2
HSS 3×3×1/8 HSS 76.2×76.2×3.2 3 76.2 0.125 3.18 0.116 2.95 1.3 839 4.75 7.06
HSS 2-1/2×2-1/2×5/16 HSS 63.5×63.5×7.9 2.5 63.5 0.3125 7.94 0.291 7.39 2.35 1520 8.45 12.5
HSS 2-1/2×2-1/2×1/4 HSS 63.5×63.5×6.4 2.5 63.5 0.25 6.35 0.233 5.92 1.97 1270 7.11 10.5
HSS 2-1/2×2-1/2×3/16 HSS 63.5×63.5×4.8 2.5 63.5 0.1875 4.76 0.174 4.42 1.54 994 5.59 8.3
HSS 2-1/2×2-1/2×1/8 HSS 63.5×63.5×3.2 2.5 63.5 0.125 3.18 0.116 2.95 1.07 690 3.9 5.8
HSS 2-1/4×2-1/4×1/4 HSS 57.2×57.2×6.4 2.25 57.2 0.25 6.35 0.233 5.92 1.74 1120 6.26 9.26
HSS 2-1/4×2-1/4×3/16 HSS 57.2×57.2×4.8 2.25 57.2 0.1875 4.76 0.174 4.42 1.37 884 4.96 7.35
HSS 2-1/4×2-1/4×1/8 HSS 57.2×57.2×3.2 2.25 57.2 0.125 3.18 0.116 2.95 0.956 617 3.48 5.16
HSS 2×2×1/4 HSS 50.8×50.8×6.4 2 50.8 0.25 6.35 0.233 5.92 1.51 974 5.41 8
HSS 2×2×3/16 HSS 50.8×50.8×4.8 2 50.8 0.1875 4.76 0.174 4.42 1.19 768 4.32 6.4
HSS 2×2×1/8 HSS 50.8×50.8×3.2 2 50.8 0.125 3.18 0.116 2.95 0.84 542 3.05 4.53

Rectangular HSS (RHS)

281 rectangular designations, grouped by the longer outside dimension.

HSS 24×… to HSS 16×…

37 designations in this group.

Swipe horizontally to view all dimensions.

Designation SI designation H×B (in) H×B (mm) tnom (in) tnom (mm) tdes (in) tdes (mm) A (in²) A (mm²) Mass (lb/ft) Mass (kg/m)
HSS 24×12×3/4 HSS 609.6×304.8×19 24×12 610×305 0.75 19.1 0.698 17.7 47.1 30400 171.16 255
HSS 24×12×5/8 HSS 609.6×304.8×15.9 24×12 610×305 0.625 15.9 0.581 14.8 39.6 25500 144.39 215
HSS 24×12×1/2 HSS 609.6×304.8×12.7 24×12 610×305 0.5 12.7 0.465 11.8 32.1 20700 116.91 174
HSS 20×12×3/4 HSS 508×304.8×19 20×12 508×305 0.75 19.1 0.698 17.7 41.5 26800 150.75 224
HSS 20×12×5/8 HSS 508×304.8×15.9 20×12 508×305 0.625 15.9 0.581 14.8 35 22600 127.37 189
HSS 20×12×1/2 HSS 508×304.8×12.7 20×12 508×305 0.5 12.7 0.465 11.8 28.3 18300 103.3 153
HSS 20×12×3/8 HSS 508×304.8×9.5 20×12 508×305 0.375 9.53 0.349 8.86 21.5 13900 78.52 117
HSS 20×12×5/16 HSS 508×304.8×7.9 20×12 508×305 0.3125 7.94 0.291 7.39 18.1 11700 65.87 97.9
HSS 20×8×5/8 HSS 508×203.2×15.9 20×8 508×203 0.625 15.9 0.581 14.8 30.3 19500 110.36 164
HSS 20×8×1/2 HSS 508×203.2×12.7 20×8 508×203 0.5 12.7 0.465 11.8 24.6 15900 89.68 133
HSS 20×8×3/8 HSS 508×203.2×9.5 20×8 508×203 0.375 9.53 0.349 8.86 18.7 12100 68.31 102
HSS 20×8×5/16 HSS 508×203.2×7.9 20×8 508×203 0.3125 7.94 0.291 7.39 15.7 10100 57.36 85.3
HSS 20×4×1/2 HSS 508×101.6×12.7 20×4 508×102 0.5 12.7 0.465 11.8 20.9 13500 76.07 113
HSS 20×4×3/8 HSS 508×101.6×9.5 20×4 508×102 0.375 9.53 0.349 8.86 16 10300 58.1 86.4
HSS 20×4×5/16 HSS 508×101.6×7.9 20×4 508×102 0.3125 7.94 0.291 7.39 13.4 8650 48.86 72.7
HSS 20×4×1/4 HSS 508×101.6×6.4 20×4 508×102 0.25 6.35 0.233 5.92 10.8 6970 39.43 58.7
HSS 18×6×5/8 HSS 457.2×152.4×15.9 18×6 457×152 0.625 15.9 0.581 14.8 25.7 16600 93.34 139
HSS 18×6×1/2 HSS 457.2×152.4×12.7 18×6 457×152 0.5 12.7 0.465 11.8 20.9 13500 76.07 113
HSS 18×6×3/8 HSS 457.2×152.4×9.5 18×6 457×152 0.375 9.53 0.349 8.86 16 10300 58.1 86.4
HSS 18×6×5/16 HSS 457.2×152.4×7.9 18×6 457×152 0.3125 7.94 0.291 7.39 13.4 8650 48.86 72.7
HSS 18×6×1/4 HSS 457.2×152.4×6.4 18×6 457×152 0.25 6.35 0.233 5.92 10.8 6970 39.43 58.7
HSS 16×12×3/4 HSS 406.4×304.8×19 16×12 406×305 0.75 19.1 0.698 17.7 35.9 23200 130.33 194
HSS 16×12×5/8 HSS 406.4×304.8×15.9 16×12 406×305 0.625 15.9 0.581 14.8 30.3 19500 110.36 164
HSS 16×12×1/2 HSS 406.4×304.8×12.7 16×12 406×305 0.5 12.7 0.465 11.8 24.6 15900 89.68 133
HSS 16×12×3/8 HSS 406.4×304.8×9.5 16×12 406×305 0.375 9.53 0.349 8.86 18.7 12100 68.31 102
HSS 16×12×5/16 HSS 406.4×304.8×7.9 16×12 406×305 0.3125 7.94 0.291 7.39 15.7 10100 57.36 85.4
HSS 16×8×5/8 HSS 406.4×203.2×15.9 16×8 406×203 0.625 15.9 0.581 14.8 25.7 16600 93.34 139
HSS 16×8×1/2 HSS 406.4×203.2×12.7 16×8 406×203 0.5 12.7 0.465 11.8 20.9 13500 76.07 113
HSS 16×8×3/8 HSS 406.4×203.2×9.5 16×8 406×203 0.375 9.53 0.349 8.86 16 10300 58.1 86.4
HSS 16×8×5/16 HSS 406.4×203.2×7.9 16×8 406×203 0.3125 7.94 0.291 7.39 13.4 8650 48.86 72.7
HSS 16×8×1/4 HSS 406.4×203.2×6.4 16×8 406×203 0.25 6.35 0.233 5.92 10.8 6970 39.43 58.7
HSS 16×4×5/8 HSS 406.4×101.6×15.9 16×4 406×102 0.625 15.9 0.581 14.8 21 13500 76.33 113
HSS 16×4×1/2 HSS 406.4×101.6×12.7 16×4 406×102 0.5 12.7 0.465 11.8 17.2 11100 62.46 92.7
HSS 16×4×3/8 HSS 406.4×101.6×9.5 16×4 406×102 0.375 9.53 0.349 8.86 13.2 8520 47.9 71.2
HSS 16×4×5/16 HSS 406.4×101.6×7.9 16×4 406×102 0.3125 7.94 0.291 7.39 11.1 7160 40.35 60
HSS 16×4×1/4 HSS 406.4×101.6×6.4 16×4 406×102 0.25 6.35 0.233 5.92 8.96 5780 32.63 48.6
HSS 16×4×3/16 HSS 406.4×101.6×4.8 16×4 406×102 0.1875 4.76 0.174 4.42 6.76 4360 24.73 36.7

HSS 14×… to HSS 10×…

86 designations in this group.

Swipe horizontally to view all dimensions.

Designation SI designation H×B (in) H×B (mm) tnom (in) tnom (mm) tdes (in) tdes (mm) A (in²) A (mm²) Mass (lb/ft) Mass (kg/m)
HSS 14×10×5/8 HSS 355.6×254×15.9 14×10 356×254 0.625 15.9 0.581 14.8 25.7 16600 93.34 139
HSS 14×10×1/2 HSS 355.6×254×12.7 14×10 356×254 0.5 12.7 0.465 11.8 20.9 13500 76.07 113
HSS 14×10×3/8 HSS 355.6×254×9.5 14×10 356×254 0.375 9.53 0.349 8.86 16 10300 58.1 86.4
HSS 14×10×5/16 HSS 355.6×254×7.9 14×10 356×254 0.3125 7.94 0.291 7.39 13.4 8650 48.86 72.7
HSS 14×10×1/4 HSS 355.6×254×6.4 14×10 356×254 0.25 6.35 0.233 5.92 10.8 6970 39.43 58.7
HSS 14×6×5/8 HSS 355.6×152.4×15.9 14×6 356×152 0.625 15.9 0.581 14.8 21 13500 76.33 113
HSS 14×6×1/2 HSS 355.6×152.4×12.7 14×6 356×152 0.5 12.7 0.465 11.8 17.2 11100 62.46 92.7
HSS 14×6×3/8 HSS 355.6×152.4×9.5 14×6 356×152 0.375 9.53 0.349 8.86 13.2 8520 47.9 71.2
HSS 14×6×5/16 HSS 355.6×152.4×7.9 14×6 356×152 0.3125 7.94 0.291 7.39 11.1 7160 40.35 60
HSS 14×6×1/4 HSS 355.6×152.4×6.4 14×6 356×152 0.25 6.35 0.233 5.92 8.96 5780 32.63 48.6
HSS 14×6×3/16 HSS 355.6×152.4×4.8 14×6 356×152 0.1875 4.76 0.174 4.42 6.76 4360 24.73 36.7
HSS 14×4×5/8 HSS 355.6×101.6×15.9 14×4 356×102 0.625 15.9 0.581 14.8 18.7 12100 67.82 101
HSS 14×4×1/2 HSS 355.6×101.6×12.7 14×4 356×102 0.5 12.7 0.465 11.8 15.3 9870 55.66 82.6
HSS 14×4×3/8 HSS 355.6×101.6×9.5 14×4 356×102 0.375 9.53 0.349 8.86 11.8 7610 42.79 63.6
HSS 14×4×5/16 HSS 355.6×101.6×7.9 14×4 356×102 0.3125 7.94 0.291 7.39 9.92 6400 36.1 53.7
HSS 14×4×1/4 HSS 355.6×101.6×6.4 14×4 356×102 0.25 6.35 0.233 5.92 8.03 5180 29.23 43.5
HSS 14×4×3/16 HSS 355.6×101.6×4.8 14×4 356×102 0.1875 4.76 0.174 4.42 6.06 3910 22.18 32.9
HSS 12×10×1/2 HSS 304.8×254×12.7 12×10 305×254 0.5 12.7 0.465 11.8 19 12300 69.27 103
HSS 12×10×3/8 HSS 304.8×254×9.5 12×10 305×254 0.375 9.53 0.349 8.86 14.6 9420 53 78.8
HSS 12×10×5/16 HSS 304.8×254×7.9 12×10 305×254 0.3125 7.94 0.291 7.39 12.2 7870 44.6 66.4
HSS 12×10×1/4 HSS 304.8×254×6.4 12×10 305×254 0.25 6.35 0.233 5.92 9.9 6390 36.03 53.6
HSS 12×8×5/8 HSS 304.8×203.2×15.9 12×8 305×203 0.625 15.9 0.581 14.8 21 13500 76.33 113
HSS 12×8×1/2 HSS 304.8×203.2×12.7 12×8 305×203 0.5 12.7 0.465 11.8 17.2 11100 62.46 92.7
HSS 12×8×3/8 HSS 304.8×203.2×9.5 12×8 305×203 0.375 9.53 0.349 8.86 13.2 8520 47.9 71.2
HSS 12×8×5/16 HSS 304.8×203.2×7.9 12×8 305×203 0.3125 7.94 0.291 7.39 11.1 7160 40.35 60.1
HSS 12×8×1/4 HSS 304.8×203.2×6.4 12×8 305×203 0.25 6.35 0.233 5.92 8.96 5780 32.63 48.5
HSS 12×8×3/16 HSS 304.8×203.2×4.8 12×8 305×203 0.1875 4.77 0.174 4.42 6.76 4360 24.73 36.9
HSS 12×6×5/8 HSS 304.8×152.4×15.9 12×6 305×152 0.625 15.9 0.581 14.8 18.7 12100 67.82 101
HSS 12×6×1/2 HSS 304.8×152.4×12.7 12×6 305×152 0.5 12.7 0.465 11.8 15.3 9870 55.66 82.6
HSS 12×6×3/8 HSS 304.8×152.4×9.5 12×6 305×152 0.375 9.53 0.349 8.86 11.8 7610 42.79 63.6
HSS 12×6×5/16 HSS 304.8×152.4×7.9 12×6 305×152 0.3125 7.94 0.291 7.39 9.92 6400 36.1 53.7
HSS 12×6×1/4 HSS 304.8×152.4×6.4 12×6 305×152 0.25 6.35 0.233 5.92 8.03 5180 29.23 43.4
HSS 12×6×3/16 HSS 304.8×152.4×4.8 12×6 305×152 0.1875 4.76 0.174 4.42 6.06 3910 22.18 33.1
HSS 12×4×5/8 HSS 304.8×101.6×15.9 12×4 305×102 0.625 15.9 0.581 14.8 16.4 10600 59.32 88
HSS 12×4×1/2 HSS 304.8×101.6×12.7 12×4 305×102 0.5 12.7 0.465 11.8 13.5 8710 48.85 72.5
HSS 12×4×3/8 HSS 304.8×101.6×9.5 12×4 305×102 0.375 9.53 0.349 8.86 10.4 6710 37.69 56
HSS 12×4×5/16 HSS 304.8×101.6×7.9 12×4 305×102 0.3125 7.94 0.291 7.39 8.76 5650 31.84 47.4
HSS 12×4×1/4 HSS 304.8×101.6×6.4 12×4 305×102 0.25 6.35 0.233 5.92 7.1 4580 25.82 38.4
HSS 12×4×3/16 HSS 304.8×101.6×4.8 12×4 305×102 0.1875 4.76 0.174 4.42 5.37 3460 19.63 29.3
HSS 12×3-1/2×3/8 HSS 304.8×88.9×9.5 12×3.5 305×88.9 0.375 9.53 0.349 8.86 10 6450 36.41 54.1
HSS 12×3-1/2×5/16 HSS 304.8×88.9×7.9 12×3.5 305×88.9 0.3125 7.94 0.291 7.39 8.46 5460 30.78 45.8
HSS 12×3×5/16 HSS 304.8×76.2×7.9 12×3 305×76.2 0.3125 7.94 0.291 7.39 8.17 5270 29.72 44.2
HSS 12×3×1/4 HSS 304.8×76.2×6.4 12×3 305×76.2 0.25 6.35 0.233 5.92 6.63 4280 24.12 35.8
HSS 12×3×3/16 HSS 304.8×76.2×4.8 12×3 305×76.2 0.1875 4.76 0.174 4.42 5.02 3240 18.35 27.4
HSS 12×2×5/16 HSS 304.8×50.8×7.9 12×2 305×50.8 0.3125 7.94 0.291 7.39 7.59 4900 27.59 41
HSS 12×2×1/4 HSS 304.8×50.8×6.4 12×2 305×50.8 0.25 6.35 0.233 5.92 6.17 3980 22.42 33.3
HSS 12×2×3/16 HSS 304.8×50.8×4.8 12×2 305×50.8 0.1875 4.76 0.174 4.42 4.67 3010 17.08 25.4
HSS 10×8×5/8 HSS 254×203.2×15.9 10×8 254×203 0.625 15.9 0.581 14.8 18.7 12100 67.82 101
HSS 10×8×1/2 HSS 254×203.2×12.7 10×8 254×203 0.5 12.7 0.465 11.8 15.3 9870 55.66 82.6
HSS 10×8×3/8 HSS 254×203.2×9.5 10×8 254×203 0.375 9.53 0.349 8.86 11.8 7610 42.79 63.6
HSS 10×8×5/16 HSS 254×203.2×7.9 10×8 254×203 0.3125 7.94 0.291 7.39 9.92 6400 36.1 53.7
HSS 10×8×1/4 HSS 254×203.2×6.4 10×8 254×203 0.25 6.35 0.233 5.92 8.03 5180 29.23 43.4
HSS 10×8×3/16 HSS 254×203.2×4.8 10×8 254×203 0.1875 4.76 0.174 4.42 6.06 3910 22.18 33.1
HSS 10×6×5/8 HSS 254×152.4×15.9 10×6 254×152 0.625 15.9 0.581 14.8 16.4 10600 59.32 88
HSS 10×6×1/2 HSS 254×152.4×12.7 10×6 254×152 0.5 12.7 0.465 11.8 13.5 8710 48.85 72.5
HSS 10×6×3/8 HSS 254×152.4×9.5 10×6 254×152 0.375 9.53 0.349 8.86 10.4 6710 37.69 56
HSS 10×6×5/16 HSS 254×152.4×7.9 10×6 254×152 0.3125 7.94 0.291 7.39 8.76 5650 31.84 47.4
HSS 10×6×1/4 HSS 254×152.4×6.4 10×6 254×152 0.25 6.35 0.233 5.92 7.1 4580 25.82 38.4
HSS 10×6×3/16 HSS 254×152.4×4.8 10×6 254×152 0.1875 4.76 0.174 4.42 5.37 3460 19.63 29.3
HSS 10×5×3/8 HSS 254×127×9.5 10×5 254×127 0.375 9.53 0.349 8.86 9.67 6240 35.13 52.2
HSS 10×5×5/16 HSS 254×127×7.9 10×5 254×127 0.3125 7.94 0.291 7.39 8.17 5270 29.72 44.2
HSS 10×5×1/4 HSS 254×127×6.4 10×5 254×127 0.25 6.35 0.233 5.92 6.63 4280 24.12 35.8
HSS 10×5×3/16 HSS 254×127×4.8 10×5 254×127 0.1875 4.76 0.174 4.42 5.02 3240 18.35 27.4
HSS 10×4×5/8 HSS 254×101.6×15.9 10×4 254×102 0.625 15.9 0.581 14.8 14 9030 50.81 75.3
HSS 10×4×1/2 HSS 254×101.6×12.7 10×4 254×102 0.5 12.7 0.465 11.8 11.6 7480 42.05 62.4
HSS 10×4×3/8 HSS 254×101.6×9.5 10×4 254×102 0.375 9.53 0.349 8.86 8.97 5790 32.58 48.4
HSS 10×4×5/16 HSS 254×101.6×7.9 10×4 254×102 0.3125 7.94 0.291 7.39 7.59 4900 27.59 41
HSS 10×4×1/4 HSS 254×101.6×6.4 10×4 254×102 0.25 6.35 0.233 5.92 6.17 3980 22.42 33.3
HSS 10×4×3/16 HSS 254×101.6×4.8 10×4 254×102 0.1875 4.76 0.174 4.42 4.67 3010 17.08 25.4
HSS 10×4×1/8 HSS 254×101.6×3.2 10×4 254×102 0.125 3.18 0.116 2.95 3.16 2040 11.56 17.2
HSS 10×3-1/2×1/2 HSS 254×88.9×12.7 10×3.5 254×88.9 0.5 12.7 0.465 11.8 11.1 7160 40.34 59.8
HSS 10×3-1/2×3/8 HSS 254×88.9×9.5 10×3.5 254×88.9 0.375 9.53 0.349 8.86 8.62 5560 31.31 46.5
HSS 10×3-1/2×5/16 HSS 254×88.9×7.9 10×3.5 254×88.9 0.3125 7.94 0.291 7.39 7.3 4710 26.53 39.5
HSS 10×3-1/2×1/4 HSS 254×88.9×6.4 10×3.5 254×88.9 0.25 6.35 0.233 5.92 5.93 3830 21.57 32
HSS 10×3-1/2×3/16 HSS 254×88.9×4.8 10×3.5 254×88.9 0.1875 4.76 0.174 4.42 4.5 2900 16.44 24.5
HSS 10×3-1/2×1/8 HSS 254×88.9×3.2 10×3.5 254×88.9 0.125 3.18 0.116 2.95 3.04 1960 11.13 16.6
HSS 10×3×3/8 HSS 254×76.2×9.5 10×3 254×76.2 0.375 9.53 0.349 8.86 8.27 5340 30.03 44.6
HSS 10×3×5/16 HSS 254×76.2×7.9 10×3 254×76.2 0.3125 7.94 0.291 7.39 7.01 4520 25.46 37.9
HSS 10×3×1/4 HSS 254×76.2×6.4 10×3 254×76.2 0.25 6.35 0.233 5.92 5.7 3680 20.72 30.8
HSS 10×3×3/16 HSS 254×76.2×4.8 10×3 254×76.2 0.1875 4.76 0.174 4.42 4.32 2790 15.8 23.5
HSS 10×3×1/8 HSS 254×76.2×3.2 10×3 254×76.2 0.125 3.18 0.116 2.95 2.93 1890 10.71 15.9
HSS 10×2×3/8 HSS 254×50.8×9.5 10×2 254×50.8 0.375 9.53 0.349 8.86 7.58 4890 27.48 40.8
HSS 10×2×5/16 HSS 254×50.8×7.9 10×2 254×50.8 0.3125 7.94 0.291 7.39 6.43 4150 23.34 34.7
HSS 10×2×1/4 HSS 254×50.8×6.4 10×2 254×50.8 0.25 6.35 0.233 5.92 5.24 3380 19.02 28.3
HSS 10×2×3/16 HSS 254×50.8×4.8 10×2 254×50.8 0.1875 4.76 0.174 4.42 3.98 2570 14.53 21.6
HSS 10×2×1/8 HSS 254×50.8×3.2 10×2 254×50.8 0.125 3.18 0.116 2.95 2.7 1740 9.86 14.7

HSS 9×… to HSS 7×…

62 designations in this group.

Swipe horizontally to view all dimensions.

Designation SI designation H×B (in) H×B (mm) tnom (in) tnom (mm) tdes (in) tdes (mm) A (in²) A (mm²) Mass (lb/ft) Mass (kg/m)
HSS 9×7×5/8 HSS 228.6×177.8×15.9 9×7 229×178 0.625 15.9 0.581 14.8 16.4 10600 59.32 88
HSS 9×7×1/2 HSS 228.6×177.8×12.7 9×7 229×178 0.5 12.7 0.465 11.8 13.5 8710 48.85 72.5
HSS 9×7×3/8 HSS 228.6×177.8×9.5 9×7 229×178 0.375 9.53 0.349 8.86 10.4 6710 37.69 56
HSS 9×7×5/16 HSS 228.6×177.8×7.9 9×7 229×178 0.3125 7.94 0.291 7.39 8.76 5650 31.84 47.4
HSS 9×7×1/4 HSS 228.6×177.8×6.4 9×7 229×178 0.25 6.35 0.233 5.92 7.1 4580 25.82 38.4
HSS 9×7×3/16 HSS 228.6×177.8×4.8 9×7 229×178 0.1875 4.76 0.174 4.42 5.37 3460 19.63 29.3
HSS 9×5×5/8 HSS 228.6×127×15.9 9×5 229×127 0.625 15.9 0.581 14.8 14 9030 50.81 75.3
HSS 9×5×1/2 HSS 228.6×127×12.7 9×5 229×127 0.5 12.7 0.465 11.8 11.6 7480 42.05 62.4
HSS 9×5×3/8 HSS 228.6×127×9.5 9×5 229×127 0.375 9.53 0.349 8.86 8.97 5790 32.58 48.4
HSS 9×5×5/16 HSS 228.6×127×7.9 9×5 229×127 0.3125 7.94 0.291 7.39 7.59 4900 27.59 41
HSS 9×5×1/4 HSS 228.6×127×6.4 9×5 229×127 0.25 6.35 0.233 5.92 6.17 3980 22.42 33.3
HSS 9×5×3/16 HSS 228.6×127×4.8 9×5 229×127 0.1875 4.76 0.174 4.42 4.67 3010 17.08 25.4
HSS 9×3×1/2 HSS 228.6×76.2×12.7 9×3 229×76.2 0.5 12.7 0.465 11.8 9.74 6280 35.24 52.2
HSS 9×3×3/8 HSS 228.6×76.2×9.5 9×3 229×76.2 0.375 9.53 0.349 8.86 7.58 4890 27.48 40.8
HSS 9×3×5/16 HSS 228.6×76.2×7.9 9×3 229×76.2 0.3125 7.94 0.291 7.39 6.43 4150 23.34 34.7
HSS 9×3×1/4 HSS 228.6×76.2×6.4 9×3 229×76.2 0.25 6.35 0.233 5.92 5.24 3380 19.02 28.3
HSS 9×3×3/16 HSS 228.6×76.2×4.8 9×3 229×76.2 0.1875 4.76 0.174 4.42 3.98 2570 14.53 21.6
HSS 8×6×5/8 HSS 203.2×152.4×15.9 8×6 203×152 0.625 15.9 0.581 14.8 14 9030 50.81 75.3
HSS 8×6×1/2 HSS 203.2×152.4×12.7 8×6 203×152 0.5 12.7 0.465 11.8 11.6 7480 42.05 62.4
HSS 8×6×3/8 HSS 203.2×152.4×9.5 8×6 203×152 0.375 9.53 0.349 8.86 8.97 5790 32.58 48.4
HSS 8×6×5/16 HSS 203.2×152.4×7.9 8×6 203×152 0.3125 7.94 0.291 7.39 7.59 4900 27.59 41
HSS 8×6×1/4 HSS 203.2×152.4×6.4 8×6 203×152 0.25 6.35 0.233 5.92 6.17 3980 22.42 33.3
HSS 8×6×3/16 HSS 203.2×152.4×4.8 8×6 203×152 0.1875 4.76 0.174 4.42 4.67 3010 17.08 25.4
HSS 8×4×5/8 HSS 203.2×101.6×15.9 8×4 203×102 0.625 15.9 0.581 14.8 11.7 7550 42.3 62.6
HSS 8×4×1/2 HSS 203.2×101.6×12.7 8×4 203×102 0.5 12.7 0.465 11.8 9.74 6280 35.24 52.2
HSS 8×4×3/8 HSS 203.2×101.6×9.5 8×4 203×102 0.375 9.53 0.349 8.86 7.58 4890 27.48 40.8
HSS 8×4×5/16 HSS 203.2×101.6×7.9 8×4 203×102 0.3125 7.94 0.291 7.39 6.43 4150 23.34 34.7
HSS 8×4×1/4 HSS 203.2×101.6×6.4 8×4 203×102 0.25 6.35 0.233 5.92 5.24 3380 19.02 28.3
HSS 8×4×3/16 HSS 203.2×101.6×4.8 8×4 203×102 0.1875 4.76 0.174 4.42 3.98 2570 14.53 21.6
HSS 8×4×1/8 HSS 203.2×101.6×3.2 8×4 203×102 0.125 3.18 0.116 2.95 2.7 1740 9.86 14.7
HSS 8×3×1/2 HSS 203.2×76.2×12.7 8×3 203×76.2 0.5 12.7 0.465 11.8 8.81 5680 31.84 47.2
HSS 8×3×3/8 HSS 203.2×76.2×9.5 8×3 203×76.2 0.375 9.53 0.349 8.86 6.88 4440 24.93 37
HSS 8×3×5/16 HSS 203.2×76.2×7.9 8×3 203×76.2 0.3125 7.94 0.291 7.39 5.85 3770 21.21 31.5
HSS 8×3×1/4 HSS 203.2×76.2×6.4 8×3 203×76.2 0.25 6.35 0.233 5.92 4.77 3080 17.32 25.7
HSS 8×3×3/16 HSS 203.2×76.2×4.8 8×3 203×76.2 0.1875 4.76 0.174 4.42 3.63 2340 13.25 19.7
HSS 8×3×1/8 HSS 203.2×76.2×3.2 8×3 203×76.2 0.125 3.18 0.116 2.95 2.46 1590 9.01 13.4
HSS 8×2×3/8 HSS 203.2×50.8×9.5 8×2 203×50.8 0.375 9.53 0.349 8.86 6.18 3990 22.37 33.2
HSS 8×2×5/16 HSS 203.2×50.8×7.9 8×2 203×50.8 0.3125 7.94 0.291 7.39 5.26 3390 19.08 28.4
HSS 8×2×1/4 HSS 203.2×50.8×6.4 8×2 203×50.8 0.25 6.35 0.233 5.92 4.3 2770 15.62 23.2
HSS 8×2×3/16 HSS 203.2×50.8×4.8 8×2 203×50.8 0.1875 4.76 0.174 4.42 3.28 2120 11.97 17.8
HSS 8×2×1/8 HSS 203.2×50.8×3.2 8×2 203×50.8 0.125 3.18 0.116 2.95 2.23 1440 8.16 12.1
HSS 7×5×1/2 HSS 177.8×127×12.7 7×5 178×127 0.5 12.7 0.465 11.8 9.74 6280 35.24 52.2
HSS 7×5×3/8 HSS 177.8×127×9.5 7×5 178×127 0.375 9.53 0.349 8.86 7.58 4890 27.48 40.8
HSS 7×5×5/16 HSS 177.8×127×7.9 7×5 178×127 0.3125 7.94 0.291 7.39 6.43 4150 23.34 34.7
HSS 7×5×1/4 HSS 177.8×127×6.4 7×5 178×127 0.25 6.35 0.233 5.92 5.24 3380 19.02 28.3
HSS 7×5×3/16 HSS 177.8×127×4.8 7×5 178×127 0.1875 4.76 0.174 4.42 3.98 2570 14.53 21.6
HSS 7×5×1/8 HSS 177.8×127×3.2 7×5 178×127 0.125 3.18 0.116 2.95 2.7 1740 9.86 14.7
HSS 7×4×1/2 HSS 177.8×101.6×12.7 7×4 178×102 0.5 12.7 0.465 11.8 8.81 5680 31.84 47.2
HSS 7×4×3/8 HSS 177.8×101.6×9.5 7×4 178×102 0.375 9.53 0.349 8.86 6.88 4440 24.93 37
HSS 7×4×5/16 HSS 177.8×101.6×7.9 7×4 178×102 0.3125 7.94 0.291 7.39 5.85 3770 21.21 31.5
HSS 7×4×1/4 HSS 177.8×101.6×6.4 7×4 178×102 0.25 6.35 0.233 5.92 4.77 3080 17.32 25.7
HSS 7×4×3/16 HSS 177.8×101.6×4.8 7×4 178×102 0.1875 4.76 0.174 4.42 3.63 2340 13.25 19.7
HSS 7×4×1/8 HSS 177.8×101.6×3.2 7×4 178×102 0.125 3.18 0.116 2.95 2.46 1590 9.01 13.4
HSS 7×3×1/2 HSS 177.8×76.2×12.7 7×3 178×76.2 0.5 12.7 0.465 11.8 7.88 5080 28.43 42.1
HSS 7×3×3/8 HSS 177.8×76.2×9.5 7×3 178×76.2 0.375 9.53 0.349 8.86 6.18 3990 22.37 33.2
HSS 7×3×5/16 HSS 177.8×76.2×7.9 7×3 178×76.2 0.3125 7.94 0.291 7.39 5.26 3390 19.08 28.4
HSS 7×3×1/4 HSS 177.8×76.2×6.4 7×3 178×76.2 0.25 6.35 0.233 5.92 4.3 2770 15.62 23.2
HSS 7×3×3/16 HSS 177.8×76.2×4.8 7×3 178×76.2 0.1875 4.76 0.174 4.42 3.28 2120 11.97 17.8
HSS 7×3×1/8 HSS 177.8×76.2×3.2 7×3 178×76.2 0.125 3.18 0.116 2.95 2.23 1440 8.16 12.1
HSS 7×2×1/4 HSS 177.8×50.8×6.4 7×2 178×50.8 0.25 6.35 0.233 5.92 3.84 2480 13.91 20.7
HSS 7×2×3/16 HSS 177.8×50.8×4.8 7×2 178×50.8 0.1875 4.76 0.174 4.42 2.93 1890 10.7 15.9
HSS 7×2×1/8 HSS 177.8×50.8×3.2 7×2 178×50.8 0.125 3.18 0.116 2.95 2 1290 7.31 10.9

HSS 6×… to HSS 5×…

43 designations in this group.

Swipe horizontally to view all dimensions.

Designation SI designation H×B (in) H×B (mm) tnom (in) tnom (mm) tdes (in) tdes (mm) A (in²) A (mm²) Mass (lb/ft) Mass (kg/m)
HSS 6×5×1/2 HSS 152.4×127×12.7 6×5 152×127 0.5 12.7 0.465 11.8 8.81 5680 31.84 47.2
HSS 6×5×3/8 HSS 152.4×127×9.5 6×5 152×127 0.375 9.53 0.349 8.86 6.88 4440 24.93 37
HSS 6×5×5/16 HSS 152.4×127×7.9 6×5 152×127 0.3125 7.94 0.291 7.39 5.85 3770 21.21 31.5
HSS 6×5×1/4 HSS 152.4×127×6.4 6×5 152×127 0.25 6.35 0.233 5.92 4.77 3080 17.32 25.7
HSS 6×5×3/16 HSS 152.4×127×4.8 6×5 152×127 0.1875 4.76 0.174 4.42 3.63 2340 13.25 19.7
HSS 6×5×1/8 HSS 152.4×127×3.2 6×5 152×127 0.125 3.18 0.116 2.95 2.46 1590 9.01 13.4
HSS 6×4×1/2 HSS 152.4×101.6×12.7 6×4 152×102 0.5 12.7 0.465 11.8 7.88 5080 28.43 42.1
HSS 6×4×3/8 HSS 152.4×101.6×9.5 6×4 152×102 0.375 9.53 0.349 8.86 6.18 3990 22.37 33.2
HSS 6×4×5/16 HSS 152.4×101.6×7.9 6×4 152×102 0.3125 7.94 0.291 7.39 5.26 3390 19.08 28.4
HSS 6×4×1/4 HSS 152.4×101.6×6.4 6×4 152×102 0.25 6.35 0.233 5.92 4.3 2770 15.62 23.2
HSS 6×4×3/16 HSS 152.4×101.6×4.8 6×4 152×102 0.1875 4.76 0.174 4.42 3.28 2120 11.97 17.8
HSS 6×4×1/8 HSS 152.4×101.6×3.2 6×4 152×102 0.125 3.18 0.116 2.95 2.23 1440 8.16 12.1
HSS 6×3×1/2 HSS 152.4×76.2×12.7 6×3 152×76.2 0.5 12.7 0.465 11.8 6.95 4480 25.03 37.1
HSS 6×3×3/8 HSS 152.4×76.2×9.5 6×3 152×76.2 0.375 9.53 0.349 8.86 5.48 3540 19.82 29.4
HSS 6×3×5/16 HSS 152.4×76.2×7.9 6×3 152×76.2 0.3125 7.94 0.291 7.39 4.68 3020 16.96 25.2
HSS 6×3×1/4 HSS 152.4×76.2×6.4 6×3 152×76.2 0.25 6.35 0.233 5.92 3.84 2480 13.91 20.7
HSS 6×3×3/16 HSS 152.4×76.2×4.8 6×3 152×76.2 0.1875 4.76 0.174 4.42 2.93 1890 10.7 15.9
HSS 6×3×1/8 HSS 152.4×76.2×3.2 6×3 152×76.2 0.125 3.18 0.116 2.95 2 1290 7.31 10.9
HSS 6×2×3/8 HSS 152.4×50.8×9.5 6×2 152×50.8 0.375 9.53 0.349 8.86 4.78 3080 17.27 25.6
HSS 6×2×5/16 HSS 152.4×50.8×7.9 6×2 152×50.8 0.3125 7.94 0.291 7.39 4.1 2650 14.83 22
HSS 6×2×1/4 HSS 152.4×50.8×6.4 6×2 152×50.8 0.25 6.35 0.233 5.92 3.37 2170 12.21 18.1
HSS 6×2×3/16 HSS 152.4×50.8×4.8 6×2 152×50.8 0.1875 4.76 0.174 4.42 2.58 1660 9.42 14
HSS 6×2×1/8 HSS 152.4×50.8×3.2 6×2 152×50.8 0.125 3.18 0.116 2.95 1.77 1140 6.46 9.59
HSS 5×4×1/2 HSS 127×101.6×12.7 5×4 127×102 0.5 12.7 0.465 11.8 6.95 4480 25.03 37.1
HSS 5×4×3/8 HSS 127×101.6×9.5 5×4 127×102 0.375 9.53 0.349 8.86 5.48 3540 19.82 29.4
HSS 5×4×5/16 HSS 127×101.6×7.9 5×4 127×102 0.3125 7.94 0.291 7.39 4.68 3020 16.96 25.2
HSS 5×4×1/4 HSS 127×101.6×6.4 5×4 127×102 0.25 6.35 0.233 5.92 3.84 2480 13.91 20.7
HSS 5×4×3/16 HSS 127×101.6×4.8 5×4 127×102 0.1875 4.76 0.174 4.42 2.93 1890 10.7 15.9
HSS 5×4×1/8 HSS 127×101.6×3.2 5×4 127×102 0.125 3.18 0.116 2.95 2 1290 7.31 10.9
HSS 5×3×1/2 HSS 127×76.2×12.7 5×3 127×76.2 0.5 12.7 0.465 11.8 6.02 3880 21.63 32
HSS 5×3×3/8 HSS 127×76.2×9.5 5×3 127×76.2 0.375 9.53 0.349 8.86 4.78 3080 17.27 25.6
HSS 5×3×5/16 HSS 127×76.2×7.9 5×3 127×76.2 0.3125 7.94 0.291 7.39 4.1 2650 14.83 22
HSS 5×3×1/4 HSS 127×76.2×6.4 5×3 127×76.2 0.25 6.35 0.233 5.92 3.37 2170 12.21 18.1
HSS 5×3×3/16 HSS 127×76.2×4.8 5×3 127×76.2 0.1875 4.76 0.174 4.42 2.58 1660 9.42 14
HSS 5×3×1/8 HSS 127×76.2×3.2 5×3 127×76.2 0.125 3.18 0.116 2.95 1.77 1140 6.46 9.59
HSS 5×2-1/2×1/4 HSS 127×63.5×6.4 5×2.5 127×63.5 0.25 6.35 0.233 5.92 3.14 2030 11.36 16.9
HSS 5×2-1/2×3/16 HSS 127×63.5×4.8 5×2.5 127×63.5 0.1875 4.76 0.174 4.42 2.41 1550 8.78 13.1
HSS 5×2-1/2×1/8 HSS 127×63.5×3.2 5×2.5 127×63.5 0.125 3.18 0.116 2.95 1.65 1060 6.03 8.96
HSS 5×2×3/8 HSS 127×50.8×9.5 5×2 127×50.8 0.375 9.53 0.349 8.86 4.09 2640 14.72 21.8
HSS 5×2×5/16 HSS 127×50.8×7.9 5×2 127×50.8 0.3125 7.94 0.291 7.39 3.52 2270 12.7 18.8
HSS 5×2×1/4 HSS 127×50.8×6.4 5×2 127×50.8 0.25 6.35 0.233 5.92 2.91 1880 10.51 15.6
HSS 5×2×3/16 HSS 127×50.8×4.8 5×2 127×50.8 0.1875 4.76 0.174 4.42 2.24 1450 8.15 12.1
HSS 5×2×1/8 HSS 127×50.8×3.2 5×2 127×50.8 0.125 3.18 0.116 2.95 1.54 994 5.61 8.33

HSS 4.5×… to HSS 2×…

53 designations in this group.

Swipe horizontally to view all dimensions.

Designation SI designation H×B (in) H×B (mm) tnom (in) tnom (mm) tdes (in) tdes (mm) A (in²) A (mm²) Mass (lb/ft) Mass (kg/m)
HSS 4×3×3/8 HSS 101.6×76.2×9.5 4×3 102×76.2 0.375 9.53 0.349 8.86 4.09 2640 14.72 21.8
HSS 4×3×5/16 HSS 101.6×76.2×7.9 4×3 102×76.2 0.3125 7.94 0.291 7.39 3.52 2270 12.7 18.8
HSS 4×3×1/4 HSS 101.6×76.2×6.4 4×3 102×76.2 0.25 6.35 0.233 5.92 2.91 1880 10.51 15.6
HSS 4×3×3/16 HSS 101.6×76.2×4.8 4×3 102×76.2 0.1875 4.76 0.174 4.42 2.24 1450 8.15 12.1
HSS 4×3×1/8 HSS 101.6×76.2×3.2 4×3 102×76.2 0.125 3.18 0.116 2.95 1.54 994 5.61 8.33
HSS 4×2-1/2×3/8 HSS 101.6×63.5×9.5 4×2.5 102×63.5 0.375 9.53 0.349 8.86 3.74 2410 13.44 19.9
HSS 4×2-1/2×5/16 HSS 101.6×63.5×7.9 4×2.5 102×63.5 0.3125 7.94 0.291 7.39 3.23 2080 11.64 17.3
HSS 4×2-1/2×1/4 HSS 101.6×63.5×6.4 4×2.5 102×63.5 0.25 6.35 0.233 5.92 2.67 1720 9.66 14.3
HSS 4×2-1/2×3/16 HSS 101.6×63.5×4.8 4×2.5 102×63.5 0.1875 4.76 0.174 4.42 2.06 1330 7.51 11.2
HSS 4×2-1/2×1/8 HSS 101.6×63.5×3.2 4×2.5 102×63.5 0.125 3.18 0.116 2.95 1.42 916 5.18 7.7
HSS 4×2×3/8 HSS 101.6×50.8×9.5 4×2 102×50.8 0.375 9.53 0.349 8.86 3.39 2190 12.17 18
HSS 4×2×5/16 HSS 101.6×50.8×7.9 4×2 102×50.8 0.3125 7.94 0.291 7.39 2.94 1900 10.58 15.7
HSS 4×2×1/4 HSS 101.6×50.8×6.4 4×2 102×50.8 0.25 6.35 0.233 5.92 2.44 1570 8.81 13.1
HSS 4×2×3/16 HSS 101.6×50.8×4.8 4×2 102×50.8 0.1875 4.76 0.174 4.42 1.89 1220 6.87 10.2
HSS 4×2×1/8 HSS 101.6×50.8×3.2 4×2 102×50.8 0.125 3.18 0.116 2.95 1.3 839 4.75 7.06
HSS 3-1/2×2-1/2×3/8 HSS 88.9×63.5×9.5 3.5×2.5 88.9×63.5 0.375 9.53 0.349 8.86 3.39 2190 12.17 18
HSS 3-1/2×2-1/2×5/16 HSS 88.9×63.5×7.9 3.5×2.5 88.9×63.5 0.3125 7.94 0.291 7.39 2.94 1900 10.58 15.6
HSS 3-1/2×2-1/2×1/4 HSS 88.9×63.5×6.4 3.5×2.5 88.9×63.5 0.25 6.35 0.233 5.92 2.44 1570 8.81 13.1
HSS 3-1/2×2-1/2×3/16 HSS 88.9×63.5×4.8 3.5×2.5 88.9×63.5 0.1875 4.76 0.174 4.42 1.89 1220 6.87 10.2
HSS 3-1/2×2-1/2×1/8 HSS 88.9×63.5×3.2 3.5×2.5 88.9×63.5 0.125 3.18 0.116 2.95 1.3 839 4.75 7.07
HSS 3-1/2×2×1/4 HSS 88.9×50.8×6.4 3.5×2 88.9×50.8 0.25 6.35 0.233 5.92 2.21 1430 7.96 11.8
HSS 3-1/2×2×3/16 HSS 88.9×50.8×4.8 3.5×2 88.9×50.8 0.1875 4.76 0.174 4.42 1.71 1100 6.23 9.27
HSS 3-1/2×2×1/8 HSS 88.9×50.8×3.2 3.5×2 88.9×50.8 0.125 3.18 0.116 2.95 1.19 768 4.33 6.43
HSS 3-1/2×1-1/2×1/4 HSS 88.9×38.1×6.4 3.5×1.5 88.9×38.1 0.25 6.35 0.233 5.92 1.97 1270 7.11 10.5
HSS 3-1/2×1-1/2×3/16 HSS 88.9×38.1×4.8 3.5×1.5 88.9×38.1 0.1875 4.76 0.174 4.42 1.54 994 5.59 8.31
HSS 3-1/2×1-1/2×1/8 HSS 88.9×38.1×3.2 3.5×1.5 88.9×38.1 0.125 3.18 0.116 2.95 1.07 690 3.9 5.8
HSS 3×2-1/2×5/16 HSS 76.2×63.5×7.9 3×2.5 76.2×63.5 0.3125 7.94 0.291 7.39 2.64 1700 9.51 14.1
HSS 3×2-1/2×1/4 HSS 76.2×63.5×6.4 3×2.5 76.2×63.5 0.25 6.35 0.233 5.92 2.21 1430 7.96 11.8
HSS 3×2-1/2×3/16 HSS 76.2×63.5×4.8 3×2.5 76.2×63.5 0.1875 4.76 0.174 4.42 1.71 1100 6.23 9.27
HSS 3×2-1/2×1/8 HSS 76.2×63.5×3.2 3×2.5 76.2×63.5 0.125 3.18 0.116 2.95 1.19 768 4.33 6.43
HSS 3×2×5/16 HSS 76.2×50.8×7.9 3×2 76.2×50.8 0.3125 7.94 0.291 7.39 2.35 1520 8.45 12.5
HSS 3×2×1/4 HSS 76.2×50.8×6.4 3×2 76.2×50.8 0.25 6.35 0.233 5.92 1.97 1270 7.11 10.5
HSS 3×2×3/16 HSS 76.2×50.8×4.8 3×2 76.2×50.8 0.1875 4.76 0.174 4.42 1.54 994 5.59 8.31
HSS 3×2×1/8 HSS 76.2×50.8×3.2 3×2 76.2×50.8 0.125 3.18 0.116 2.95 1.07 690 3.9 5.8
HSS 3×1-1/2×1/4 HSS 76.2×38.1×6.4 3×1.5 76.2×38.1 0.25 6.35 0.233 5.92 1.74 1120 6.26 9.26
HSS 3×1-1/2×3/16 HSS 76.2×38.1×4.8 3×1.5 76.2×38.1 0.1875 4.76 0.174 4.42 1.37 884 4.96 7.36
HSS 3×1-1/2×1/8 HSS 76.2×38.1×3.2 3×1.5 76.2×38.1 0.125 3.18 0.116 2.95 0.956 617 3.48 5.16
HSS 3×1×3/16 HSS 76.2×25.4×4.8 3×1 76.2×25.4 0.1875 4.76 0.174 4.42 1.19 768 4.32 6.41
HSS 3×1×1/8 HSS 76.2×25.4×3.2 3×1 76.2×25.4 0.125 3.18 0.116 2.95 0.84 542 3.05 4.53
HSS 2-1/2×2×1/4 HSS 63.5×50.8×6.4 2.5×2 63.5×50.8 0.25 6.35 0.233 5.92 1.74 1120 6.26 9.26
HSS 2-1/2×2×3/16 HSS 63.5×50.8×4.8 2.5×2 63.5×50.8 0.1875 4.76 0.174 4.42 1.37 884 4.96 7.36
HSS 2-1/2×2×1/8 HSS 63.5×50.8×3.2 2.5×2 63.5×50.8 0.125 3.18 0.116 2.95 0.956 617 3.48 5.16
HSS 2-1/2×1-1/2×1/4 HSS 63.5×38.1×6.4 2.5×1.5 63.5×38.1 0.25 6.35 0.233 5.92 1.51 974 5.41 8
HSS 2-1/2×1-1/2×3/16 HSS 63.5×38.1×4.8 2.5×1.5 63.5×38.1 0.1875 4.76 0.174 4.42 1.19 768 4.32 6.41
HSS 2-1/2×1-1/2×1/8 HSS 63.5×38.1×3.2 2.5×1.5 63.5×38.1 0.125 3.18 0.116 2.95 0.84 542 3.05 4.53
HSS 2-1/2×1×3/16 HSS 63.5×25.4×4.8 2.5×1 63.5×25.4 0.1875 4.76 0.174 4.42 1.02 658 3.68 5.46
HSS 2-1/2×1×1/8 HSS 63.5×25.4×3.2 2.5×1 63.5×25.4 0.125 3.18 0.116 2.95 0.724 467 2.63 3.9
HSS 2-1/4×2×3/16 HSS 57.2×50.8×4.8 2.25×2 57.2×50.8 0.1875 4.76 0.174 4.42 1.28 826 4.64 6.89
HSS 2-1/4×2×1/8 HSS 57.2×50.8×3.2 2.25×2 57.2×50.8 0.125 3.18 0.116 2.95 0.898 579 3.27 4.85
HSS 2×1-1/2×3/16 HSS 50.8×38.1×4.8 2×1.5 50.8×38.1 0.1875 4.76 0.174 4.42 1.02 658 3.68 5.46
HSS 2×1-1/2×1/8 HSS 50.8×38.1×3.2 2×1.5 50.8×38.1 0.125 3.18 0.116 2.95 0.724 467 2.63 3.9
HSS 2×1×3/16 HSS 50.8×25.4×4.8 2×1 50.8×25.4 0.1875 4.76 0.174 4.42 0.845 545 3.04 4.51
HSS 2×1×1/8 HSS 50.8×25.4×3.2 2×1 50.8×25.4 0.125 3.18 0.116 2.95 0.608 392 2.2 3.26

Round HSS (CHS)

128 round designations, grouped by outside diameter. These are HSS, not AISC Pipe and not ASTM A53 pipe, even when the outside diameter looks familiar.

HSS 20.000 to HSS 10.000

27 designations in this group.

Swipe horizontally to view all dimensions.

Designation SI designation OD (in) OD (mm) tnom (in) tnom (mm) tdes (in) tdes (mm) A (in²) A (mm²) Mass (lb/ft) Mass (kg/m)
HSS 20.000×0.500 HSS 508×12.7 20 508 0.5 12.7 0.465 11.8 28.5 18400 104 155
HSS 20.000×0.375 HSS 508×9.5 20 508 0.375 9.53 0.349 8.86 21.5 13900 78.67 117
HSS 18.000×0.500 HSS 457.2×12.7 18 457 0.5 12.7 0.465 11.8 25.6 16500 93.54 139
HSS 18.000×0.375 HSS 457.2×9.5 18 457 0.375 9.53 0.349 8.86 19.4 12500 70.66 105
HSS 16.000×0.625 HSS 406.4×15.9 16 406 0.625 15.9 0.581 14.8 28.1 18100 103 153
HSS 16.000×0.500 HSS 406.4×12.7 16 406 0.5 12.7 0.465 11.8 22.7 14600 82.85 123
HSS 16.000×0.438 HSS 406.4×11.1 16 406 0.438 11.1 0.407 10.3 19.9 12800 72.87 108
HSS 16.000×0.375 HSS 406.4×9.5 16 406 0.375 9.53 0.349 8.86 17.2 11100 62.64 93.2
HSS 16.000×0.312 HSS 406.4×7.9 16 406 0.312 7.94 0.291 7.39 14.4 9290 52.32 77.9
HSS 16.000×0.250 HSS 406.4×6.4 16 406 0.25 6.35 0.233 5.92 11.5 7420 42.09 62.6
HSS 14.000×0.625 HSS 355.6×15.9 14 356 0.625 15.9 0.581 14.8 24.5 15800 89.36 133
HSS 14.000×0.500 HSS 355.6×12.7 14 356 0.5 12.7 0.465 11.8 19.8 12800 72.16 107
HSS 14.000×0.375 HSS 355.6×9.5 14 356 0.375 9.53 0.349 8.86 15 9680 54.62 81.3
HSS 14.000×0.312 HSS 355.6×7.9 14 356 0.312 7.94 0.291 7.39 12.5 8060 45.65 67.9
HSS 14.000×0.250 HSS 355.6×6.4 14 356 0.25 6.35 0.233 5.92 10.1 6520 36.75 54.7
HSS 12.750×0.500 HSS 323.9×12.7 12.8 324 0.5 12.7 0.465 11.8 17.9 11500 65.48 97.4
HSS 12.750×0.375 HSS 323.9×9.5 12.8 324 0.375 9.53 0.349 8.86 13.6 8770 49.61 73.8
HSS 12.750×0.250 HSS 323.9×6.4 12.8 324 0.25 6.35 0.233 5.92 9.16 5910 33.41 49.7
HSS 10.750×0.500 HSS 273.1×12.7 10.8 273 0.5 12.7 0.465 11.8 15 9680 54.79 81.5
HSS 10.750×0.375 HSS 273.1×9.5 10.8 273 0.375 9.53 0.349 8.86 11.4 7350 41.59 61.9
HSS 10.750×0.250 HSS 273.1×6.4 10.8 273 0.25 6.35 0.233 5.92 7.7 4970 28.06 41.8
HSS 10.000×0.625 HSS 254×15.9 10 254 0.625 15.9 0.581 14.8 17.2 11100 62.64 93.2
HSS 10.000×0.500 HSS 254×12.7 10 254 0.5 12.7 0.465 11.8 13.9 8970 50.78 75.6
HSS 10.000×0.375 HSS 254×9.5 10 254 0.375 9.53 0.349 8.86 10.6 6840 38.58 57.4
HSS 10.000×0.312 HSS 254×7.9 10 254 0.312 7.94 0.291 7.39 8.88 5730 32.31 48.1
HSS 10.000×0.250 HSS 254×6.4 10 254 0.25 6.35 0.233 5.92 7.15 4610 26.06 38.8
HSS 10.000×0.188 HSS 254×4.8 10 254 0.188 4.78 0.174 4.42 5.37 3460 19.72 29.3

HSS 9.625 to HSS 5.563

49 designations in this group.

Swipe horizontally to view all dimensions.

Designation SI designation OD (in) OD (mm) tnom (in) tnom (mm) tdes (in) tdes (mm) A (in²) A (mm²) Mass (lb/ft) Mass (kg/m)
HSS 9.625×0.500 HSS 244.5×12.7 9.63 244 0.5 12.7 0.465 11.8 13.4 8650 48.77 72.6
HSS 9.625×0.375 HSS 244.5×9.5 9.63 244 0.375 9.53 0.349 8.86 10.2 6580 37.08 55.2
HSS 9.625×0.312 HSS 244.5×7.9 9.63 244 0.312 7.94 0.291 7.39 8.53 5500 31.06 46.2
HSS 9.625×0.250 HSS 244.5×6.4 9.63 244 0.25 6.35 0.233 5.92 6.87 4430 25.06 37.3
HSS 9.625×0.188 HSS 244.5×4.8 9.63 244 0.188 4.78 0.174 4.42 5.17 3340 18.97 28.2
HSS 8.625×0.625 HSS 219.1×15.9 8.63 219 0.625 15.9 0.581 14.8 14.7 9480 53.45 79.5
HSS 8.625×0.500 HSS 219.1×12.7 8.63 219 0.5 12.7 0.465 11.8 11.9 7680 43.43 64.6
HSS 8.625×0.375 HSS 219.1×9.5 8.63 219 0.375 9.53 0.349 8.86 9.07 5850 33.07 49.2
HSS 8.625×0.322 HSS 219.1×8.2 8.63 219 0.322 8.18 0.3 7.62 7.85 5060 28.58 42.5
HSS 8.625×0.250 HSS 219.1×6.4 8.63 219 0.25 6.35 0.233 5.92 6.14 3960 22.38 33.3
HSS 8.625×0.188 HSS 219.1×4.8 8.63 219 0.188 4.78 0.174 4.42 4.62 2980 16.96 25.2
HSS 7.625×0.375 HSS 193.7×9.5 7.63 194 0.375 9.53 0.349 8.86 7.98 5150 29.06 43.2
HSS 7.625×0.328 HSS 193.7×8.3 7.63 194 0.328 8.33 0.305 7.75 7.01 4520 25.59 38.1
HSS 7.500×0.500 HSS 190.5×12.7 7.5 191 0.5 12.7 0.465 11.8 10.3 6650 37.42 55.7
HSS 7.500×0.375 HSS 190.5×9.5 7.5 191 0.375 9.53 0.349 8.86 7.84 5060 28.56 42.5
HSS 7.500×0.312 HSS 190.5×7.9 7.5 191 0.312 7.94 0.291 7.39 6.59 4250 23.97 35.7
HSS 7.500×0.250 HSS 190.5×6.4 7.5 191 0.25 6.35 0.233 5.92 5.32 3430 19.38 28.8
HSS 7.500×0.188 HSS 190.5×4.8 7.5 191 0.188 4.78 0.174 4.42 4 2580 14.7 21.9
HSS 7.000×0.500 HSS 177.8×12.7 7 178 0.5 12.7 0.465 11.8 9.55 6160 34.74 51.7
HSS 7.000×0.375 HSS 177.8×9.5 7 178 0.375 9.53 0.349 8.86 7.29 4700 26.56 39.5
HSS 7.000×0.312 HSS 177.8×7.9 7 178 0.312 7.94 0.291 7.39 6.13 3950 22.31 33.2
HSS 7.000×0.250 HSS 177.8×6.4 7 178 0.25 6.35 0.233 5.92 4.95 3190 18.04 26.8
HSS 7.000×0.188 HSS 177.8×4.8 7 178 0.188 4.78 0.174 4.42 3.73 2410 13.69 20.4
HSS 7.000×0.125 HSS 177.8×3.2 7 178 0.125 3.18 0.116 2.95 2.51 1620 9.19 13.7
HSS 6.875×0.500 HSS 174.6×12.7 6.88 175 0.5 12.7 0.465 11.8 9.36 6040 34.07 50.7
HSS 6.875×0.375 HSS 174.6×9.5 6.88 175 0.375 9.53 0.349 8.86 7.16 4620 26.06 38.8
HSS 6.875×0.312 HSS 174.6×7.9 6.88 175 0.312 7.94 0.291 7.39 6.02 3880 21.89 32.6
HSS 6.875×0.250 HSS 174.6×6.4 6.88 175 0.25 6.35 0.233 5.92 4.86 3140 17.71 26.3
HSS 6.875×0.188 HSS 174.6×4.8 6.88 175 0.188 4.78 0.174 4.42 3.66 2360 13.44 20
HSS 6.625×0.500 HSS 168.3×12.7 6.63 168 0.5 12.7 0.465 11.8 9 5810 32.74 48.7
HSS 6.625×0.432 HSS 168.3×11 6.63 168 0.432 11.1 0.402 10.2 7.86 5070 28.6 42.6
HSS 6.625×0.375 HSS 168.3×9.5 6.63 168 0.375 9.53 0.349 8.86 6.88 4440 25.06 37.3
HSS 6.625×0.312 HSS 168.3×7.9 6.63 168 0.312 7.94 0.291 7.39 5.79 3740 21.06 31.3
HSS 6.625×0.280 HSS 168.3×7.1 6.63 168 0.28 7.11 0.26 6.6 5.2 3350 18.99 28.3
HSS 6.625×0.250 HSS 168.3×6.4 6.63 168 0.25 6.35 0.233 5.92 4.68 3020 17.04 25.4
HSS 6.625×0.188 HSS 168.3×4.8 6.63 168 0.188 4.78 0.174 4.42 3.53 2280 12.94 19.2
HSS 6.625×0.125 HSS 168.3×3.2 6.63 168 0.125 3.18 0.116 2.95 2.37 1530 8.69 12.9
HSS 6.000×0.500 HSS 152.4×12.7 6 152 0.5 12.7 0.465 11.8 8.09 5220 29.4 43.7
HSS 6.000×0.375 HSS 152.4×9.5 6 152 0.375 9.53 0.349 8.86 6.2 4000 22.55 33.6
HSS 6.000×0.312 HSS 152.4×7.9 6 152 0.312 7.94 0.291 7.39 5.22 3370 18.97 28.2
HSS 6.000×0.280 HSS 152.4×7.1 6 152 0.28 7.11 0.26 6.6 4.69 3030 17.12 25.5
HSS 6.000×0.250 HSS 152.4×6.4 6 152 0.25 6.35 0.233 5.92 4.22 2720 15.37 22.9
HSS 6.000×0.188 HSS 152.4×4.8 6 152 0.188 4.78 0.174 4.42 3.18 2050 11.68 17.4
HSS 6.000×0.125 HSS 152.4×3.2 6 152 0.125 3.18 0.116 2.95 2.14 1380 7.85 11.7
HSS 5.563×0.500 HSS 141.3×12.7 5.56 141 0.5 12.7 0.465 11.8 7.45 4810 27.06 40.3
HSS 5.563×0.375 HSS 141.3×9.5 5.56 141 0.375 9.53 0.349 8.86 5.72 3690 20.8 30.9
HSS 5.563×0.258 HSS 141.3×6.6 5.56 141 0.258 6.55 0.24 6.1 4.01 2590 14.63 21.8
HSS 5.563×0.188 HSS 141.3×4.8 5.56 141 0.188 4.78 0.174 4.42 2.95 1900 10.8 16.1
HSS 5.563×0.134 HSS 141.3×3.4 5.56 141 0.134 3.4 0.124 3.15 2.12 1370 7.78 11.6

HSS 5.000 to HSS 1.660

52 designations in this group.

Swipe horizontally to view all dimensions.

Designation SI designation OD (in) OD (mm) tnom (in) tnom (mm) tdes (in) tdes (mm) A (in²) A (mm²) Mass (lb/ft) Mass (kg/m)
HSS 5.500×0.500 HSS 139.7×12.7 5.5 140 0.5 12.7 0.465 11.8 7.36 4750 26.73 39.8
HSS 5.500×0.375 HSS 139.7×9.5 5.5 140 0.375 9.53 0.349 8.86 5.65 3650 20.55 30.6
HSS 5.500×0.258 HSS 139.7×6.6 5.5 140 0.258 6.55 0.24 6.1 3.97 2560 14.46 21.5
HSS 5.000×0.500 HSS 127×12.7 5 127 0.5 12.7 0.465 11.8 6.62 4270 24.05 35.8
HSS 5.000×0.375 HSS 127×9.5 5 127 0.375 9.53 0.349 8.86 5.1 3290 18.54 27.6
HSS 5.000×0.312 HSS 127×7.9 5 127 0.312 7.94 0.291 7.39 4.3 2770 15.64 23.3
HSS 5.000×0.258 HSS 127×6.6 5 127 0.258 6.55 0.24 6.1 3.59 2320 13.08 19.5
HSS 5.000×0.250 HSS 127×6.4 5 127 0.25 6.35 0.233 5.92 3.49 2250 12.69 18.9
HSS 5.000×0.188 HSS 127×4.8 5 127 0.188 4.78 0.174 4.42 2.64 1700 9.67 14.4
HSS 5.000×0.125 HSS 127×3.2 5 127 0.125 3.18 0.116 2.95 1.78 1150 6.51 9.69
HSS 4.500×0.375 HSS 114.3×9.5 4.5 114 0.375 9.53 0.349 8.86 4.55 2940 16.54 24.6
HSS 4.500×0.337 HSS 114.3×8.6 4.5 114 0.337 8.56 0.313 7.95 4.12 2660 15 22.3
HSS 4.500×0.237 HSS 114.3×6 4.5 114 0.237 6.02 0.22 5.59 2.96 1910 10.8 16.1
HSS 4.500×0.188 HSS 114.3×4.8 4.5 114 0.188 4.78 0.174 4.42 2.36 1520 8.67 12.9
HSS 4.500×0.125 HSS 114.3×3.2 4.5 114 0.125 3.18 0.116 2.95 1.6 1030 5.85 8.7
HSS 4.000×0.313 HSS 101.6×8 4 102 0.313 7.94 0.291 7.39 3.39 2190 12.34 18.4
HSS 4.000×0.250 HSS 101.6×6.4 4 102 0.25 6.35 0.233 5.92 2.76 1780 10 14.9
HSS 4.000×0.237 HSS 101.6×6 4 102 0.237 6.02 0.22 5.59 2.61 1680 9.53 14.2
HSS 4.000×0.226 HSS 101.6×5.7 4 102 0.226 5.74 0.21 5.33 2.5 1610 9.12 13.6
HSS 4.000×0.220 HSS 101.6×5.6 4 102 0.22 5.59 0.205 5.21 2.44 1570 8.89 13.2
HSS 4.000×0.188 HSS 101.6×4.8 4 102 0.188 4.78 0.174 4.42 2.09 1350 7.66 11.4
HSS 4.000×0.125 HSS 101.6×3.2 4 102 0.125 3.18 0.116 2.95 1.42 916 5.18 7.7
HSS 3.500×0.313 HSS 88.9×8 3.5 88.9 0.313 7.95 0.291 7.39 2.93 1890 10.66 15.9
HSS 3.500×0.300 HSS 88.9×7.6 3.5 88.9 0.3 7.62 0.279 7.09 2.82 1820 10.26 15.3
HSS 3.500×0.250 HSS 88.9×6.4 3.5 88.9 0.25 6.35 0.233 5.92 2.39 1540 8.69 12.9
HSS 3.500×0.216 HSS 88.9×5.5 3.5 88.9 0.216 5.49 0.201 5.11 2.08 1340 7.58 11.3
HSS 3.500×0.203 HSS 88.9×5.2 3.5 88.9 0.203 5.16 0.189 4.8 1.97 1270 7.15 10.6
HSS 3.500×0.188 HSS 88.9×4.8 3.5 88.9 0.188 4.78 0.174 4.42 1.82 1170 6.66 9.9
HSS 3.500×0.125 HSS 88.9×3.2 3.5 88.9 0.125 3.18 0.116 2.95 1.23 794 4.51 6.71
HSS 3.000×0.250 HSS 76.2×6.4 3 76.2 0.25 6.35 0.233 5.92 2.03 1310 7.35 10.9
HSS 3.000×0.216 HSS 76.2×5.5 3 76.2 0.216 5.49 0.201 5.11 1.77 1140 6.43 9.57
HSS 3.000×0.203 HSS 76.2×5.2 3 76.2 0.203 5.16 0.189 4.8 1.67 1080 6.07 9.03
HSS 3.000×0.188 HSS 76.2×4.8 3 76.2 0.188 4.78 0.174 4.42 1.54 994 5.65 8.41
HSS 3.000×0.152 HSS 76.2×3.9 3 76.2 0.152 3.86 0.141 3.58 1.27 819 4.63 6.89
HSS 3.000×0.134 HSS 76.2×3.4 3 76.2 0.134 3.4 0.124 3.15 1.12 723 4.11 6.11
HSS 3.000×0.125 HSS 76.2×3.2 3 76.2 0.125 3.18 0.116 2.95 1.05 677 3.84 5.72
HSS 2.875×0.250 HSS 73×6.4 2.88 73 0.25 6.35 0.233 5.92 1.93 1250 7.02 10.4
HSS 2.875×0.203 HSS 73×5.2 2.88 73 0.203 5.16 0.189 4.8 1.59 1030 5.8 8.63
HSS 2.875×0.188 HSS 73×4.8 2.88 73 0.188 4.78 0.174 4.42 1.48 955 5.4 8.04
HSS 2.875×0.125 HSS 73×3.2 2.88 73 0.125 3.18 0.116 2.95 1.01 652 3.67 5.47
HSS 2.500×0.250 HSS 63.5×6.4 2.5 63.5 0.25 6.35 0.233 5.92 1.66 1070 6.01 8.95
HSS 2.500×0.188 HSS 63.5×4.8 2.5 63.5 0.188 4.78 0.174 4.42 1.27 819 4.65 6.91
HSS 2.500×0.125 HSS 63.5×3.2 2.5 63.5 0.125 3.18 0.116 2.95 0.869 561 3.17 4.72
HSS 2.375×0.250 HSS 60.3×6.4 2.38 60.3 0.25 6.35 0.233 5.92 1.57 1010 5.68 8.45
HSS 2.375×0.218 HSS 60.3×5.5 2.38 60.3 0.218 5.54 0.203 5.16 1.39 897 5.03 7.48
HSS 2.375×0.188 HSS 60.3×4.8 2.38 60.3 0.188 4.78 0.174 4.42 1.2 774 4.4 6.54
HSS 2.375×0.154 HSS 60.3×3.9 2.38 60.3 0.154 3.91 0.143 3.63 1 645 3.66 5.44
HSS 2.375×0.125 HSS 60.3×3.2 2.38 60.3 0.125 3.18 0.116 2.95 0.823 531 3.01 4.47
HSS 1.900×0.188 HSS 48.3×4.8 1.9 48.3 0.188 4.78 0.174 4.42 0.943 608 3.44 5.12
HSS 1.900×0.145 HSS 48.3×3.7 1.9 48.3 0.145 3.68 0.135 3.43 0.749 483 2.72 4.05
HSS 1.900×0.120 HSS 48.3×3.0 1.9 48.3 0.12 3.05 0.111 2.82 0.624 403 2.28 3.4
HSS 1.660×0.140 HSS 42.2×3.6 1.66 42.2 0.14 3.56 0.13 3.3 0.625 403 2.27 3.38

ASTM A500 Grade C Chemical Composition (Heat and Product Analysis)

Heat and product analysis limits below are the Grade C columns of ASTM A500/A500M-23 Table 1. Grade C allows slightly less carbon than Grade B (0.23 % versus 0.26 % on heat analysis). A dual Grade B and Grade C certificate has to satisfy the more restrictive of the two chemistries where they differ. Values are mass percent.

ASTM A500/A500M-23 chemical requirements for Grade C.

Swipe horizontally to view all dimensions.

Element Heat analysis Product analysis
Carbon, maxA 0.23 0.27
Manganese, maxA 1.35 1.40
Phosphorus, max 0.035 0.045
Sulfur, max 0.035 0.045
Copper, minB 0.20 0.18

A For each reduction of 0.01 percentage point below the specified carbon maximum, an increase of 0.06 percentage point above the specified manganese maximum is permitted, up to 1.50 % by heat analysis and 1.60 % by product analysis.

B Copper minimum applies only if copper-containing steel is specified in the purchase order.

ASTM A500 Grade C Mechanical Properties: Yield, Tensile and Elongation

From ASTM A500/A500M-23 Table 2, Grade C uses one set of tensile requirements for round, square, rectangular and special tubular shapes: 50 ksi [345 MPa] minimum yield and 62 ksi [425 MPa] minimum tensile strength. Earlier editions set round Grade C at 46 ksi; that split was removed in the 2021 revision. Do not take 46 ksi as the Grade C round yield when the order is A500/A500M-21, 21a or 23.

Swipe horizontally to view all dimensions.

Property Grade C (all shapes)
Tensile strength, min, psi [MPa] 62 000 [425]
Yield strength, min, psi [MPa] 50 000 [345]
Elongation in 2 in [50 mm], min, % 21

The 21 % elongation in 2 in [50 mm] applies to specified wall thicknesses of 0.120 in [3.05 mm] and greater. For lighter specified walls the elongation is by agreement with the manufacturer. Specified elongation applies to tests performed before shipment.

Delivery, Inspection and Identification of ASTM A500 Grade C HSS

Grade C is delivered as cold-formed welded or seamless tubing unless a further treatment is ordered. Grade D’s mandatory heat treatment is not a Grade C requirement. The mill certificate should name ASTM A500/A500M, the edition, Grade C, the size and specified wall, and welded or seamless manufacture. A dual Grade B and Grade C certificate is a Grade C document only when Grade C is named and the reported tests meet the Grade C tensile and chemistry limits.

Do not rely on a default Charpy test; A500 does not impose one. If toughness has to be demonstrated, write the test, the temperature and the absorbed-energy requirement on the order.

Weldability and Surface Condition of ASTM A500 Grade C HSS

Grade C remains a weldable carbon steel, with a slightly lower carbon maximum than Grade B, which is a help rather than a hindrance for welding procedures. Procedures still have to match thickness, weld-seam condition and any coating. An as-formed ERW seam is acceptable under A500 unless the order requires a finished or ground seam. Higher specified strength is not a substitute for a notch-toughness test on a dynamically loaded, welded member.

Dimensional Tolerances and Theoretical Mass for ASTM A500 Grade C HSS

Grade C uses the same A500/A500M dimensional tolerances as Grade B. Switching the grade letter does not tighten the wall, the mass or the straightness. If the design needs the tighter package associated with ASTM A1085, that specification has to be named; it is not implied by Grade C.

The tabulated tdes values are the AISC design-wall figures (about 0.93 of tnom on these rows). Order the specified wall, not the design wall, unless the purchase documents explicitly say otherwise. Masses are theoretical reference values from the AISC file.

Applications and Service Limits for ASTM A500 Grade C Steel Hollow Sections

Grade C is the usual choice when the structural notes already assume a 50 ksi HSS yield: columns, trusses, moment frames, bracing and fabricated assemblies in buildings and similar work. It does not become a toughness grade, a weathering grade, or a hot-finished section by virtue of the higher yield. EN 10210 and ASTM A501 remain different products. Round Grade C HSS is still not ASTM A53 pipe.

Where a project mixed older 46 ksi round Grade C tables with new 50 ksi shaped tables, the whole enquiry should be brought onto one edition — preferably the edition that will appear on the certificate — before members are sized.

ASTM A500 Grade C Compared with Grade B, A1085, A501 and EN 10219

Grade B is 46 ksi [315 MPa] / 58 ksi [400 MPa] on the same shape family under A500/A500M-23. It is a lower specified grade, not a lesser size table. A dual-grade certificate that meets Grade C will usually meet Grade B tensile minima as well, but chemistry and naming still have to be checked; do not assume the reverse, that Grade B always meets Grade C.

ASTM A1085 should be compared on tolerances, yield range and testing, not treated as “Grade C with another name”. ASTM A501 is hot-formed. EN 10219-1 S355 families and GB/T 6728 Q355B are sometimes placed next to Grade C in a substitution study because the 345–355 MPa yield band looks familiar; they remain different standards, with different geometry series and different weld and toughness options. ASME SA-500 is a Code-mark question and is not opened on this page.

Near-Equivalents for ASTM A500 Grade C HSS: Not Automatic Substitutes

Near-equivalent talk around Grade C usually points at EN 10219-1 S355JRH or S355J2H, or at GB/T 6728 Q355B. Those grades can look close on a one-line yield comparison and still fail a project review on impact testing, elongation rules, corner radius, wall tolerance or design-wall convention. They are listed as a starting point only. Grade B, A1085, A501 and SA-500 are neighbouring products, not substitutes.

Sourcing ASTM A500 Grade C Steel Hollow Sections from SHH STEEL

SHH STEEL reviews enquiries for ASTM A500 Grade C HSS against the grade letter, the A500/A500M edition, the outside size and specified wall, and the certificate — including whether a dual Grade B and Grade C document actually reports Grade C chemistry and tensile results. The 516-row table is a shared AISC reference, not a Grade C stock list. Additional tests, lengths and surface condition should be stated on the enquiry and checked before quotation.

ASTM A500 Grade C HSS FAQs

Is round ASTM A500 Grade C still 46 ksi?
Not under A500/A500M-21, 21a or 23. Those editions set 50 ksi [345 MPa] minimum yield for rounds as well as for squares and rectangles. Use 46 ksi for round Grade C only when the certificate names an earlier edition that still had that split.
Can a Grade B certificate be used where Grade C is specified?
No. Grade B is a lower specified yield and tensile grade. A dual Grade B and Grade C certificate is acceptable for a Grade C order only when Grade C is named and the reported properties meet Grade C.
Is ASTM A1085 the same as A500 Grade C?
No. A1085 is a separate HSS specification with a different tolerance and property package. Naming Grade C does not silently invoke A1085, and naming A1085 does not silently invoke Grade C.
Why do the Grade C size tables match the Grade B tables?
Because both grades use the same AISC Manual, 15th Edition, HSS geometry file. The tables are a shared dimensional reference. They are not evidence that the two grades are the same product, and they are not a stock list for either grade.
Does Grade C include a Charpy test?
Not by default. If low-temperature notch toughness has to be demonstrated, the CVN test, temperature and energy requirement must be written on the order.

Conclusion

ASTM A500 Grade C HSS is the 50 ksi [345 MPa] / 62 ksi [425 MPa] cold-formed carbon steel hollow section of A500/A500M-23, for square, rectangular and round tubing inside the 88 in periphery and 1.000 in wall envelope. The size tables are the 516 AISC Manual, 15th Edition, HSS designations, shared as a reference with the Grade B page and not offered as a stock list. Confirm the edition, the grade letter and the certificate — especially on dual-grade paper — before the tubes are released to the job.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X